Abstract
All materials can suffer from environmental degradation; the rate and extent of degradation depend on the details of the material composition and structure as well as the environment. The corrosion of silicate glasses, crystalline ceramics, and metals, particularly as related to nuclear waste forms, has received a lot of attention. The corrosion phenomena and mechanisms of these materials are different, but also have many similarities. This review compares and contrasts the mechanisms of environmental degradation of glass, crystalline ceramics, and metals, with the goal of identifying commonalities that can seed synergistic activities and advance the current knowledge in each area.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Implicit solvation model for density-functional study of nanocrystal surfaces and reaction pathways
Mathew, K., Sundararaman, R., Letchworth-Weaver, K., Arias, T. A., & Hennig, R. G. (2014) · The Journal of Chemical Physics · doi:10.1063/1.4865107 · Cited by 3,196
Theory of the oxidation of metals
Cabrera, N., & Mott, N. F. (1949) · Reports on Progress in Physics · doi:10.1088/0034-4885/12/1/308 · Cited by 2,986
Pitting Corrosion of Metals: A Review of the Critical Factors
Frankel, G. S. (1998) · Journal of The Electrochemical Society · doi:10.1149/1.1838615 · Cited by 2,135
Self-citationThe surface chemistry of soils
Sposito, G. (1984) · Cited by 1,850
(1979) · Springer eBooks · doi:10.1007/978-1-4615-9107-8 · Cited by 1,769
The Point Defect Model for the Passive State
Macdonald, D. D. (1992) · Journal of The Electrochemical Society · doi:10.1149/1.2069096 · Cited by 1,574
Introduction to Corrosion Science
McCafferty, E. (2010) · Springer eBooks · doi:10.1007/978-1-4419-0455-3 · Cited by 1,322
Putnis, A. (2009) · Reviews in Mineralogy and Geochemistry · doi:10.2138/rmg.2009.70.3 · Cited by 1,160
Surface and interface stress effects in thin films
Cammarata, R. C. (1994) · Progress in Surface Science · doi:10.1016/0079-6816(94)90005-1 · Cited by 950
A Point Defect Model for Anodic Passive Films: I . Film Growth Kinetics
Chao, C. Y., Lin, L. F., & Macdonald, D. D. (1981) · Journal of The Electrochemical Society · doi:10.1149/1.2127591 · Cited by 894
Aagaard, P., & Helgeson, H. C. (1982) · American Journal of Science · doi:10.2475/ajs.282.3.237 · Cited by 894
Chemical Weathering Rates of Silicate Minerals
(1995) · De Gruyter eBooks · doi:10.1515/9781501509650 · Cited by 868
Kinetics of Water-Rock Interaction
(2008) · Springer eBooks · doi:10.1007/978-0-387-73563-4 · Cited by 739
A Point Defect Model for Anodic Passive Films: II . Chemical Breakdown and Pit Initiation
Lin, L. F., Chao, C. Y., & Macdonald, D. D. (1981) · Journal of The Electrochemical Society · doi:10.1149/1.2127592 · Cited by 664
Fehlner, F. P., & Mott, N. F. (1970) · Oxidation of Metals · doi:10.1007/bf00603582 · Cited by 652
Molecular mechanisms for corrosion of silica and silicate glasses
Bunker, B. C. (1994) · Journal of Non-Crystalline Solids · doi:10.1016/0022-3093(94)90708-0 · Cited by 635
Kinetics of Geochemical Processes
(1981) · De Gruyter eBooks · doi:10.1515/9781501508233 · Cited by 605
An international initiative on long-term behavior of high-level nuclear waste glass
Gin, S., Abdelouas, A., Criscenti, L. J., Ebert, W. L., Ferrand, K., Geisler, T., Harrison, M. T., Inagaki, Y., Mitsui, S., Mueller, K. T., et al. (2013) · Materials Today · doi:10.1016/j.mattod.2013.06.008 · Cited by 546
Self-citationGeneral kinetic description of multioxide silicate mineral and glass dissolution
Oelkers, E. H. (2001) · Geochimica et Cosmochimica Acta · doi:10.1016/s0016-7037(01)00710-4 · Cited by 531
Variation of Crystal Dissolution Rate Based on a Dissolution Stepwave Model
Lasaga, A. C., & Luttge, A. (2001) · Science · doi:10.1126/science.1058173 · Cited by 496
Oelkers, E. H., Schott, J., & Devidal, J.-L. (1994) · Geochimica et Cosmochimica Acta · doi:10.1016/0016-7037(94)90281-x · Cited by 493
Greeley, J., & Nørskov, J. K. (2007) · Electrochimica Acta · doi:10.1016/j.electacta.2007.02.082 · Cited by 491
Geochim. Cosmochim. Acta5 1951–1955 (1981)
Schmitter, J. M., Arpino, P. J., & Guiochon, G. (1982) · Geochimica et Cosmochimica Acta · doi:10.1016/0016-7037(82)90171-5 · Cited by 488
Insight into silicate-glass corrosion mechanisms
Cailleteau, C., Angeli, F., Devreux, F., Gin, S., Jestin, J., Jollivet, P., & Spalla, O. (2008) · Nature Materials · doi:10.1038/nmat2301 · Cited by 488
Self-citationCoupled dissolution and precipitation at mineral–fluid interfaces
Ruiz-Agudo, E., Putnis, C. V., & Putnis, A. (2014) · Chemical Geology · doi:10.1016/j.chemgeo.2014.06.007 · Cited by 439
Rate control of mineral dissolution under Earth surface conditions
Berner, R. A. (1978) · American Journal of Science · doi:10.2475/ajs.278.9.1235 · Cited by 430
The Link Between Mineral Dissolution/Precipitation Kinetics and Solution Chemistry
Schott, J., Pokrovsky, O. S., & Oelkers, E. H. (2009) · Reviews in Mineralogy and Geochemistry · doi:10.2138/rmg.2009.70.6 · Cited by 414
Frugier, P., Gin, S., Minet, Y., Chave, T., Bonin, B., Godon, N., Lartigue, J.-E., Jollivet, P., Ayral, A., De Windt, L., et al. (2008) · Journal of Nuclear Materials · doi:10.1016/j.jnucmat.2008.06.044 · Cited by 395
Self-citationPrediction of Fatigue Crack Initiation Life Based on Pit Growth
Kondo, Y. (1989) · Corrosion · doi:10.5006/1.3577891 · Cited by 369
Kinetics of Mineral Dissolution
Brantley, S. L. (2008) · Kinetics of Water-Rock Interaction · doi:10.1007/978-0-387-73563-4_5 · Cited by 349
Hellmann, R., Wirth, R., Daval, D., Barnes, J.-P., Penisson, J.-M., Tisserand, D., Epicier, T., Florin, B., & Hervig, R. L. (2012) · Chemical Geology · doi:10.1016/j.chemgeo.2011.12.002 · Cited by 327
Machet, A., Galtayries, A., Zanna, S., Klein, L. H., Maurice, V., Jolivet, P., Foucault, M., Combrade, P., Scott, P., & Marcus, P. (2004) · Electrochimica Acta · doi:10.1016/j.electacta.2004.04.032 · Cited by 317
Hellmann, R., Cotte, S., Cadel, E., Malladi, S., Karlsson, L. S., Lozano-Perez, S., Cabié, M., & Seyeux, A. (2015) · Nature Materials · doi:10.1038/nmat4172 · Cited by 315
Free energy dependence of albite dissolution kinetics at 80°C and pH 8.8
Burch, T. E., Nagy, K. L., & Lasaga, A. C. (1993) · Chemical Geology · doi:10.1016/0009-2541(93)90123-z · Cited by 311
Origin and consequences of silicate glass passivation by surface layers
Gin, S., Jollivet, P., Fournier, M., Angeli, F., Frugier, P., & Charpentier, T. (2015) · Nature Communications · doi:10.1038/ncomms7360 · Cited by 303
Self-citationExperimental study of anorthite dissolution and the relative mechanism of feldspar hydrolysis
Oelkers, E. H., & Schott, J. (1995) · Geochimica et Cosmochimica Acta · doi:10.1016/0016-7037(95)00326-6 · Cited by 299
Nagy, K. L., Blum, A. E., & Lasaga, A. C. (1991) · American Journal of Science · doi:10.2475/ajs.291.7.649 · Cited by 284
Vienna, J. D., Ryan, J. V., Gin, S., & Inagaki, Y. (2013) · International Journal of Applied Glass Science · doi:10.1111/ijag.12050 · Cited by 266
Self-citationFirst-order dissolution rate law and the role of surface layers in glass performance assessment
Grambow, B., & Müller, R. (2001) · Journal of Nuclear Materials · doi:10.1016/s0022-3115(01)00619-5 · Cited by 243
Leaching and reconstruction at the surfaces of dissolving chain-silicate minerals
Casey, W. H., Westrich, H. R., Banfield, J. F., Ferruzzi, G., & Arnold, G. W. (1993) · Nature · doi:10.1038/366253a0 · Cited by 241
Oelkers, E. H., & Schott, J. (2001) · Geochimica et Cosmochimica Acta · doi:10.1016/s0016-7037(00)00564-0 · Cited by 240
Aqueous corrosion of borosilicate glass under acidic conditions: A new corrosion mechanism
Geisler, T., Janssen, A., Scheiter, D., Stephan, T., Berndt, J., & Putnis, A. (2010) · Journal of Non-Crystalline Solids · doi:10.1016/j.jnoncrysol.2010.04.033 · Cited by 240
Gautier, J.-M., Oelkers, E. H., & Schott, J. (1994) · Geochimica et Cosmochimica Acta · doi:10.1016/0016-7037(94)90190-2 · Cited by 235
Hellmann, R., & Tisserand, D. (2006) · Geochimica et Cosmochimica Acta · doi:10.1016/j.gca.2005.10.007 · Cited by 234
Perspective—Localized Corrosion: Passive Film Breakdown vs Pit Growth Stability
Frankel, G. S., Li, T., & Scully, J. R. (2017) · Journal of The Electrochemical Society · doi:10.1149/2.1381704jes · Cited by 234
Self-citationAlpha-decay damage and aqueous durability of actinide host phases in natural systems
Lumpkin, G. R. (2001) · Journal of Nuclear Materials · doi:10.1016/s0022-3115(00)00693-0 · Cited by 231
XPS and STM Study of Passive Films Formed on Fe‐22Cr(110) Single‐Crystal Surfaces
Maurice, V., Yang, W. Y., & Marcus, P. (1996) · Journal of The Electrochemical Society · doi:10.1149/1.1836616 · Cited by 222
(1999) · ASM International eBooks · doi:10.31399/asm.tb.caaa.t67870045 · Cited by 208
Durable Glass for Thousands of Years
Jantzen, C. M., Brown, K. G., & Pickett, J. B. (2010) · International Journal of Applied Glass Science · doi:10.1111/j.2041-1294.2010.00007.x · Cited by 204
Surface chemistry of labradorite feldspar reacted with aqueous solutions at pH = 2, 3, and 12
Casey, W. H., Westrich, H. R., & Arnold, G. W. (1988) · Geochimica et Cosmochimica Acta · doi:10.1016/0016-7037(88)90147-0 · Cited by 200
Nuclear Waste Glasses - How Durable?
Grambow, B. (2006) · Elements · doi:10.2113/gselements.2.6.357 · Cited by 194
Resumption of nuclear glass alteration: State of the art
Fournier, M., Gin, S., & Frugier, P. (2014) · Journal of Nuclear Materials · doi:10.1016/j.jnucmat.2014.02.022 · Cited by 193
Self-citationThe mechanism of borosilicate glass corrosion revisited
Geisler, T., Nagel, T., Kilburn, M. R., Janssen, A., Icenhower, J. P., Fonseca, R. O. C., Grange, M., & Nemchin, A. A. (2015) · Geochimica et Cosmochimica Acta · doi:10.1016/j.gca.2015.02.039 · Cited by 188
Crovisier, J. L., Advocat, T., & Dussossoy, J. (2003) · Journal of Nuclear Materials · doi:10.1016/s0022-3115(03)00206-x · Cited by 186
The structure of Na2O–Al2O3–SiO2 glass: impact on sodium ion exchange in H2O and D2O
McGrail, B. P., Icenhower, J. P., Shuh, D. K., Liu, P., Darab, J. G., Baer, D. R., Thevuthasen, S., Shutthanandan, V., Engelhard, M. H., Booth, C. H., et al. (2001) · Journal of Non-Crystalline Solids · doi:10.1016/s0022-3093(01)00890-0 · Cited by 173
Thermodynamics and Kinetics of Water-Rock Interaction
(2009) · De Gruyter eBooks · doi:10.1515/9781501508462 · Cited by 171
Crystal dissolution kinetics and Gibbs free energy
Lüttge, A. (2006) · Journal of Electron Spectroscopy and Related Phenomena · doi:10.1016/j.elspec.2005.06.007 · Cited by 170
Chemical weathering rates of pyroxenes and amphiboles
Brantley, S. L., & Chen, Y. (1995) · Reviews in Mineralogy and Geochemistry · Cited by 168
Gin, S., Ryan, J. V., Schreiber, D. K., Neeway, J. J., & Cabié, M. (2013) · Chemical Geology · doi:10.1016/j.chemgeo.2013.04.001 · Cited by 158
Self-citationThe surface chemistry of multi-oxide silicates
Oelkers, É. H., Golubev, S. V., Chaïrat, C., Сергеевич, П. О., & Schott, J. (2009) · Geochimica et Cosmochimica Acta · doi:10.1016/j.gca.2009.05.028 · Cited by 157
Criscenti, L. J., Kubicki, J. D., & Brantley, S. L. (2006) · The Journal of Physical Chemistry A · doi:10.1021/jp044360a · Cited by 149
The effect of composition on the leaching of three nuclear waste glasses: R7T7, AVM and VRZ
Frugier, P., Martin, C., Ribet, I., Advocat, T., & Gin, S. (2005) · Journal of Nuclear Materials · doi:10.1016/j.jnucmat.2005.06.023 · Cited by 142
Self-citationElemental and isotopic (29Si and 18O) tracing of glass alteration mechanisms
Valle, N., Verney‐Carron, A., Sterpenich, J., Libourel, G., Deloule, É., & Jollivet, P. (2010) · Geochimica et Cosmochimica Acta · doi:10.1016/j.gca.2010.03.028 · Cited by 141
The discovery and acceptance of the Kirkendall Effect: The result of a short research career
Nakajima, H. (1997) · JOM · doi:10.1007/bf02914706 · Cited by 140
Schott, J., Pokrovsky, O. S., Spalla, O., Devreux, F., Gloter, A., & Mielczarski, J. A. (2012) · Geochimica et Cosmochimica Acta · doi:10.1016/j.gca.2012.09.030 · Cited by 138
Leaching of borosilicate glasses. I. Experiments
Ledieu, A., Devreux, F., Barboux, P., Sicard, L., & Spalla, O. (2004) · Journal of Non-Crystalline Solids · doi:10.1016/j.jnoncrysol.2004.06.006 · Cited by 138
Relation between rates of aluminosilicate mineral dissolution, pH, temperature, and surface charge
Walther, J. V. (1996) · American Journal of Science · doi:10.2475/ajs.296.7.693 · Cited by 138
The controversial role of inter-diffusion in glass alteration
Gin, S., Neill, L., Fournier, M., Frugier, P., Ducasse, T., Tribet, M., Abdelouas, A., Parruzot, B., Neeway, J. J., & Wall, N. A. (2016) · Chemical Geology · doi:10.1016/j.chemgeo.2016.07.014 · Cited by 133
Self-citationGin, S., Jollivet, P., Rossa, G. B., Tribet, M., Mougnaud, S., Collin, M., Fournier, M., Cadel, E., Cabié, M., & Dupuy, L. (2016) · Geochimica et Cosmochimica Acta · doi:10.1016/j.gca.2016.12.029 · Cited by 130
Self-citationRimsza, J., Yeon, J., van Duin, A. C. T., & Du, J. (2016) · The Journal of Physical Chemistry C · doi:10.1021/acs.jpcc.6b07939 · Cited by 129
Self-citationThe Dissolution Rates of SiO2 Nanoparticles As a Function of Particle Size
Diedrich, T., Dybowska, A. D., Schott, J., Valsami‐Jones, E., & Oelkers, É. H. (2012) · Environmental Science & Technology · doi:10.1021/es2045053 · Cited by 104
Why Do Certain Glasses with a High Dissolution Rate Undergo a Low Degree of Corrosion?
Cailleteau, C., Devreux, F., Spalla, O., Angeli, F., & Gin, S. (2011) · The Journal of Physical Chemistry C · doi:10.1021/jp111458f · Cited by 100
Self-citationGlass dissolution rate measurement and calculation revisited
Fournier, M., Ull, A., Nicoleau, E., Inagaki, Y., Odorico, M., Frugier, P., & Gin, S. (2016) · Journal of Nuclear Materials · doi:10.1016/j.jnucmat.2016.04.028 · Cited by 100
Self-citationDissolution rates of talc as a function of solution composition, pH and temperature
Saldi, G. D., Köhler, S. J., Marty, N. C. M., & Oelkers, É. H. (2007) · Geochimica et Cosmochimica Acta · doi:10.1016/j.gca.2007.04.015 · Cited by 98
Long-term modeling of alteration-transport coupling: Application to a fractured Roman glass
Verney‐Carron, A., Gin, S., Frugier, P., & Libourel, G. (2010) · Geochimica et Cosmochimica Acta · doi:10.1016/j.gca.2010.01.001 · Cited by 93
Self-citationInvestigation of gel porosity clogging during glass leaching
Jollivet, P., Angeli, F., Cailleteau, C., Devreux, F., Frugier, P., & Gin, S. (2008) · Journal of Non-Crystalline Solids · doi:10.1016/j.jnoncrysol.2008.07.023 · Cited by 91
Self-citationAtomistic computer simulations of water interactions and dissolution of inorganic glasses
Du, J., & Rimsza, J. (2017) · npj Materials Degradation · doi:10.1038/s41529-017-0017-y · Cited by 85
Self-citationpH-dependent control of feldspar dissolution rate by altered surface layers
Wild, B., Daval, D., Guyot, F., Knauss, K. G., Pollet-Villard, M., & Imfeld, G. (2016) · Chemical Geology · doi:10.1016/j.chemgeo.2016.08.035 · Cited by 84
Electrochemical Stability of Magnesium Surfaces in an Aqueous Environment
Yuwono, J. A., Birbilis, N., Williams, K. S., & Medhekar, N. V. (2016) · The Journal of Physical Chemistry C · doi:10.1021/acs.jpcc.6b09232 · Cited by 79
Chapter 4. CHEMICAL WEATHERING RATES OF PYROXENES AND AMPHIBOLES
Brantley, S. L., & Chen, Y. (1995) · De Gruyter eBooks · doi:10.1515/9781501509650-006 · Cited by 79
Taylor, C. D., Neurock, M., & Scully, J. R. (2008) · Journal of The Electrochemical Society · doi:10.1149/1.2926598 · Cited by 76
Self-citationNanoscale Morphology and Atomic Structure of Passive Films on Stainless Steel
Massoud, T., Maurice, V., Klein, L. H., & Marcus, P. (2013) · Journal of The Electrochemical Society · doi:10.1149/2.067306jes · Cited by 76
Lecrivain, L., Gin, S., Ducasse, T., Echave, T. D., Fournier, M., Jollivet, P., Gourgiotis, A., & Wall, N. A. (2017) · npj Materials Degradation · doi:10.1038/s41529-017-0001-6 · Cited by 72
Self-citationThe effect of crystal size variation on the rate of dissolution – A kinetic Monte Carlo study
Briese, L. C., Arvidson, R. S., & Lüttge, A. (2017) · Geochimica et Cosmochimica Acta · doi:10.1016/j.gca.2017.06.010 · Cited by 69
The dissolution behavior of borosilicate glasses in far-from equilibrium conditions
Neeway, J. J., Rieke, P. C., Parruzot, B., Ryan, J. V., & Asmussen, R. M. (2018) · Geochimica et Cosmochimica Acta · doi:10.1016/j.gca.2018.02.001 · Cited by 64
Self-citationRimsza, J., & Du, J. (2017) · The Journal of Physical Chemistry C · doi:10.1021/acs.jpcc.7b02734 · Cited by 61
Self-citationContribution of zeolite-seeded experiments to the understanding of resumption of glass alteration
Fournier, M., Gin, S., Frugier, P., & Mercado-Depierre, S. (2017) · npj Materials Degradation · doi:10.1038/s41529-017-0018-x · Cited by 57
Self-citationEffect of natural and synthetic iron corrosion products on silicate glass alteration processes
Dillmann, P., Gin, S., Neff, D., Gentaz, L., & Rébiscoul, D. (2015) · Geochimica et Cosmochimica Acta · doi:10.1016/j.gca.2015.09.033 · Cited by 56
Self-citationNeeway, J. J., Kerisit, S., Liu, J., Zhang, J., Zhu, Z., Riley, B. J., & Ryan, J. V. (2016) · The Journal of Physical Chemistry C · doi:10.1021/acs.jpcc.6b03681 · Cited by 45
Self-citationStudies of (Cs,Ba)-hollandite dissolution under gamma irradiation at 95°C and at pH 2.5, 4.4 and 8.6
Suzuki‐Muresan, T., Vandenborre, J., Abdelouas, A., Grambow, B., & Utsunomiya, S. (2011) · Journal of Nuclear Materials · doi:10.1016/j.jnucmat.2011.09.001 · Cited by 27
Chen, Y., Brantley, S. L., & Ilton, E. S. (2000) · Chemical Geology · doi:10.1016/s0009-2541(99)00096-0 · Cited by 27
Jantzen, C. M., Trivelpiece, C. L., Crawford, C., Pareizs, J. M., & Pickett, J. B. (2017) · International Journal of Applied Glass Science · doi:10.1111/ijag.12264 · Cited by 26
Cited by
Water Electrolysis toward Elevated Temperature: Advances, Challenges and Frontiers
Zhang, W., Liu, M., Gu, X., Shi, Y., Deng, Z., & Cai, N. (2023) · Chemical Reviews · doi:10.1021/acs.chemrev.2c00573 · Cited by 441
Approaches to Disposal of Nuclear Waste
Ojovan, M. I., & Steinmetz, H. J. (2022) · Energies · doi:10.3390/en15207804 · Cited by 132
“Isolation of waste from near-surface processes and human activities.”
BackgroundCriado, M., Walkley, B., Ke, X., Provis, J. L., & Bernal, S. A. (2018) · Sustainability · doi:10.3390/su10124709 · Cited by 63
“However, the presence of sulfide or other redox-active components is generally believed to increase, rather than decrease, the dissolution rates of solids [21], so it is not very clear how such a mechanism would take place from a chemical perspective.”
BackgroundGong, K., & White, C. E. (2022) · Cement and Concrete Research · doi:10.1016/j.cemconres.2021.106642 · Cited by 21
Metadata
- Authors
- Frankel, G. S., Vienna, J. D., Lian, J., Scully, J. R., Gin, S., Ryan, J. V., Wang, J., Kim, S. H., Windl, W., & Du, J.
- Venue
- npj Materials Degradation
- Published
- 2018-05-03
- Volume
- 2
- Issue
- 1
- ISSN
- 2397-2106 (ISSN-L)
- OpenAlex
- W2800960419
- Cited by
- 276
- References
- 92
- FWCI
- 9.94
- Type
- journal article
- Language
- en
- Open access
- gold
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.