Study of the Failure Mechanisms of LiNi0.8Mn0.1Co0.1O2Cathode Material for Lithium Ion Batteries
Open accessAbstract
LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) can deliver a high capacity of ∼200 mAh/g with an average discharge potential of ∼3.8 V (vs. Li + /Li), making it a promising positive electrode material for high energy density lithium ion batteries. However, electrochemical tests from half cells and full cells show poor cycling performance when charged to potentials above 4.2 V. The calendar and cycle lifetimes of cells are affected by the structural stability of the active electrode materials as well as the parasitic reactions that occur in lithium ion batteries. In order to explore the major failure mechanisms of the material, half cells (coin cells) with control electrolyte and full cells (pouch cells) with control electrolyte and with selected electrolyte additives were tested over four different potential ranges. Isothermal microcalorimetry was used to explore the parasitic reactions and their potential dependence. In-situ and ex-situ X-ray diffraction and scanning electron microscopy were used to investigate the structural and morphological degradation of the materials over cycling. It was found that the dramatic c-axis change of the active material during charge and discharge may not be the major problem for cells that are cycled to higher potentials. The parasitic reactions that arise from the interactions between the electrolyte and the highly reactive delithiated cathode surface at high potentials are suggested as the main reason for the failure of cells cycled above 4.2 V. It should be possible to further improve the performance of NMC811 at high potentials by modifying the cathode surface and/or identifying and using electrolyte blends which reduce parasitic reactions.
Overview
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Electrolytes and Interphases in Li-Ion Batteries and Beyond
Xu, K. (2014) · Chemical Reviews · doi:10.1021/cr500003w · Cited by 5,566
Noh, H.-J., Youn, S., Yoon, C. S., & Sun, Y.-K. (2013) · Journal of Power Sources · doi:10.1016/j.jpowsour.2013.01.063 · Cited by 2,302
Lu, Z., & Dahn, J. R. (2002) · Journal of The Electrochemical Society · doi:10.1149/1.1480014 · Cited by 1,016
Self-citationLu, Z., MacNeil, D. D., & Dahn, J. R. (2001) · Electrochemical and Solid-State Letters · doi:10.1149/1.1407994 · Cited by 941
Self-citationFormation of the Spinel Phase in the Layered Composite Cathode Used in Li-Ion Batteries
Gu, M., Belharouak, I., Zheng, J., Wu, H., Xiao, J., Genc, A., Amine, K., Thevuthasan, S., Baer, D. R., Zhang, J.-G., et al. (2013) · ACS Nano · doi:10.1021/nn305065u · Cited by 918
Lu, Z., Beaulieu, L. Y., Donaberger, R. A., Thomas, C. L., & Dahn, J. R. (2002) · Journal of The Electrochemical Society · doi:10.1149/1.1471541 · Cited by 906
Self-citationIn situ x-ray diffraction and electrochemical studies of Li1−xNiO2
LI, W., Reimers, J. N., & Dahn, J. R. (1993) · Solid State Ionics · doi:10.1016/0167-2738(93)90317-v · Cited by 745
Self-citationMohanty, D., Kalnaus, S., Meisner, R. A., Rhodes, K. J., Li, J., Payzant, E. A., Wood, D. L., & Daniel, C. (2012) · Journal of Power Sources · doi:10.1016/j.jpowsour.2012.11.144 · Cited by 531
Self-citationBoulineau, A., Simonin, L., Colin, J.-F., Bourbon, C., & Patoux, S. (2013) · Nano Letters · doi:10.1021/nl4019275 · Cited by 467
Smith, A. J., Burns, J. C., Trussler, S., & Dahn, J. R. (2010) · Journal of The Electrochemical Society · doi:10.1149/1.3268129 · Cited by 369
Self-citationEffect of Residual Lithium Compounds on Layer Ni-Rich Li[Ni0.7Mn0.3]O2
Cho, D.-H., Jo, C.-H., Cho, W., Kim, Y.-J., Yashiro, H., Sun, Y.-K., & Myung, S.-T. (2014) · Journal of The Electrochemical Society · doi:10.1149/2.042406jes · Cited by 340
Predicting and Extending the Lifetime of Li-Ion Batteries
Burns, J. C., Kassam, A., Sinha, N. N., Downie, L. E., Solnickova, L., Way, B. M., & Dahn, J. R. (2013) · Journal of The Electrochemical Society · doi:10.1149/2.060309jes · Cited by 321
Self-citationInterpreting High Precision Coulometry Results on Li-ion Cells
Smith, A. J., Burns, J. C., Xiong, D., & Dahn, J. R. (2011) · Journal of The Electrochemical Society · doi:10.1149/1.3625232 · Cited by 308
Self-citationCobalt-Free Nickel Rich Layered Oxide Cathodes for Lithium-Ion Batteries
Sun, Y.-K., Lee, D.-J., Lee, Y. J., Chen, Z., & Myung, S.-T. (2013) · ACS Applied Materials & Interfaces · doi:10.1021/am403684z · Cited by 296
A High Precision Coulometry Study of the SEI Growth in Li/Graphite Cells
Smith, A. J., Burns, J. C., Zhao, X., Xiong, D., & Dahn, J. R. (2011) · Journal of The Electrochemical Society · doi:10.1149/1.3557892 · Cited by 288
Self-citationA High Precision Study of the Coulombic Efficiency of Li-Ion Batteries
Smith, A. J., Burns, J. C., & Dahn, J. R. (2010) · Electrochemical and Solid-State Letters · doi:10.1149/1.3487637 · Cited by 170
Self-citationSmart design of lithium-rich layered oxide cathode compositions with suppressed voltage decay
Lee, E. S., & Manthiram, A. (2014) · Journal of Materials Chemistry A · doi:10.1039/c3ta14975g · Cited by 111
A Systematic Study of Electrolyte Additives in Li[Ni1/3Mn1/3Co1/3]O2 (NMC)/Graphite Pouch Cells
Wang, D., Xia, J., Ma, L., Nelson, K. J., Harlow, J., Xiong, D., Downie, L., Petibon, R., Burns, J. C., Xiao, A., et al. (2014) · Journal of The Electrochemical Society · doi:10.1149/2.0511412jes · Cited by 110
Self-citationMa, L., Xia, J., Xia, X., & Dahn, J. R. (2014) · Journal of The Electrochemical Society · doi:10.1149/2.0091410jes · Cited by 77
Self-citationMa, L., Xia, J., & Dahn, J. R. (2014) · Journal of The Electrochemical Society · doi:10.1149/2.1041414jes · Cited by 72
Self-citationJiang, J.-S., Eberman, K. W., Krause, L. J., & Dahn, J. R. (2005) · Journal of The Electrochemical Society · doi:10.1149/1.1995690 · Cited by 69
Self-citationWang, D. Y., Xiao, A., Wells, L., & Dahn, J. R. (2014) · Journal of The Electrochemical Society · doi:10.1149/2.0821501jes · Cited by 60
Self-citationDownie, L. E., & Dahn, J. R. (2014) · Journal of The Electrochemical Society · doi:10.1149/2.0301412jes · Cited by 57
Self-citationDownie, L. E., Hyatt, S. R., Wright, A. T. B., & Dahn, J. R. (2014) · The Journal of Physical Chemistry C · doi:10.1021/jp508912z · Cited by 46
Self-citationWang, D. Y., Sinha, N., Burns, J. C., Petibon, R., & Dahn, J. R. (2014) · Journal of Power Sources · doi:10.1016/j.jpowsour.2014.07.053 · Cited by 23
Self-citation
Cited by
Ryu, H.-H., Park, K.-J., Yoon, C. S., & Sun, Y.-K. (2018) · Chemistry of Materials · doi:10.1021/acs.chemmater.7b05269 · Cited by 1,629
Non-flammable electrolyte enables Li-metal batteries with aggressive cathode chemistries
Fan, X., Chen, L., Borodin, O., Ji, X., Chen, J., Hou, S., Deng, T., Zheng, J., Yang, C., Liou, S.-C., et al. (2018) · Nature Nanotechnology · doi:10.1038/s41565-018-0183-2 · Cited by 1,371
Jung, R., Metzger, M., Maglia, F., Stinner, C., & Gasteiger, H. A. (2017) · Journal of The Electrochemical Society · doi:10.1149/2.0021707jes · Cited by 1,350
High-voltage positive electrode materials for lithium-ion batteries
Li, W., Song, B., & Manthiram, A. (2017) · Chemical Society Reviews · doi:10.1039/c6cs00875e · Cited by 1,339
Enabling High-Voltage Lithium-Metal Batteries under Practical Conditions
Ren, X., Zou, L., Cao, X., Engelhard, M. H., Liu, W., Burton, S. D., Lee, H., Niu, C., Matthews, B. E., Zhu, Z., et al. (2019) · Joule · doi:10.1016/j.joule.2019.05.006 · Cited by 1,092
Metadata
- Authors
- Li, J., Downie, L. E., Ma, L., Qiu, W., & Dahn, J. R.
- Venue
- Journal of The Electrochemical Society
- Publisher
- The Electrochemical Society
- Published
- 2015
- Volume
- 162
- Issue
- 7
- Pages
- A1401-A1408
- ISSN
- 0013-4651 (ISSN-L)
- 1945-7111
- OpenAlex
- W2151378845
- Cited by
- 516
- References
- 25
- FWCI
- 16.36
- Type
- journal article
- Language
- en
- Open access
- hybrid
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.