Fuel Cell Catalyst Layers: A Polymer Science Perspective
The DOI matches its Crossref record; 119 of the 119 references it cites were found in a registry or an index.
Abstract
The polymeric ionomer plays a vital role in PEM fuel cell device technology, not simply as the membrane that transports protons and water from one electrode to another but as the binder and transport medium responsible for electrochemical activity within the catalyst layer. This perspective examines critical features of the catalyst layer ionomer. It highlights the current understanding of interactions of ionomer in catalyst inks, where the microstructure of the catalyst layer is largely formed, and in the catalyst layer itself. Properties important to the design and function of next generation ionomers and the challenges faced in replacing PFSA ionomers with hydrocarbon-based analogues are closely examined.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“Although typical CLs only have a thickness of 5-10 µm [21], they have a complicated multiscale structure, i.e., micro-, meso-, and macro-structure, due to the catalyst particles and ionomer, primary agglomerate particles, and secondary aggregation of primary agglomerates.”
From Effect of Catalyst Ink and Formation Process on the Multiscale Structure of Catalyst Layers in PEM Fuel Cells (2022) · cites this paper as [21]
In the citing paper
“Although typical CLs only have a thickness of 5-10 µm [21], they have a complicated multiscale structure”
From Effect of Catalyst Ink and Formation Process on the Multiscale Structure of Catalyst Layers in PEM Fuel Cells (2022) · cites this paper as [21]
Citations
Cites
Electrocatalyst approaches and challenges for automotive fuel cells
Debe, M. K. (2012) · Nature · doi:10.1038/nature11115 · Cited by 5,885
Gasteiger, H. A., Kocha, S. S., Sompalli, B., & Wagner, F. T. (2005) · Applied Catalysis B: Environmental · doi:10.1016/j.apcatb.2004.06.021 · Cited by 4,876
State of Understanding of Nafion
Mauritz, K. A., & Moore, R. B. (2004) · Chemical Reviews · doi:10.1021/cr0207123 · Cited by 4,791
Larminie, J., & Dicks, A. (2003) · Wiley eBooks · doi:10.1002/9781118878330 · Cited by 3,935
On the development of proton conducting polymer membranes for hydrogen and methanol fuel cells
Kreuer, K. D. (2001) · Journal of Membrane Science · doi:10.1016/s0376-7388(00)00632-3 · Cited by 2,969
Alternative Polymer Systems for Proton Exchange Membranes (PEMs)
Hickner, M. A., Ghassemi, H., Kim, Y. S., Einsla, B. R., & McGrath, J. E. (2004) · Chemical Reviews · doi:10.1021/cr020711a · Cited by 2,834
A review on non-precious metal electrocatalysts for PEM fuel cells
Chen, Z., Higgins, D., Yu, A., Zhang, L., & Zhang, J. (2011) · Energy & Environmental Science · doi:10.1039/c0ee00558d · Cited by 1,832
Li, Q., He, R., Jensen, J. O., & Bjerrum, N. J. (2003) · Chemistry of Materials · doi:10.1021/cm0310519 · Cited by 1,689
High temperature proton exchange membranes based on polybenzimidazoles for fuel cells
Li, Q., Jensen, J. O., Savinell, R. F., & Bjerrum, N. J. (2009) · Progress in Polymer Science · doi:10.1016/j.progpolymsci.2008.12.003 · Cited by 1,323
Carbon—Electrochemical and Physicochemical Properties
Brown, O. R. (1989) · Electrochimica Acta · doi:10.1016/0013-4686(89)87066-5 · Cited by 1,211
Research works printed but not linked: 5
- Hamrock S. J., 2006, Polym. Rev., 46, 219
- Maier G., 2008, Fuel Cells II, 216, 1
- Wang Q. P., 2004, J. Electroanal. Chem., 573, 61
- Gebel G., 2000, Polymer, 41, 5829, 10.1016/S0032-3861(99)00770-3 · DOI · Paper page
- Dong L., 2003, Polym. Prepr., 44, 355
Cited by
Items 101–200 of 480
Multicomponent, multiphase interactions in fuel-cell inks
Berlinger, S. A., Garg, S., & Weber, A. Z. (2021) · Current Opinion in Electrochemistry · doi:10.1016/j.coelec.2021.100744 · Cited by 62
Influence of ionomer adsorption on agglomerate structures in high-solid catalyst inks
Kumano, N., Kudo, K., Akimoto, Y., Ishii, M., & Nakamura, H. (2020) · Carbon · doi:10.1016/j.carbon.2020.07.047 · Cited by 61
Andersen, S. M., & Grahl-Madsen, L. (2016) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2015.11.101 · Cited by 61
Structure and conductivity of ionomer in PEM fuel cell catalyst layers: a model-based analysis
Olbrich, W., Kadyk, T., Sauter, U., Eikerling, M. H., & Gostick, J. T. (2023) · Scientific Reports · doi:10.1038/s41598-023-40637-0 · Cited by 69
Qiao, M., & Titirici, M. (2018) · Chemistry - A European Journal · doi:10.1002/chem.201804610 · Cited by 61
Kim, T.-H., Yoo, J. H., Maiyalagan, T., & Yi, S.-C. (2019) · Applied Surface Science · doi:10.1016/j.apsusc.2019.03.113 · Cited by 59
Andersen, S. M. (2015) · Applied Catalysis B: Environmental · doi:10.1016/j.apcatb.2015.07.049 · Cited by 61
Morris, D. R. P., Liu, S. P., Villegas Gonzalez, D., & Gostick, J. T. (2014) · ACS Applied Materials & Interfaces · doi:10.1021/am503509j · Cited by 59
So, M., Ohnishi, T., Park, K., Ono, M., Tsuge, Y., & Inoue, G. (2019) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2019.09.012 · Cited by 58
Xing, L., Shi, W., Das, P. K., & Scott, K. (2017) · AIChE Journal · doi:10.1002/aic.15826 · Cited by 61
Yang, Z., Moriguchi, I., & Nakashima, N. (2015) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.5b01724 · Cited by 58
Khandavalli, S., Iyer, R., Park, J. H., Myers, D. J., Neyerlin, K. C., Ulsh, M., & Mauger, S. A. (2020) · Langmuir · doi:10.1021/acs.langmuir.0c02015 · Cited by 56
Polymer Fuel Cell Based on Polybenzimidazole Membrane: A Review
Kalathil, A., Raghavan, A., & Kandasubramanian, B. (2018) · Polymer-Plastics Technology and Materials · doi:10.1080/03602559.2018.1482919 · Cited by 68
Liu, F., & Miyatake, K. (2022) · Journal of Materials Chemistry A · doi:10.1039/d1ta10480b · Cited by 57
Harada, M., Takata, S.-I., Iwase, H., Kajiya, S., Kadoura, H., & Kanaya, T. (2021) · ACS Omega · doi:10.1021/acsomega.1c01535 · Cited by 57
Hasegawa, N., Kamiya, A., Matsunaga, T., Kitano, N., & Harada, M. (2021) · Colloids and Surfaces A: Physicochemical and Engineering Aspects · doi:10.1016/j.colsurfa.2021.127153 · Cited by 54
Zaccarine, S. F., Shviro, M., Weker, J. N., Dzara, M. J., Foster, J. G., Carmo, M., & Pylypenko, S. (2022) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/ac7258 · Cited by 62
Du, X., Zhang, P., Zhang, G., Gao, H., Zhang, L., Zhang, M., Wang, T., & Gong, J. (2023) · National Science Review · doi:10.1093/nsr/nwad149 · Cited by 58
Shahgaldi, S., Alaefour, I., Zhao, J., & Li, X. (2018) · Fuel · doi:10.1016/j.fuel.2018.04.076 · Cited by 52
Novel Trends in Proton Exchange Membrane Fuel Cells
Olabi, A. G., Wilberforce, T., Alanazi, A. M., Vichare, P., Sayed, E. T., Maghrabie, H. M., Elsaid, K., & Abdelkareem, M. A. (2022) · Energies · doi:10.3390/en15144949 · Cited by 60
Muzaffar, T. A., Kadyk, T., & Eikerling, M. H. (2018) · Sustainable Energy & Fuels · doi:10.1039/c8se00026c · Cited by 55
Mao, L., Fu, K., Jin, J., Yang, S., & Li, G. (2019) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2019.05.058 · Cited by 53
Martens, I., Vamvakeros, A., Martínez, N., Chattot, R., Pusa, J., Blanco, M. V., Fisher, E. A., Asset, T., Escribano, S., Micoud, F., et al. (2021) · ACS Energy Letters · doi:10.1021/acsenergylett.1c00718 · Cited by 56
Yoshimune, W., & Harada, M. (2019) · Chemistry Letters · doi:10.1246/cl.190017 · Cited by 51
Singh, R. K., Akhgar, A., Sui, P., Lange, K. J., & Djilali, N. (2014) · Journal of The Electrochemical Society · doi:10.1149/2.036404jes · Cited by 52
Oh, K., Kang, H. S., Choo, M., Jang, D., Lee, D., Lee, D. G., Kim, T., Hong, Y. T., Park, J., & Kim, H. (2015) · Advanced Materials · doi:10.1002/adma.201500328 · Cited by 51
Substrate‐Dependent Molecular and Nanostructural Orientation of Nafion Thin Films
Kushner, D. I., Kusoglu, A., Podraza, N. J., & Hickner, M. A. (2019) · Advanced Functional Materials · doi:10.1002/adfm.201902699 · Cited by 53
Balogun, E., Barnett, A. O., & Holdcroft, S. (2020) · Journal of Power Sources Advances · doi:10.1016/j.powera.2020.100012 · Cited by 52
Self-citationPu, X., Duan, Y., Li, J., Ru, C., & Zhao, C. (2021) · Journal of Power Sources · doi:10.1016/j.jpowsour.2021.229671 · Cited by 50
Dang, D., Zhang, L., Zeng, X., Tian, X., Qu, C., Nan, H., Shu, T., Hou, S., Yang, L., Zeng, J., et al. (2017) · Journal of Power Sources · doi:10.1016/j.jpowsour.2017.04.050 · Cited by 49
Du, S., Lin, K., Malladi, S. K., Lu, Y., Sun, S., Xu, Q., Steinberger‐Wilckens, R., & Dong, H. (2014) · Scientific Reports · doi:10.1038/srep06439 · Cited by 49
Cho, M. K., Park, H., Lee, S. Y., Lee, B.-S., Kim, H., Henkensmeier, D., Yoo, S. J., Kim, J. Y., Han, J., Park, H. S., et al. (2016) · Electrochimica Acta · doi:10.1016/j.electacta.2016.12.009 · Cited by 54
Hiesgen, R., Morawietz, T., Handl, M., Corasaniti, M., & Friedrich, K. A. (2014) · Electrochimica Acta · doi:10.1016/j.electacta.2014.11.122 · Cited by 50
“analyzed using transmission electron microscopy (TEM)[34][35] [36] in combination with energy dispersive elementary analysis (EDX) or energy filtering to obtain a mapping of the fluorine content.”
MethodRoles of chain stiffness and segmental rattling in ionomer glass formation
Ruan, D., & Simmons, D. (2015) · Journal of Polymer Science Part B Polymer Physics · doi:10.1002/polb.23788 · Cited by 51
Ahadi, M., Tam, M., Stumper, J., & Bahrami, M. (2019) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2018.12.016 · Cited by 53
Nederstedt, H., & Jannasch, P. (2022) · Journal of Membrane Science · doi:10.1016/j.memsci.2022.120270 · Cited by 47
Evolution of Ionomer Morphology from Dispersion to Film: An in Situ X-ray Study
Dudenas, P. J., & Kusoglu, A. (2019) · Macromolecules · doi:10.1021/acs.macromol.9b01024 · Cited by 46
“2 Moreover, there has been a growing interest in understanding ionomers as thin-films (< 100 nm thickness), which stems from the need to understand their behavior in the catalyst layers (CLs) of a fuel cell or electrolyzer.(1-5) In CLs, ionomer thin-films act as a binder and conducting media, transporting reactants an…”
BackgroundTalukdar, K., Ripan, M. A., Jahnke, T., Gazdzicki, P., Morawietz, T., & Friedrich, K. A. (2020) · Journal of Power Sources · doi:10.1016/j.jpowsour.2020.228169 · Cited by 45
Paul, D. K., Shim, H. K., Giorgi, J. B., & Karan, K. (2016) · Journal of Polymer Science Part B Polymer Physics · doi:10.1002/polb.24034 · Cited by 48
Impact of Nonadsorbed Ionomer on Viscosity of Catalyst Inks for Polymer Electrolyte Fuel Cells
Yoshimune, W., & Harada, M. (2020) · Bulletin of the Chemical Society of Japan · doi:10.1246/bcsj.20190321 · Cited by 44
Lou, Y., Hao, M., & Li, Y. (2022) · Journal of Power Sources · doi:10.1016/j.jpowsour.2022.231827 · Cited by 46
How Catalyst Dispersion Solvents Affect CO2 Electrolyzer Gas Diffusion Electrodes
Mowbray, B. A. W., Dvořák, D., Taherimakhsousi, N., & Berlinguette, C. P. (2021) · Energy & Fuels · doi:10.1021/acs.energyfuels.1c01731 · Cited by 50
Berlinger, S. A., Chowdhury, A., Cleve, T. V., He, A., Dagan, N., Neyerlin, K. C., McCloskey, B. D., Radke, C. J., & Weber, A. Z. (2022) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.2c10499 · Cited by 49
Shin, S., Kim, A., & Um, S. (2018) · Electrochimica Acta · doi:10.1016/j.electacta.2018.04.138 · Cited by 44
Sun, Y., Cui, L., Gong, J., Zhang, J., Xiang, Y., & Lu, S. (2019) · ACS Sustainable Chemistry & Engineering · doi:10.1021/acssuschemeng.8b03910 · Cited by 43
Poojary, S., Islam, M. N., Shrivastava, U. N., Roberts, E. P. L., & Karan, K. (2020) · Molecules · doi:10.3390/molecules25153387 · Cited by 43
Alinejad, S., Quinson, J., Schröder, J., Kirkensgaard, J. J. K., & Arenz, M. (2020) · ACS Catalysis · doi:10.1021/acscatal.0c03184 · Cited by 43
Li, B., Liu, Y., Guo, Y., Yang, D., Yang, D., Ming, P., & Zhang, C. (2021) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2021.06.216 · Cited by 44
Wu, J., Zhu, X., West, M. M., Tyliszczak, T., Shiu, H., Shapiro, D. A., Berejnov, V., Susac, D., Stumper, J., & Hitchcock, A. P. (2018) · The Journal of Physical Chemistry C · doi:10.1021/acs.jpcc.8b02933 · Cited by 45
Hyun, J., Jeon, J. Y., Doo, G., Jung, J., Choi, S.-G., Lee, D., Lee, D. W., Kwen, J., Jo, W., Bae, C., et al. (2021) · Chemical Engineering Journal · doi:10.1016/j.cej.2021.131737 · Cited by 44
Giesbrecht, P. K., & Freund, M. S. (2022) · The Journal of Physical Chemistry C · doi:10.1021/acs.jpcc.2c05104 · Cited by 45
Wu, N., Liu, Y., Tian, X., Liu, F., Ma, Y., Zhang, S., Zhang, Q., Hou, D., Qi, Y., Yang, R., et al. (2023) · Journal of Power Sources · doi:10.1016/j.jpowsour.2023.233412 · Cited by 46
Wei, Z., Su, K., Sui, S., He, A., & Du, S. (2015) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2015.01.009 · Cited by 42
Yang, D., Guo, Y., Tang, H., Wang, Y., Yang, D., Ming, P., Zhang, C., Li, B., & Zhu, S. (2021) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2021.07.172 · Cited by 44
Sánchez-Ramos, A., Gostick, J. T., & García‐Salaberri, P. A. (2021) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/ac4456 · Cited by 43
2023 Roadmap on molecular modelling of electrochemical energy materials
Zhang, C., Cheng, J., Chen, Y., Chan, M. K. Y., Cai, Q., de Carvalho, R. P., Marchiori, C. F. N., Brandell, D., Araujo, C. M., Chen, M., et al. (2023) · Journal of Physics Energy · doi:10.1088/2515-7655/acfe9b · Cited by 50
Chen, Y., Zhong, Q. D., Li, G., Tian, T., Tan, J., & Pan, M. (2018) · Ionics · doi:10.1007/s11581-018-2533-3 · Cited by 42
Impact of the Solid Interface on Proton Conductivity in Nafion Thin Films
Ogata, Y., Abe, T., Yonemori, S., Yamada, N. L., Kawaguchi, D., & Tanaka, K. (2018) · Langmuir · doi:10.1021/acs.langmuir.8b03396 · Cited by 44
Yang, Z., & Nakashima, N. (2015) · Journal of Materials Chemistry A · doi:10.1039/c5ta06735a · Cited by 39
Ebenezer, D., Deshpande, A. P., & Haridoss, P. (2015) · Journal of Power Sources · doi:10.1016/j.jpowsour.2015.11.048 · Cited by 39
Obermaier, M., Bandarenka, A. S., & Lohri, C. (2018) · Scientific Reports · doi:10.1038/s41598-018-23071-5 · Cited by 39
Kuo, A.-T., Urata, S., Nakabayashi, K., Watabe, H., & Honmura, S. (2021) · Macromolecules · doi:10.1021/acs.macromol.0c02364 · Cited by 40
Novalin, T., Pan, D., Lindbergh, G., Lagergren, C., Jannasch, P., & Lindström, R. W. (2021) · Journal of Power Sources · doi:10.1016/j.jpowsour.2021.230287 · Cited by 38
Thuc, V. D., Tinh, V. D. C., & Kim, D. (2022) · Journal of Power Sources · doi:10.1016/j.jpowsour.2022.232418 · Cited by 40
On the state and stability of fuel cell catalyst inks
Bapat, S., Giehl, C., Kohsakowski, S., Peinecke, V., Schäffler, M., & Segets, D. (2021) · Advanced Powder Technology · doi:10.1016/j.apt.2021.08.030 · Cited by 38
Alkali Metals Activated High Entropy Double Perovskites for Boosted Hydrogen Evolution Reaction
Sun, N., Lai, Z., Ding, W., Li, W., Wang, T., Zheng, Z., Zhang, B., Dong, X., Wei, P., Du, P., et al. (2024) · Advanced Science · doi:10.1002/advs.202406453 · Cited by 39
High Proton Conduction of Organized Sulfonated Polyimide Thin Films with Planar and Bent Backbones
Ono, Y., Goto, R., Hara, M., Nagano, S., Abe, T., & Nagao, Y. (2018) · Macromolecules · doi:10.1021/acs.macromol.8b00301 · Cited by 37
Effect of rheological properties of catalyst slurry on the structure of catalyst layer in PEMFC
Yang, D., Guo, Y., Tang, H., Yang, D., Ming, P., Zhang, C., Li, B., & Zhu, S. (2022) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2021.12.227 · Cited by 41
Mezzavilla, S., Cherevko, S., Baldizzone, C., Pizzutilo, E., Polymeros, G., & Mayrhofer, K. J. J. (2016) · ChemElectroChem · doi:10.1002/celc.201600170 · Cited by 41
Sohn, Y.-J., Yim, S., Park, G., Kim, M., Won, S., & Kim, K. (2017) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2017.04.036 · Cited by 36
Highly Stable, Low Gas Crossover, Proton‐Conducting Phenylated Polyphenylenes
Adamski, M., Skalski, T. J. G., Britton, B., Peckham, T. J., Metzler, L., & Holdcroft, S. (2017) · Angewandte Chemie · doi:10.1002/ange.201703916 · Cited by 37
Self-citationStrong, A., Britton, B., Edwards, D., Peckham, T. J., Lee, H.-F., Huang, W. Y., & Holdcroft, S. (2015) · Journal of The Electrochemical Society · doi:10.1149/2.0251506jes · Cited by 40
Self-citationYang, Z., Fujigaya, T., & Nakashima, N. (2015) · Journal of Power Sources · doi:10.1016/j.jpowsour.2015.09.069 · Cited by 36
De, B. S., Singh, A., Elias, A. L., Khare, N., & Basu, S. (2020) · Sustainable Energy & Fuels · doi:10.1039/d0se01474e · Cited by 35
Ren, R., Wang, X., Chen, H., Miller, H. A., Salam, I., Varcoe, J. R., Wu, L., Chen, Y., Liao, H., Liu, E., et al. (2020) · Angewandte Chemie International Edition · doi:10.1002/anie.202012547 · Cited by 35
Nykaza, J. R., Benjamin, R., Meek, K. M., & Elabd, Y. A. (2016) · Chemical Engineering Science · doi:10.1016/j.ces.2016.05.041 · Cited by 37
Formulation of carbon black-ionomer dispersions for thin film formation in fuel cells
Hoffmann, E., Zhang, S., Thoma, M., Damm, C., & Peukert, W. (2019) · Particuology · doi:10.1016/j.partic.2018.08.001 · Cited by 34
Ionomer degradation in catalyst layers of anion exchange membrane fuel cells
Li, Q., Hu, M., Ge, C., Yang, Y., Xiao, L., Zhuang, L., & Abruña, H. D. (2023) · Chemical Science · doi:10.1039/d3sc03649a · Cited by 34
Structure property relationships affecting the proton conductivity in imidazole loaded Al-MOFs
Homburg, T., Hartwig, C., Reinsch, H., Wark, M., & Stock, N. (2016) · Dalton Transactions · doi:10.1039/c6dt03048c · Cited by 36
Morphology Changes in Perfluorosulfonated Ionomer from Thickness and Thermal Treatment Conditions
Gao, X. P., Yamamoto, K., Hirai, T., Uchiyama, T., Ohta, N., Takao, N., Matsumoto, M., Imai, H., Sugawara, S., Shinohara, K., et al. (2020) · Langmuir · doi:10.1021/acs.langmuir.9b03564 · Cited by 35
Influence of Ionic Interaction Strength on Glass Formation of an Ion-Containing Polymer Melt
Yang, Z., Xu, X., & Xu, W. (2021) · Macromolecules · doi:10.1021/acs.macromol.1c01719 · Cited by 34
Control of Cluster Structures in Catalyst Inks by a Dispersion Medium
Yang, D., Zhu, S., Guo, Y., Tang, H., Yang, D., Zhang, C., Ming, P., & Li, B. (2021) · ACS Omega · doi:10.1021/acsomega.1c05026 · Cited by 37
Liang, X., Ge, X., He, Y., Xu, M., Shehzad, M. A., Sheng, F., Bance‐Soualhi, R., Zhang, J., Yu, W., Ge, Z., et al. (2021) · Advanced Science · doi:10.1002/advs.202102637 · Cited by 34
Morawietz, T., Handl, M., Oldani, C., Friedrich, K. A., & Hiesgen, R. (2018) · Fuel Cells · doi:10.1002/fuce.201700113 · Cited by 36
Liu, C., Luo, M., Zeis, R., Chuang, P. A., Zhang, R., Du, S., & Sui, P. (2023) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2023.08.154 · Cited by 33
Theory of electrostatic phenomena in water-filled Pt nanopores
Huang, J., Zhang, J., & Eikerling, M. H. (2016) · Faraday Discussions · doi:10.1039/c6fd00094k · Cited by 34
Lee, J. K., Kim, P. J., Krause, K., Shrestha, P., Balakrishnan, M., Fahy, K. F., Fatih, K., Shaigan, N., Ge, M., Lee, W.-K., et al. (2023) · Cell Reports Physical Science · doi:10.1016/j.xcrp.2022.101232 · Cited by 32
Mechanical Response of Thermally Annealed Nafion Thin Films
Frieberg, B. R., Page, K. A., Graybill, J. R., Walker, M. L., Stafford, C. M., Stafford, G. R., & Soles, C. L. (2016) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.6b12423 · Cited by 33
Kim, O. ‐., Oh, S. ‐., Ahn, C. ‐., Kim, S., Kim, J. K., Kim, J., Yang, S., Choi, M., Cho, Y. ‐., & Sung, Y. ‐. (2018) · Fuel Cells · doi:10.1002/fuce.201800083 · Cited by 31
Wang, B., Pan, J. S., Zou, X., Zhao, J., Xu, G., Jin, Z., Sun, Z., & Yan, F. (2022) · Journal of Materials Chemistry A · doi:10.1039/d2ta02632e · Cited by 31
Zhang, X., & Ding, Y. (2014) · RSC Advances · doi:10.1039/c4ra05523c · Cited by 31
Communication—Non-Fluorous, Hydrocarbon PEMFCs, Generating > 1 W cm −2 Power
Balogun, E., Adamski, M., & Holdcroft, S. (2020) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/ab88bd · Cited by 33
Self-citationIonomers From Kraft Lignin for Renewable Energy Applications
Farzin, S., Johnson, T. J., Chatterjee, S., Zamani, E., & Dishari, S. K. (2020) · Frontiers in Chemistry · doi:10.3389/fchem.2020.00690 · Cited by 32
“But when the same ionomer is coated over a substrate as a submicron-thick film (Dishari and Hickner, 2013; Holdcroft, 2013; Modestino et al., 2013; Dishari, 2014; Kusoglu and Weber, 2017; Farzin et al., 2019) or over catalyst particles on cathodes as a ∼2–30-nm thick catalyst-binder (Astill et al.”
BackgroundInfluentialTsipoaka, M., Aziz, M. A., & Shanmugam, S. (2021) · ACS Sustainable Chemistry & Engineering · doi:10.1021/acssuschemeng.0c07846 · Cited by 33
Balogun, E., Cassegrain, S., Mardle, P., Adamski, M., Saatkamp, T., & Holdcroft, S. (2022) · ACS Energy Letters · doi:10.1021/acsenergylett.2c01038 · Cited by 31
Self-citationModeling of wetting phenomena in cathode catalyst layers for PEM fuel cells
Olbrich, W., Kadyk, T., Sauter, U., & Eikerling, M. H. (2022) · Electrochimica Acta · doi:10.1016/j.electacta.2022.140850 · Cited by 30
Kakati, N., Li, G., & Chuang, P. A. (2021) · ACS Applied Energy Materials · doi:10.1021/acsaem.1c00607 · Cited by 29
Choo, M., Oh, K., Kim, H., & Park, J. (2014) · ChemSusChem · doi:10.1002/cssc.201402015 · Cited by 29
Spéder, J., Zana, A., & Arenz, M. (2015) · Catalysis Today · doi:10.1016/j.cattod.2015.09.021 · Cited by 32
“carbon surface area and thus increases NP agglomeration or blocks the Pt surface itself [40, 43].”
BackgroundUtilizing thiol–ene chemistry for crosslinked nickel cation‐based anion exchange membranes
Kwasny, M. T., Zhu, L. J., Hickner, M. A., & Tew, G. N. (2017) · Journal of Polymer Science Part A Polymer Chemistry · doi:10.1002/pola.28894 · Cited by 29
Metadata
- Authors
- Holdcroft, S.
- Affiliations
- Simon Fraser University (CA)
- Corresponding author
- Holdcroft, Steven
- ORCID
- Holdcroft, Steven
- Venue
- Chemistry of Materials
- Publisher
- American Chemical Society (ACS)
- Published
- 2013-07-12
- Volume
- 26
- Issue
- 1
- Pages
- 381-393
- ISSN
- 0897-4756 (ISSN-L)
- 1520-5002
- OpenAlex
- W2329419691
- Cited by
- 481
- References
- 119
- Citations by year
- 2026: 31 · 2025: 35 · 2024: 35 · 2023: 47 · 2022: 40 · 2021: 56 · 2020: 52 · 2019: 36 · 2018: 41 · 2017: 38 · 2016: 24 · 2015: 28 · 2014: 18
- FWCI
- 13.98
- Type
- journal article
- Language
- en
- Open access
- closed
- Locations
- Chemistry of Materials (publishedVersion)
- Topics
- Physical Sciences › Engineering › Electrical and Electronic Engineering › Fuel Cells and Related Materials
- Physical Sciences › Energy › Renewable Energy, Sustainability and the Environment › Electrocatalysts for Energy Conversion
- Physical Sciences › Materials Science › Materials Chemistry › Advancements in Solid Oxide Fuel Cells
- Keywords
- proton exchange membrane fuel cells, catalyst layer, ionomer binder, catalyst ink, catalyst layer microstructure, perfluorosulfonic acid ionomer, proton transport, water transport
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.