The DOI matches its Crossref record; 41 of the 41 references it cites were found in a registry or an index.
Nucleation and Growth Mechanism of Lithium Metal Electroplating
Abstract
Understanding the mechanism of Li nucleation and growth is essential for providing long cycle life and safe lithium ion batteries or lithium metal batteries. However, no quantitative report on Li metal deposition is available, to the best of our knowledge. We propose a model for quantitatively understanding the Li nucleation and growth mechanism associated with the solid–electrolyte interphase (SEI) formation, which we name the Li-SEI model. The current transients at various overpotentials initiate the nucleation and growth of Li metal on bare Cu foil. The Li-SEI model considering a three-dimensional diffusion-controlled instantaneous process ( J 3D-DC ) with the simultaneous reduction of electrolyte decomposition ( J SEI ) due to the SEI fracture is employed for investigating the Li nucleation and growth mechanism. The individual contributions of experimental and theoretical transient states, i.e., the fundamental kinetic values of diffusion coefficient ( D ), rate of nucleation ( N 0 ), and rate constant of electrolyte decomposition ( k SEI ), can be determined from the Li-SEI model. Interestingly, J SEI increases with time, indicating that the current contributing from the electrolyte decomposition increases with time due to the SEI fracture upon Li deposition. Meanwhile, the k SEI increases with overpotential, indicating the SEI fracture is more serious at higher overpotential or higher growth rate. The k SEI is smaller in the electrolyte with fluoroethylene carbonate (FEC) additive, indicating that FEC additive can significantly suppress the SEI fracture during Li metal deposition. This proposed model opens a new way to quantitatively understand the Li nucleation and growth mechanism and electrolyte decomposition on various substrates or in different electrolytes.
Overview
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Li-O2 and Li-S batteries with high energy storage
Bruce, P. G., Freunberger, S. A., Hardwick, L. J., & Tarascon, J.-M. (2012) · Nature Materials · doi:10.1038/nmat3191 · Cited by 9,479
Reviving the lithium metal anode for high-energy batteries
Lin, D., Liu, Y., & Cui, Y. (2017) · Nature Nanotechnology · doi:10.1038/nnano.2017.16 · Cited by 6,763
Toward Safe Lithium Metal Anode in Rechargeable Batteries: A Review
Cheng, X.-B., Zhang, R., Zhao, C.-Z., & Zhang, Q. (2017) · Chemical Reviews · doi:10.1021/acs.chemrev.7b00115 · Cited by 6,197
Lithium metal anodes for rechargeable batteries
Xu, W., Wang, J., Ding, F., Chen, X., Nasybulin, E., Zhang, Y., & Zhang, J.-G. (2014) · Energy Environ. Sci. · doi:10.1039/c3ee40795k · Cited by 4,704
High rate and stable cycling of lithium metal anode
Qian, J., Henderson, W. A., Xu, W., Bhattacharya, P., Engelhard, M., Borodin, O., & Zhang, J.-G. (2015) · Nature Communications · doi:10.1038/ncomms7362 · Cited by 2,561
Aurbach, D. (2000) · Journal of Power Sources · doi:10.1016/s0378-7753(00)00431-6 · Cited by 2,130
Selective deposition and stable encapsulation of lithium through heterogeneous seeded growth
Yan, K., Lu, Z., Lee, H.-W., Xiong, F., Hsu, P.-C., Li, Y., Zhao, J., Chu, S., & Cui, Y. (2016) · Nature Energy · doi:10.1038/nenergy.2016.10 · Cited by 2,116
Dendrite-Free Lithium Deposition via Self-Healing Electrostatic Shield Mechanism
Ding, F., Xu, W., Graff, G. L., Zhang, J., Sushko, M. L., Chen, X., Shao, Y., Engelhard, M. H., Nie, Z., Xiao, J., et al. (2013) · Journal of the American Chemical Society · doi:10.1021/ja312241y · Cited by 2,107
Interconnected hollow carbon nanospheres for stable lithium metal anodes
Zheng, G., Lee, S. W., Liang, Z., Lee, H.-W., Yan, K., Yao, H., Wang, H., Li, W., Chu, S., & Cui, Y. (2014) · Nature Nanotechnology · doi:10.1038/nnano.2014.152 · Cited by 1,764
Nanoscale Nucleation and Growth of Electrodeposited Lithium Metal
Pei, A., Zheng, G., Shi, F., Li, Y., & Cui, Y. (2017) · Nano Letters · doi:10.1021/acs.nanolett.6b04755 · Cited by 1,726
Cited by
Toward Critical Electrode/Electrolyte Interfaces in Rechargeable Batteries
Yan, C., Xu, R., Xiao, Y., Ding, J., Xu, L., Li, B., & Huang, J. (2020) · Advanced Functional Materials · doi:10.1002/adfm.201909887 · Cited by 510
Review on Li Deposition in Working Batteries: From Nucleation to Early Growth
Chen, X., Zhao, B., Yan, C., & Zhang, Q. (2021) · Advanced Materials · doi:10.1002/adma.202004128 · Cited by 456
Gel polymer electrolytes for rechargeable batteries toward wide-temperature applications
Zhou, X., Zhou, Y., Yu, L., Qi, L., Oh, K.-S., Hu, P., Lee, S.-Y., & Chen, C. (2024) · Chemical Society Reviews · doi:10.1039/d3cs00551h · Cited by 333
Decoupling the origins of irreversible coulombic efficiency in anode-free lithium metal batteries
Huang, C.-J., Thirumalraj, B., Tao, H.-C., Shitaw, K. N., Sutiono, H., Hagos, T. T., Beyene, T. T., Kuo, L.-M., Wang, C.-C., Wu, S.-H., et al. (2021) · Nature Communications · doi:10.1038/s41467-021-21683-6 · Cited by 287
Self-citationHeubner, C., Maletti, S., Auer, H., Hüttl, J., Voigt, K., Lohrberg, O., Nikolowski, K., Partsch, M., & Michaelis, A. (2021) · Advanced Functional Materials · doi:10.1002/adfm.202106608 · Cited by 277
Metadata
- Authors
- Thirumalraj, B., Hagos, T. T., Huang, C.-J., Teshager, M. A., Cheng, J.-H., Su, W.-N., & Hwang, B.-J.
- Venue
- Journal of the American Chemical Society
- Publisher
- American Chemical Society (ACS)
- Published
- 2019-10-23
- Volume
- 141
- Issue
- 46
- Pages
- 18612-18623
- ISSN
- 0002-7863 (ISSN-L)
- 1520-5126
- OpenAlex
- W2981445017
- Cited by
- 273
- References
- 41
- FWCI
- 8.19
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
How to cite
Cite CoChat for the checks on this page, and the paper for its own findings.
- This page
- CoChat. (2026). Citation check: Nucleation and Growth Mechanism of Lithium Metal Electroplating. https://app.cochat.ai/papers/10.1021/jacs.9b10195
- The paper
- Thirumalraj, B., Hagos, T. T., Huang, C.-J., Teshager, M. A., Cheng, J.-H., Su, W.-N., & Hwang, B.-J. (2019). Nucleation and Growth Mechanism of Lithium Metal Electroplating. Journal of the American Chemical Society. https://doi.org/10.1021/jacs.9b10195
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.