Battery Cycle Life Prediction with Coupled Chemical Degradation and Fatigue Mechanics
The DOI matches its Crossref record; 50 of the 50 references it cites were found in a registry or an index.
Abstract
Coupled mechanical-chemical degradation of electrodes upon charging and discharging has been recognized as a major failure mechanism in lithium ion batteries. The instability of commonly employed electrolytes results in solid electrolyte interphase (SEI) formation. Although the SEI layer is necessary, as it passivates the electrode-electrolyte interface from further solvent decomposition, SEI formation consumes lithium and thus contributes to irreversible capacity loss. In this paper, we study irreversible capacity loss in a graphite-LiFePO 4 cell. Our results support the mechanism of irreversible capacity loss due to the consumption of lithium in forming SEI. We attribute irreversible capacity loss to diffusion induced stresses (DISs) that cause pre-existing cracks on the electrode surfaces to grow gradually upon cycling, leading to the growth of SEI on the newly exposed electrode surfaces. Because lithium is consumed in forming the new SEI, irreversible capacity loss continues with cycling. Along with the SEI formation upon newly exposed (cracked) surfaces, the existing SEI thickness also grows with cycling, resulting in additional loss of lithium. In this study, we provide, a simple mathematical model, based on the Paris’ Law formulation of mechanical fatigue, in combination with chemical degradation to explain battery life. We compare the predicted capacity at different temperatures with the experimental data obtained from electrochemical measurements on graphite-LiFePO 4 cells.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“which is why most physics-based models focus only on the most dominant mechanisms, such as the formation and growth of the solid electrolyte interphase (SEI) [11,12] or electronic contact loss through particle cracking [13,14].”
From Degradation diagnostics for lithium ion cells (2017) · cites this paper as [14]
Citations
Cites
Phospho‐olivines as Positive‐Electrode Materials for Rechargeable Lithium Batteries
Padhi, A. K., Nanjundaswamy, K. S., & Goodenough, J. B. (1997) · Journal of The Electrochemical Society · doi:10.1149/1.1837571 · Cited by 7,933
A Critical Analysis of Crack Propagation Laws
Paris, P., & Erdogan, F. (1963) · Journal of Basic Engineering · doi:10.1115/1.3656900 · Cited by 7,122
Lawn, B. (1993) · Cambridge University Press eBooks · doi:10.1017/cbo9780511623127 · Cited by 4,759
Suresh, S. (1998) · Cambridge University Press eBooks · doi:10.1017/cbo9780511806575 · Cited by 4,526
Battery materials for ultrafast charging and discharging
Kang, B., & Ceder, G. (2009) · Nature · doi:10.1038/nature07853 · Cited by 3,480
Insertion Electrode Materials for Rechargeable Lithium Batteries
Winter, M., Besenhard, J. O., Spahr, M. E., & Novák, P. (1998) · Advanced Materials · doi:10.1002/(sici)1521-4095(199807)10:10<808::aid-adma808>3.0.co;2-r · Cited by 2,998
Insertion Electrode Materials for Rechargeable Lithium Batteries
Winter, M., Besenhard, J. O., Spahr, M. E., & Novák, P. (1998) · Advanced Materials · doi:10.1002/(sici)1521-4095(199807)10:10<725::aid-adma725>3.0.co;2-z · Cited by 2,965
Electronically conductive phospho-olivines as lithium storage electrodes
Chung, S.-Y., Bloking, J. T., & Chiang, Y.-M. (2002) · Nature Materials · doi:10.1038/nmat732 · Cited by 2,939
Aurbach, D. (2000) · Journal of Power Sources · doi:10.1016/s0378-7753(00)00431-6 · Cited by 2,130
Fracture Mechanics: Fundamentals and Applications, Third Edition
Anderson, T. L., & Anderson, T. L. (2005) · CRC Press eBooks · doi:10.1201/9781420058215 · Cited by 1,854
Research works printed but not linked: 1
- Ragab A. R. Bayoumi S. B. , Engineering Solid Mechanics- Fundamental and Applications. (CRC Press, Boca Ranton, FL, 1999).
Cited by
Items 301–389 of 389
Porous Agglomerate Model for Battery Electrodes and Application to the Lithium-Silicon System
Verbrugge, M. W., & Baker, D. R. (2025) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/adbf51 · Cited by 5
Self-citationMeasurement of a health index for Li-Ion batteries
Gross, G., & Landi, M. (2013) · IEEE International Instrumentation and Measurement Technology Conference · doi:10.1109/i2mtc.2013.6555405 · Cited by 4
“Instead the cycle life regards the number of cycles of charge/discharge that a battery is capable of sustaining: this value is strongly dependent on usage and on environmental and operational parameters [7].”
BackgroundPuech, A., Dimitrov, G., & D’Ambrosio, C. (2023) · IEEE PES Innovative Smart Grid Technologies Europe · doi:10.1109/isgteurope56780.2023.10408725 · Cited by 4
“1) Capacity fading: During the life of the battery, its capacity decreases with the number of cycles [13].”
BackgroundSong, H., Xie, H., Zhang, Z., Zhang, Q., & Kang, Y. (2025) · Acta Mechanica Solida Sinica · doi:10.1007/s10338-025-00585-w · Cited by 5
Bezzola, A., Bales, B. B., Petzold, L. R., & Alkire, R. C. (2014) · Journal of The Electrochemical Society · doi:10.1149/2.001408jes · Cited by 4
Zheng, H., Zhu, G., Qu, Q., Yang, S., & Zheng, H. (2017) · Electrochimica Acta · doi:10.1016/j.electacta.2017.03.001 · Cited by 4
Verbrugge, M. W., Wampler, C. W., & Baker, D. R. (2018) · Journal of The Electrochemical Society · doi:10.1149/2.0951816jes · Cited by 4
Self-citationRaj, P., Richter, E., Schofer, K., Kempf, J., Michel, F., Fill, A., & Birke, K. P. (2025) · e-Prime - Advances in Electrical Engineering Electronics and Energy · doi:10.1016/j.prime.2025.101103 · Cited by 8
Long, Z., Chen, K., Tang, M., Zheng, X., Wang, H., Luo, Y., Li, Y., Nie, G., Zhang, X., Gao, G., et al. (2026) · International Journal of Green Energy · doi:10.1080/15435075.2026.2619449 · Cited by 9
“The resulting SEI thickening progressively consumes electrolyte and lithium inventory, raising internal resistance and accelerating capacity fade (Koltypin et al. 2002; Christensen and Newman 2003; Deshpande et al. 2012; An et al. 2016; Lin et al. 2017).”
Wei, Y., Liu, K., Rui, J., & Zhao, Q. (2026) · Energy and AI · doi:10.1016/j.egyai.2026.100713 · Cited by 4
SEI-Coated Carbon Particles: Electrochemomechanical Fracture Mechanisms
Sanjuan, A., Mitra, A. S., & García, R. E. (2024) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/ad1d92 · Cited by 3
Somakettarin, N., Sugihara, H., & Funaki, T. (2017) · IEICE Electronics Express · doi:10.1587/elex.14.20170690 · Cited by 3
“The cycling capacity fade is mainly due to the loss of cycleable lithium with growing of the solid electrolyte interface (SEI) layer on the surface of the carbon-based negative electrode [20], and is partly due to the loss of active electrode materials [21].”
BackgroundZhao, T., Huang, X., Meng, Y., Shen, J., Zheng, Y., Chang, L., & Chen, S. (2022) · Journal of Materials Science · doi:10.1007/s10853-022-07576-z · Cited by 3
“In addition, the less decomposition of Li2O can interrupt the disinsertion of Li ions during the first charging process [45, 46].”
BackgroundMoser, S., Aribia, A., Scaffidi, R., Gilshtein, E., Brammertz, G., Vermang, B., Tiwari, A. N., & Carron, R. (2023) · ACS Applied Energy Materials · doi:10.1021/acsaem.3c02483 · Cited by 3
Online detection and identification of cathode cracking in Lithium-ion battery cells
Padisala, S. K., Sattarzadeh, S., & Dey, S. (2024) · Journal of Energy Storage · doi:10.1016/j.est.2024.112441 · Cited by 4
Ding, X., Ni, Y., Zhu, D., Li, Z., Jiao, Y., & Wang, Q. (2025) · Journal of Applied Electrochemistry · doi:10.1007/s10800-025-02262-9 · Cited by 3
Battery management in V2G-based aggregations
Landi, M., & Gross, G. (2014) · Power Systems Computation Conference · doi:10.1109/pscc.2014.7038109 · Cited by 6
“As described in [6], the electrochemical reactions, related to energy conversion, that take place inside the single cell tend to lower the battery capacity.”
BackgroundInvestigation into the Effect of Thermal Management on the Capacity Fade of Lithium-ion Batteries
Carnovale, A. (2017) · UWSpace (University of Waterloo) · Cited by 3
Zhao, K. (2021) · Elsevier eBooks · doi:10.1016/b978-0-12-819723-3.00047-0 · Cited by 2
EV Battery Degradation Assessment Under Standard Drive Cycles Using Simulated EIS
Jayasinghe, A. E., Fernando, N., Kumarawadu, S., Wang, L., & Karunadasa, J. P. (2025) · Vehicles · doi:10.3390/vehicles7010021 · Cited by 5
“They can be categorized as empirical models and physical models [36].”
Xiao, M., Bai, X., Ma, Y., Zhang, S., & Ye, J. (2026) · Journal of Energy Storage · doi:10.1016/j.est.2025.120000 · Cited by 2
Effects of electrolyte infiltration on the cracking of active materials in lithium-ion batteries
Peng, Y., & Hao, F. (2026) · Extreme Mechanics Letters · doi:10.1016/j.eml.2026.102452 · Cited by 2
Structural and thermal regulation of strain behavior in batteries under air and immersion cooling
He, H., Liu, Q., He, K., Zhu, X., Xu, C., & Jü, X. (2026) · Energy · doi:10.1016/j.energy.2026.140112 · Cited by 2
Modeling effect of magnetic field on multicycle aging under fast charging of lithium battery
Tomar, I., & Sarkar, A. (2026) · Applied Energy · doi:10.1016/j.apenergy.2026.127788 · Cited by 2
Wu, H., Zhang*, Y., & Mu*, D. (2026) · Energy Z · doi:10.20517/energyz.2026.24 · Cited by 2
One-Time Prediction of Battery Capacity Fade Curve under Multiple Fast Charging Strategies
Han, X., Dai, Z., Ren, M., Cui, J., & Shi, Y. (2024) · Batteries · doi:10.3390/batteries10030074 · Cited by 2
Han, J., Zhu, C., Fan, G., Guo, B., Zeng, Z., & Zhang, X. (2024) · IEEE Transactions on Transportation Electrification · doi:10.1109/tte.2024.3392371 · Cited by 3
“To describe the sub-critical crack growth resulting from mechanical fatigue, Paris’ Law, a well-known empirical expression, is commonly employed [19], [20]. where a is the depth of the surface crack, N is heating times, and σ max θ is the maximum tangential stress during self-heating.”
Training-improved electrochemical performances of silicon-based lithium-ion batteries
Zhang, K., Zhou, J., Zheng, B., Li, Y., & Yang, F. (2024) · Journal of Power Sources · doi:10.1016/j.jpowsour.2024.236020 · Cited by 2
A Mean-Covariance Decomposition Modeling Method for Battery Capacity Prognostics
Guo, J. H., & Li, Z. S. (2017) · International Conference on Sensing, Diagnostics, Prognostics, and Control (SDPC) · doi:10.1109/sdpc.2017.110 · Cited by 2
“For example, the chemical analytic model from [29], [38] can be referred as the basic model of mean, which would be discussed in Section 3.”
BackgroundAlipour, M., & Kizilel, R. (2020) · Journal of Thermal Engineering · doi:10.18186/thermal.822509 · Cited by 2
“As a result, the LiFePO4 electrode forms Fe ions and catalysis the side reactions on the anode, causing the SEI film to increase in thickness [33-35].”
BackgroundImproving the Efficiency of Electric Buses in a City Transport Company
Solntsev, A. A., Максимов, В. А., Evarestov, V. M., & Nguyen, V. T. (2022) · Intelligent Technologies and Electronic Devices in Vehicle and Road Transport Complex (TIRVED) · doi:10.1109/tirved56496.2022.9965554 · Cited by 2
“The biggest decrease in battery lifespan occurs during constant operation at a high level of battery charge discharging the battery only up to 75% based on research on lithium-ion batteries of electric vehicles [3, 6, 8, 9].”
BackgroundLiu, S. (2020) · UVic’s Research and Learning Repository (University of Victoria) · Cited by 5
Energy Storage Battery Life Prediction Based on CSA-BiLSTM
Zhao, R., Zhou, S., Xu, X., & Zhang, S. (2024) · Lecture notes in electrical engineering · doi:10.1007/978-981-99-9251-5_12 · Cited by 1
Mechanics of Lithium-Ion Batteries: Aging and Diagnostics
Clerici, D., Pistorio, F., & Somà, A. (2026) · World Electric Vehicle Journal · doi:10.3390/wevj17010055 · Cited by 4
“However, these two effects are generally treated independently in the literature, often assuming a constant number of cracks throughout the battery lifetime [35], a simplification that limits physical accuracy.”
Lithium-ion battery degradation: comparison of three modeling methodologies
Bessler, W. G., & Dubarry, M. (2026) · Elsevier eBooks · doi:10.1016/b978-0-12-819987-9.00007-x · Cited by 4
Acker, L., Fiore, L. V., Stenger, E., & Konrad, J. (2026) · Batteries · doi:10.3390/batteries12040134 · Cited by 2
Zhou, H., Lei, Q., Jiang, Y., Zhou, K., He, L., Peng, C., Qiu, Z., & Chen, W. Q. (2026) · Resources Conservation and Recycling · doi:10.1016/j.resconrec.2026.108955 · Cited by 1
Xiao, J., Wang, Y., Wang, S., Soo, Y., & Chen, Z. (2026) · IEEE Transactions on Industrial Electronics · doi:10.1109/tie.2026.3682394 · Cited by 3
“This term softly penalizes parameters θ p ∈ Θ k that violate predefined realistic bounds [ θ p , θ p ] , enhancing stability and interpretability [22] To dynamically balance the loss components and prevent any term from overwhelming the gradients, the weights ω for each physics-related loss are…”
Avila, A., Remírez, A., Gandiaga, I., Carreras, L., & Maimí, P. (2026) · eTransportation · doi:10.1016/j.etran.2026.100599 · Cited by 1
Electric vehicles in Smart Grids: Performance considerations
Nath, U. K. D. (2015) · Cited by 1
Gao, Y., Cho, M., & Zhou, M. (2013) · Cited by 1
Thermal Management of the Li-Ion Battery Pack with Phase Change Material (PCM)
Kumar, T. M., & Vijay Ram, C. (2021) · SAE technical papers on CD-ROM/SAE technical paper series · doi:10.4271/2021-26-0140 · Cited by 1
Performance degradation modeling in silicon anodes
Mukherjee, P. P., & Verma, A. (2021) · Elsevier eBooks · doi:10.1016/b978-0-12-819660-1.00004-9 · Cited by 1
Hwang, G., Sitapure, N., Moon, J., Hwang, S., & Kwon, J. S. (2022) · Proceedings of the ... American Control Conference/Proceedings of the American Control Conference · doi:10.23919/acc53348.2022.9867429 · Cited by 1
“layer of thickness (δSEI,0) between the electrode and the electrolyte [14].”
BackgroundDiffusion, Deformation, and Damage in Lithium-Ion Batteries and Microelectronics
Pharr, M. (2014) · Digital Access to Scholarship at Harvard (DASH) (Harvard University) · Cited by 1
The Material Separation Process for Recycling End-of-life Li-ion Batteries
Li, L. (2020) · VTechWorks (Virginia Tech) · Cited by 2
Santoki, J. (2021) · Repository KITopen (Karlsruhe Institute of Technology) · doi:10.5445/ir/1000128098 · Cited by 1
Microscopy of Chemical and Mechanical Heterogeneities in Lithium Cobalt Oxide
Diercks, D. R., Musselman, M. A., Kumar, M., Gorman, B. P., & Packard, C. E. (2015) · Microscopy and Microanalysis · doi:10.1017/s1431927615003414
Analysis of Impedance Response in Lithium-ion Battery Electrodes
Cho, S. (2013) · OakTrust (Texas A&M University Libraries)
Tahmasbi, A. A. (2019) · Summit (Simon Fraser University)
An Insight into the Battery Degradation and a Proposal for a Battery Friendly Charging TechniquePreprint
Sah, B., & Kumar, P. (2021) · Research Square · doi:10.21203/rs.3.rs-710085/v1
Chemo-Mechanical Model of SEI Growth on SiliconPreprint
von Kolzenberg, L., Latz, A., & Horstmann, B. (2021) · arXiv (Cornell University)
Electrochemical Flow System for Li-Ion Battery Recycling and Energy Storage
Yang, T. (2021) · VTechWorks (Virginia Tech)
Simulation Study on Thermal Runaway of Lithiumion Batteries in Different Aging States
Xu, Y., Yu, X., Huang, R. N., & Lu, G. (2023) · International Conference on Energy Engineering and Power Systems (EEPS) · doi:10.1109/eeps58791.2023.10256891
Influence of magnetic field on charge and discharge performance of electric vehicle power battery
Ruan, G., Fu, X., Hu, X., Cao, J., & Yan, R. (2023) · Proceedings of the Institution of Mechanical Engineers Part D Journal of Automobile Engineering · doi:10.1177/09544070231207915 · Cited by 1
“Deshpande et al. 3 and An et al. 4 found that the SEI film formation with increasing film thickness was the key cause of battery aging.”
The Impact of Thermal Damage Accumulation on Thermal Runaway Behavior of Lithium-Ion BatteriesPreprint
Xiao, Y., Liu, M., Lu, H., Gao, Z., Wang, D., Yang, F., Wang, J., Kou, Z., Huang, Z., Zhang, S., et al. (2024) · SSRN Electronic Journal · doi:10.2139/ssrn.4767710
Self-citationSong, H., Xie, H., Zhang, Z., Zhang, Q., & Kang, Y. (2024) · SSRN Electronic Journal · doi:10.2139/ssrn.4775283
Williams, D., Green, J., Bugryniec, P. J., Brown, S., & Dwyer-Joyce, R. S. (2024) · SSRN Electronic Journal · doi:10.2139/ssrn.4812332
The Impact of Thermal Damage Accumulation on Thermal Runaway Behavior of Lithium-Ion BatteriesPreprint
Xiao, Y., Liu, M., Lu, H., Gao, Z., Wang, D., Yang, F., Wang, J., Kou, Z., & Yuan, Q. (2024) · SSRN Electronic Journal · doi:10.2139/ssrn.4861862
Self-citationAnalytical design of electrode particle debonding for battery applications
Mitra, A. S., Anapolsky, A., & García, R. E. (2024) · Modelling and Simulation in Materials Science and Engineering · doi:10.1088/1361-651x/ad5f49
“Electrochemically induced cycling fatigue was first modeled by Deshpande et al [51], using a Paris law-type description [26].”
Xiao, J., Jiang, C., Terzi, S., Anwer, N., & Eynard, B. (2024) · SSRN Electronic Journal · doi:10.2139/ssrn.4960301
Bharathamani, D. K., Nagarajan, M., Ravi, S., & Sugumaran, N. (2025) · Future Batteries · doi:10.1016/j.fub.2025.100097
Modeling the Coupled Stress Relaxation and SEI Evolution in Preload-Constrained Lithium-Ion Cells
Li, J., Li, X., Yang, Z., Li, H., Liu, S., Shi, J., Fan, X., Cong, Z., Feng, X., & Yang, X.-G. (2025) · Applied Sciences · doi:10.3390/app152312528
Kim, S.-S., Lee, I., Jeon, Y., Lee, C., Lee, T., Koo, J., Jung, I., Moon, J., Park, J., & Jeong, K. (2025) · Journal of Power Sources · doi:10.1016/j.jpowsour.2025.238934
Chaoyi, S., Geng, S., Kai, Z., Junwu, Z., XinYang, W., Li, Y., & Bailin, Z. (2026) · Acta Physica Sinica · doi:10.7498/aps.75.20251423
Xiong, R., Wang, X., Chen, H., & Luan, W. (2026) · Fatigue & Fracture of Engineering Materials & Structures · doi:10.1111/ffe.70187
Xuyang, L., Jian, L., Bingyu, X., Lei, S., Xuzhi, L., & Hongfei, W. (2025) · International Conference on Robotics, Control and Automation Engineering (RCAE) · doi:10.1109/rcae66389.2025.11355192
“For instance, based on the Single Particle (SP) model [6], [7] derived a degradation rate model that simultaneously accounts for diffusion-induced stress (DIS), crack propagation, and solid electrolyte interphase (SEI) thickness growth, thereby enabling degradation modeling under DIS-dominated…”
Control-Centric Comprehensive Degradation Model for Prediction of Battery LifespanPreprint
Zhu, Y., Plateau, T. P., Riemann, B. J. C., Landers, R. G., & Park, J. (2025) · SSRN Electronic Journal · doi:10.2139/ssrn.5391512
Simulation-Based Evaluation of Lithium-Ion Batteries Manufacturing Performance
Yan, Y., Meng, J., Song, Z., zhang, S., Pan, Y., Yang, P., & Peng, J. (2026) · SAE International Journal of Advances and Current Practices in Mobility · doi:10.4271/2026-01-7005
Tabaković, J., Katrašnik, T., & Zelič, K. (2026) · SSRN Electronic Journal · doi:10.2139/ssrn.6352728
Fast charging strategies of a lithium-ion battery using aging model
Mohajer, S. (2019) · theses.fr (ABES) · doi:10.70675/a5737791zf505z4657zb5bez3f86357d5300
Optimisation de couches minces de PZT antiferroélectrique pour le stockage d'énergie
Coulibaly, M. D. (2019) · theses.fr (ABES) · doi:10.70675/738c7ac3z848cz4439zb24fze257b57d2b58
Li, X., Zhao, S., Wei, X., Zhu, Y., & Tian, J. (2026) · Chinese Journal of Electrical Engineering · doi:10.23919/cjee.2025.000193
Natterer, J., Oehler, F. F., O’Kane, S. E. J., Marinescu, M., Offer, G. J., & Jossen, A. (2026) · Journal of Power Sources · doi:10.1016/j.jpowsour.2026.240036
Wei, Y., Liu, K., Rui, J., Zhao, S., & Zhao, Q. (2026) · Measurement · doi:10.1016/j.measurement.2026.122305
Zhang, B., Zou, X., Wen, X., Wu, J., Pan, J., Tan, X., & Cross, J. L. (2026) · Carbon Neutralization · doi:10.1002/cnl2.70180
“Battery degradation involves complex phenomena occurring at multiple lengths and time scales, ranging from atomistic processes to macroscopic system‐level behavior [151, 152].”
A meta-learning framework for battery lifetime prediction across unseen operating conditions
Zhang, Y. B., Zhang, J., Jiang, W., Shen, L., & Song, Z. (2026) · Energy storage materials · doi:10.1016/j.ensm.2026.105296 · Cited by 1
Modak, A., Gupta, A., Gangwar, T., Chowdhury, R., & Duddu, R. (2026) · Engineering Fracture Mechanics · doi:10.1016/j.engfracmech.2026.112420
A physics-enhanced multimodal neural network for lithium-ion battery state of health estimation
Yang, Y., & Ling, Q. (2026) · Journal of Energy Storage · doi:10.1016/j.est.2026.123497
Sachdeva, L., & Anand, U. (2026) · Energy Storage and Conversion · doi:10.59400/esc4509
“…cycle count from rainflow decomposition of the current SoC trajectory, SoC Ray is the manufacturer-rated full cycle count at the corresponding depth-of-discharge (DoD), and w ( DoD i ) is a depth-severity weighting factor derived from Wöhler curve fitting to experimental aging data [28].”
Gao, J., Wang, S., Chen, R., Zio, E., Dui, H., & Zhang, C. (2026) · Measurement Science and Technology · doi:10.1088/1361-6501/ae978b
“Instead, internal lattice strain accumulates over consecutive cycles before culminating in structural isolation and measurable capacity fade [52].”
Electrode-Level Diagnosis of Lithium-Ion Battery Path-Dependent Degradation Using a Half-Cell Model
Wang, B., Gao, Y., & Zhang, Y. (2026) · Batteries · doi:10.3390/batteries12080313
3D printing in battery technology: Leveraging magnetism for superior energy storage
Thakur, K., & Sarkar, A. (2026) · Renewable and Sustainable Energy Reviews · doi:10.1016/j.rser.2026.117473
Physics-Informed Gaussian Process Regression for Battery Health Estimation Under Distribution Shift
Kuntambila, D., & Chen, J. S. (2026) · IEEE Systems Man and Cybernetics Letters · doi:10.1109/lsmc.2026.3739153
“Frameworks coupling electrochemical, thermal, and mechanical degradation pathways exist for this purpose: building on the Doyle–Fuller– Newman (DFN) formulation [14], the open-source PyBaMM library jointly captures the dominant degradation mechanisms [15], [16], [17], [18].”
Lei, G., Planella, F. B., Baird, S. G., & Cooper, S. J. (2026) · Advanced Science · doi:10.1002/advs.78012
“The cell was parameterized using the Ai2020 dataset [ 32 ] and equipped with the following degradation submodels: swelling-induced cracking [ 33 ], stress-driven loss of active material [ 34 ], reaction-limited SEI growth with porosity change [ 35 ], and SEI formation on cracks [ 33 ].”
Kwon, H., Lee, C., Park, J., Son, H., & Jo, E. (2026) · Micro and Nano Systems Letters · doi:10.1186/s40486-026-00268-2
“Most of these nodes are battery-powered, and their repeated charging, replacement, and disposal incur considerable cost and labor over long-term operation [6, 7].”
Raj, P., Richter, E., Schofer, K., Kempf, J., Michel, F., Fill, A., & Birke, K. P. (2026) · Journal of Energy Storage · doi:10.1016/j.est.2026.125113
Metadata
- Authors
- Deshpande, R., Verbrugge, M., Cheng, Y.-T., Wang, J., & Liu, P.
- Affiliations
- University of Kentucky (US)
- General Motors (United States) (US)
- HRL Laboratories (United States) (US)
- Venue
- Journal of The Electrochemical Society
- Publisher
- The Electrochemical Society
- Published
- 2012
- Volume
- 159
- Issue
- 10
- Pages
- A1730-A1738
- ISSN
- 0013-4651 (ISSN-L)
- 1945-7111
- OpenAlex
- W2021615999
- Cited by
- 389
- References
- 49
- Citations by year
- 2026: 33 · 2025: 30 · 2024: 33 · 2023: 31 · 2022: 27 · 2021: 29 · 2020: 31 · 2019: 25 · 2018: 25 · 2017: 30 · 2016: 28 · 2015: 29 · 2014: 21 · 2013: 17
- FWCI
- 38.54
- Type
- journal article
- Language
- en
- Open access
- closed
- Locations
- Journal of The Electrochemical Society (publishedVersion)
- Funders
- National Science Foundation
- Topics
- Physical Sciences › Engineering › Automotive Engineering › Battery Modeling and Management
- Physical Sciences › Engineering › Electrical and Electronic Engineering › Advancements in Battery Materials
- Physical Sciences › Engineering › Electrical and Electronic Engineering › Advanced Battery Materials and Technologies
- Keywords
- lithium-ion batteries, irreversible capacity, solid electrolyte interphase, lithium consumption, diffusion-induced stress, electrode cracking, Paris law, temperature effects, electrode-electrolyte interface
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.