Guided cracks were successfully generated in an electrode using the concentrated surface stress of a prism-patterned Nafion membrane. An electrode with guided cracks was formed by stretching the catalyst-coated Nafion membrane. The morphological features of the stretched membrane electrode assembly (MEA) were investigated with respect to variation in the prism pattern dimension (prism pitches of 20 μm and 50 μm) and applied strain ( S ≈ 0.5 and 1.0). The behaviour of water on the surface of the cracked electrode was examined using environmental scanning electron microscopy. Guided cracks in the electrode layer were shown to be efficient water reservoirs and liquid water passages. The MEAs with and without guided cracks were incorporated into fuel cells, and electrochemical measurements were conducted. As expected, all MEAs with guided cracks exhibited better performance than conventional MEAs, mainly because of the improved water transport.

Overview

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Integrity signals

Registry

Crossref · 10.1038/s41598-018-19861-6

Cites

34 of 34 references verified0 citation errors · 0 not checkable

Statistics

Figures

Figure 1 Schematic illustration of guided crack generation in an electrode by stretching the prism-patterned membrane electrode assembly.
Figure 1 Schematic illustration of guided crack generation in an electrode by stretching the prism-patterned membrane electrode assembly.CC BY · PubMed Central
Figure 2 (a,b) SEM images of a Nafion membrane imprinted with a prism mould with a pitch of 20 μm (P-20 membrane) (a) and 50 μm (P-50 membrane) (b). (c,d) Stretching properties of the Nafion membranes: (c) strain–stress curves of the Nafion 212 membrane, 20 μm prism-patterned Nafion membrane, and 50 μm prism-patterned Nafion membrane measured by applying strain to the membranes (Inset: optical image showing the operation of the stretching machine); (d) ratio of height, width, and thickness changes of the Nafion membranes with varying strains (~0.5, ~1.0, and ~1.5).
Figure 2 (a,b) SEM images of a Nafion membrane imprinted with a prism mould with a pitch of 20 μm (P-20 membrane) (a) and 50 μm (P-50 membrane) (b). (c,d) Stretching properties of the Nafion membranes: (c) strain–stress curves of the Nafion 212 membrane, 20 μm prism-patterned Nafion membrane, and 50 μm prism-patterned Nafion membrane measured by applying strain to the membranes (Inset: optical image showing the operation of the stretching machine); (d) ratio of height, width, and thickness changes of the Nafion membranes with varying strains (~0.5, ~1.0, and ~1.5).CC BY · PubMed Central
Figure 3 Morphological features of the generated guided cracks: (a–d) SEM images of the cracks generated after applying strains (S) of ~0.5 and ~1.0 to the prism-patterned MEAs with pitches of 20 μm and 50 μm: (a) P-20 MEA with S ≈ 0.5, (b) P-20 MEA with S ≈ 1.0, (c) P-50 MEA with S ≈ 0.5, and (d) P-50 MEA with S ≈ 1.0. (e,f) Simulations of the stress distributions on the prism-patterned MEAs with pitches of 20 μm (e) and 50 μm (f).
Figure 3 Morphological features of the generated guided cracks: (a–d) SEM images of the cracks generated after applying strains (S) of ~0.5 and ~1.0 to the prism-patterned MEAs with pitches of 20 μm and 50 μm: (a) P-20 MEA with S ≈ 0.5, (b) P-20 MEA with S ≈ 1.0, (c) P-50 MEA with S ≈ 0.5, and (d) P-50 MEA with S ≈ 1.0. (e,f) Simulations of the stress distributions on the prism-patterned MEAs with pitches of 20 μm (e) and 50 μm (f).CC BY · PubMed Central
Figure 4 Schematic illustrations of the behaviour of generated water in the controlled cracks in the catalyst layer.
Figure 4 Schematic illustrations of the behaviour of generated water in the controlled cracks in the catalyst layer.CC BY · PubMed Central
Figure 5 ESEM images of water behaviour on a 20 µm cracked catalyst layer (strain ≈ 0.5) with respect to time: (a) 60 s, (b) 180 s, and (c) 360 s. The chamber pressure and substrate temperature were maintained at ~5.1 Torr and ~2 °C, respectively (RH = 95%).
Figure 5 ESEM images of water behaviour on a 20 µm cracked catalyst layer (strain ≈ 0.5) with respect to time: (a) 60 s, (b) 180 s, and (c) 360 s. The chamber pressure and substrate temperature were maintained at ~5.1 Torr and ~2 °C, respectively (RH = 95%).CC BY · PubMed Central
Figure 6 Electrochemical measurements of the MEAs: (a,b) Polarization curves of a conventional MEA and the MEAs with cracks generated using a 20 μm prism pattern (a) and a 50 μm prism pattern (b) with various strains (~0.5 and ~1.0) under H2/air. (c) Oxygen gains obtained under ambient pressure. (d) Cyclic voltammetry (CV) measurements of the prism-patterned MEAs with the same strain (~0.5) and a conventional MEA at the cathode catalyst layers (NHE = normal hydrogen electrode).
Figure 6 Electrochemical measurements of the MEAs: (a,b) Polarization curves of a conventional MEA and the MEAs with cracks generated using a 20 μm prism pattern (a) and a 50 μm prism pattern (b) with various strains (~0.5 and ~1.0) under H2/air. (c) Oxygen gains obtained under ambient pressure. (d) Cyclic voltammetry (CV) measurements of the prism-patterned MEAs with the same strain (~0.5) and a conventional MEA at the cathode catalyst layers (NHE = normal hydrogen electrode).CC BY · PubMed Central
Figure 7 Electrochemical impedance spectroscopy (EIS) measurements of prism-patterned MEAs with the same strain (~0.5) and a conventional MEA at 0.6 V vs. a reversible hydrogen electrode (a) and at 1.6 A cm−2 (b). (c) Equivalent circuit of the PEMFC (L1 = inductance of the electric wire, R1 = internal membrane resistance, R3 (2) = charge transfer resistance of the cathode (anode), CPE2 (1) = constant phase element of the cathode (anode), and W1 = Warburg impedance).
Figure 7 Electrochemical impedance spectroscopy (EIS) measurements of prism-patterned MEAs with the same strain (~0.5) and a conventional MEA at 0.6 V vs. a reversible hydrogen electrode (a) and at 1.6 A cm−2 (b). (c) Equivalent circuit of the PEMFC (L1 = inductance of the electric wire, R1 = internal membrane resistance, R3 (2) = charge transfer resistance of the cathode (anode), CPE2 (1) = constant phase element of the cathode (anode), and W1 = Warburg impedance).CC BY · PubMed Central

Verification

Claims the paper makes

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Claims other papers make about this one

Each is checked against this paper’s own text: does it say what the citing paper says it does?

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

The self-check needs the paper’s full text.

Citations

Cites

Show all 34 references

Cited by

See all 82

Metadata

Authors
Ahn, C.-Y., Jang, S., Cho, Y.-H., Choi, J., Kim, S., Kim, S. M., Sung, Y.-E., & Choi, M.
Affiliations
  • Seoul National University (KR)
  • Kangwon National University (KR)
Corresponding author
  • Kim, Sungjun
  • Kim, Sang Moon
  • Sung, Yung-Eun
  • Choi, Mansoo
Venue
Scientific Reports
Published
2018-01-19
Volume
8
Issue
1
Pages
1257-1257
ISSN
2045-2322 (ISSN-L)
OpenAlex
W2783645472
Cited by
80
References
34
Citations by year
2026: 8 · 2025: 15 · 2024: 11 · 2023: 9 · 2022: 13 · 2021: 12 · 2020: 4 · 2019: 6 · 2018: 2
FWCI
2.30
Type
journal article
Language
en
Open access
Licence
Locations
  • Scientific Reports (publishedVersion, cc-by)
  • PubMed Central (publishedVersion, cc-by)
  • PubMed (publishedVersion)
  • DOAJ (DOAJ: Directory of Open Access Journals) (submittedVersion)
  • Seoul National University Open Repository (Seoul National University) (submittedVersion)
Funders
  • National Research Foundation (2012M3A6A7054855)
  • National Research Foundation of Korea (2016R1C1B1014564, 2012M3A6A7054855, IBS-R006-A2)
  • Ministry of Education, Science and Technology (2012M3A6A7054855)
  • Institute for Basic Science (IBS−R006-A2, R006‐A2, 2016R1C1B1014564, 2016R1D1A3B03934752)
Topics
  • Physical Sciences › Engineering › Electrical and Electronic Engineering › Fuel Cells and Related Materials
  • Physical Sciences › Materials Science › Materials Chemistry › Advancements in Solid Oxide Fuel Cells
  • Physical Sciences › Chemical Engineering › Filtration and Separation › Membrane-based Ion Separation Techniques
Keywords
membrane electrode assembly, Nafion membrane, membrane stretching, catalyst coated membranes, surface stress, water transport, water reservoirs, fuel cell performance

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

How to cite

Cite CoChat for the checks on this page, and the paper for its own findings.

This page
CoChat. (2026). Citation check: Guided cracking of electrodes by stretching prism-patterned membrane electrode assemblies for high-performance fuel cells. https://app.cochat.ai/papers/10.1038/s41598-018-19861-6
The paper
Ahn, C.-Y., Jang, S., Cho, Y.-H., Choi, J., Kim, S., Kim, S. M., Sung, Y.-E., & Choi, M. (2018). Guided cracking of electrodes by stretching prism-patterned membrane electrode assemblies for high-performance fuel cells. Scientific Reports. https://doi.org/10.1038/s41598-018-19861-6

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.