Influence of processing conditions on the properties of thermal sprayed coating: a review
The DOI matches its Crossref record; 72 of the 72 references it cites were found in a registry or an index.
Abstract
Thermal spray coatings are a group of coating processes that enhance the performance of parts by adding functionality to surfaces. In the past few decades, thermal spray coatings technology was used to resist wear, erosion, corrosion, cavitation, repair and dimensional restoration of parts. However, the consideration of process parameters setting develops a reliable coating having high mechanical and morphological properties for demanding coating applications. Hence the aim of this review paper is to provide an overview of distinct thermal spray coatings, historical development, hot corrosion mechanism and effect of chemical composition and alloying elements on the hot corrosion resistance of super alloys in USC power plants. Then the effects of processing conditions on the mechanical properties of distinct thermal sprayed coatings obtained at distinct process parameters are summarised. Finally, the distinct thermal post treatments such as fusing of self-flux alloys, remelting and solid heat treatments, merits, demerits and future challenges are discussed.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
The Science and Engineering of Thermal Spray Coatings
Pawlowski, L. (2008) · Wiley eBooks · doi:10.1002/9780470754085 · Cited by 2,033
Fauchais, P. L., Heberlein, J. V. R., & Boulos, M. I. (2014) · Springer eBooks · doi:10.1007/978-0-387-68991-3 · Cited by 857
Cold spray coating: review of material systems and future perspectives
Moridi, A., Hassani-Gangaraj, S. M., Guagliano, M., & Dao, M. (2014) · Surface Engineering · doi:10.1179/1743294414y.0000000270 · Cited by 754
Cold spray additive manufacturing and repair: Fundamentals and applications
Yin, S., Cavaliere, P., Aldwell, B., Jenkins, R., Liao, H., Li, W., & Lupoi, R. (2018) · Additive Manufacturing · doi:10.1016/j.addma.2018.04.017 · Cited by 599
Handbook of tribology: materials, coatings, and surface treatments
(1992) · Choice Reviews Online · doi:10.5860/choice.29-3326 · Cited by 531
Introduction to High Temperature Oxidation and Corrosion
Khanna, A. S. (2002) · Cited by 364
Thermal Sprayed Coatings Used Against Corrosion and Corrosive Wear
Fauchais, P. L., & Vardelle, A. M. (2012) · InTech eBooks · doi:10.5772/34448 · Cited by 177
Sadeghi, E., Markocsan, N., & Joshi, S. V. (2019) · Journal of Thermal Spray Technology · doi:10.1007/s11666-019-00938-1 · Cited by 165 · cited 1×
“Historical development of thermal spray coatings processes [5,6].”
BackgroundCritical review of corrosion protection by cold spray coatings
Hassani-Gangaraj, S. M., Moridi, A., & Guagliano, M. (2015) · Surface Engineering · doi:10.1179/1743294415y.0000000018 · Cited by 164
Pereira, J. M., & Lerch, B. A. (2001) · International Journal of Impact Engineering · doi:10.1016/s0734-743x(01)00018-5 · Cited by 148
Some studies on hot corrosion performance of plasma sprayed coatings on a Fe-based superalloy
Singh, H., Puri, D., & Prakash, S. (2004) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2004.03.030 · Cited by 138 · cited 3×
“Stellite-6 −180 µm+53 µm Bond coat = 172 µm, outer coat = 214 µm 2–3.5% Ni3Al Ni: 74 µm Al: fine powder Bond coat = 178 µm, outer coat = 198 µm 2–4.5% T22 NiCrAlY −45 µm+10 µm 384 µm 2–4% Ni-20Cr −45 µm+5 µm Bond coat = 152 µm, outer coat = 213 µm 2.5–4% Stellite-6 −180 µm+53 µm Bond coat = 172 µm, outer coat = 214 µm…”
InfluentialKumar, S., Handa, A., Chawla, V., Grover, N. K., & Kumar, R. (2021) · Surface Engineering · doi:10.1080/02670844.2021.1924506 · Cited by 133
Self-citationSidhu, T. S., Prakash, S., & Agrawal, R. D. (2006) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2005.12.030 · Cited by 131 · cited 3×
“(2006) [96] Superni 600 Cr3C2-NiCr −45 +5 μm 250 L/ min 60 L/min 900 L/min – – 6 kg/cm(2) 8 kg/cm(2) – 6 kg/cm(2) 200 mm – – 290 μm – 870–950Hv <1.”
InfluentialAccelerated hot corrosion studies of cold spray Ni–50Cr coating on boiler steels
Bala, N., Singh, H., & Prakash, S. (2010) · Materials & Design · doi:10.1016/j.matdes.2009.06.033 · Cited by 128 · cited 1×
“(2010) [121] T22 Ni-50Cr 45±15 μm 400 °C 2.”
Cold spray as an emerging technology for biocompatible and antibacterial coatings: state of art
Vilardell, A. M., Cinca, N., Concustell, A., Dosta, S., Cano, I. G., & Guilemany, J. M. (2015) · Journal of Materials Science · doi:10.1007/s10853-015-9013-1 · Cited by 128
Overview of cold spray coatings applications and comparisons: a critical review
Kumar, S., Kumar, M., & Jindal, N. (2020) · World Journal of Engineering · doi:10.1108/wje-01-2019-0021 · Cited by 123 · cited 1×
“1 Kumar et al. (2020) [71] SA 516 Ni-20Cr 80% Ni 14 µm 260 slpm 60 slpm 600 slpm – 6 Kg/cm2 10 Kg/ cm2 – – 7 Kg/cm2 150 mm – 35–40 g/ min 200– 300 μm 4.7 μm 506–525 Hv – Ni-20Cr 72% Ni 13 µm 4.1 μm Ni-20Cr 64% Ni 11 µm 4 μm 2 Tailor et al. (2019) [72] T91 Cr3 C2-25%NiCr 15–45 μm 260 LPM 65 LPM 65…”
InfluentialSelf-citationKumar, S., Kumar, M., & Handa, A. (2019) · Engineering Failure Analysis · doi:10.1016/j.engfailanal.2019.104173 · Cited by 119
Self-citationSidhu, T. S., Prakash, S., & Agrawal, R. D. (2005) · Acta Materialia · doi:10.1016/j.actamat.2005.10.009 · Cited by 116 · cited 3×
“…– – 8 kg/cm2 6 kg/cm2 – 6 kg/cm2 200 mm – – 290 µm 930 Hv Less than 1.4% Superni 600 280 µm 750Hv Less than 1.4% Superni 601 252 µm 800HV Less than 1.4% Superni 718 266 µm 750 Hv Less than 1.4% SF 800H 288 µm 930Hv 19 Sidhu et al. (2006) [89] Superni 600 NiCrBSi ±45 µm 250 L/ min 60 L/min 900…”
InfluentialHot Corrosion Behavior of CM 247 LC Alloy in Na2SO4 and NaCl Environments
Gurrappa, I. (1999) · Oxidation of Metals · doi:10.1023/a:1018831025272 · Cited by 112
Hidalgo, V. H., Varela, J. B., Menéndez, A., & Martı́nez, S. P. (2001) · Wear · doi:10.1016/s0043-1648(00)00540-8 · Cited by 109
Kumar, S., Kumar, M., & Handa, A. (2020) · Materials at High Temperatures · doi:10.1080/09603409.2020.1810922 · Cited by 101 · cited 1×
“1 Kumar et al. (2020) [71] SA 516 Ni-20Cr 80% Ni 14 µm 260 slpm 60 slpm 600 slpm – 6 Kg/cm2 10 Kg/ cm2 – – 7 Kg/cm2 150 mm – 35–40 g/ min 200– 300 μm 4.7 μm 506–525 Hv – Ni-20Cr 72% Ni 13 µm 4.1 μm Ni-20Cr 64% Ni 11 µm 4 μm 2 Tailor et al. (2019) [72] T91 Cr3 C2-25%NiCr 15–45 μm 260 LPM 65 LPM 65…”
InfluentialSelf-citationKamal, S., Jayaganthan, R., & Prakash, S. (2008) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2008.04.087 · Cited by 98 · cited 1×
“ity is also a major problem in many applications [181,182].”
BackgroundStein-Brzozowska, G., Flórez, D. M., Maier, J., & Scheffknecht, G. (2012) · Fuel · doi:10.1016/j.fuel.2012.11.081 · Cited by 96 · cited 1×
“[157] evaluated the fireside corrosion behaviour of three Ni-base alloys (Alloys”
BackgroundSidhu, T. S., Prakash, S., & Agrawal, R. D. (2006) · Thin Solid Films · doi:10.1016/j.tsf.2005.12.041 · Cited by 93 · cited 3×
“…– – 8 kg/cm2 6 kg/cm2 – 6 kg/cm2 200 mm – – 290 µm 930 Hv Less than 1.4% Superni 600 280 µm 750Hv Less than 1.4% Superni 601 252 µm 800HV Less than 1.4% Superni 718 266 µm 750 Hv Less than 1.4% SF 800H 288 µm 930Hv 19 Sidhu et al. (2006) [89] Superni 600 NiCrBSi ±45 µm 250 L/ min 60 L/min 900…”
InfluentialFireside and steamside corrosion of alloys for USC plants
Natesan, K., & Park, J. (2006) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2006.08.038 · Cited by 86 · cited 1×
“operating pressure and temperature of the steam systems [12].”
BackgroundSidhu, T. S., Prakash, S., & Agrawal, R. D. (2006) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2006.02.047 · Cited by 81 · cited 3×
“(2006) [97] Superni-75 NiCrBSi −45 μm 250 L/ min 60 L/min 900 L/min – – 6 kg/cm(2) 8 kg/cm(2) – 6 kg/cm(2) 200 mm – – 285 μm 800–850Hv <1.”
InfluentialCold spray technology in nuclear energy applications: A review of recent advances
Yeom, H., & Sridharan, K. (2020) · Annals of Nuclear Energy · doi:10.1016/j.anucene.2020.107835 · Cited by 74
Diagnostics of thermal spraying plasma jets
Fauchais, P. L., Coudert, J.-F., Vardelle, M., Vardelle, A. M., & Denoirjean, A. (1992) · Journal of Thermal Spray Technology · doi:10.1007/bf02659011 · Cited by 72
Hot corrosion performance of a NiCr coated Ni-based alloy
SIDHU, T., PRAKASH, S., & AGRAWAL, R. (2006) · Scripta Materialia · doi:10.1016/j.scriptamat.2006.03.054 · Cited by 70
Bala, N., Singh, H., & Prakash, S. (2009) · Journal of Thermal Spray Technology · doi:10.1007/s11666-009-9437-8 · Cited by 67 · cited 1×
“(2010) [122] SA516 Ni-20Cr 45 μm 400 °C 20.”
Sidhu, T. S., Prakash, S., & Agrawal, R. D. (2006) · Journal of Thermal Spray Technology · doi:10.1361/105996306x124392 · Cited by 67 · cited 4×
“, (2006) [90] Superni 601 Cr3C2-NiCr −45 +5 μm 250 L/ min 60 L/min 900 L/min – – 6 kg/cm(2) 8 kg/cm(2) – 6 kg/cm(2) 200 mm – – 250– 300 μm – 900Hv <2%”
InfluentialHigh-Temperature Behavior of a High-Velocity Oxy-Fuel Sprayed Cr3C2-NiCr Coating
Kaur, M., Singh, H., & Prakash, S. (2012) · Metallurgical and Materials Transactions A · doi:10.1007/s11661-012-1118-4 · Cited by 63 · cited 2×
“(2012) [82] T22 Cr3C2-NiCr −45 +15 μm 250 L/ min 60–70 L/ min 600 L/min – – – – – – 150– 180 mm – 25 g/min 225 ± 25 μm 697–1205 Hv –”
InfluentialThe corrosion of INCONEL alloy 740 in simulated environments for pulverized coal-fired boiler
Zhao, S., Xie, X., Smith, G. D., & Patel, S. J. (2005) · Materials Chemistry and Physics · doi:10.1016/j.matchemphys.2004.04.006 · Cited by 62 · cited 1×
“[156] investigated the corrosion performance of Inconel alloy-740 at 550°C and 700°C in”
BackgroundSidhu, T. S., Prakash, S., & Agrawal, R. D. (2006) · Journal of Thermal Spray Technology · doi:10.1361/105996306x147162 · Cited by 62 · cited 3×
“(2006) [95] Superni 75 Cr3C2Ni-Cr <44 μm 250 L/ min 60 L/min 900 L/min – – 6 kg/cm(2) 8 kg/cm(2) – 6 kg/cm(2) 200 mm – – 200– 250 μm – 850–900Hv <1.”
InfluentialEffect of temperature on coal ash hot corrosion resistance of Inconel 740 superalloy
Aung, N. N., & Liu, X. (2014) · Corrosion Science · doi:10.1016/j.corsci.2014.01.020 · Cited by 57
Sidhu, T. S., Prakash, S., & Agrawal, R. D. (2006) · Materials Science and Engineering A · doi:10.1016/j.msea.2006.05.099 · Cited by 57 · cited 3×
“(2006) [94] Superni 75 Cr3C2-NiCr −45 +5 μm 250 L/ min 60 L/min 900 L/min – – 6 kg/cm(2) 8 kg/cm(2) – 6 kg/cm(2) 200 mm – – 290 μm 870–950 Hv <1.”
InfluentialPerformance of cold sprayed Ni based coatings in actual boiler environment
Bala, N., Singh, H., & Prakash, S. (2017) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2016.11.075 · Cited by 53
Sidhu, B. S., & Prakash, S. (2006) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2006.02.035 · Cited by 51 · cited 1×
“(2006) [56] GrA1 NiCrAlY −45 μm+10 μm – – 700 35 90–110 mm – 384 μm 2–4% Ni-20Cr −45 μm+5 μm Bond coat = 152 μm, outer coat = 213 μm 2.”
Sidhu, T. S., Prakash, S., & Agrawal, R. D. (2006) · Materials Science and Engineering A · doi:10.1016/j.msea.2006.09.015 · Cited by 51 · cited 3×
“…– – 8 kg/cm2 6 kg/cm2 – 6 kg/cm2 200 mm – – 290 µm 930 Hv Less than 1.4% Superni 600 280 µm 750Hv Less than 1.4% Superni 601 252 µm 800HV Less than 1.4% Superni 718 266 µm 750 Hv Less than 1.4% SF 800H 288 µm 930Hv 19 Sidhu et al. (2006) [89] Superni 600 NiCrBSi ±45 µm 250 L/ min 60 L/min 900…”
InfluentialThe corrosion behaviours of plasma-sprayed Fe-based amorphous coatings
Jiang, C., Liu, W., Wang, G., Chen, Y., Xing, Y., Zhang, C., & Dargusch, M. (2018) · Surface Engineering · doi:10.1080/02670844.2017.1319647 · Cited by 50
Bala, N., Singh, H., & Prakash, S. (2011) · Metallurgical and Materials Transactions A · doi:10.1007/s11661-011-0759-z · Cited by 45 · cited 1×
“(2011) [120] T22 Ni-20Cr −45+15 μm 400 °C 20.”
Kaur, M., Singh, H., & Prakash, S. (2010) · Surface Engineering · doi:10.1179/026708409x12490360425963 · Cited by 43
Ruiz-Luna, H., Lozano-Mandujano, D., Alvarado-Orozco, J. M., Valarezo, A., Poblano-Salas, C. A., Trapaga, G., Espinoza‐Beltrán, F. J., & Muñoz‐Saldaña, J. (2014) · Journal of Thermal Spray Technology · doi:10.1007/s11666-014-0121-2 · Cited by 43
Chatha, S. S., Sidhu, H. S., & Sidhu, B. S. (2013) · Journal of Thermal Spray Technology · doi:10.1007/s11666-013-9899-6 · Cited by 41 · cited 1×
“…(Ni-20Cr) 350 µm – 862 < 1.5 pct 80% Cr3C2-20% (Ni-20Cr) 325 µm 887 1167 90% Cr3C2-10% (Ni-20Cr) 375 µm – 1167 1167 1352 S.KU M A R A N D R.KU M A R 11 Chatha et al. (2013) [81] T91 Ni-20Cr −53 +15 µm 250 L/ min 60 L/min 600 L/min – – – 6 kg/cm2 9 kg/cm2 7.5 kg/cm2 180 mm – – 260– 310 µm 9.21…”
InfluentialKaushal, G., Bala, N., Kaur, N., Singh, H., & Prakash, S. (2014) · Metallurgical and Materials Transactions A · doi:10.1007/s11661-013-1984-4 · Cited by 39 · cited 1×
“(2014) [118] T22 Ni-20Cr −45+15 μm 400 °C 20.”
Goyal, K., Singh, H., & Bhatia, R. (2018) · World Journal of Engineering · doi:10.1108/wje-10-2017-0315 · Cited by 35 · cited 2×
“3 – 5 Goyal et al. (2018) [75] T22 Cr2O3 45±10 μm 250 L/ min.”
Hot Corrosion Behavior of HVOF Sprayed Coatings on ASTM SA213-T11 Steel
Sidhu, H. S., Sidhu, B. S., & Prakash, S. (2007) · Journal of Thermal Spray Technology · doi:10.1007/s11666-007-9029-4 · Cited by 35 · cited 4×
“…NiCrBSi ±45 µm 250 L/ min 60 L/min 900 L/min – – 8 kg/cm2 6 kg/cm2 – 6 kg/cm2 200 mm – – 270 µm – 810–850Hv <1.5% Stellite-6 −53 ±45 µm 265 µm – 850–900Hv <2% SF 800H 45 µm – – – 17 Sidhu et al. (2007) [87] Superni 718 Cr3C2-NiCr ±45 µm 250 L/ min 60 L/min 900 L/min – – 8 kg/cm2 6 kg/cm2 –…”
InfluentialKumar, M., Singh, H., Singh, N., & Joshi, R. S. (2015) · Wear · doi:10.1016/j.wear.2015.01.043 · Cited by 32 · cited 1×
“(2015) [115] T22 Ni-20Cr Ni (CA): 74 μm, Ni (BM) 67nm and CR (BM):60nm 450 °C 19 bar Air – 1.”
Erosion–corrosion behaviour of Ni–20Cr plasma coating in actual boiler environment
Mishra, S. B., & Prakash, S. (2015) · Surface Engineering · doi:10.1179/1743294414y.0000000338 · Cited by 31
Singh, H., Bala, N., Kaur, N., Sharma, S. K., Kim, D. Y., & Prakash, S. (2015) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2015.08.002 · Cited by 31
Saladi, S., Menghani, J. V., & Prakash, S. (2015) · Journal of Materials Engineering and Performance · doi:10.1007/s11665-015-1400-x · Cited by 29
Influence of Process Parameters on the Deposition Footprint in Plasma-Spray Coating
Remesh, K., Ng, H. W., & Yu, S. C. M. (2003) · Journal of Thermal Spray Technology · doi:10.1361/105996303770348258 · Cited by 28
Performance of 75Cr3C2-25NiCr Coating Produced by HVOF Process in a Coal-Fired Thermal Power Plant
Chatha, S. S., Sidhu, H. S., & Sidhu, B. S. (2016) · Advanced materials research · doi:10.4028/www.scientific.net/amr.1137.88 · Cited by 28 · cited 2×
“3 0.85% 7 Chatha et al. (2016) [77] T91 75Cr3C2-25NiCr −45 µm +15 µm 250 L/ min 60 L/min 600 L/min – 6 kg/cm2 9 kg/cm2 – – 7.5 kg/cm2 180 mm – – 260– 310 µm 5.27± 0.53 µm 860Hv < 2.5% 8 Somasundaram et al. (2016) [78] T22 WC-CrC-Ni 15–45 µm 250 L/ min 65–70 L/ min 550 L/min – – 981 KPa 588 KPa –…”
InfluentialSingh, V., Goyal, K., & Goyal, R. (2019) · Anti-Corrosion Methods and Materials · doi:10.1108/acmm-10-2018-2009 · Cited by 26
Microstructure and High Temperature Corrosion Behavior of Wire-Arc Sprayed FeCrSiB Coating
Li, R., Zhou, Z., He, D., Wang, Y., Wu, X., & Song, X. (2015) · Journal of Thermal Spray Technology · doi:10.1007/s11666-015-0244-0 · Cited by 26 · cited 1×
“(2015) [144] SA213-T2 steel FeCrSiB – – – – – 200 mm 30 V and 190–200 A – – – 650Hv 4.”
Somasundaram, B., Kadoli, R., & Ramesh, M. R. (2014) · Transactions of the Indian Institute of Metals · doi:10.1007/s12666-014-0453-0 · Cited by 25 · cited 2×
“…250 L/ min 65–70 L/ min 550 L/min – – 981 KPa 588 KPa – 681 KPa 178 mm – 23 g/min 270– 300 µm – 1,093 Hv 2.33% MDN 310 270– 300 µm – 1,093 Hv 2.33% SF 800H 270– 300 µm – 1,093 Hv 2.33% 9 Somasundaram et al. (2015) [79] T22 Cr3C2-35% NiCr + 5% Si −45 µm +15 µm 250 L/ min 65–70 L/ min 550 L/min –…”
InfluentialHigh temperature corrosion behaviour of HVOF sprayed WC-CrC-Ni coatings
Somasundaram, B., Kadoli, R., Ramesh, M. R., & Ramesh, C. S. (2016) · International Journal of Surface Science and Engineering · doi:10.1504/ijsurfse.2016.077542 · Cited by 24 · cited 2×
“…al. (2016) [77] T91 75Cr3C2-25NiCr −45 µm +15 µm 250 L/ min 60 L/min 600 L/min – 6 kg/cm2 9 kg/cm2 – – 7.5 kg/cm2 180 mm – – 260– 310 µm 5.27± 0.53 µm 860Hv < 2.5% 8 Somasundaram et al. (2016) [78] T22 WC-CrC-Ni 15–45 µm 250 L/ min 65–70 L/ min 550 L/min – – 981 KPa 588 KPa – 681 KPa 178 mm – 23…”
InfluentialCyclic Oxidation Behavior of Some Plasma-Sprayed Coatings in Na2SO4-60%V2O5 Environment
Singh, H., Prakash, S., Puri, D., & Phase, D. M. (2006) · Journal of Materials Engineering and Performance · doi:10.1361/105994906x150858 · Cited by 21 · cited 3×
“…outer coat = 213 µm 2.5–4% Stellite-6 −180 µm+53 µm Bond coat = 172 µm, outer coat = 214 µm 2–3.5% Ni3Al Ni: 74 µm Al: fine powder Bond coat = 178 µm, outer coat = 198 µm 2–4.5% 5 Singh et al. (2006) [54] Superni 600 NiCrAlY −45±10 µm – – 700 35 90–110 mm – 59Psi 40Psi Bond coat = 228 µm 390Hv…”
InfluentialStudy of High Temperature Oxidation Behavior of Wire Arc Sprayed Coatings
Kant, S., Kumar, M., Chawla, V., & Singh, S. (2020) · Materials Today Proceedings · doi:10.1016/j.matpr.2020.01.226 · Cited by 21
Kumar, M., Singh, H., & Singh, N. (2020) · Materials Today Proceedings · doi:10.1016/j.matpr.2020.01.321 · Cited by 20 · cited 1×
“1 Kumar et al. (2020) [71] SA 516 Ni-20Cr 80% Ni 14 µm 260 slpm 60 slpm 600 slpm – 6 Kg/cm2 10 Kg/ cm2 – – 7 Kg/cm2 150 mm – 35–40 g/ min 200– 300 μm 4.7 μm 506–525 Hv – Ni-20Cr 72% Ni 13 µm 4.1 μm Ni-20Cr 64% Ni 11 µm 4 μm 2 Tailor et al. (2019) [72] T91 Cr3 C2-25%NiCr 15–45 μm 260 LPM 65 LPM 65…”
InfluentialReduction of Wustite Scale by Dissolved Carbon in Steel at 650–900 °C
Chen, R. Y. (2017) · Oxidation of Metals · doi:10.1007/s11085-017-9810-9 · Cited by 19
Hari, P. R., Arivazhagan, N., Rao, M. N., & Pavan, A. H. V. (2017) · Transactions of the Indian Institute of Metals · doi:10.1007/s12666-017-1079-9 · Cited by 16
Thermal Spray Coatings for Erosion-Corrosion Protection
Keshavamurthy, R., Naveena, B. E., & Sekhar, N. (2017) · Advances in chemical and materials engineering book series · doi:10.4018/978-1-5225-4194-3.ch010 · Cited by 15
Effect of Sulfur and Chlorine on Fireside Corrosion Behavior of Inconel 740 H Superalloy
Lu, J., Li, Y., Yang, Z., Huang, J., Ming, Z., & Gu, Y. (2017) · High Temperature Materials and Processes · doi:10.1515/htmp-2016-0186 · Cited by 14
Hot corrosion behavior of thermal spray coatings on superalloy in coal-fired boiler environment
Kamal, S., Sharma, K. V., Jayaganthan, R., & Prakash, S. (2015) · Journal of materials research/Pratt's guide to venture capital sources · doi:10.1557/jmr.2015.264 · Cited by 14
Remelting of Flame Spraying PEEK Coating Using Lasers
Soveja, A., Costil, S., Liao, H., Sallamand, P., & Coddet, C. (2009) · Journal of Thermal Spray Technology · doi:10.1007/s11666-009-9421-3 · Cited by 14
Behaviour of cold sprayed superalloy in incinerator at 900°C
Singh, H., Sidhu, T. S., & Kalsi, S. B. S. (2014) · Surface Engineering · doi:10.1179/1743294414y.0000000390 · Cited by 14 · cited 1×
“(2014) [117] Superni75 75Cr3C2– 25(Ni– 20Cr) – 650 °C 38 bar Nitrogen – 95m(3)/h – – 3 m(3)/h – 293 μm 6.”
Sundaresan, C., Rajasekaran, B., Sivakumar, G., & Rao, D. S. (2020) · IOP Conference Series: Materials Science and Engineering · doi:10.1088/1757-899x/872/1/012092 · Cited by 13 · cited 1×
“(2020) [53] T91 NiCoCrAlY 22–45 μm 90 Scfh 11 Scfh 500 60–65 100 – – 1bar – 7 μ = 335 with σ = 57 2.”
Hot Corrosion Behavior of High-Chromium, High-Carbon Cast Irons in NaCl-KCl Molten Salts
Rayo, S. V., Gonzalez-Rodriguez, J. G., Porcayo-Calderón, J., Salinas-Bravo, V. M., & Maldonado-Ruiz, S. I. (2012) · International Journal of Corrosion · doi:10.1155/2012/479761 · Cited by 12 · cited 1×
“weight loss owing to hot corrosion decreases with the increase in chromium content [160,161].”
BackgroundInvestigations on role of HVOF sprayed Co and Ni based coatings to combat hot corrosion
Sidhu, T. S., Prakash, S., & Agrawal, R. D. (2008) · Corrosion Engineering Science and Technology The International Journal of Corrosion Processes and Corrosion Control · doi:10.1179/174327808x286446 · Cited by 11 · cited 2×
“(2008) [84] Superni 718 Stellite-6 −53 ±45 μm 250 L/ min 250 L/min 60 L/min – – 6 kg/cm(2) 6 kg/cm(2) – 6 kg/cm(2) 200 mm – 25 g/min 265 μm – 850–900Hv 2%”
InfluentialOxidation behaviour of alloy S16 in superheated steam and supercritical water
Xiao, B., Tepylo, N., Fawcett, A., Yao, M., & Huang, X. (2019) · Materials at High Temperatures · doi:10.1080/09603409.2019.1680125 · Cited by 3
Kaur, M., Singh, H., & Prakash, S. (2011) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2011.07.077
Cited by
Comprehensive review on high entropy alloy-based coating
Kumar, S. (2024) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2023.130327 · Cited by 208
Self-citationOverview on metamaterial: History, types and applications
Kumar, R., Kumar, M., Chohan, J. S., & Kumar, S. (2022) · Materials Today: Proceedings · doi:10.1016/j.matpr.2021.11.423 · Cited by 178
Self-citation
Metadata
- Authors
- Kumar, S., & Kumar, R.
- Venue
- Surface Engineering
- Publisher
- SAGE Publications
- Published
- 2021-11
- Volume
- 37
- Issue
- 11
- Pages
- 1339-1372
- ISSN
- 0267-0844 (ISSN-L)
- 1743-2944
- OpenAlex
- W3197943534
- Cited by
- 168
- References
- 72
- FWCI
- 13.57
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.