Alkali-activated slag mortars
The DOI matches its Crossref record; 8 of the 8 references it cites were found in a registry or an index.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Addelman, S. (1979) · Technometrics · doi:10.1080/00401706.1979.10489788 · Cited by 6,750
Factors affecting the strength of alkali-activated slag
Wang, S.-D., Scrivener, K. L., & Pratt, P. L. (1994) · Cement and Concrete Research · doi:10.1016/0008-8846(94)90026-4 · Cited by 716
Alkali-activated slag cement and concrete: a review of properties and problems
Wang, S.-D., Pu, X.-C., Scrivener, K. L., & Pratt, P. L. (1995) · Advances in Cement Research · doi:10.1680/adcr.1995.7.27.93 · Cited by 474
Alkali-activated slag cements: Kinetic studies
Fernández-Jiménez, A., & Puertas, F. (1997) · Cement and Concrete Research · doi:10.1016/s0008-8846(97)00040-9 · Cited by 227
Self-citationPresent State and Future of Alkali-Activated Slag Concretes
Talling, B., & Brandštetr, J. (1989) · CANMET/ACI International Conference on Fly Ash, Silica Fume, Slag, and Natural Pozzolans in Concrete · doi:10.14359/1873 · Cited by 190
Investigation on some factors affecting the characteristics of alkali-phosphorus slag cement
Shi, C., & Yinyu, L. (1989) · Cement and Concrete Research · doi:10.1016/0008-8846(89)90004-5 · Cited by 129
Cementos de escorias activadas alcalinamente: Situación actual y perspectivas de futuro
Puertas, F. (1995) · Materiales de Construcción · doi:10.3989/mc.1995.v45.i239.553 · Cited by 98
Self-citationEffect of Curing Conditions on Alkali-Activated Slags
Talling, B. (1989) · CANMET/ACI International Conference on Fly Ash, Silica Fume, Slag, and Natural Pozzolans in Concrete · doi:10.14359/1850 · Cited by 38
Cited by
New cements for the 21st century: The pursuit of an alternative to Portland cement
Shi, C., Jiménez, A. F., & Palomo, A. (2011) · Cement and Concrete Research · doi:10.1016/j.cemconres.2011.03.016 · Cited by 1,691
Geopolymers and Related Alkali-Activated Materials
Provis, J. L., & Bernal, S. A. (2014) · Annual Review of Materials Research · doi:10.1146/annurev-matsci-070813-113515 · Cited by 1,597
Ben Haha, M., Le Saout, G., Winnefeld, F., & Lothenbach, B. (2011) · Cement and Concrete Research · doi:10.1016/j.cemconres.2010.11.016 · Cited by 1,059
NaOH-activated ground fly ash geopolymer cured at ambient temperature
Somna, K., Jaturapitakkul, C., Kajitvichyanukul, P., & Chindaprasirt, P. (2011) · Fuel · doi:10.1016/j.fuel.2011.01.018 · Cited by 995
Alkali-activated fly ash/slag cements
Puertas, F., Martı́nez-Ramı́rez, S., Alonso, S., & Vázquez, T. (2000) · Cement and Concrete Research · doi:10.1016/s0008-8846(00)00298-2 · Cited by 921
Self-citationHaha, M. B., Lothenbach, B., Le Saout, G., & Winnefeld, F. (2011) · Cement and Concrete Research · doi:10.1016/j.cemconres.2011.05.002 · Cited by 914
A model for the C-A-S-H gel formed in alkali-activated slag cements
Puertas, F., Palacios, M., Manzano, H., Dolado, J. S., Rico, A., & Rodríguez, J. (2011) · Journal of the European Ceramic Society · doi:10.1016/j.jeurceramsoc.2011.04.036 · Cited by 898
Self-citationCharacterisation of fly ashes. Potential reactivity as alkaline cements☆
Fernández-Jiménez, A., & Palomo, A. (2003) · Fuel · doi:10.1016/s0016-2361(03)00194-7 · Cited by 690
Self-citationInfluence of activator on the strength and drying shrinkage of alkali-activated slag mortar
Duran Atiş, C., Bilim, C., Çelik, Ö., & Karahan, O. (2009) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2007.10.011 · Cited by 658
Hassan, A., Arif, M., & Shariq, M. (2019) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2019.03.051 · Cited by 639
Görhan, G., & Kürklü, G. (2014) · Composites Part B: Engineering · doi:10.1016/j.compositesb.2013.10.082 · Cited by 637
Haha, M. B., Lothenbach, B., Le Saout, G., & Winnefeld, F. (2012) · Cement and Concrete Research · doi:10.1016/j.cemconres.2011.08.005 · Cited by 580
Alkali-activated binders: A review. Part 2. About materials and binders manufacture
Pacheco-Torgal, F., Castro-Gomes, J., & Jalali, S. (2008) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2007.03.019 · Cited by 519
Bernal, S. A., San Nicolas, R., Myers, R. J., Mejía de Gutiérrez, R., Puertas, F., van Deventer, J. S. J., & Provis, J. L. (2014) · Cement and Concrete Research · doi:10.1016/j.cemconres.2013.12.003 · Cited by 493
Self-citationFernández‐Jiménez, A., Puertas, F., Sobrados, I., & Sanz, J. (2003) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.2003.tb03481.x · Cited by 481
Self-citationMineralogical and microstructural characterisation of alkali-activated fly ash/slag pastes
Puertas, F., & Fernández-Jiménez, A. (2003) · Cement and Concrete Composites · doi:10.1016/s0958-9465(02)00059-8 · Cited by 452
Self-citationAbdalqader, A. F., Jin, F., & Al-Tabbaa, A. (2016) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2015.12.010 · Cited by 444
Effect of fire exposure on cracking, spalling and residual strength of fly ash geopolymer concrete
Sarker, P. K., Kelly, S., & Yao, Z. (2014) · Materials & Design · doi:10.1016/j.matdes.2014.06.059 · Cited by 438
Effect of activator type and content on properties of alkali-activated slag mortars
Aydın, S., & Baradan, B. (2014) · Composites Part B: Engineering · doi:10.1016/j.compositesb.2013.10.001 · Cited by 435
Binding mechanism and properties of alkali-activated fly ash/slag mortars
Chi, M., & Huang, R. (2013) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2012.11.003 · Cited by 428
Puertas, F., & Torres-Carrasco, M. (2014) · Cement and Concrete Research · doi:10.1016/j.cemconres.2013.12.005 · Cited by 420
Self-citationMicrostructural changes in alkali activated fly ash/slag geopolymers with sulfate exposure
Ismail, I., Bernal, S. A., Provis, J. L., Hamdan, S., & van Deventer, J. S. J. (2013) · Materials and Structures · doi:10.1617/s11527-012-9906-2 · Cited by 417
Puertas, F., Fernández-Jiménez, A., & Blanco-Varela, M. T. (2004) · Cement and Concrete Research · doi:10.1016/s0008-8846(03)00254-0 · Cited by 409
Self-citationVery early-age reaction kinetics and microstructural development in alkali-activated slag
Gebregziabiher, B. S., Thomas, R., & Peethamparan, S. (2015) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2014.09.001 · Cited by 393
“Product formation, microstructural development, and mechanical properties of all cementitious systems are governed by the hydration process [9—16, 18—20].”
BackgroundRashad, A. M. (2013) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2013.04.011 · Cited by 387
Influence of aggregate content on the behavior of fly ash based geopolymer concrete
Joseph, B., & Mathew, G. (2012) · Scientia Iranica · doi:10.1016/j.scient.2012.07.006 · Cited by 374
Palacios, M., & Puertas, F. (2005) · Cement and Concrete Research · doi:10.1016/j.cemconres.2004.10.014 · Cited by 364
Self-citationPalacios, M., & Puertas, F. (2007) · Cement and Concrete Research · doi:10.1016/j.cemconres.2006.11.021 · Cited by 362
Self-citationCarbonation process of alkali-activated slag mortars
Puertas, F., Palacios, M., & Vázquez, T. (2006) · Journal of Materials Science · doi:10.1007/s10853-005-1821-2 · Cited by 346
Self-citationHydration and properties of sodium sulfate activated slag
Rashad, A. M., Bai, Y., Basheer, P. A. M., Milestone, N. B., & Collier, N. C. (2013) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2012.12.010 · Cited by 335
Chi, M. (2012) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2012.04.005 · Cited by 335
A study on the setting characteristics of sodium silicate-activated slag pastes
Chang, J. J. (2003) · Cement and Concrete Research · doi:10.1016/s0008-8846(02)01096-7 · Cited by 330
Properties of cementless mortars activated by sodium silicate
Yang, K.-H., Song, J.-K., Ashour, A. F., & Lee, E.-T. (2008) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2007.07.003 · Cited by 319
Effect of activator mix on the hydration and strength behaviour of alkali-activated slag cements
Fernandez-Jimenez, A., & Puertas, F. (2003) · Advances in Cement Research · doi:10.1680/adcr.15.3.129.36623 · Cited by 285
Self-citationHydration Products and Reactivity of Blast‐Furnace Slag Activated by Various Alkalis
Escalante‐García, J. I., Fuentes, A. F., Gorokhovsky, A., Fraire‐Luna, P. E., & Mendoza‐Suarez, G. (2003) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.2003.tb03623.x · Cited by 284
Freeze–thaw cycle test and damage mechanics models of alkali-activated slag concrete
Fu, Y., Cai, L., & Yonggen, W. (2011) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2010.12.006 · Cited by 279
Alkali-activated concrete: Engineering properties and stress–strain behavior
Thomas, R. J., & Peethamparan, S. (2015) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2015.04.039 · Cited by 277
Pore solution composition of alkali-activated slag/fly ash pastes
Zuo, Y., Nedeljković, M., & Ye, G. (2019) · Cement and Concrete Research · doi:10.1016/j.cemconres.2018.10.010 · Cited by 274
Hydration Characteristics and Microstructure of Alkali-Activated Slag Concrete: A Review
Fu, Q., Bu, M., Zhang, Z., Xu, W., Yuan, Q., & Niu, D. (2023) · Engineering · doi:10.1016/j.eng.2021.07.026 · Cited by 272
Jiang, H., Qi, Z., Yilmaz, E., Han, J., Qiu, J., & Dong, C. (2019) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2019.05.162 · Cited by 256
Li, N., Shi, C., & Zhang, Z. (2019) · Composites Part B: Engineering · doi:10.1016/j.compositesb.2019.04.024 · Cited by 249
Ravikumar, D., & Neithalath, N. (2012) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2012.03.006 · Cited by 244
“The influence of several parameters relating to the source material and the activator that can potentially influence the reaction kinetics as well as the mechanical and durability properties of the final product has been reported [1,7,14,18].”
BackgroundMethodAlkali-activated slag concrete: Fresh and hardened behaviour
Puertas, F., González-Fonteboa, B., González-Taboada, I., Alonso, M. M., Torres-Carrasco, M., Rojo, G., & Martínez-Abella, F. (2018) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2017.10.003 · Cited by 242
Self-citationMechanism of sulfate attack on alkali-activated slag: The role of activator composition
Ye, H., Chen, Z., & Huang, L. (2019) · Cement and Concrete Research · doi:10.1016/j.cemconres.2019.105868 · Cited by 218
Shrinkage and strength development of alkali-activated fly ash-slag binary cements
Hojati, M., & Radlińska, A. (2017) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2017.06.040 · Cited by 217
Temperature and activator effect on early-age reaction kinetics of alkali-activated slag binders
Gebregziabiher, B. S., Thomas, R. J., & Peethamparan, S. (2016) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2016.03.098 · Cited by 207
Hu, X., Shi, C., Shi, Z., & Zhang, L. (2019) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2019.103392 · Cited by 206
Alkali-activated Portland blast-furnace slag cement: Mechanical properties and hydration
Angulo-Ramírez, D. E., Mejía de Gutiérrez, R., & Puertas, F. (2017) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2017.02.092 · Cited by 198
Self-citationGreen chemistry for sustainable cement production and use
Phair, J. W. (2006) · Green Chemistry · doi:10.1039/b603997a · Cited by 197
Chen, W., Li, B., Wang, J., & Thom, N. (2021) · Cement and Concrete Research · doi:10.1016/j.cemconres.2020.106322 · Cited by 196
A Comprehensive Review on Fly Ash-Based Geopolymer
Luhar, I., & Luhar, S. (2022) · Journal of Composites Science · doi:10.3390/jcs6080219 · Cited by 192
Ravikumar, D., & Neithalath, N. (2012) · Thermochimica Acta · doi:10.1016/j.tca.2012.07.010 · Cited by 191
“Alkali activated binders have been reported to exhibit mechanical and durability characteristics similar to or superior than those of ordinary Portland cement binders [12–16].”
BackgroundChemical acceleration of a neutral granulated blast-furnace slag activated by sodium carbonate
Kovtun, M., Kearsley, E. P., & Shekhovtsova, J. (2015) · Cement and Concrete Research · doi:10.1016/j.cemconres.2015.02.014 · Cited by 190
Mechanical properties and setting time of ferrochrome slag based geopolymer paste and mortar
Karakoç, M. B., Türkmen, İ., Maraş, M. M., Kantarci, F., Demirboğa, R., & Uğur Toprak, M. (2014) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2014.09.021 · Cited by 186
Pacheco-Torgal, F., Castro-Gomes, J., & Jalali, S. (2007) · Cement and Concrete Research · doi:10.1016/j.cemconres.2007.02.006 · Cited by 176
Effects of activator properties and GGBFS/FA ratio on the structural build-up and rheology of AAC
Dai, X., Aydın, S., Yardımcı, M. Y., Lesage, K., & De Schutter, G. (2020) · Cement and Concrete Research · doi:10.1016/j.cemconres.2020.106253 · Cited by 173
Performance of alkali-activated slag mortars exposed to acids
Bernal, S. A., Rodríguez, E. D., Mejía de Gutiérrez, R., & Provis, J. L. (2012) · Journal of Sustainable Cement-Based Materials · doi:10.1080/21650373.2012.747235 · Cited by 173
Sodium silicate solutions from dissolution of glasswastes. Statistical analysis
Torres-Carrasco, M., Palomo, J. G., & Puertas, F. (2014) · Materiales de Construcción · doi:10.3989/mc.2014.05213 · Cited by 168
Self-citationCharacterisation of reactive magnesia and sodium carbonate-activated fly ash/slag paste blends
Abdalqader, A. F., Jin, F., & Al-Tabbaa, A. (2015) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2015.06.015 · Cited by 166
“84 Compared to other conventional activators, Na2CO3 yields a lower early age strength due to 85 its lower pH but it can demonstrate higher strength at late ages than NaOH resulting from the 86 effect of CO3 -2 ions [16], which lead to the formation of carbonated compounds that improve 87 the mechanical strength [17].”
BackgroundDurability assessment of alkali activated slag (AAS) concrete
Law, D. W., Adam, A. A., Molyneaux, T. K., & Patnaikuni, I. (2012) · Materials and Structures · doi:10.1617/s11527-012-9842-1 · Cited by 164
Alkali-activated mortars: Workability and rheological behaviour
Alonso, M. M., Gismera, S., Blanco, M. T., Lanzón, M., & Puertas, F. (2017) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2017.04.020 · Cited by 160
Self-citationInfluence of activator composition on the chloride binding capacity of alkali-activated slag
Ye, H., Huang, L., & Chen, Z. (2019) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2019.103368 · Cited by 142
Ke, X., Bernal, S. A., Provis, J. L., & Lothenbach, B. (2020) · Cement and Concrete Research · doi:10.1016/j.cemconres.2020.106158 · Cited by 117
“In comparison, the NC-AAS slag binder can develop denser microstructure than the NH-AAS slag binder under similar activation conditions before carbonation [50].”
BackgroundThe Characterization of Steel Slag by Alkali Activation
Aziz, I. H., Zulkifly, K., Sakkas, K., Panias, D., Tsaousi, G. M., Bakri, M. M. A. A., & Yong, H. C. (2017) · OALib · doi:10.4236/oalib.1103816 · Cited by 14
Metadata
- Authors
- Fernández-Jiménez, A., Palomo, J. G., & Puertas, F.
- Venue
- Cement and Concrete Research
- Publisher
- Elsevier BV
- Published
- 1999-08
- Volume
- 29
- Issue
- 8
- Pages
- 1313-1321
- ISSN
- 0008-8846 (ISSN-L)
- OpenAlex
- W40831481
- Cited by
- 598
- References
- 8
- FWCI
- 12.36
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.