Abstract
Natural materials such as bone, tooth, and nacre are nanocomposites of proteins and minerals with superior strength. Why is the nanometer scale so important to such materials? Can we learn from this to produce superior nanomaterials in the laboratory? These questions motivate the present study where we show that the nanocomposites in nature exhibit a generic mechanical structure in which the nanometer size of mineral particles is selected to ensure optimum strength and maximum tolerance of flaws (robustness). We further show that the widely used engineering concept of stress concentration at flaws is no longer valid for nanomaterial design.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
The source backs part of the claim, not all of it — or backs it for a different population, condition or comparison.
In the citing paper
“This considerable tensile strength of limpet teeth is attributed to a high mineral volume fraction of reinforcing goethite nanofibres with diameters below a defect-controlled critical size, suggesting that natural design in limpet teeth is optimized towards theoretical strength limits.”
From Extreme strength observed in limpet teeth (2015) · cites this paper as [5]
Experimental — accuracy not yet measuredThe source backs part of the claim, not all of it — or backs it for a different population, condition or comparison.
In the citing paper
“Limpet teeth therefore present a natural structure with the potential to optimize composite strength towards a theoretical maximum by the incorporation of nanofibre constituents below a critical size that defines tolerance to flaws [5].”
From Extreme strength observed in limpet teeth (2015) · cites this paper as [5]
Experimental — accuracy not yet measuredThe source backs part of the claim, not all of it — or backs it for a different population, condition or comparison.
In the citing paper
“The lack of a significant change in the tensile strength of limpet tooth samples in figure 6, despite a fourfold increase in the length of the sample, suggest the mineral phase within the limpet tooth is below a flaw tolerant critical size of approximately 30 nm, as reported in previous literature [5].”
From Extreme strength observed in limpet teeth (2015) · cites this paper as [5]
Experimental — accuracy not yet measuredThe cited source says what the claim attributes to it.
In the citing paper
“The results in figure 6 therefore show that limpet teeth material shows tolerance to flaws as proposed by previous work [5].”
From Extreme strength observed in limpet teeth (2015) · cites this paper as [5]
The cited source says what the claim attributes to it.
In the citing paper
“Specifically, the reinforcing mineral phase in many organisms approaches nanometre length scales, at least in one-dimension, which has been proposed as promoting flaw insensitivity to increase the tensile strength of mineralized tissue [5].”
From Extreme strength observed in limpet teeth (2015) · cites this paper as [5]
2 more claims about this paper
Create a free account to see every claim other papers make about this one.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
THE MATERIAL BONE: Structure-Mechanical Function Relations
Weiner, S., & Wagner, H. D. (1998) · Annual Review of Materials Science · doi:10.1146/annurev.matsci.28.1.271 · Cited by 2,724
Mechanical properties and the hierarchical structure of bone
Rho, J.-Y., Kuhn-Spearing, L., & Zioupos, P. (1998) · Medical Engineering & Physics · doi:10.1016/s1350-4533(98)00007-1 · Cited by 2,588
The mechanical design of nacre
Jackson, A. P., Vincent, J. F. V., & Turner, R. M. (1988) · Proceedings of the Royal Society of London. Series B. Biological Sciences · doi:10.1098/rspb.1988.0056 · Cited by 1,269
Molecular mechanistic origin of the toughness of natural adhesives, fibres and composites
Smith, B. L., Schäffer, T. E., Viani, M., Thompson, J. B., Frederick, N. A., Kindt, J., Belcher, A., Stucky, G. D., Morse, D. E., & Hansma, P. K. (1999) · Nature · doi:10.1038/21607 · Cited by 1,218
Direct Measurements of the Surface Energies of Crystals
Gilman, J. J. (1960) · Journal of Applied Physics · doi:10.1063/1.1735524 · Cited by 837
Deformation mechanisms in nacre
Wang, R. Z., Suo, Z., Evans, A. G., Yao, N., & Aksay, I. A. (2001) · Journal of Materials Research · doi:10.1557/jmr.2001.0340 · Cited by 835
Mineralized Collagen Fibrils: A Mechanical Model with a Staggered Arrangement of Mineral Particles
Jäger, I., & Fratzl, P. (2000) · Biophysical Journal · doi:10.1016/s0006-3495(00)76426-5 · Cited by 793
Self-citationMechanical properties of mother of pearl in tension
Currey, J. D. (1977) · Proceedings of the Royal Society of London. Series B. Biological Sciences · doi:10.1098/rspb.1977.0050 · Cited by 722
Structural basis for the fracture toughness of the shell of the conch Strombus gigas
Kamat, S., Su, X., Ballarini, R., & Heuer, A. H. (2000) · Nature · doi:10.1038/35016535 · Cited by 714
Nucleation and inhibition of hydroxyapatite formation by mineralized tissue proteins
HUNTER, G. K., HAUSCHKA, P. V., POOLE, R. A., ROSENBERG, L. C., & GOLDBERG, H. A. (1996) · Biochemical Journal · doi:10.1042/bj3170059 · Cited by 621
Research works printed but not linked: 2
- Taylor J D. Palaeontology. 1973;16:519–534. [Google Scholar]
- Kessler H, Ballarini R, Mullen R L, Kuhn L T, Heuer A H. Comput Mater Sci. 1996;5:157–166. [Google Scholar]
Cited by
Items 101–200 of 1,000
Nanoconfinement of Spider Silk Fibrils Begets Superior Strength, Extensibility, and Toughness
Giesa, T., Arslan, M., Pugno, N. M., & Buehler, M. J. (2011) · Nano Letters · doi:10.1021/nl203108t · Cited by 274
Influence of Aspect Ratio on Barrier Properties of Polymer-Clay Nanocomposites
Lu, C., & Mai, Y. (2005) · Physical Review Letters · doi:10.1103/physrevlett.95.088303 · Cited by 274
Mechanical properties of graphene papers
Liu, Y., Xie, B., Zhang, Z., Zheng, Q., & Xu, Z. (2012) · Journal of the Mechanics and Physics of Solids · doi:10.1016/j.jmps.2012.01.002 · Cited by 272
“ng superior stiffness, strength and energy dissipation capacities are reported as the next-generation multifunctional super-materials (Buehler, 2006; Dunlop and Fratzl, 2010; Fratzl and Weiner, 2010; Gao et al., 2003; Ji and Gao, 2004, 2010; Kotov, 2006; Rafiee et al., 2009). For example, super-strong nanofibers such…”
BackgroundInfluentialHigh-resolution AFM imaging of intact and fractured trabecular bone
Hassenkam, T., Fantner, G. E., Cutroni, J. A., Weaver, J. C., Morse, D. E., & Hansma, P. K. (2004) · Bone · doi:10.1016/j.bone.2004.02.024 · Cited by 270
“An important aspect of this challenge is understanding of the nanoscopic interplay between the basic building blocks of bone [7,8].”
BackgroundDorozhkin, S. V. (2009) · Materials · doi:10.3390/ma2041975 · Cited by 267
“mechanical structure in which the nanometer sizes of mineral particles are used to ensure the optimum strength and maximum tolerance of flaws [196,197].”
BackgroundRepair of enamel by using hydroxyapatite nanoparticles as the building blocks
Li, L., Pan, H., Tao, J., Xu, X., Mao, C., Gu, X., & Tang, R. (2008) · Journal of Materials Chemistry · doi:10.1039/b806090h · Cited by 266
Dilatational band formation in bone
Poundarik, A. A., Diab, T., Sroga, G. E., Ural, A., Boskey, A. L., Gundberg, C. M., & Vashishth, D. (2012) · Proceedings of the National Academy of Sciences · doi:10.1073/pnas.1201513109 · Cited by 265
“Stick/slip-type matrix flow (13) and the presence of a “crack-like flaw” within mineral crystals of bone (16) have also been invoked to explain the remarkable strength of bone.”
BackgroundThe hidden structure of human enamel
Beniash, E., Stifler, C. A., Sun, C.-Y., Jung, G. S., Qin, Z., Buehler, M. J., & Gilbert, P. U. P. A. (2019) · Nature Communications · doi:10.1038/s41467-019-12185-7 · Cited by 265
Toughness amplification in natural composites
Barthelat, F., & Rabiei, R. (2011) · Journal of the Mechanics and Physics of Solids · doi:10.1016/j.jmps.2011.01.001 · Cited by 265
Bone quality: where do we go from here?
Bouxsein, M. L. (2003) · Osteoporosis International · doi:10.1007/s00198-003-1489-x · Cited by 264
Tran, P., Ngo, T. D., Ghazlan, A., & Hui, D. (2017) · Composites Part B: Engineering · doi:10.1016/j.compositesb.2016.09.083 · Cited by 261
Artful interfaces within biological materials
Dunlop, J. W. C., Weinkamer, R., & Fratzl, P. (2011) · Materials Today · doi:10.1016/s1369-7021(11)70056-6 · Cited by 261
Self-citationOn optimal hierarchy of load-bearing biological materials
Zhang, Z., Zhang, Y.-W., & Gao, H. (2011) · Proceedings of the Royal Society B: Biological Sciences · doi:10.1098/rspb.2010.1093 · Cited by 259
Self-citationThree Structural Roles for Water in Bone Observed by Solid-State NMR
Wilson, E. E., Awonusi, A., Morris, M. D., Kohn, D. H., Tecklenburg, M. M. J., & Beck, L. W. (2006) · Biophysical Journal · doi:10.1529/biophysj.105.070243 · Cited by 256
Calcium phosphate bone graft substitutes: Failures and hopes
Bohner, M., Galea, L., & Doebelin, N. (2012) · Journal of the European Ceramic Society · doi:10.1016/j.jeurceramsoc.2012.02.028 · Cited by 256
Arzt, E., Quan, H., McMeeking, R. M., & Hensel, R. (2021) · Progress in Materials Science · doi:10.1016/j.pmatsci.2021.100823 · Cited by 253
Self-citationA review on application of mechanical metamaterials for vibration control
Dalela, S., Balaji, P. S., & Jena, D. P. (2021) · Mechanics of Advanced Materials and Structures · doi:10.1080/15376494.2021.1892244 · Cited by 253
The structure and mechanics of bone
Currey, J. D. (2012) · Journal of Materials Science · doi:10.1007/s10853-011-5914-9 · Cited by 251
Flaw Insensitive Fracture in Nanocrystalline Graphene
Zhang, T., Li, X., Kadkhodaei, S., & Gao, H. (2012) · Nano Letters · doi:10.1021/nl301908b · Cited by 251
Self-citationDentin matrix protein 1 induces cytodifferentiation of dental pulp stem cells into odontoblasts
Almushayt, A., Narayanan, K., Zaki, A. E., & George, A. (2006) · Gene Therapy · doi:10.1038/sj.gt.3302687 · Cited by 250
Powering Nanodevices with Biomolecular Motors
Hess, H., Bachand, G. D., & Vogel, V. (2004) · Chemistry – A European Journal · doi:10.1002/chem.200305712 · Cited by 249
Hydrogel Actuators and Sensors for Biomedical Soft Robots: Brief Overview with Impending Challenges
Banerjee, H., Suhail, M., & Ren, H. (2018) · Biomimetics · doi:10.3390/biomimetics3030015 · Cited by 249
“Finally, to quantify the flaw-sensitive length scale of a polymer as given in principle (iii), it can be harnessed as the following critical length scale [290,291]:”
BackgroundWhy are so many adhesive pads hairy?
Federle, W. (2006) · Journal of Experimental Biology · doi:10.1242/jeb.02323 · Cited by 249
“Similar concepts have been applied to the detachment of adhesive setae (Gao et al., 2003; Gao and Yao, 2004; Hui et al., 2004).”
BackgroundHierarchically Structured Nanomaterials for Electrochemical Energy Conversion
Trogadas, P., Ramani, V., Strasser, P., Fuller, T. F., & Coppens, M. (2016) · Angewandte Chemie International Edition · doi:10.1002/anie.201506394 · Cited by 245
Energy absorbent natural materials and bioinspired design strategies: A review
McKittrick, J., Chen, P.-Y., Tombolato, L., Novitskaya, E. E., Trim, M. W., Hirata, G. A., Olevsky, E. A., Horstemeyer, M. F., & Meyers, M. A. (2010) · Materials Science and Engineering: C · doi:10.1016/j.msec.2010.01.011 · Cited by 240
Deformation and Fracture Mechanisms of Bone and Nacre
Wang, R., & Gupta, H. S. (2011) · Annual Review of Materials Research · doi:10.1146/annurev-matsci-062910-095806 · Cited by 238
The bone mineralization density distribution as a fingerprint of the mineralization process
Ruffoni, D., Fratzl, P., Roschger, P., Klaushofer, K., & Weinkamer, R. (2007) · Bone · doi:10.1016/j.bone.2007.01.012 · Cited by 235
“The mean mineral content of the bone matrix and the heterogeneity of the mineralization, together with its spatial distribution are all fundamental factors for bone material quality since they affect the basic mechanical properties of bone tissue: the stiffness, the strength and the toughness [1–6].”
BackgroundSelf-citationThe role of mechanics in biological and bio-inspired systems
Egan, P., Sinko, R., LeDuc, P. R., & Keten, S. (2015) · Nature Communications · doi:10.1038/ncomms8418 · Cited by 234
Biominerals—hierarchical nanocomposites: the example of bone
Beniash, E. (2011) · WIREs Nanomedicine and Nanobiotechnology · doi:10.1002/wnan.105 · Cited by 233
Lightweight, flaw-tolerant, and ultrastrong nanoarchitected carbon
Zhang, X., Vyatskikh, A., Gao, H., Greer, J. R., & Li, X. (2019) · Proceedings of the National Academy of Sciences · doi:10.1073/pnas.1817309116 · Cited by 230
“Existing theoretical, computational, and experimental studies (4, 38, 39) demonstrated that brittle materials become insensitive to flaws when their dimensions are reduced below a critical size, which drives their strength toward theoretical limit.”
BackgroundSelf-citationThe biomechanics of seed germination
Steinbrecher, T., & Leubner-Metzger, G. (2016) · Journal of Experimental Botany · doi:10.1093/jxb/erw428 · Cited by 228
Size-dependence of the dielectric breakdown strength from nano- to millimeter scale
Neusel, C., & Schneider, G. A. (2013) · Journal of the Mechanics and Physics of Solids · doi:10.1016/j.jmps.2013.09.009 · Cited by 228
“Also in the mechanical case, the transition from a thickness-independent to a thickness-dependent regime is used to estimate the length of the failure-initiating cracks (Gao et al. 2003).”
MethodThe nanocomposite nature of bone drives its strength and damage resistance
Tertuliano, O. A., & Greer, J. R. (2016) · Nature Materials · doi:10.1038/nmat4719 · Cited by 227
Gupta, H. S., Schratter, S., Tesch, W., Roschger, P., Berzlanovich, A., Schoeberl, T., Klaushofer, K., & Fratzl, P. (2005) · Journal of Structural Biology · doi:10.1016/j.jsb.2004.10.010 · Cited by 224
“3 with the predicted values from the staggered model arrangement of mineral particles in a collagenous matrix (Gao et al., 2003; Jager and Fratzl, 2000).”
BackgroundSelf-citationMicromechanical models to guide the development of synthetic ‘brick and mortar’ composites
Begley, M. R., Philips, N. R., Compton, B. G., Wilbrink, D. V., Ritchie, R. O., & Utz, M. (2012) · Journal of the Mechanics and Physics of Solids · doi:10.1016/j.jmps.2012.03.002 · Cited by 222
“…is arguably straightforward (e.g. Jackson et al., 1988; Espinosa et al., 2009; Jager and Fratzl, 2000; Currey et al., 2001; Evans et al., 2001; Gao et al., 2003; Ji and Gao, 2004a,b; Barthelat et al., 2006; Tang et al., 2007; Rabiei et al., 2010; Wang and Boyce, 2010; Zhang et al., 2010,…”
BackgroundInfluentialSu, Y., Ji, B., Zhang, K., Gao, H., Huang, Y., & Hwang, K. (2010) · Langmuir · doi:10.1021/la9036452 · Cited by 221
Self-citationWei, X., Naraghi, M., & Espinosa, H. D. (2012) · ACS Nano · doi:10.1021/nn204506d · Cited by 221
“The characteristic overlap length in eq 24 takes the identical form to that reported by Gao et al.(15) However, we want to emphasize the solution in eq 24 comes from a rigorous derivation and is a specific solution in the plastic regime.”
MethodInfluentialShao, C., Zhao, R., Jiang, S., Yao, S., Wu, Z., Jin, B., Yang, Y., Pan, H., & Tang, R. (2018) · Advanced Materials · doi:10.1002/adma.201704876 · Cited by 219
Li, S., Niu, J., Zhao, Y. C., So, K. P., Wang, C., Wang, C. A., & Li, J. (2015) · Nature Communications · doi:10.1038/ncomms8872 · Cited by 214
RetractedGuan, F., Xie, Y., Wu, H., Meng, Y., Shi, Y., Gao, M., Zhang, Z., Chen, S., Chen, Y., Wang, H., et al. (2020) · ACS Nano · doi:10.1021/acsnano.0c06063 · Cited by 214
Extreme strength observed in limpet teeth
Barber, A. H., Lu, D., & Pugno, N. M. (2015) · Journal of the Royal Society Interface · doi:10.1098/rsif.2014.1326 · Cited by 212
“below a flaw tolerant critical size of ∼30 nm, as reported in previous literature [5].”
BackgroundResultInfluentialBioinspired Design Criteria for Damage‐Resistant Materials with Periodically Varying Microstructure
Kolednik, O., Predan, J., Fischer, F. D., & Fratzl, P. (2011) · Advanced Functional Materials · doi:10.1002/adfm.201100443 · Cited by 211
Self-citationInspiration from Nature's body armours – A review of biological and bioinspired composites
Ghazlan, A., Ngo, T., Tan, P., Xie, Y. M., Tran, P., & Donough, M. (2021) · Composites Part B: Engineering · doi:10.1016/j.compositesb.2020.108513 · Cited by 211
Chemical gradients in human enamel crystallites
DeRocher, K. A., Smeets, P. J. M., Goodge, B. H., Zachman, M. J., Balachandran, P. V., Stegbauer, L., Cohen, M. J., Gordon, L. M., Rondinelli, J. M., Kourkoutis, L. F., et al. (2020) · Nature · doi:10.1038/s41586-020-2433-3 · Cited by 210
Barthelat, F. (2015) · International Materials Reviews · doi:10.1179/1743280415y.0000000008 · Cited by 209
“In particular, the nanoscopic size of the hard inclusions they contain imparts them to extremely high strength.(55) Examples include the nanosize of hydroxyapatite crystals in bone,(55) the b-sheet nanocrystals of proteins in spider silk,(56) the cellulose nanocrystals in plant(57) or of the nanofibres of the mineral…”
BackgroundStress generation during lithiation of high-capacity electrode particles in lithium ion batteries
Huang, S., Fan, F., Li, J., Zhang, S., & Zhu, T. (2013) · Acta Materialia · doi:10.1016/j.actamat.2013.04.007 · Cited by 209
Deformation behavior of brittle/ductile multilayered composites under interface constraint effect
Wu, H., Fan, G., Huang, M., Geng, L., Cui, X., & Xie, H. (2016) · International Journal of Plasticity · doi:10.1016/j.ijplas.2016.11.005 · Cited by 208
Sen, D., & Buehler, M. J. (2011) · Scientific Reports · doi:10.1038/srep00035 · Cited by 207
A Model for the Ultrastructure of Bone Based on Electron Microscopy of Ion-Milled Sections
McNally, E. A., Schwarcz, H. P., Botton, G. A., & Arsenault, A. L. (2012) · PLoS ONE · doi:10.1371/journal.pone.0029258 · Cited by 206
Advances in mechanics of hierarchical composite materials
Chen, Y., Ma, Y., Yin, Q., Pan, F., Cui, C., Zhang, Z., & Liu, B. (2021) · Composites Science and Technology · doi:10.1016/j.compscitech.2021.108970 · Cited by 205
Biological materials: A materials science approach
Meyers, M. A., Chen, P.-Y., Lopez, M. I., Seki, Y., & Lin, A. Y. M. (2011) · Journal of the Mechanical Behavior of Biomedical Materials · doi:10.1016/j.jmbbm.2010.08.005 · Cited by 204
Barthelat, F. (2014) · Journal of the Mechanics and Physics of Solids · doi:10.1016/j.jmps.2014.08.008 · Cited by 207
Nature-inspired adhesive systems
Li, M., Mao, A., Guan, Q., & Saiz, E. (2024) · Chemical Society Reviews · doi:10.1039/d3cs00764b · Cited by 203
Bhandakkar, T. K., & Gao, H. (2010) · International Journal of Solids and Structures · doi:10.1016/j.ijsolstr.2010.02.001 · Cited by 202
“We note that the concept of flaw tolerant electrodes at nanoscale is reminiscent of biological nanocomposites such as bone in which evolution may have selected the basic structural units to be at nanoscale for flaw tolerance (Gao et al., 2003).”
BackgroundSelf-citationLe, J.-L., Bažant, Z. P., & Bazant, M. Z. (2011) · Journal of the Mechanics and Physics of Solids · doi:10.1016/j.jmps.2011.03.002 · Cited by 199
“In highly orthotropic materials such as uniaxial fiber composites and biological nanocomposites (Gao et al., 2003; Chen et al., 2007), the problem is more complicated, since the length and width of the RVE are not the same.”
BackgroundFracture of graphene: a review
Zhang, T., Li, X., & Gao, H. (2015) · International Journal of Fracture · doi:10.1007/s10704-015-0039-9 · Cited by 199
“…17.16 nm, i.e., the strip will always fail at the theoretical strength regardless of the flaw size, a state commonly referred to as flaw tolerance (Gao et al. 2003; Gao and Chen 2005; Kumar et al. 2009; Keten et al. 2010; Kumar et al. 2011; Qin and Buehler 2011; Kumar et al. 2013; Gu et al.…”
BackgroundInfluentialSelf-citationInterfibrillar shear stress is the loading mechanism of collagen fibrils in tendon
Szczesny, S. E., & Elliott, D. M. (2014) · Acta Biomaterialia · doi:10.1016/j.actbio.2014.01.032 · Cited by 200
“While formulations of shear lag models have been applied to several biological tissues [21] [22] [23] [24] [25] [26] [27] [28] [29] [30] [31] [32] [33], this is the first time to our knowledge that a shear lag model has been applied to data obtained from multiscale tendon testing.”
Zhang, Z., Liu, B., Huang, Y., Hwang, K., & Gao, H. (2010) · Journal of the Mechanics and Physics of Solids · doi:10.1016/j.jmps.2010.07.004 · Cited by 198
Self-citationLee, N., Horstemeyer, M. F., Rhee, H., Nabors, B., Liao, J., & Williams, L. N. (2014) · Journal of The Royal Society Interface · doi:10.1098/rsif.2014.0274 · Cited by 197
“The overlapping structure induces a physical restraint against free movement of the blocks, and hence it does not allow crack propagation, thus providing a greater fracture toughness and robustness to biological materials [37–39].”
BackgroundCellulose nanocomposites by supramolecular chemistry engineering
Chen, L., Yu, L., Qi, L., Eichhorn, S. J., Isogai, A., Lizundia, E., Zhu, J. Y., & Chen, C. (2025) · Nature Reviews Materials · doi:10.1038/s41578-025-00810-5 · Cited by 196
“At the nanoscale, defects are decreased to the extent that the materials theoretically become insensitive to any flaws, yielding high modulus and strength 145 .”
Programmable multi-physical mechanics of mechanical metamaterials
Sinha, P., & Mukhopadhyay, T. (2023) · Materials Science and Engineering: R: Reports · doi:10.1016/j.mser.2023.100745 · Cited by 196
“The reduction in material scale in design essentially amplifies the mechanical characteristics of material [27,28].”
Bio-mimetic mechanisms of natural hierarchical materials: A review
Chen, Q., & Pugno, N. M. (2013) · Journal of the Mechanical Behavior of Biomedical Materials · doi:10.1016/j.jmbbm.2012.10.012 · Cited by 196
“Following this model, Gao et al. (2003) reported that the strength and toughness of natural composites materials, including nacre and bone, are insensitive to flaws at nano-scale, which is called principle of flaw-tolerance; this principle plays an important role in determining the materials’ high…”
BackgroundBUEHLER, M., KETEN, S., & ACKBAROW, T. (2008) · Progress in Materials Science · doi:10.1016/j.pmatsci.2008.06.002 · Cited by 194
Ultrastrong and High Thermal Insulating Porous High‐Entropy Ceramics up to 2000 °C
Wen, Z., Tang, Z., Liu, Y., Zhuang, L., Yu, H., & Chu, Y. (2024) · Advanced Materials · doi:10.1002/adma.202311870 · Cited by 192
Mechanical Principles of Biological Nanocomposites
Ji, B., & Gao, H. (2010) · Annual Review of Materials Research · doi:10.1146/annurev-matsci-070909-104424 · Cited by 191
Self-citationChoi, G., Jin, J., Shin, D., Kim, Y. H., Ko, J., Im, H., Jang, J., Jang, D., & Bae, B. (2017) · Advanced Materials · doi:10.1002/adma.201700205 · Cited by 190
The mechanics of tessellations – bioinspired strategies for fracture resistance
Fratzl, P., Kolednik, O., Fischer, F. D., & Dean, M. N. (2016) · Chemical Society Reviews · doi:10.1039/c5cs00598a · Cited by 189
Self-citationWu, K., Song, Z., Zhang, S., Ni, Y., Cai, S., Gong, X., He, L., & Yu, S.-H. (2020) · Proceedings of the National Academy of Sciences · doi:10.1073/pnas.2000639117 · Cited by 189
Kannan, R. Y., Salacinski, H. J., Odlyha, M., Butler, P. E., & Seifalian, A. M. (2006) · Biomaterials · doi:10.1016/j.biomaterials.2005.10.006 · Cited by 187
Hierarchies in Biomineral Structures
Currey, J. D. (2005) · Science · doi:10.1126/science.1113954 · Cited by 185
Nanotwin-governed toughening mechanism in hierarchically structured biological materials
Shin, Y. A., Yin, S., Li, X., Lee, S., Moon, S., Jeong, J., Kwon, M., Yoo, S. J., Kim, Y.-M., Zhang, T., et al. (2016) · Nature Communications · doi:10.1038/ncomms10772 · Cited by 182
Self-citationVincent, J. F. V. (2009) · Proceedings of the Institution of Mechanical Engineers, Part H: Journal of Engineering in Medicine · doi:10.1243/09544119jeim561 · Cited by 181
Li, L., & Christine Ortiz, B. (2014) · Nature Materials · doi:10.1038/nmat3920 · Cited by 181
Hyperelasticity with softening for modeling materials failure
VOLOKH, K. (2007) · Journal of the Mechanics and Physics of Solids · doi:10.1016/j.jmps.2007.02.012 · Cited by 180
Dreyer, A., Feld, A., Kornowski, A., Yilmaz, E. D., Noei, H., Meyer, A., Krekeler, T., Jiao, C., Stierle, A., Abetz, V., et al. (2016) · Nature Materials · doi:10.1038/nmat4553 · Cited by 180
Biomimetic additive manufactured polymer composites for improved impact resistance
Gu, G. X., Takaffoli, M., Hsieh, A. J., & Buehler, M. J. (2016) · Extreme Mechanics Letters · doi:10.1016/j.eml.2016.09.006 · Cited by 180
“Nacre, the featured biological composite of this study, is composed of 95 wt% mineral content and 5 wt% soft biopolymeric matrix structured in a brickand-mortar arrangement [14,19].”
BackgroundHe, G., Gajjeraman, S., Schultz, D. G., Cookson, D., Qin, C., Butler, W. T., Hao, J., & George, A. (2005) · Biochemistry · doi:10.1021/bi051045l · Cited by 181
“The rigidity and compressive strength of bone and dentin are directly dependent upon temporally and spatially controlled mineral nucleation and hierarchically assembled matrix (2,3).”
BackgroundPark, J., Lee, Y., Barbee, M. H., Cho, S., Cho, S., Shanker, R., Kim, J., Myoung, J., Kim, M. P., Baig, C., et al. (2019) · Advanced Materials · doi:10.1002/adma.201808148 · Cited by 178
Hydraulic fracture during epithelial stretching
Casares, L., Vincent, R., Zalvidea, D., Campillo, N., Navajas, D., Arroyo, M., & Trepat, X. (2015) · Nature Materials · doi:10.1038/nmat4206 · Cited by 176
“Interestingly, other biological materials such as protein materials 44 or nacre 45,46 also enhance toughness by distributed cracking, using however seemingly unrelated mechanisms and architectures 47 .”
Mineral Changes in Osteoporosis: A Review
Faibish, D., Ott, S. M., & Boskey, A. L. (2006) · Clinical Orthopaedics & Related Research · doi:10.1097/01.blo.0000200241.14684.4e · Cited by 156
“Increased bone mineral particle size is associated with increased bone fragility(27); crystals that are too small do not reinforce the bone composite, suggesting there also is an optimal size range for bone mineral crystals.(50) Compositional changes may be caused by alterations in crystal size (smaller crystals have…”
BackgroundIntrafibrillar Collagen Mineralization Produced by Biomimetic Hierarchical Nanoapatite Assembly
Liu, Y., Li, N., Qi, Y., Dai, L., Bryan, T. E., Mao, J., Pashley, D. H., & Tay, F. R. (2011) · Advanced Materials · doi:10.1002/adma.201003882 · Cited by 175
Bone‐Inspired Materials by Design: Toughness Amplification Observed Using 3D Printing and Testing
Libonati, F., Gu, G. X., Qin, Z., Vergani, L., & Buehler, M. J. (2016) · Advanced Engineering Materials · doi:10.1002/adem.201600143 · Cited by 175
Podsiadlo, P., Tang, Z., Shim, B. S., & Kotov, N. A. (2007) · Nano Letters · doi:10.1021/nl0700649 · Cited by 175
Intermolecular channels direct crystal orientation in mineralized collagen
Xu, Y., Nudelman, F., Eren, E. D., Wirix, M. J. M., Cantaert, B., Nijhuis, W. H., Hermida-Merino, D., Portale, G., Bomans, P. H. H., Ottmann, C., et al. (2020) · Nature Communications · doi:10.1038/s41467-020-18846-2 · Cited by 174
Nanolaminates Utilizing Size‐Dependent Homogeneous Plasticity of Metallic Glasses
Kim, J., Jang, D., & Greer, J. R. (2011) · Advanced Functional Materials · doi:10.1002/adfm.201101164 · Cited by 172
Development of Biomedical Polymer-Silicate Nanocomposites: A Materials Science Perspective
Wu, C., Gaharwar, A. K., Schexnailder, P. J., & Schmidt, G. (2010) · Materials · doi:10.3390/ma3052986 · Cited by 177
“Unique combinations of hard and soft components found in biological tissues inspired materials researchers to design and develop polymer nanocomposites with improved mechanical properties [13,22,25-28].”
BackgroundJroundi, F., Schiro, M., Ruíz-Agudo, E., Elert, K., Martín-Sánchez, I., González‐Muñoz, M. T., & Rodriguez-Navarro, C. M. (2017) · Nature Communications · doi:10.1038/s41467-017-00372-3 · Cited by 172
Impact‐Resistant Hydrogels by Harnessing 2D Hierarchical Structures
Liang, X., Chen, G., Lei, I. M., Zhang, P., Wang, Z., Chen, X., Lu, M., Zhang, J., Wang, Z., Sun, T., et al. (2022) · Advanced Materials · doi:10.1002/adma.202207587 · Cited by 174
Designing toughness and strength for soft materials
Zhao, X. (2017) · Proceedings of the National Academy of Sciences · doi:10.1073/pnas.1710942114 · Cited by 171
Size-Dependent Brittle-to-Ductile Transition in Silica Glass Nanofibers
Luo, J., Wang, J., Bitzek, E., Huang, J. Y., Zheng, H., Tong, L., Yang, Q., Li, J., & Mao, S. X. (2016) · Nano Letters · doi:10.1021/acs.nanolett.5b03070 · Cited by 171
A study of fracture mechanisms in biological nano-composites via the virtual internal bond model
Ji, B., & Gao, H. (2003) · Materials Science and Engineering A · doi:10.1016/j.msea.2003.08.121 · Cited by 172
Self-citationEngineering lattice metamaterials for extreme property, programmability, and multifunctionality
Jia, Z., Liu, F., Jiang, X., & Wang, L. (2020) · Journal of Applied Physics · doi:10.1063/5.0004724 · Cited by 170
Screening the Incorporation of Amino Acids into an Inorganic Crystalline Host: the Case of Calcite
Borukhin, S., Bloch, L., Radlauer, T., Hill, A. H., Fitch, A. N., & Pokroy, B. (2012) · Advanced Functional Materials · doi:10.1002/adfm.201201079 · Cited by 157
Physiology of Calcium Homeostasis
Matikainen, N., Pekkarinen, T., Ryhänen, E. M., & Schalin-Jäntti, C. (2021) · Endocrinology and Metabolism Clinics of North America · doi:10.1016/j.ecl.2021.07.005 · Cited by 169
Hierarchically Staggered Nanostructure of Mineralized Collagen as a Bone‐Grafting Scaffold
Liu, Y., Liu, S., Luo, D., Xue, Z., Yang, X., Gu, L., Zhou, Y., & Wang, T. (2016) · Advanced Materials · doi:10.1002/adma.201602628 · Cited by 169
A New Transferable Forcefield for Simulating the Mechanics of CaCO3 Crystals
Xiao, S., Edwards, S. A., & Gräter, F. (2011) · The Journal of Physical Chemistry C · doi:10.1021/jp202743v · Cited by 168
Toughening mechanisms in bioinspired multilayered materials
Askarinejad, S., & Rahbar, N. (2015) · Journal of The Royal Society Interface · doi:10.1098/rsif.2014.0855 · Cited by 168
Internal strains and stresses measured in cortical bone via high-energy X-ray diffraction
Almer, J., & Stock, S. R. (2005) · Journal of Structural Biology · doi:10.1016/j.jsb.2005.08.003 · Cited by 172
Bioinspired Additive Manufacturing of Hierarchical Materials: From Biostructures to Functions
Wei, J., Pan, F., Ping, H., Yang, K., Wang, Y., Wang, Q., & Fu, Z. (2023) · Research · doi:10.34133/research.0164 · Cited by 170
The Organic-Mineral Interface in Biominerals
Gilbert, P. U. P. A. (2005) · Reviews in Mineralogy and Geochemistry · doi:10.2138/rmg.2005.59.7 · Cited by 157
Metadata
- Authors
- Gao, H., Ji, B., Jäger, I. L., Arzt, E., & Fratzl, P.
- Affiliations
- Austrian Academy of Sciences (AT)
- Venue
- Proceedings of the National Academy of Sciences
- Publisher
- National Academy of Sciences
- Published
- 2003-05-05
- Volume
- 100
- Issue
- 10
- Pages
- 5597-5600
- ISSN
- 0027-8424 (ISSN-L)
- 1091-6490
- PMC
- PMC156246
- OpenAlex
- W2040957028
- Cited by
- 1,922
- References
- 24
- Citations by year
- 2026: 74 · 2025: 91 · 2024: 74 · 2023: 89 · 2022: 95 · 2021: 109 · 2020: 129 · 2019: 103 · 2018: 93 · 2017: 93 · 2016: 105 · 2015: 112 · 2014: 81 · 2013: 87 · 2012: 101
- FWCI
- 24.62
- Type
- journal article
- Language
- en
- Open access
- green
- www.ncbi.nlm.nih.gov
- Locations
- Proceedings of the National Academy of Sciences (publishedVersion)
- Europe PMC (PubMed Central) (publishedVersion)
- PubMed Central (publishedVersion)
- PubMed (publishedVersion)
- Max Planck Institute for Plasma Physics (submittedVersion)
- Max Planck Digital Library (submittedVersion)
- MPG.PuRe (Max Planck Society) (submittedVersion)
- Funders
- National Natural Science Foundation of China
- Tsinghua University
- Max-Planck-Gesellschaft
- Changjiang Scholar Program of Chinese Ministry of Education
- Topics
- Physical Sciences › Materials Science › Biomaterials › Calcium Carbonate Crystallization and Inhibition
- Physical Sciences › Materials Science › Metals and Alloys › Microstructure and mechanical properties
- Physical Sciences › Engineering › Mechanical Engineering › Advanced Materials and Mechanics
- Keywords
- nanocomposites, fracture toughness, flaw tolerance, stress concentration, bone, teeth, nacre, biomimetic materials, mechanical strength, nanomaterial design
- MeSH terms
- Animals, Bone and Bones, Minerals, Miniaturization, Ostreidae, Sensitivity and Specificity, Stress, Mechanical, Tooth, Vertebrates
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.