Erosion–corrosion behaviour of Ni–20Cr plasma coating in actual boiler environment
The DOI matches its Crossref record; 29 of the 29 references it cites were found in a registry or an index.
Abstract
Erosion–corrosion is encountered in a large variety of engineering industries. In such environments, protective coatings are used. In this investigation, erosion–corrosion of the Ni–20Cr coating on nickel and iron based superalloys has been investigated by subjecting them to the boiler of coal fired thermal power plant at the temperature zone of 540°C for 1000 h duration. The erosion–corrosion kinetics of the plasma sprayed Ni–20Cr coating on different superalloys has been investigated. XRD, SEM with EDS and EPMA have been used to analyse the eroded–corroded products along the surface and cross-section. Main phases identified in all the Ni–20Cr coated superalloys after exposure are NiO, Cr 2 O 3, Al 2 O 3 and SiO 2. Aluminium has penetrated from the bond coat to the top coat along the splat boundaries. Oxides of chromium, nickel and aluminium are recognized as protective oxides for boiler environment. The probable mechanism of attack for Ni–20Cr coating in the given boiler environment is discussed.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Citations
Cites
Mechanisms for the hot corrosion of nickel-base alloys
Goebel, J. A., Pettit, F. S., & Goward, G. W. (1973) · Metallurgical Transactions · doi:10.1007/bf02649626 · Cited by 420
Designing oxidation-resistant coatings
Nicholls, J. R. (2000) · JOM · doi:10.1007/s11837-000-0112-2 · Cited by 300 · cited 3×
“Nelson et al.22 have reported the possibility for formation of such phases in ash constituents during combustion.”
BackgroundInfluentialProtective coatings – purpose, role, and design
Goward, G. W. (1986) · Materials Science and Technology · doi:10.1179/026708386790123314 · Cited by 162 · cited 1×
“In Ni–Cr alloy, when chromium oxidises to Cr2O3, it makes the alloy suitable for use upto about 1473 K, although in practice, its use is limited to temperatures below about 1073 K.(17) Link et al.”
BackgroundMatthews, S. J., James, B., & Hyland, M. H. (2013) · Corrosion Science · doi:10.1016/j.corsci.2013.01.030 · Cited by 140
Oxidation Mechanism of Ni—20Cr Foils and Its Relation to the Oxide-Scale Microstructure
Calvarin, G., Molins, R., & Huntz, A. M. (2000) · Oxidation of Metals · doi:10.1023/a:1004578513020 · Cited by 130
Characterisation and Corrosion-Erosion Behaviour of Carbide based Thermal Spray Coatings
Chatha, S. S., Sidhu, H. S., & Sidhu, B. S. (2012) · Journal of Minerals and Materials Characterization and Engineering · doi:10.4236/jmmce.2012.116041 · Cited by 107
Studies on erosion behaviour of plasma sprayed coatings on a Ni-based superalloy
Mishra, S. B., Prakash, S., & Chandra, K. S. (2005) · Wear · doi:10.1016/j.wear.2005.02.098 · Cited by 79 · cited 1×
“Similar type results were obtained during erosion tests at 90u impact angle at room temperature.(27,28) Kunioshi et al.”
ResultSelf-citationErosion - Corrosion of Cermet Coating
Rayes, M. M. E., Abdo, H. S., & Khalil, K. A. (2013) · International Journal of Electrochemical Science · doi:10.1016/s1452-3981(23)14085-5 · Cited by 78 · cited 1×
“Nickel based coatings are used in applications when wear resistance combined with oxidation or hot corrosion resistance is required.(13,14) Nickel–chromium alloys have been used as coating material to deal with the oxidation environments at high temperature.”
BackgroundHiguera Hidalgo, V., Belzunce Varela, F. J., & Fernández Rico, E. (1997) · Tribology International · doi:10.1016/s0301-679x(97)00029-7 · Cited by 76
Oxidation behavior of sputter-deposited NiCrAlY coating
Li, M., Zhang, Z., Sun, X., Li, J., Yin, F., Hu, W., Guan, H. R., & Hu, Z. Q. (2002) · Surface and Coatings Technology · doi:10.1016/s0257-8972(02)00738-7 · Cited by 70
Bala, N., Singh, H., Prakash, S., & Karthikeyan, J. (2012) · Journal of Thermal Spray Technology · doi:10.1007/s11666-011-9698-x · Cited by 63
Self-citationMishra, S. B., Chandra, K., & Prakash, S. (2013) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2012.09.044 · Cited by 56 · cited 4×
“6 and 7).(19,25) This indicates that nickel has either not oxidised or oxidised to a lesser extent, whereas Cr, Al and Y have oxidised and generally persisted along the splat interfaces.”
BackgroundMethodInfluentialSelf-citationAlegría-Ortega, J., Ocampo-Carmona, L. M., Suárez-Bustamante, F. A., & Olaya, J. J. (2012) · Wear · doi:10.1016/j.wear.2012.04.007 · Cited by 44
Kaushal, G., Singh, H., & Prakash, S. (2010) · Metallurgical and Materials Transactions A · doi:10.1007/s11661-010-0587-6 · Cited by 40 · cited 1×
“Nickel–chromium alloys have been used as coating material to deal with the oxidation environments at high temperature.(15,16) In Ni–Cr alloy, when chromium oxidises to Cr2O3, it makes the alloy suitable for use upto about 1473 K, although in practice, its use is limited to temperatures below about 1073 K.”
BackgroundSelf-citationKaushal, G., Bala, N., Kaur, N., Singh, H., & Prakash, S. (2014) · Metallurgical and Materials Transactions A · doi:10.1007/s11661-013-1984-4 · Cited by 39 · cited 1×
“Nickel–chromium alloys have been used as coating material to deal with the oxidation environments at high temperature.(15,16) In Ni–Cr alloy, when chromium oxidises to Cr2O3, it makes the alloy suitable for use upto about 1473 K, although in practice, its use is limited to temperatures below about 1073 K.”
BackgroundSelf-citationErosion-corrosion mechanisms and rates in fe-cr steels
Levy, A. V., & Yong-Fa, M. (1989) · Wear · doi:10.1016/0043-1648(89)90244-5 · Cited by 35
Erosion resistance of coatings for metal protection at elevated temperatures
Shanov, V. N., & Tabakoff, W. (1996) · Surface and Coatings Technology · doi:10.1016/s0257-8972(96)02965-9 · Cited by 28 · cited 1×
“Moreover the erosion resistance of coatings is strongly dependent on the coating process and on the substrate material.(23) Taking into consideration the above facts for the effect of substrate on the plasma sprayed coatings, four different superalloys (namely Superni 75, Superni 600, Superni 718 and Superfer 800H sup…”
BackgroundMishra, S. B., Chandra, K. S., & Prakash, S. (2007) · Materials Letters · doi:10.1016/j.matlet.2007.11.002 · Cited by 27
Self-citationThe Response of Alloys to Erosion-Corrosion at High Temperatures
Link, R., Birks, N., Pettit, F. S., & Dethorey, F. (1998) · Oxidation of Metals · doi:10.1023/a:1018886509459 · Cited by 23 · cited 1×
“The investigators concluded that that nickel, Ni–20Cr and Ni–30Cr degrade at the same rate under identical conditions of erosionoxidation.(18) Roy et al.”
BackgroundThe Influence of Erosion-Induced Roughness on the Oxidation Kinetics of Ni and Ni-20Cr Alloys
Roy, M., Ray, K. K., & Sundararajan, G. (1999) · Oxidation of Metals · doi:10.1023/a:1018870606617 · Cited by 22 · cited 2×
“6 and 7).(19,25) This indicates that nickel has either not oxidised or oxidised to a lesser extent, whereas Cr, Al and Y have oxidised and generally persisted along the splat interfaces.”
BackgroundPlasma spraying as an advanced tool in surface engineering
Steffens, H. ‐., & Mack, M. (1990) · Pure and Applied Chemistry · doi:10.1351/pac199062091801 · Cited by 19 · cited 5×
“XRD phases are also found to be in agreement with those reported by Calvarin et al.21 Presence of SiO2, Al2O3, SO3 and Fe2O3 in micrographs of Figs.”
BackgroundResultInfluentialMicrostructure-Wear and -Corrosion Relationships for Thermally Sprayed Metallic Deposits
Ilavský, J., Písačka, J., Chráska, P., Margandant, N., Siegmann, S., Wagner, W., Fiala, P., & Barbezat, G. (2000) · Thermal spray · doi:10.31399/asm.cp.itsc2000p0449 · Cited by 19
Jegadeeswaran, N., Ramesh, M. R., & Bhat, K. U. (2013) · International Journal of Corrosion · doi:10.1155/2013/824659 · Cited by 18
High temperature degradation by erosion-corrosion in bubbling fluidized \nbed combustors
Hou, P. Y., MacAdam, S., Niu, Y., et al. (2003) · eScholarship (California Digital Library) · Cited by 18
High temperature degradation by erosion-corrosion in bubbling fluidized bed combustors
Hou, P. Y., MacAdam, S., Niu, Y., & Stringer, J. (2004) · Materials Research · doi:10.1590/s1516-14392004000100011 · Cited by 18 · cited 1×
“The condition at which this layer forms depends on the amount of fine dust particles retained in the bed, which is closely related to the composition of the bed, the specimen and bed temperatures and the oxidation rate of the specimen.(4) Currently superalloys are being used to increase the service life of the boilers…”
BackgroundErosion-corrosion of steels in simulated and actual fluidized bed combustor environments
Levy, A. V., Wang, B., Yong-Faman, & Jee, N. (1989) · Wear · doi:10.1016/0043-1648(89)90247-0 · Cited by 17
Erosion-oxidation behavior of thermal sprayed Ni20Cr alloy and WC and Cr3C2 cermet coatings
Kunioshi, C. T., Corrêa, O. V., & Ramanathan, L. V. (2005) · Materials Research · doi:10.1590/s1516-14392005000200005 · Cited by 17
Mishra, S. B., Chandra, K. S., & Prakash, S. (2006) · Journal of Tribology · doi:10.1115/1.2197843 · Cited by 13 · cited 1×
“Similar type results were obtained during erosion tests at 90u impact angle at room temperature.(27,28) Kunioshi et al.”
ResultSelf-citationMishra, N. K., & Mishra, S. B. (2014) · Corrosion Engineering Science and Technology The International Journal of Corrosion Processes and Corrosion Control · doi:10.1179/1743278214y.0000000166 · Cited by 5
Self-citation
Research works printed but not linked: 6
- Chatha SS, 2012, J. Miner. Mater. Character. Eng., 11, 569
- 10.1179/mst.1986.2.3.194 · doi:10.1179/mst.1986.2.3.194 · Paper page
- Berndt CC, 1979, Austr. Weld. Res., 6, 75
- Nicholls, 2000, J. Mater., 52, 28
- Prakash S, Singh S, Sidhu BS and Madeshia A: ‘Tube failures in coal fired boilers’, Proc. National Seminar on ‘Advances in material and processing’, Roorkee, India, November 2001, 245–253.
- Nelson HW, Krause HH, Ungar EW, Putnam AA, Slunder CJ, Miller PD, Hummel JD and Landry BA: ‘A review of available information on corrosion and deposits in coal and oil-fired boilers and gas turbines’, Report of ASME Research Committee on Corrosion and Deposits from Combustion Gases, Pub. Pergamon Press and ASME, New York, 1959.
Cited by
Combating hot corrosion of boiler tubes – A study
Kumar, S., Kumar, M., & Handa, A. (2018) · Engineering Failure Analysis · doi:10.1016/j.engfailanal.2018.08.004 · Cited by 207
Influence of processing conditions on the properties of thermal sprayed coating: a review
Kumar, S., & Kumar, R. (2021) · Surface Engineering · doi:10.1080/02670844.2021.1967024 · Cited by 168
Kumar, S., Handa, A., Chawla, V., Grover, N. K., & Kumar, R. (2021) · Surface Engineering · doi:10.1080/02670844.2021.1924506 · Cited by 133
“lying surface of the substrate, thus forming a coating on the prepared substrate [21, 22].”
BackgroundKumar, S., Kumar, M., & Handa, A. (2020) · Materials at High Temperatures · doi:10.1080/09603409.2020.1810922 · Cited by 101
“As the oxidising species generally grow along the pores, voids and splat boundries [37,56].”
BackgroundKumar, S., Kumar, M., & Handa, A. (2020) · Materials Research Express · doi:10.1088/2053-1591/ab5fae · Cited by 74
Metadata
- Authors
- Mishra, S. B., & Prakash, S.
- Affiliations
- Motilal Nehru National Institute of Technology (IN)
- Indian Institute of Technology Roorkee (IN)
- Corresponding author
- Mishra, S. B.
- ORCID
- Mishra, S. B.
- Venue
- Surface Engineering
- Publisher
- SAGE Publications
- Published
- 2015-01
- Volume
- 31
- Issue
- 1
- Pages
- 29-38
- ISSN
- 0267-0844 (ISSN-L)
- 1743-2944
- OpenAlex
- W1981425852
- Cited by
- 31
- References
- 29
- Citations by year
- 2025: 2 · 2024: 5 · 2023: 2 · 2022: 2 · 2021: 5 · 2020: 5 · 2019: 4 · 2018: 1 · 2017: 3 · 2016: 1 · 2015: 1
- FWCI
- 2.46
- Type
- journal article
- Language
- en
- Open access
- closed
- Licence
- journals.sagepub.com/page/policies/text-and-data-mining-license (tdm)
- Locations
- Surface Engineering (publishedVersion)
- Topics
- Physical Sciences › Materials Science › Surfaces, Coatings and Films › High-Temperature Coating Behaviors
- Physical Sciences › Engineering › Mechanical Engineering › Erosion and Abrasive Machining
- Physical Sciences › Engineering › Mechanical Engineering › Surface Treatment and Coatings
- Keywords
- erosion-corrosion, plasma-sprayed coatings, coal-fired power plants, nickel-based superalloy, iron-based superalloys, protective oxide scale, bond coat, coating degradation mechanisms
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.