Battery Cycle Life Prediction with Coupled Chemical Degradation and Fatigue Mechanics
The DOI matches its Crossref record; 50 of the 50 references it cites were found in a registry or an index.
Abstract
Coupled mechanical-chemical degradation of electrodes upon charging and discharging has been recognized as a major failure mechanism in lithium ion batteries. The instability of commonly employed electrolytes results in solid electrolyte interphase (SEI) formation. Although the SEI layer is necessary, as it passivates the electrode-electrolyte interface from further solvent decomposition, SEI formation consumes lithium and thus contributes to irreversible capacity loss. In this paper, we study irreversible capacity loss in a graphite-LiFePO 4 cell. Our results support the mechanism of irreversible capacity loss due to the consumption of lithium in forming SEI. We attribute irreversible capacity loss to diffusion induced stresses (DISs) that cause pre-existing cracks on the electrode surfaces to grow gradually upon cycling, leading to the growth of SEI on the newly exposed electrode surfaces. Because lithium is consumed in forming the new SEI, irreversible capacity loss continues with cycling. Along with the SEI formation upon newly exposed (cracked) surfaces, the existing SEI thickness also grows with cycling, resulting in additional loss of lithium. In this study, we provide, a simple mathematical model, based on the Paris’ Law formulation of mechanical fatigue, in combination with chemical degradation to explain battery life. We compare the predicted capacity at different temperatures with the experimental data obtained from electrochemical measurements on graphite-LiFePO 4 cells.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“which is why most physics-based models focus only on the most dominant mechanisms, such as the formation and growth of the solid electrolyte interphase (SEI) [11,12] or electronic contact loss through particle cracking [13,14].”
From Degradation diagnostics for lithium ion cells (2017) · cites this paper as [14]
Citations
Cites
Phospho‐olivines as Positive‐Electrode Materials for Rechargeable Lithium Batteries
Padhi, A. K., Nanjundaswamy, K. S., & Goodenough, J. B. (1997) · Journal of The Electrochemical Society · doi:10.1149/1.1837571 · Cited by 7,933
A Critical Analysis of Crack Propagation Laws
Paris, P., & Erdogan, F. (1963) · Journal of Basic Engineering · doi:10.1115/1.3656900 · Cited by 7,122
Lawn, B. (1993) · Cambridge University Press eBooks · doi:10.1017/cbo9780511623127 · Cited by 4,759
Suresh, S. (1998) · Cambridge University Press eBooks · doi:10.1017/cbo9780511806575 · Cited by 4,526
Battery materials for ultrafast charging and discharging
Kang, B., & Ceder, G. (2009) · Nature · doi:10.1038/nature07853 · Cited by 3,480
Insertion Electrode Materials for Rechargeable Lithium Batteries
Winter, M., Besenhard, J. O., Spahr, M. E., & Novák, P. (1998) · Advanced Materials · doi:10.1002/(sici)1521-4095(199807)10:10<808::aid-adma808>3.0.co;2-r · Cited by 2,998
Insertion Electrode Materials for Rechargeable Lithium Batteries
Winter, M., Besenhard, J. O., Spahr, M. E., & Novák, P. (1998) · Advanced Materials · doi:10.1002/(sici)1521-4095(199807)10:10<725::aid-adma725>3.0.co;2-z · Cited by 2,965
Electronically conductive phospho-olivines as lithium storage electrodes
Chung, S.-Y., Bloking, J. T., & Chiang, Y.-M. (2002) · Nature Materials · doi:10.1038/nmat732 · Cited by 2,939
Aurbach, D. (2000) · Journal of Power Sources · doi:10.1016/s0378-7753(00)00431-6 · Cited by 2,130
Fracture Mechanics: Fundamentals and Applications, Third Edition
Anderson, T. L., & Anderson, T. L. (2005) · CRC Press eBooks · doi:10.1201/9781420058215 · Cited by 1,854
Research works printed but not linked: 1
- Ragab A. R. Bayoumi S. B. , Engineering Solid Mechanics- Fundamental and Applications. (CRC Press, Boca Ranton, FL, 1999).
Cited by
Items 101–200 of 389
Kim, J., Pieczonka, N. P. W., Lu, P., Liu, Z., Qiao, R., Yang, W., Tessema, M. M., Sun, Y., & Powell, B. R. (2015) · Advanced Materials Interfaces · doi:10.1002/admi.201500109 · Cited by 70
Pharr, M., Choi, Y. S., Lee, D., Oh, K. H., & Vlassak, J. J. (2015) · Journal of Power Sources · doi:10.1016/j.jpowsour.2015.11.036 · Cited by 70
Hwang, G., Sitapure, N., Moon, J., Lee, H., Hwang, S., & Kwon, J. S. (2022) · Chemical Engineering Journal · doi:10.1016/j.cej.2022.134768 · Cited by 69
Yang, D., Cui, Y., Xia, Q., Jiang, F., Ren, Y., Sun, B., Feng, Q., Wang, Z., & Yang, C. Q. (2022) · Materials · doi:10.3390/ma15093331 · Cited by 77
“In practice, because of inevitable differences in the production process, connection conditions, and operating conditions, the degradation process of the battery life cycle has the characteristics of multistate, dynamic, and random uncertainty [36,37].”
BackgroundMethodShao, J., Li, J., Yuan, W.-Z., Dai, C., Wang, Z., Zhao, M. S., & PECHT, M. G. (2023) · Journal of Energy Storage · doi:10.1016/j.est.2023.106788 · Cited by 70
Sarker, M. R., Murbach, M. D., Schwartz, D. T., & Ortega‐Vazquez, M. A. (2017) · Electric Power Systems Research · doi:10.1016/j.epsr.2017.07.007 · Cited by 75
Mesgarnejad, A., & Karma, A. (2019) · Journal of the Mechanics and Physics of Solids · doi:10.1016/j.jmps.2019.103696 · Cited by 67
Optimal charging profiles for mechanically constrained lithium-ion batteries
Suthar, B., Ramadesigan, V., De, S., Braatz, R. D., & Subramanian, V. R. (2013) · Physical Chemistry Chemical Physics · doi:10.1039/c3cp52806e · Cited by 74
Analytical Solution for Coupled Diffusion Induced Stress Model for Lithium-Ion Battery
Clerici, D., Mocera, F., & Somà, A. (2020) · Energies · doi:10.3390/en13071717 · Cited by 66
“In Figures 6c and 7c it is highlighted that the particle experiences tensile hoop stress on its surface during galvanostatic extraction, which is supposed to be the driving force for crack propagation in active material [30].”
BackgroundQiao, D., Wei, X., Zhu, J., Zhang, G., Yang, S., Wang, X., Jiang, B., Lai, X., Zheng, Y., & Dai, H. (2025) · eTransportation · doi:10.1016/j.etran.2025.100450 · Cited by 83
Li, C., Shi, T., Li, D., Yoshitake, H., & Wang, H. (2016) · RSC Advances · doi:10.1039/c5ra28021d · Cited by 63
Battery Adaptive Observer for a Single-Particle Model With Intercalation-Induced Stress
Zhang, D., Dey, S., Couto, L. D., & Moura, S. J. (2019) · IEEE Transactions on Control Systems Technology · doi:10.1109/tcst.2019.2910797 · Cited by 62
“Examples include the growth of particle surface cracks as a function of maximum tangential stress according to Paris’ Law [40], and mechanical fatigue described by the Palmgren–Milner (PM) rule [41].”
BackgroundHao, F., & Fang, D. (2013) · Journal of Power Sources · doi:10.1016/j.jpowsour.2013.05.098 · Cited by 61
Sutter, L. D., Berckmans, G. J., Marinaro, M., Smekens, J., Firouz, Y., Wohlfahrt‐Mehrens, M., Mierlo, J. V., & Omar, N. (2018) · Energies · doi:10.3390/en11112948 · Cited by 64
Strain derivatives for practical charge rate characterization of lithium ion electrodes
Schiffer, Z. J., Cannarella, J., & Arnold, C. B. (2016) · Journal of The Electrochemical Society · doi:10.1149/2.0091603jes · Cited by 59
Review on the numerical modeling of fracture in active materials for lithium ion batteries
Pistorio, F., Clerici, D., Mocera, F., & Somà, A. (2023) · Journal of Power Sources · doi:10.1016/j.jpowsour.2023.232875 · Cited by 62
Modeling crack growth during Li extraction and insertion within the second half cycle
Klinsmann, M., Rosato, D., Kamlah, M., & McMeeking, R. M. (2016) · Journal of Power Sources · doi:10.1016/j.jpowsour.2016.08.142 · Cited by 57
Lithium-ion battery physics and statistics-based state of health model
Crawford, A., Choi, D., Balducci, P., Subramanian, V. R., & Viswanathan, V. (2021) · Journal of Power Sources · doi:10.1016/j.jpowsour.2021.230032 · Cited by 63
“Some groups have attempted to quantify graphite particle cracking, which results in fresh graphite exposure for further SEI formation [39, 40].”
BackgroundLithium-Ion Battery Life Model with Electrode Cracking and Early-Life Break-in Processes
Smith, K. A., Gasper, P. J., Colclasure, A. M., Shimonishi, Y., & Yoshida, S. (2021) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/ac2ebd · Cited by 69
Barai, P., Smith, K. A., Chen, C., Kim, G., & Mukherjee, P. P. (2015) · Journal of The Electrochemical Society · doi:10.1149/2.0241509jes · Cited by 63
Advancements, Challenges, and Future Trajectories in Advanced Battery Safety Detection
Wei, Y., Wang, M., Zhang, M., Cai, T., Huang, Y., & Xu, M. (2025) · Electrochemical Energy Reviews · doi:10.1007/s41918-025-00245-0 · Cited by 77
“They proposed a mathematical model integrating Paris’ law formulation of mechanical fatigue with chemical degradation to elucidate battery life decay [108].”
The Limited Effect of VC in Graphite/NMC Cells
Deshpande, R. D., Ridgway, P. L., Fu, Y., Zhang, W., Cai, J., & Battaglia, V. (2014) · Journal of The Electrochemical Society · doi:10.1149/2.0221503jes · Cited by 56
Self-citationZhu, W., Zhou, P., Ren, D., Yang, M., Rui, X., Jin, C., Shen, T., Han, X., Zheng, Y., Lu, L., et al. (2022) · International Journal of Energy Research · doi:10.1002/er.8249 · Cited by 55
“Moreover, the volume of graphite will change by about 10% during the Li intercalation and de-intercalation process, resulting in the crack of the original SEI layer, exposure of the graphite to the electrolyte, and finally the formation of a new SEI layer.(5) As the SEI continues to grow, the porosity of the anode wil…”
BackgroundEstimation of cost savings from participation of electric vehicles in vehicle to grid (V2G) schemes
Kiaee, M., Cruden, A. J., & Sharkh, S. M. (2015) · Journal of Modern Power Systems and Clean Energy · doi:10.1007/s40565-015-0130-2 · Cited by 63
Modeling the degradation mechanisms of C6/LiFePO4 batteries
Li, D., Danilov, D. L., Zwikirsch, B., Fichtner, M., Yang, Y., Eichel, R., & Notten, P. H. L. (2017) · Journal of Power Sources · doi:10.1016/j.jpowsour.2017.11.049 · Cited by 57
Chemo‐Mechanical Model of SEI Growth on Silicon Electrode Particles**
von Kolzenberg, L., Latz, A., & Horstmann, B. (2021) · Batteries & Supercaps · doi:10.1002/batt.202100216 · Cited by 65
Bonkile, M. P., Jiang, Y., Kirkaldy, N., Sulzer, V., Timms, R., Wang, H., Offer, G. J., & Wu, B. (2023) · Journal of Energy Storage · doi:10.1016/j.est.2023.108609 · Cited by 59
Evidence for Anisotropic Mechanical Behavior and Nanoscale Chemical Heterogeneity in Cycled LiCoO 2
Diercks, D. R., Musselman, M. A., Morgenstern, A., Wilson, T., Kumar, M., Smith, K. A., Kawase, M., Gorman, B. P., Eberhart, M. E., & Packard, C. E. (2014) · Journal of The Electrochemical Society · doi:10.1149/2.0071411jes · Cited by 50
Effects of Cycling Ranges on Stress and Capacity Fade in Lithium-Ion Pouch Cells
Liu, X. M., & Arnold, C. B. (2016) · Journal of The Electrochemical Society · doi:10.1149/2.1131610jes · Cited by 50
Shi, Q., Heng, S., Qu, Q., Gao, T., Liu, W., Li, H., & Zheng, H. (2017) · Journal of Materials Chemistry A · doi:10.1039/c7ta02706k · Cited by 51
Li-ion Battery State of Health Estimation based on an improved Single Particle model
Lotfi, N., Li, J., Landers, R. G., & Park, J. (2017) · 2017 American Control Conference (ACC) · doi:10.23919/acc.2017.7962935 · Cited by 43
Wu, W. T., Guo, J., Qin, X., Bi, C., Wang, J., Wang, L., & Liang, G. (2017) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2017.06.060 · Cited by 49
Self-citationChen, L., Tong, Y., & Dong, Z. (2020) · Energies · doi:10.3390/en13071629 · Cited by 51
“The small peaks of the dV/dQ curves at the bottom shifted to t e center as the number of the charge/discharge cycle increased, leading to a narrower span of the curve with a reduced distance between the two boundaries, indicating c pacity reduction [14].”
BackgroundMethodInfluentialBonkile, M. P., Jiang, Y., Kirkaldy, N., Sulzer, V., Timms, R., Wang, H., Offer, G. J., & Wu, B. (2024) · Journal of Power Sources · doi:10.1016/j.jpowsour.2024.234256 · Cited by 63
Modelling Solvent Consumption from SEI Layer Growth in Lithium-Ion Batteries
Li, R., O’Kane, S. E. J., Marinescu, M., & Offer, G. J. (2022) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/ac6f84 · Cited by 69
Weeks, J. A., Burrow, J. N., Diao, J., Paul‐Orecchio, A. G., Srinivasan, H. S., Vaidyula, R. R., Dolocan, A., Henkelman, G., & Mullins, C. B. (2023) · Advanced Materials · doi:10.1002/adma.202305645 · Cited by 52
Lü, B., Song, Y., & Zhang, J. (2016) · Journal of Power Sources · doi:10.1016/j.jpowsour.2016.04.079 · Cited by 46
The influence of anomalous diffusion on the impedance response of LiCoO2|C batteries
Erol, S., & Orazem, M. E. (2015) · Journal of Power Sources · doi:10.1016/j.jpowsour.2015.05.047 · Cited by 49
“[20] suggested that the cracks at the graphite particle surface propagate upon electrochemical cycling.”
BackgroundPannala, S., Movahedi, H., Garrick, T. R., Stefanopoulou, A. G., & Siegel, J. B. (2023) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/ad1294 · Cited by 54
Chıacchıo, F., Famoso, F., D’Urso, D., & Cedola, L. (2019) · Energies · doi:10.3390/en12122356 · Cited by 48
“[24] coupled electrochemistry and chemical degradation to model life performance of Li-ion cells.”
BackgroundStorch, M., Hahn, S. L., Stadler, J., Swaminathan, R., Vranković, D., Krupp, C., & Riedel, R. (2019) · Journal of Power Sources · doi:10.1016/j.jpowsour.2019.227243 · Cited by 48
Ghosh, A., Foster, J. M., Offer, G. J., & Marinescu, M. (2021) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/abdc71 · Cited by 53
Deshpande, R. D., & Uddin, K. (2020) · Journal of Energy Storage · doi:10.1016/j.est.2020.101932 · Cited by 50
Self-citationNumerical Modeling of Damage Evolution Phenomenon in Solid-State Lithium-Ion Batteries
Behrou, R., & Maute, K. K. (2017) · Journal of The Electrochemical Society · doi:10.1149/2.1101712jes · Cited by 46
Choi, Y. S., Pharr, M., Oh, K. H., & Vlassak, J. J. (2015) · Journal of Power Sources · doi:10.1016/j.jpowsour.2015.06.063 · Cited by 45
Systematic feature design for cycle life prediction of lithium-ion batteries during formation
Rhyu, J., Schaeffer, J., Li, M. L., Cui, X., Chueh, W. C., Bazant, M. Z., & Braatz, R. D. (2025) · Joule · doi:10.1016/j.joule.2025.101884 · Cited by 51
Energy storage model with gridable vehicles for economic load dispatch in the smart grid
Debnath, U. K., Ahmad, I., Habibi, D., & Saber, A. Y. (2014) · International Journal of Electrical Power & Energy Systems · doi:10.1016/j.ijepes.2014.09.004 · Cited by 42
Electrochemistry-Mechanics Coupling in Intercalation Electrodes
Kotak, N., Barai, P., Verma, A., Mistry, A. N., & Mukherjee, P. P. (2018) · Journal of The Electrochemical Society · doi:10.1149/2.0621805jes · Cited by 43
Mechanical reliability of alloy-based electrode materials for rechargeable Li-ion batteries
Gao, Y., Cho, M., & Zhou, M. (2013) · Journal of Mechanical Science and Technology · doi:10.1007/s12206-013-0401-7 · Cited by 40
“Even when fatigue is important, analyses using relations such as the Paris law [113] generally require the calculation of fracture driving force in the form of KI or J.”
BackgroundMethodLuo, T., Zeng, T., Chen, S.-L., Li, R., Fan, R.-Z., Chen, H., Han, S., & Fan, C. (2020) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2020.155143 · Cited by 41
Axially and radially inhomogeneous swelling in commercial 18650 Li-ion battery cells
Blažek, P., Westenberger, P., Erker, S., Břínek, A., Zikmund, T., Rettenwander, D., Wagner, N. P., Keckes, J., Kaiser, J., Kazda, T., et al. (2022) · Journal of Energy Storage · doi:10.1016/j.est.2022.104563 · Cited by 42
Physics-based, reduced order degradation model of lithium-ion batteries
Jana, A., Mitra, A. S., Das, S., Chueh, W. C., Bazant, M. Z., & García, R. E. (2022) · Journal of Power Sources · doi:10.1016/j.jpowsour.2022.231900 · Cited by 40
Graphite: the new critical mineral
Bhattacharyya, S., Roy, S., Lin, X., Campagnol, N., Vlad, A., & Ajayan, P. M. (2025) · Nature Reviews Materials · doi:10.1038/s41578-025-00848-5 · Cited by 54
“These new SEI surfaces eventually lead to particle isolation from the electronic network, resulting in impedance growth and capacity fade 52 .”
Stress-limited fast charging methods with time-varying current in lithium-ion batteries
Lü, B., Zhao, Y., Song, Y., & Zhang, J. (2018) · Electrochimica Acta · doi:10.1016/j.electacta.2018.09.009 · Cited by 42
A simulation approach to sizing batteries for integration with net-zero energy residential buildings
Heine, K., Thatte, A., & Tabares-Velasco, P. C. (2019) · Renewable Energy · doi:10.1016/j.renene.2019.02.033 · Cited by 47
Ko, H.-J., Kwon, D., Pyo, S., & Kim, J. (2022) · Nano Energy · doi:10.1016/j.nanoen.2022.107717 · Cited by 40
Innovations and prognostics in battery degradation and longevity for energy storage systems
Tebbe, J., Hartwig, A., Jamali, A., Senobar, H., Wahab, A., Kabak, M., Kemper, H., & Khayyam, H. (2025) · Journal of Energy Storage · doi:10.1016/j.est.2025.115724 · Cited by 47
Gupta, P., & Gudmundson, P. (2021) · Journal of Power Sources · doi:10.1016/j.jpowsour.2021.230465 · Cited by 39
Effects of variability and rate on battery charge storage and lifespan
Krieger, E. M. (2013) · PhDT · Cited by 38
Lin, W., & Chen, K.-C. (2022) · Applied Energy · doi:10.1016/j.apenergy.2022.118925 · Cited by 35
Long-range, low-cost electric vehicles enabled by robust energy storage
Liu, P., Ross, R. B., & Newman, A. E. (2015) · MRS Energy & Sustainability · doi:10.1557/mre.2015.13 · Cited by 41
Self-citationZhao, Y., Lü, B., Song, Y., & Zhang, J. (2018) · Frontiers of Structural and Civil Engineering · doi:10.1007/s11709-018-0460-z · Cited by 35
“Particularly, the bi-axially stretched surface of the particle in delithiation process is commonly focused, because it could lead to surface crack which may result in growth of solid electrolyte interphase (SEI) and subsequent battery degradation [17,19,24].”
BackgroundDong, S., Li, C., Li, Z., Ge, X., Miao, X., Wang, P., Zhang, Z., & Yin, L. (2018) · Energy storage materials · doi:10.1016/j.ensm.2018.10.024 · Cited by 35
Alipour, M., Esen, E., Varzeghani, A. R., & Kizilel, R. (2020) · Journal of Electroanalytical Chemistry · doi:10.1016/j.jelechem.2020.113903 · Cited by 39
Aannir, M., Hakkou, R., Levard, C., Taha, Y., Ghennioui, A., Rose, J., & Saadoune, I. (2023) · Journal of Power Sources · doi:10.1016/j.jpowsour.2023.233341 · Cited by 34
“LiCoO 2 was the first cathode material used in LiB technologies and in particular in the portable electronics field given its high volumetric energy density and stable cyclability [3,11,12].”
MethodSarkar, A., Shrotriya, P., & Nlebedim, I. (2022) · Computational materials science · doi:10.1016/j.commatsci.2021.110979 · Cited by 29
Mechano-Electrochemical Stochastics in High-Capacity Electrodes for Energy Storage
Barai, P., & Mukherjee, P. P. (2016) · Journal of The Electrochemical Society · doi:10.1149/2.01191606jes · Cited by 35
Yi, J., Koo, B., Shin, C. B., Han, T., & Park, S. (2017) · Computers & Chemical Engineering · doi:10.1016/j.compchemeng.2017.01.006 · Cited by 33
Karger, A., O’Kane, S. E. J., Rogge, M., Kirst, C., Singer, J., Marinescu, M., Offer, G. J., & Jossen, A. (2024) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/ad76da · Cited by 42
Nagda, V., Ekström, H., & Kulachenko, A. (2024) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/ad5622 · Cited by 32
Zhu, K., Wang, T., Wu, Y., Luo, J., & Huang, Y. (2024) · Energy storage materials · doi:10.1016/j.ensm.2024.103620 · Cited by 51
Zhou, H., Yang, Y., Zhang, Z., Wang, W., Yang, L., & Du, X. (2024) · Journal of Energy Storage · doi:10.1016/j.est.2024.113484 · Cited by 31
Ladpli, P., Kopsaftopoulos, F. P., Nardari, R., & Chang, F. (2017) · Proceedings of SPIE, the International Society for Optical Engineering/Proceedings of SPIE · doi:10.1117/12.2260107 · Cited by 35
“The shift of dV/dQ and dToF/dQ is therefore ascribed to the irreversible loss of lithium ions, most probably due to the solid electrolyte interface (SEI) layer formation on the graphitic electrode [27].”
BackgroundFlügel, M., Richter, K., Wohlfahrt‐Mehrens, M., & Waldmann, T. (2022) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/ac70af · Cited by 31
Baggu, M., Nagarajan, A., Cutler, D. S., Olis, D., Bialek, T., & Symko-Davies, M. (2018) · IEEE Transactions on Sustainable Energy · doi:10.1109/tste.2018.2853673 · Cited by 29
“These include calendar life [7], cycling degradation including electrode stress and fracture (including temperature impacts) [8]–[10], as well as coupling of calendar and cycling mechanisms [11].”
BackgroundStatistical physics-based model of mechanical degradation in lithium ion batteries
Tahmasbi, A. A., & Eikerling, M. H. (2018) · Electrochimica Acta · doi:10.1016/j.electacta.2018.06.119 · Cited by 29
Fan, G., Zhou, B., Ye, S., Shen, H., Huo, D., & Zhang, X. (2024) · Journal of Energy Storage · doi:10.1016/j.est.2024.114086 · Cited by 34
Derating Guidelines for Lithium-Ion Batteries
Sun, Y., Saxena, S., & PECHT, M. G. (2018) · Energies · doi:10.3390/en11123295 · Cited by 34
“Additionally, cycling-induced cracks in the SEI layer provide new sites for the generation and growth of the SEI layer [24].”
BackgroundXia, Q., Wang, Z., Ren, Y., Yang, D., Sun, B., Feng, Q., & Qian, C. (2021) · Journal of Power Sources · doi:10.1016/j.jpowsour.2021.229567 · Cited by 28
Investigation of inhomogeneous degradation in large-format lithium-ion batteries
Li, X., Zeng, T., Qin, H., Huo, R., Liu, Y., Wei, D., & Ding, X. (2021) · Journal of Energy Storage · doi:10.1016/j.est.2021.103113 · Cited by 28
Mechanical stresses at the cathode–electrolyte interface in lithium-ion batteries
Kim, S., & Huang, H. S. (2016) · Journal of materials research/Pratt's guide to venture capital sources · doi:10.1557/jmr.2016.373 · Cited by 26
“…most signi fi cant problems in lithium-ion batteries and can be associated with diffusion-induced stresses, 7 – 15 which have been studied in many electrode materials such as LiCoO 2 , LiMn 2 O 4 , LiFePO 4 , graphite, 16 – 23 etc. 22 – 26 material structural characterization characterization, and”
BackgroundConnecting Particle Fracture with Electrochemical Impedance in LiXMn2O4
McGrogan, F. P., Bishop, S. R., Chiang, Y., & Vliet, K. J. V. (2017) · Journal of The Electrochemical Society · doi:10.1149/2.0941714jes · Cited by 28
Mechanistic Analysis of Mechano-Electrochemical Interaction in Silicon Electrodes with Surface Film
Verma, A., & Mukherjee, P. P. (2017) · Journal of The Electrochemical Society · doi:10.1149/2.0391714jes · Cited by 28
McGrogan, F. P., Raja, S. N., Chiang, Y., & Vliet, K. J. V. (2018) · Journal of The Electrochemical Society · doi:10.1149/2.0191811jes · Cited by 31
Degradation mechanisms and lifetime prediction for lithium-ion batteries — A control perspective
Smith, K. A., Shi, Y., & Santhanagopalan, S. (2015) · Proceedings of the ... American Control Conference/Proceedings of the American Control Conference · doi:10.1109/acc.2015.7170820 · Cited by 45
“multiplicative coupling between calendar and cycling degradation [23].”
BackgroundZhang, Y., & Guo, Z. (2018) · Acta Mechanica Sinica · doi:10.1007/s10409-018-0764-1 · Cited by 26
Huang, P., & Guo, Z. (2021) · Mechanics of Materials · doi:10.1016/j.mechmat.2021.103843 · Cited by 27
Metal–Metal Bonding as an Electrode Design Principle in the Low-Strain Cluster Compound LiScMo 3 O 8
Wyckoff, K. E., Kaufman, J. L., Baek, S. W., Dolle, C., Zak, J. J., Bienz, J. M., Kautzsch, L., Vincent, R. C., Zohar, A., See, K. A., et al. (2022) · Journal of the American Chemical Society · doi:10.1021/jacs.1c12070 · Cited by 25
Basu, S., & Hwang, G. S. (2022) · Acta Materialia · doi:10.1016/j.actamat.2022.118077 · Cited by 26
The scaling of charging rate and cycle number of commercial batteries
Wen, J., Zou, Q., Zhang, Z., Shi, J., & Wei, Y. (2022) · Acta Mechanica Sinica · doi:10.1007/s10409-022-22108-x · Cited by 25
Mathematical Modeling of Aging of Li-Ion Batteries
Delacourt, C., & Safari, M. (2015) · Green energy and technology · doi:10.1007/978-1-4471-5677-2_5 · Cited by 33
“Fractures in the SEI account for newly exposed surface of the graphite particles to the electrolyte and therefore promote electrolyte decomposition [23].”
BackgroundNovel Data-Efficient Mechanism-Agnostic Capacity Fade Model for Li-Ion Batteries
Kim, M., & Han, S. (2020) · IEEE Transactions on Industrial Electronics · doi:10.1109/tie.2020.2996156 · Cited by 26
Guo, D., Yang, G., Han, X., Feng, X., Lu, L., & Ouyang, M. (2021) · International Journal of Energy Research · doi:10.1002/er.6614 · Cited by 28
A Calculation Model to Assess Two Irreversible Capacities Evolved in Silicon Negative Electrodes
Lee, J. G., Kim, J., Park, H. S., Lee, J. B., Ryu, J. H., Kim, J. J., & Oh, S. M. (2015) · Journal of The Electrochemical Society · doi:10.1149/2.0821508jes · Cited by 24
Stress Evolution on the Phase Boundary in LiFePO4Particles
ChiuHuang, C.-K., & Huang, H. S. (2013) · Journal of The Electrochemical Society · doi:10.1149/2.079311jes · Cited by 23
Simulation Study on Heat Generation Characteristics of Lithium-Ion Battery Aging Process
Huang, R. N., Xu, Y., Wu, Q., Chen, J., Chen, F., & Yu, X. (2023) · Electronics · doi:10.3390/electronics12061444 · Cited by 26
Clerici, D., Mocera, F., & Somà, A. (2020) · Energies · doi:10.3390/en14010134 · Cited by 23
Battery age monitoring: Ultrasonic monitoring of ageing and degradation in lithium-ion batteries
Williams, D., Green, J., Bugryniec, P. J., Brown, S., & Dwyer-Joyce, R. S. (2025) · Journal of Power Sources · doi:10.1016/j.jpowsour.2025.236174 · Cited by 26
Mechanical contact in composite electrodes of lithium-ion batteries
Lü, B., Zhao, Y., Feng, J., Song, Y., & Zhang, J. (2019) · Journal of Power Sources · doi:10.1016/j.jpowsour.2019.227115 · Cited by 22
Study of aging mechanisms in lithium-ion batteries for working vehicle applications
Mocera, F., Somà, A., & Clerici, D. (2020) · International Conference on Ecological Vehicles and Renewable Energies (EVER) · doi:10.1109/ever48776.2020.9243079 · Cited by 33
“The concentration gradient causes a mechanical stress state within the particle, which is the driving force for damage and crack propagation [4], [11].”
Background
Metadata
- Authors
- Deshpande, R., Verbrugge, M., Cheng, Y.-T., Wang, J., & Liu, P.
- Affiliations
- University of Kentucky (US)
- General Motors (United States) (US)
- HRL Laboratories (United States) (US)
- Venue
- Journal of The Electrochemical Society
- Publisher
- The Electrochemical Society
- Published
- 2012
- Volume
- 159
- Issue
- 10
- Pages
- A1730-A1738
- ISSN
- 0013-4651 (ISSN-L)
- 1945-7111
- OpenAlex
- W2021615999
- Cited by
- 389
- References
- 49
- Citations by year
- 2026: 33 · 2025: 30 · 2024: 33 · 2023: 31 · 2022: 27 · 2021: 29 · 2020: 31 · 2019: 25 · 2018: 25 · 2017: 30 · 2016: 28 · 2015: 29 · 2014: 21 · 2013: 17
- FWCI
- 38.54
- Type
- journal article
- Language
- en
- Open access
- closed
- Locations
- Journal of The Electrochemical Society (publishedVersion)
- Funders
- National Science Foundation
- Topics
- Physical Sciences › Engineering › Automotive Engineering › Battery Modeling and Management
- Physical Sciences › Engineering › Electrical and Electronic Engineering › Advancements in Battery Materials
- Physical Sciences › Engineering › Electrical and Electronic Engineering › Advanced Battery Materials and Technologies
- Keywords
- lithium-ion batteries, irreversible capacity, solid electrolyte interphase, lithium consumption, diffusion-induced stress, electrode cracking, Paris law, temperature effects, electrode-electrolyte interface
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.