The DOI matches its Crossref record; 59 of the 59 references it cites were found in a registry or an index.
Sulfide solid electrolytes for all-solid-state lithium batteries: Structure, conductivity, stability and application
Abstract
This review focuses on the research progress of sulfide solid electrolytes. Two systems of (100-x)Li2S-xP2S5 and Li2S-MxSy-P2S5 are systematically reviewed from four aspects, the crystal structure, conductivity, stability and application. The methods for preparing sulfide solid electrolytes are summarized, and, their advantages and disadvantages are compared and analysed. Sulfide solid electrolytes with high conductivities are closely related to their crystal structures, and they can be improved via doping, such as substitution doping, interstitial doping, dual-doping, etc. The conductivities are introduced and summarized according to their classifications. Experimental studies and theoretical results are discussed in parallel to illustrate the relationship between the conductivity and crystal structure. Furthermore, the stabilities of sulfide electrolytes with lithium metal, active materials, organic solvents and humid air are reviewed separately, and corresponding methods for improvement are proposed. Finally, according to the different functions of sulfide electrolytes in all-solid-state lithium batteries (ASSLBs), they are categorized and generalized scientifically in terms of composite electrolyte, buffer material and electrolyte. Additionally, the techniques proposed in the recent works to achieve sufficient contact between the sulfide solid electrolyte and the electrode in the ASSLBs are summarized. The present review aims to provide a thorough understanding of the properties of sulfide solid electrolytes, including conductivity, structure, and stability, to allow for more efficient and target-oriented research to improve the performance of sulfides-based ASSLBs.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
A lithium superionic conductor
Kamaya, N., Homma, K., Yamakawa, Y., Hirayama, M., Kanno, R., Yonemura, M., Kamiyama, T., Kato, Y., Hama, S., Kawamoto, K., et al. (2011) · Nature Materials · doi:10.1038/nmat3066 · Cited by 4,978
High-power all-solid-state batteries using sulfide superionic conductors
Kato, Y., Hori, S., Saito, T., Suzuki, K., Hirayama, M., Mitsui, A., Yonemura, M., Iba, H., & Kanno, R. (2016) · Nature Energy · doi:10.1038/nenergy.2016.30 · Cited by 3,517
Interface Stability in Solid-State Batteries
Richards, W. D., Miara, L. J., Wang, Y., Kim, J. C., & Ceder, G. (2016) · Chemistry of Materials · doi:10.1021/acs.chemmater.5b04082 · Cited by 1,652
Design principles for solid-state lithium superionic conductors
Wang, Y., Richards, W. D., Ong, S. P., Miara, L. J., Kim, J. C., Mo, Y., & Ceder, G. (2015) · Nature Materials · doi:10.1038/nmat4369 · Cited by 1,485
Seino, Y., Ota, T., Takada, K., Hayashi, A., & Tatsumisago, M. (2014) · Energy Environ. Sci. · doi:10.1039/c3ee41655k · Cited by 1,302
Electrochemical Stability of Li10GeP2S12 and Li7La3Zr2O12 Solid Electrolytes
Han, F., Zhu, Y., He, X., Mo, Y., & Wang, C. (2016) · Advanced Energy Materials · doi:10.1002/aenm.201501590 · Cited by 1,095
Lithium Ionic Conductor Thio-LISICON: The Li[sub 2]S-GeS[sub 2]-P[sub 2]S[sub 5] System
Kanno, R., & Murayama, M. (2001) · Journal of The Electrochemical Society · doi:10.1149/1.1379028 · Cited by 1,066
Progress and prospective of solid-state lithium batteries
Takada, K. (2013) · Acta Materialia · doi:10.1016/j.actamat.2012.10.034 · Cited by 1,056
Koerver, R., Aygün, I., Leichtweiß, T., Dietrich, C., Zhang, W., Binder, J. O., Hartmann, P., Zeier, W. G., & Janek, J. (2017) · Chemistry of Materials · doi:10.1021/acs.chemmater.7b00931 · Cited by 1,020
Anomalous High Ionic Conductivity of Nanoporous β-Li3PS4
Liu, Z., Fu, W., Payzant, E. A., Yu, X., Wu, Z., Dudney, N. J., Kiggans, J., Hong, K., Rondinone, A. J., & Liang, C. (2013) · Journal of the American Chemical Society · doi:10.1021/ja3110895 · Cited by 879
History, Evolution, and Future Status of Energy Storage
Whittingham, M. S. (2012) · Proceedings of the IEEE · doi:10.1109/jproc.2012.2190170 · Cited by 873
Wenzel, S., Randau, S., Leichtweiß, T., Weber, D. A., Sann, J., Zeier, W. G., & Janek, J. (2016) · Chemistry of Materials · doi:10.1021/acs.chemmater.6b00610 · Cited by 854
Review—Practical Challenges Hindering the Development of Solid State Li Ion Batteries
Kerman, K., Luntz, A., Viswanathan, V., Chiang, Y.-M., & Chen, Z. (2017) · Journal of The Electrochemical Society · doi:10.1149/2.1571707jes · Cited by 712
Ong, S. P., Mo, Y., Richards, W. D., Miara, L., Lee, H. S., & Ceder, G. (2013) · Energy Environ. Sci. · doi:10.1039/c2ee23355j · Cited by 710
Li10SnP2S12: An Affordable Lithium Superionic Conductor
Bron, P., Johansson, S., Zick, K., Schmedt auf der Günne, J., Dehnen, S., & Roling, B. (2013) · Journal of the American Chemical Society · doi:10.1021/ja407393y · Cited by 655
Sakuda, A., Hayashi, A., & Tatsumisago, M. (2010) · Chemistry of Materials · doi:10.1021/cm901819c · Cited by 651
Wenzel, S., Sedlmaier, S. J., Dietrich, C., Zeier, W. G., & Janek, J. (2018) · Solid State Ionics · doi:10.1016/j.ssi.2017.07.005 · Cited by 609
Haruyama, J., Sodeyama, K., Han, L., Takada, K., & Tateyama, Y. (2014) · Chemistry of Materials · doi:10.1021/cm5016959 · Cited by 605
Structural change of Li2S–P2S5 sulfide solid electrolytes in the atmosphere
Muramatsu, H., Hayashi, A., Ohtomo, T., Hama, S., & Tatsumisago, M. (2010) · Solid State Ionics · doi:10.1016/j.ssi.2010.10.013 · Cited by 568
Zhang, W., Weber, D. A., Weigand, H., Arlt, T., Manke, I., Schröder, D., Koerver, R., Leichtweiss, T., Hartmann, P., Zeier, W. G., et al. (2017) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.7b01137 · Cited by 538
Wenzel, S., Weber, D. A., Leichtweiß, T., Busche, M. R., Sann, J., & Janek, J. (2015) · Solid State Ionics · doi:10.1016/j.ssi.2015.11.034 · Cited by 505
Tatsumisago, M., Nagao, M., & Hayashi, A. (2013) · Journal of Asian Ceramic Societies · doi:10.1016/j.jascer.2013.03.005 · Cited by 471
Zhao, Y., Wu, C., Peng, G., Chen, X., Yao, X., Bai, Y., Wu, F., Chen, S., & Xu, X. (2016) · Journal of Power Sources · doi:10.1016/j.jpowsour.2015.09.111 · Cited by 454
Self-citationCrystal structure and phase transitions of the lithium ionic conductor Li3PS4
Homma, K., Yonemura, M., Kobayashi, T., Nagao, M., Hirayama, M., & Kanno, R. (2011) · Solid State Ionics · doi:10.1016/j.ssi.2010.10.001 · Cited by 413
The Detrimental Effects of Carbon Additives in Li10GeP2S12-Based Solid-State Batteries
Zhang, W., Leichtweiß, T., Culver, S. P., Koerver, R., Das, D., Weber, D. A., Zeier, W. G., & Janek, J. (2017) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.7b11530 · Cited by 392
A Battery Made from a Single Material
Han, F., Gao, T., Zhu, Y., Gaskell, K. J., & Wang, C. (2015) · Advanced Materials · doi:10.1002/adma.201500180 · Cited by 367
High-Energy All-Solid-State Lithium Batteries with Ultralong Cycle Life
Yao, X., Liu, D., Wang, C., Long, P., Peng, G., Hu, Y.-S., Li, H., Chen, L., & Xu, X. (2016) · Nano Letters · doi:10.1021/acs.nanolett.6b03448 · Cited by 360
Self-citationKim, D. H., Oh, D. Y., Park, K. H., Choi, Y. E., Nam, Y. J., Lee, H. A., Lee, S.-M., & Jung, Y. S. (2017) · Nano Letters · doi:10.1021/acs.nanolett.7b00330 · Cited by 359
Ionic conductivity of and phase transition in lithium thiophosphate Li3PS4
TACHEZ, M., MALUGANI, J., MERCIER, R., & ROBERT, G. (1984) · Solid State Ionics · doi:10.1016/0167-2738(84)90097-3 · Cited by 356
Solution‐Processable Glass LiI‐Li4SnS4 Superionic Conductors for All‐Solid‐State Li‐Ion Batteries
Park, K. H., Oh, D. Y., Choi, Y. E., Nam, Y. J., Han, L., Kim, J., Xin, H. L., Lin, F., Oh, S. M., & Jung, Y. S. (2015) · Advanced Materials · doi:10.1002/adma.201505008 · Cited by 321
Kuhn, A., Gerbig, O., Zhu, C., Falkenberg, F., Maier, J., & Lotsch, B. V. (2014) · Phys. Chem. Chem. Phys. · doi:10.1039/c4cp02046d · Cited by 316
Oh, G., Hirayama, M., Kwon, O., Suzuki, K., & Kanno, R. (2016) · Chemistry of Materials · doi:10.1021/acs.chemmater.5b04940 · Cited by 278
Ultra‐thin Solid‐State Li‐Ion Electrolyte Membrane Facilitated by a Self‐Healing Polymer Matrix
Whiteley, J. M., Taynton, P., Zhang, W., & Lee, S. (2015) · Advanced Materials · doi:10.1002/adma.201502636 · Cited by 245
Shin, B. R., Nam, Y. J., Oh, D. Y., Kim, D. H., Kim, J. W., & Jung, Y. S. (2014) · Electrochimica Acta · doi:10.1016/j.electacta.2014.08.139 · Cited by 214
Xu, R.-C., Xia, X.-H., Wang, X.-L., Xia, Y., & Tu, J.-P. (2017) · Journal of Materials Chemistry A · doi:10.1039/c6ta10142a · Cited by 207
Preparation and ionic conductivity of new B2S3-Li2S-LiI glasses
Wada, H., Menetrier, M., Levasseur, A., & Hagenmuller, P. (1983) · Materials Research Bulletin · doi:10.1016/0025-5408(83)90080-6 · Cited by 205
Zhang, Z., Zhao, Y., Chen, S., Xie, D., Yao, X., Cui, P., & Xu, X. (2017) · Journal of Materials Chemistry A · doi:10.1039/c7ta04320a · Cited by 194
Self-citationThe Application of Atomic Force Microscopy for the Study of Li Deposition Processes
Aurbach, D., & Cohen, Y. (1996) · Journal of The Electrochemical Society · doi:10.1149/1.1837248 · Cited by 192
Empowering the Lithium Metal Battery through a Silicon-Based Superionic Conductor
Whiteley, J. M., Woo, J. H., Hu, E., Nam, K.-W., & Lee, S.-H. (2014) · Journal of The Electrochemical Society · doi:10.1149/2.0501412jes · Cited by 191
Kaib, T., Haddadpour, S., Kapitein, M., Bron, P., Schröder, C., Eckert, H., Roling, B., & Dehnen, S. (2012) · Chemistry of Materials · doi:10.1021/cm3011315 · Cited by 169
Xu, R.-C., Xia, X.-H., Li, S.-H., Zhang, S.-Z., Wang, X.-L., & Tu, J.-P. (2017) · Journal of Materials Chemistry A · doi:10.1039/c7ta01147d · Cited by 167
Evolution at the Solid Electrolyte/Gold Electrode Interface during Lithium Deposition and Stripping
Sang, L., Haasch, R. T., Gewirth, A. A., & Nuzzo, R. G. (2017) · Chemistry of Materials · doi:10.1021/acs.chemmater.7b00034 · Cited by 163
Oh, D. Y., Kim, D. H., Jung, S. H., Han, J., Choi, N., & Jung, Y. S. (2017) · Journal of Materials Chemistry A · doi:10.1039/c7ta06873e · Cited by 154
Li10Si0.3Sn0.7P2S12 – A low-cost and low-grain-boundary-resistance lithium superionic conductor
Bron, P., Dehnen, S., & Roling, B. (2016) · Journal of Power Sources · doi:10.1016/j.jpowsour.2016.08.115 · Cited by 153
Haruyama, J., Sodeyama, K., & Tateyama, Y. (2016) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.6b08435 · Cited by 153
Preparation and ionic conductivities of (100 − x)(0.75Li2S·0.25P2S5)·xLiBH4 glass electrolytes
Yamauchi, A., Sakuda, A., Hayashi, A., & Tatsumisago, M. (2012) · Journal of Power Sources · doi:10.1016/j.jpowsour.2012.12.001 · Cited by 117
Peng, G., Yao, X., Wan, H., Huang, B., Yin, J., Ding, F., & Xu, X. (2016) · Journal of Power Sources · doi:10.1016/j.jpowsour.2016.01.039 · Cited by 79
Self-citationHayashi, A., Nishio, Y., Kitaura, H., & Tatsumisago, M. (2008) · Electrochemistry Communications · doi:10.1016/j.elecom.2008.09.026 · Cited by 73
Nishio, Y., Kitaura, H., Hayashi, A., & Tatsumisago, M. (2008) · Journal of Power Sources · doi:10.1016/j.jpowsour.2008.09.064 · Cited by 71
Aso, K., Sakuda, A., Hayashi, A., & Tatsumisago, M. (2013) · ACS Applied Materials & Interfaces · doi:10.1021/am302164e · Cited by 70
Hori, S., Suzuki, K., Hirayama, M., Kato, Y., & Kanno, R. (2016) · Frontiers in Energy Research · doi:10.3389/fenrg.2016.00038 · Cited by 69
Preparation and ionic conductivity of (100−x)(0.8Li2S·0.2P2S5)·xLiI glass–ceramic electrolytes
Ujiie, S., Hayashi, A., & Tatsumisago, M. (2012) · Journal of Solid State Electrochemistry · doi:10.1007/s10008-012-1900-7 · Cited by 65
Ulissi, U., Agostini, M., Ito, S., Aihara, Y., & Hassoun, J. (2016) · Solid State Ionics · doi:10.1016/j.ssi.2016.08.014 · Cited by 54
Nickel sulfides as a cathode for all-solid-state ceramic lithium batteries
Matsumura, T., Nakano, K., Kanno, R., Hirano, A., Imanishi, N., & Takeda, Y. (2007) · Journal of Power Sources · doi:10.1016/j.jpowsour.2007.06.168 · Cited by 51
Sun, Y. J., Yan, W., Li, A., et al. (2017) · Solid State Ionics · doi:10.1016/j.ssi.2017.01.014 · Cited by 51
Preparation and characterization of lithium ion conducting Li2S–P2S5–GeS2 glasses and glass-ceramics
Minami, K., Hayashi, A., & Tatsumisago, M. (2010) · Journal of Non-Crystalline Solids · doi:10.1016/j.jnoncrysol.2010.05.016 · Cited by 42
Structural Evidence for High Ionic Conductivity of Li7P3S11 Metastable Crystal
Onodera, Y., Mori, K. J., Otomo, T., Sugiyama, M., & Fukunaga, T. (2012) · Journal of the Physical Society of Japan · doi:10.1143/jpsj.81.044802 · Cited by 30
Aluminum based sulfide solid lithium ionic conductors for all solid state batteries
Amaresh, S., Karthikeyan, K., Kim, K. J., Lee, Y. G., & Lee, Y. S. (2014) · Nanoscale · doi:10.1039/c4nr00804a · Cited by 26
Ujiie, S., Hayashi, A., & Tatsumisago, M. (2013) · Materials for Renewable and Sustainable Energy · doi:10.1007/s40243-013-0018-x · Cited by 25
Cited by
Chen, R., Li, Q., Yu, X., Chen, L., & Li, H. (2020) · Chemical Reviews · doi:10.1021/acs.chemrev.9b00268 · Cited by 1,678
Physicochemical Concepts of the Lithium Metal Anode in Solid-State Batteries
Krauskopf, T., Richter, F. H., Zeier, W. G., & Janek, J. (2020) · Chemical Reviews · doi:10.1021/acs.chemrev.0c00431 · Cited by 892
Recent Advances in Energy Chemistry between Solid-State Electrolyte and Safe Lithium-Metal Anodes
Cheng, X.-B., Zhao, C.-Z., Yao, Y.-X., Liu, H., & Zhang, Q. (2019) · Chem · doi:10.1016/j.chempr.2018.12.002 · Cited by 874
Self-citationLithium/Sulfide All‐Solid‐State Batteries using Sulfide Electrolytes
Wu, J., Liu, S., Han, F., Yao, X., & Wang, C. (2021) · Advanced Materials · doi:10.1002/adma.202000751 · Cited by 809
Self-citationArtificial Interphases for Highly Stable Lithium Metal Anode
Xu, R., Cheng, X.-B., Yan, C., Zhang, X.-Q., Xiao, Y., Zhao, C.-Z., Huang, J.-Q., & Zhang, Q. (2019) · Matter · doi:10.1016/j.matt.2019.05.016 · Cited by 721
Self-citation
Metadata
- Authors
- Chen, S., Xie, D., Liu, G., Mwizerwa, J. P., Zhang, Q., Zhao, Y., Xu, X., & Yao, X.
- Venue
- Energy Storage Materials
- Publisher
- Elsevier BV
- Published
- 2018-09
- Volume
- 14
- Pages
- 58-74
- ISSN
- 2405-8289 (ISSN-L)
- 2405-8297
- OpenAlex
- W2793336898
- Cited by
- 696
- References
- 59
- FWCI
- 17.78
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.