Erosion–corrosion behaviour of Ni–20Cr plasma coating in actual boiler environment
The DOI matches its Crossref record; 29 of the 29 references it cites were found in a registry or an index.
Abstract
Erosion–corrosion is encountered in a large variety of engineering industries. In such environments, protective coatings are used. In this investigation, erosion–corrosion of the Ni–20Cr coating on nickel and iron based superalloys has been investigated by subjecting them to the boiler of coal fired thermal power plant at the temperature zone of 540°C for 1000 h duration. The erosion–corrosion kinetics of the plasma sprayed Ni–20Cr coating on different superalloys has been investigated. XRD, SEM with EDS and EPMA have been used to analyse the eroded–corroded products along the surface and cross-section. Main phases identified in all the Ni–20Cr coated superalloys after exposure are NiO, Cr 2 O 3, Al 2 O 3 and SiO 2. Aluminium has penetrated from the bond coat to the top coat along the splat boundaries. Oxides of chromium, nickel and aluminium are recognized as protective oxides for boiler environment. The probable mechanism of attack for Ni–20Cr coating in the given boiler environment is discussed.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Citations
Cites
Mechanisms for the hot corrosion of nickel-base alloys
Goebel, J. A., Pettit, F. S., & Goward, G. W. (1973) · Metallurgical Transactions · doi:10.1007/bf02649626 · Cited by 420
Designing oxidation-resistant coatings
Nicholls, J. R. (2000) · JOM · doi:10.1007/s11837-000-0112-2 · Cited by 300 · cited 3×
“Nelson et al.22 have reported the possibility for formation of such phases in ash constituents during combustion.”
BackgroundInfluentialProtective coatings – purpose, role, and design
Goward, G. W. (1986) · Materials Science and Technology · doi:10.1179/026708386790123314 · Cited by 162 · cited 1×
“In Ni–Cr alloy, when chromium oxidises to Cr2O3, it makes the alloy suitable for use upto about 1473 K, although in practice, its use is limited to temperatures below about 1073 K.(17) Link et al.”
BackgroundMatthews, S. J., James, B., & Hyland, M. H. (2013) · Corrosion Science · doi:10.1016/j.corsci.2013.01.030 · Cited by 140
Oxidation Mechanism of Ni—20Cr Foils and Its Relation to the Oxide-Scale Microstructure
Calvarin, G., Molins, R., & Huntz, A. M. (2000) · Oxidation of Metals · doi:10.1023/a:1004578513020 · Cited by 130
Characterisation and Corrosion-Erosion Behaviour of Carbide based Thermal Spray Coatings
Chatha, S. S., Sidhu, H. S., & Sidhu, B. S. (2012) · Journal of Minerals and Materials Characterization and Engineering · doi:10.4236/jmmce.2012.116041 · Cited by 107
Studies on erosion behaviour of plasma sprayed coatings on a Ni-based superalloy
Mishra, S. B., Prakash, S., & Chandra, K. S. (2005) · Wear · doi:10.1016/j.wear.2005.02.098 · Cited by 79 · cited 1×
“Similar type results were obtained during erosion tests at 90u impact angle at room temperature.(27,28) Kunioshi et al.”
ResultSelf-citationErosion - Corrosion of Cermet Coating
Rayes, M. M. E., Abdo, H. S., & Khalil, K. A. (2013) · International Journal of Electrochemical Science · doi:10.1016/s1452-3981(23)14085-5 · Cited by 78 · cited 1×
“Nickel based coatings are used in applications when wear resistance combined with oxidation or hot corrosion resistance is required.(13,14) Nickel–chromium alloys have been used as coating material to deal with the oxidation environments at high temperature.”
BackgroundHiguera Hidalgo, V., Belzunce Varela, F. J., & Fernández Rico, E. (1997) · Tribology International · doi:10.1016/s0301-679x(97)00029-7 · Cited by 76
Oxidation behavior of sputter-deposited NiCrAlY coating
Li, M., Zhang, Z., Sun, X., Li, J., Yin, F., Hu, W., Guan, H. R., & Hu, Z. Q. (2002) · Surface and Coatings Technology · doi:10.1016/s0257-8972(02)00738-7 · Cited by 70
Research works printed but not linked: 6
- Chatha SS, 2012, J. Miner. Mater. Character. Eng., 11, 569
- 10.1179/mst.1986.2.3.194 · doi:10.1179/mst.1986.2.3.194 · Paper page
- Berndt CC, 1979, Austr. Weld. Res., 6, 75
- Nicholls, 2000, J. Mater., 52, 28
- Prakash S, Singh S, Sidhu BS and Madeshia A: ‘Tube failures in coal fired boilers’, Proc. National Seminar on ‘Advances in material and processing’, Roorkee, India, November 2001, 245–253.
- Nelson HW, Krause HH, Ungar EW, Putnam AA, Slunder CJ, Miller PD, Hummel JD and Landry BA: ‘A review of available information on corrosion and deposits in coal and oil-fired boilers and gas turbines’, Report of ASME Research Committee on Corrosion and Deposits from Combustion Gases, Pub. Pergamon Press and ASME, New York, 1959.
Cited by
Combating hot corrosion of boiler tubes – A study
Kumar, S., Kumar, M., & Handa, A. (2018) · Engineering Failure Analysis · doi:10.1016/j.engfailanal.2018.08.004 · Cited by 207
Influence of processing conditions on the properties of thermal sprayed coating: a review
Kumar, S., & Kumar, R. (2021) · Surface Engineering · doi:10.1080/02670844.2021.1967024 · Cited by 168
Kumar, S., Handa, A., Chawla, V., Grover, N. K., & Kumar, R. (2021) · Surface Engineering · doi:10.1080/02670844.2021.1924506 · Cited by 133
“lying surface of the substrate, thus forming a coating on the prepared substrate [21, 22].”
BackgroundKumar, S., Kumar, M., & Handa, A. (2020) · Materials at High Temperatures · doi:10.1080/09603409.2020.1810922 · Cited by 101
“As the oxidising species generally grow along the pores, voids and splat boundries [37,56].”
BackgroundKumar, S., Kumar, M., & Handa, A. (2020) · Materials Research Express · doi:10.1088/2053-1591/ab5fae · Cited by 74
Singh, J., Vasudev, H., & Singh, S. (2020) · Materials Today: Proceedings · doi:10.1016/j.matpr.2020.01.156 · Cited by 69
The corrosion behaviours of plasma-sprayed Fe-based amorphous coatings
Jiang, C., Liu, W., Wang, G., Chen, Y., Xing, Y., Zhang, C., & Dargusch, M. (2018) · Surface Engineering · doi:10.1080/02670844.2017.1319647 · Cited by 50
“The surface of the coating following hot corrosion exhibited the presence of Fe2O3, NiO, NiCr2O4 and Cr2O3.”
BackgroundInfluentialZavareh, M. A., Sarhan, A. A. D., Zavareh, P. A., & Basirun, W. J. (2015) · Ceramics International · doi:10.1016/j.ceramint.2015.10.134 · Cited by 48
Prashar, G., Vasudev, H., & Thakur, L. (2021) · Surface Review and Letters · doi:10.1142/s0218625x22300039 · Cited by 43
Behaviour of carbon nanotubes-Cr 2 O 3 thermal barrier coatings in actual boiler
Goyal, K., Singh, H., & Bhatia, R. (2019) · Surface Engineering · doi:10.1080/02670844.2019.1584966 · Cited by 42
Singh, P. K., & Mishra, S. B. (2020) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2020.125353 · Cited by 41
Self-citationDhand, D., Kumar, P., & Grewal, J. S. (2021) · Corrosion Reviews · doi:10.1515/corrrev-2020-0043 · Cited by 31
High Temperature Corrosion Resistant and Anti-slagging Coatings for Boilers: A Review
Khantisopon, K., Singh, S., Jitputti, J., Berndt, C. C., & Ang, A. S. M. (2024) · High Temperature Corrosion of Materials · doi:10.1007/s11085-024-10251-0 · Cited by 30
Thermal Spray Coatings for Erosion–Corrosion Resistant Applications
Babu, P. S., Madhavi, Y., Krishna, L. R., Sivakumar, G., Rao, D. S., & Padmanabham, G. (2020) · Transactions of the Indian Institute of Metals · doi:10.1007/s12666-020-02053-0 · Cited by 26
Mishra, S. B., Chandra, K., & Prakash, S. (2017) · Anti-Corrosion Methods and Materials · doi:10.1108/acmm-11-2015-1592 · Cited by 19
Self-citationCorrosion-resistant coatings: advances in deposition methods, nanostructures, and self-healing films
Yelwa, J. M., Musa, H., Fasanya, O. O., & Yahaya, J. Y. (2025) · Academia Materials Science · doi:10.20935/acadmatsci7829 · Cited by 18
High-temperature erosion of Fe-based coatings reinforced with cermet particles
Surzhenkov, A., Antonov, M., Goljandin, D., Kulu, P., Viljus, M., Traksmaa, R., & Mere, A. (2016) · Surface Engineering · doi:10.1080/02670844.2016.1145377 · Cited by 14
The effect of saline environment on the fatigue behaviour of HVOF-sprayed WC–CrC–Ni coatings
Murariu, A. C., Cernescu, A. V., & Perianu, I. A. (2017) · Surface Engineering · doi:10.1080/02670844.2017.1388561 · Cited by 14
Hot Corrosion Behavior and Mechanism of High-Velocity Arc-Sprayed Ni-Cr Alloy Coatings
Cheng, J., Wu, Y., Chen, L., Hong, S., Qiao, L., & Wei, Z. (2019) · Journal of Thermal Spray Technology · doi:10.1007/s11666-019-00890-0 · Cited by 13
Singh, S., Goyal, K., & Bhatia, R. (2024) · Anti-Corrosion Methods and Materials · doi:10.1108/acmm-08-2024-3071 · Cited by 12
Comparative erosion performance of HVOF and LVOF sprayed NiCrSiBCFe-WC-Co coating
Yadav, A. S., & Mishra, S. B. (2024) · Surface Engineering · doi:10.1177/02670844241273542 · Cited by 10
“23”
Self-citationSingh, P. K., & Mishra, S. B. (2020) · Tribology - Materials Surfaces & Interfaces · doi:10.1080/17515831.2020.1785232 · Cited by 10
“The boiler tubes failure in thermal power plants occurs due to the impact of unburnt carbon, alumina and other fl y ash particles entrained in a fl uid medium causing erosion wear along with oxidation and hot corrosion [3 – 5].”
BackgroundSelf-citationFu, C., Li, Y., & Wang, Y. F. (2021) · Oxidation of Metals · doi:10.1007/s11085-020-10016-5 · Cited by 10
Roshith, P. (2024) · Canadian Metallurgical Quarterly · doi:10.1080/00084433.2024.2357870 · Cited by 8
Kumar, S., & Kumar, R. (2022) · Advances in chemical and materials engineering book series · doi:10.4018/978-1-7998-9683-8.ch005 · Cited by 7
Influence of HVOF deposition thickness on adhesion strength of WC–CrC–Ni coatings
Murariu, A. C., & Perianu, I. A. (2019) · Advanced Technologies & Materials · doi:10.24867/atm-2019-1-006 · Cited by 6
Agnihotri, A., Vasudev, H., Singh, G., Singh, S., Hosalli, R., Veeresha, G., Prasad, C. D., Balu, R., & Tiwari, A. (2025) · Journal of Bio- and Tribo-Corrosion · doi:10.1007/s40735-025-00975-0 · Cited by 5
“13a, b, as indicated by the detection of chromium and oxygen at these places [59, 60].”
RetractedSundaram, S., Singaravelu, C., & Vikneswaran, M. (2022) · Surface Topography Metrology and Properties · doi:10.1088/2051-672x/aca3be · Cited by 5
“NiO, Cr2O4, Al2O3, and SiO2 were the primary phases found in all Ni–20Cr-coated superalloys during exposure and acting as a boiler environment protector [22].”
BackgroundEffect of burnishing on HVOF coated boiler steel against hot corrosion in actual boiler environment
Agnihotri, A., Kalsi, S. S., & Kansal, H. K. (2023) · Surface Engineering · doi:10.1080/02670844.2023.2242117 · Cited by 3
“ation (Figure 8) shows Cr2O3, Al2O3, Fe2O3, SiO2, NiO, and NiCr2O4 as surface band phases [56,61,62].”
BackgroundSingh, S., Goyal, K., & Bhatia, R. (2024) · Discover Materials · doi:10.1007/s43939-024-00166-7 · Cited by 3
(2023) · NanoWorld Journal · doi:10.17756/nwj.2023-s1-073 · Cited by 1
“The higher operating temperature of modern power plants causes high-temperature oxidation of the boiler materials [6, 7].”
BackgroundA Comprehensive Analysis on Breakthrough Trends in Coatings Technology for Industry 4.0
Gupta, V., Saxena, D., Asthana, N., & Srivastava, A. (2025) · Springer Proceedings in Materials · doi:10.1007/978-981-96-5166-5_21
Metadata
- Authors
- Mishra, S. B., & Prakash, S.
- Affiliations
- Motilal Nehru National Institute of Technology (IN)
- Indian Institute of Technology Roorkee (IN)
- Corresponding author
- Mishra, S. B.
- ORCID
- Mishra, S. B.
- Venue
- Surface Engineering
- Publisher
- SAGE Publications
- Published
- 2015-01
- Volume
- 31
- Issue
- 1
- Pages
- 29-38
- ISSN
- 0267-0844 (ISSN-L)
- 1743-2944
- OpenAlex
- W1981425852
- Cited by
- 31
- References
- 29
- Citations by year
- 2025: 2 · 2024: 5 · 2023: 2 · 2022: 2 · 2021: 5 · 2020: 5 · 2019: 4 · 2018: 1 · 2017: 3 · 2016: 1 · 2015: 1
- FWCI
- 2.46
- Type
- journal article
- Language
- en
- Open access
- closed
- Licence
- journals.sagepub.com/page/policies/text-and-data-mining-license (tdm)
- Locations
- Surface Engineering (publishedVersion)
- Topics
- Physical Sciences › Materials Science › Surfaces, Coatings and Films › High-Temperature Coating Behaviors
- Physical Sciences › Engineering › Mechanical Engineering › Erosion and Abrasive Machining
- Physical Sciences › Engineering › Mechanical Engineering › Surface Treatment and Coatings
- Keywords
- erosion-corrosion, plasma-sprayed coatings, coal-fired power plants, nickel-based superalloy, iron-based superalloys, protective oxide scale, bond coat, coating degradation mechanisms
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.