Abstract To solve the problem of insufficient interface bond strength of concrete-filled square steel tubes (CFSSTs), 16 large CFSST specimens with eight different types of connectors (no additional connectors, built-in studs, built-in circular ribs, built-in vertical ribs, built-in reinforcement cage, and various combinations of the above) were designed for push-out testing. Specimens were constructed using high-strength concrete or high-strength recycled aggregate concrete (RAC). The bond behavior and slip failure mechanism were analyzed by comparing the force-slip curves, slip displacements, and steel tube strains. The bond strength calculation method and bond-slip constitutive relationship of the interface under multiple parameters were obtained. Experiments revealed the following: bond-slip curves for CFSST without additional connectors were composed of an ascending section and a residual section; for tubes with different connectors, the peak values of the curves were higher; the performance-price ratio of studs and circular ribs for improving bond strength was high, and the combined use of studs and circular ribs can work well; the combination of circular ribs and vertical ribs can significantly improve bond strength and energy dissipation capacity; RAC had better bond behavior than normal concrete in HSCFSST without additional connectors or built-in vertical ribs. The predicted force-slip curves agreed well with the test curves, providing a theoretical basis for CFSST applications.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Axial performance of short concrete filled steel tubes with high- and ultra-high-strength materials
Xiong, M.-X., Xiong, D.-X., & Liew, J. Y. R. (2017) · Engineering Structures · doi:10.1016/j.engstruct.2017.01.037 · Cited by 438
Bond behavior in concrete-filled steel tubes
Tao, Z., Song, T.-Y., Uy, B., & Han, L.-H. (2016) · Journal of Constructional Steel Research · doi:10.1016/j.jcsr.2015.12.030 · Cited by 296
Lyu, W.-Q., & Han, L.-H. (2019) · Journal of Constructional Steel Research · doi:10.1016/j.jcsr.2018.12.028 · Cited by 168
Xu, C., Chengkui, H., Decheng, J., & Yuancheng, S. (2009) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2007.10.021 · Cited by 130
Bond-slip behaviour of concrete-filled stainless steel circular hollow section tubes
Chen, Y., Feng, R., Shao, Y., & Zhang, X. (2017) · Journal of Constructional Steel Research · doi:10.1016/j.jcsr.2016.12.012 · Cited by 111
Bond behaviour of concrete-filled steel tubes at the Arctic low temperatures
Yan, J.-B., Xie, W., Zhang, L., & Lin, X.-C. (2019) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2019.03.168 · Cited by 90
Aly, T., Elchalakani, M., Thayalan, P., & Patnaikuni, I. (2010) · Journal of Constructional Steel Research · doi:10.1016/j.jcsr.2009.08.002 · Cited by 89
Bond strength in concrete filled steel tubes
Virdi, K. S., & Dowling, P. J. (1980) · IABSE · doi:10.5169/seals-34958 · Cited by 81
Research works printed but not linked: 26
- Ibañez, 2018, Shape effect on axially loaded high strength CFST stub columns, J Constr Steel Res, 147, 247, 10.1016/j.jcsr.2018.04.005 · doi:10.1016/j.jcsr.2018.04.005
- Wang, 2019, Experimental study on seismic behavior of high-strength circular concretefilled thin-walled steel tubular columns, Eng Struct, 182, 403, 10.1016/j.engstruct.2018.12.098 · doi:10.1016/j.engstruct.2018.12.098
- Zhou, 2018, Cyclic testing of square tubed-reinforced-concrete column to RC beam joints, Eng Struct, 176, 439, 10.1016/j.engstruct.2018.09.053 · doi:10.1016/j.engstruct.2018.09.053
- Qiao, 2019, Seismic behavior of exposed concrete filled steel tube column bases with embedded reinforcing bars: experimental investigation, Thin-Walled Struct, 136, 367, 10.1016/j.tws.2018.12.039 · DOI
- Zhang, 2019, The hysteretic behavior of recycled aggregate concrete-filled square steel tube columns, Eng Struct, 198, 10.1016/j.engstruct.2019.109523 · DOI
- Liu, 2005, Experimental research on the bond behaviours of concrete-filled rectangular tube, Archit Technol, 02, 97
- Li, 2012, Experimental research on the bond-slip behaviour of recycled aggregate concrete-filled square steel tubes, J Guangxi Univ, 37, 68
- Tomii, 1980, A method of improving bond strength in between steel tube and concrete core cast in square and octagonal steel tubular columns, Trans Jpn Concr Inst, 2, 327
- Shakir, 1993, Pushout strength of concrete-filled steel hollow sections, Struct Eng, 71, 230
- Xue, 1998, Experimental study on shear connectors of concrete-filled steel tube, Build Sci, 14, 13
- Xu, 2013, Research on impact of steel tube inner surface roughness on interfacial bonding behavior of CFST, J Build Struct, 34, 420
- Chen, 2016, Experimental studies on shear-bearing capacity of headed stud in concrete-filled steel tube, Eng Mechanics, 33, 66
- Dong, 2019, Flexural bond behavior of reinforced recycled aggregate concrete, Constr Build Mater, 213, 514, 10.1016/j.conbuildmat.2019.03.238 · DOI
- Kilpatrick, 1999, Influence of interfacial shear transfer on behaviour of concrete-filled steel tubular columns, ACI Struct J, 6, 642
- Roeder, 1999, Composite action in concrete filled tubes, J Struct Eng ASCE, 125, 477, 10.1061/(ASCE)0733-9445(1999)125:5(477) · doi:10.1061/(asce)0733-9445(1999)125:5(477 · Paper page
- Industry Standard of the People’s Republic of China, GB/T 14684-2011. Specification of Sand for Building. Beijing: China Standards Press; 2011 [in Chinese].
- Industry Standard of the People’s Republic of China, GB/T 50152-2012. Standard for test method of concrete structures. Beijing: China Architecture & Building Press; 2012 [in Chinese].
- Industry Standard of the People’s Republic of China, GB/T 228.1-2010. Metallic Materials-Tensile Testing-Part 1: Method of Test at Room Temperature. Beijing: China Planning Press; 2010 [in Chinese].
- Dong, 2018, Uniaxial compression performance of rectangular CFST columns with different internal construction characteristics, Eng Struct, 176, 763, 10.1016/j.engstruct.2018.09.051 · DOI
- Nguyen, 2018, Finite element model for the interface between steel and concrete of CFST (concrete-filled steel tube), Eng Struct, 185, 141, 10.1016/j.engstruct.2019.01.068 · doi:10.1016/j.engstruct.2019.01.068
- Liu, 2010, Shear bond behaviors at interface of concrete-filled steel tube, J Guangxi Univ: Nat Sci Ed., 35
- Kang, 2006, Summarized review of the bond-slip problems of concrete filled steel tubes (CFST), J Xi’an Univ Architec Technol (Nat Sci Ed), 38, 321
- Chen, 2016, Review analysis on study of bond behavior of concrete-filled steel tube, Build Struct, 46, 78
- Cosenza, 1997, Behavior and modeling of bond of FRP rebars to concrete, J Compos Constr, 1, 40, 10.1061/(ASCE)1090-0268(1997)1:2(40) · doi:10.1061/(asce)1090-0268(1997)1:2(40 · Paper page
- Xue, 2008, Static behavior and theoretical model of stud shear connectors, J Bridge Eng ASCE, 13, 623, 10.1061/(ASCE)1084-0702(2008)13:6(623) · doi:10.1061/(asce)1084-0702(2008)13:6(623 · Paper page
- Akihiko, 2005, A quantitative evaluation of the stress transfer effect between steel tube and infill concrete by horizontal diaphragms in a CFT column, Architec Inst Jpn, 598, 163
Cited by
Zhao, H., Li, J., Wang, R., Lam, D., & Zhang, Y. (2021) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2021.125532 · Cited by 50
Bond stress-slip relationship in concrete-filled square stainless steel tubes
Dai, P., Yang, L., Wang, J., Lin, M., & Fan, J. (2022) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2022.127001 · Cited by 45
Dai, P., Yang, L., Wang, J., Fan, J., & Lin, M. (2021) · Thin-Walled Structures · doi:10.1016/j.tws.2021.108506 · Cited by 42
Li, H., Liu, Y., & Zhang, N. (2020) · Structures · doi:10.1016/j.istruc.2020.10.062 · Cited by 31
Investigation on the bond-slip behavior of recycled aggregate concrete-filled steel tube with studs
Cai, G., Sun, B., Zeng, S., Yang, P., & Zhang, J. (2025) · PLoS ONE · doi:10.1371/journal.pone.0325279 · Cited by 1
Metadata
- Authors
- Dong, H., Chen, X., Cao, W., & Zhao, Y.
- Venue
- Engineering Structures
- Publisher
- Elsevier BV
- Published
- 2020-05
- Volume
- 211
- Pages
- 110392
- ISSN
- 0141-0296 (ISSN-L)
- OpenAlex
- W3007244272
- Cited by
- 40
- References
- 8
- FWCI
- 2.04
- Type
- journal article
- Language
- en
- Open access
- closed
- Licence
- www.elsevier.com/tdm/userlicense/1.0/ (tdm)
- www.elsevier.com/legal/tdmrep-license (tdm)
- Funders
- National Natural Science Foundation of China (51878015)
- Beijing Natural Science Foundation of China (8182005)
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
How to cite
Cite CoChat for the checks on this page, and the paper for its own findings.
- This page
- CoChat. (2026). Citation check: Bond behavior of high-strength recycled aggregate concrete-filled large square steel tubes with different connectors. https://app.cochat.ai/papers/10.1016/j.engstruct.2020.110392
- The paper
- Dong, H., Chen, X., Cao, W., & Zhao, Y. (2020). Bond behavior of high-strength recycled aggregate concrete-filled large square steel tubes with different connectors. Engineering Structures. https://doi.org/10.1016/j.engstruct.2020.110392
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.