CoChat

Investigations of the Sulfonated Poly(ether ether ketone) Membranes with Various Degrees of Sulfonation by Considering Durability for the Proton Exchange Membrane Fuel Cell (PEMFC) Applications

Open access
Song, Yinfeng, Guo, Zhenshuo, Yin, Jiayi, Liu, Mengjie, Tolj, Ivan, Grigoriev, Sergey A., Ge, Mingming, Sun, Chuanyu · 2025 · Polymers

The DOI matches its Crossref record; 60 of the 60 references it cites were found in a registry or an index; none of the 24 sources its claims cite is checked for support yet.

Abstract

The optimum degree of sulfonation for SPEEK membranes is determined by combining proton conductivity, swelling, water uptake, chemical stability, thermal stability, mechanical tests, and PEMFC performance.

Overview

CoChat Summary

## TL;DR

This paper studies SPEEK membranes with different degrees of sulfonation (DS) for PEMFCs and shows a tradeoff: higher DS improves proton conductivity, but lowers mechanical, thermal, and chemical durability. Considering both performance and durability, the authors argue that SPEEK membranes with DS around 51–62% are more suitable than the previously favored higher-DS membranes.

## Key findings

  • Water uptake increased from 7.3% to 43.3% and swelling ratio from 4.2% to 15.4% as sulfonation duration increased from 1.5 to 4 h at 55 °C.
  • The paper states that proton conductivity increased with DS, but mechanical, thermal, and chemical stability decreased as DS increased.
  • In the Fenton durability test, SPEEK-51 showed the best chemical stability among the membranes discussed; its complete degradation time was about twice that of SPEEK-62, and at crack formation its WU was below 35% versus 107% for SPEEK-62.
  • In PEMFC single-cell testing at 80 °C and 100% RH, the SPEEK-62 membrane reached a peak power density of 482.08 mW/cm², exceeding Nafion-212 at 365.16 mW/cm²; SPEEK-51 reached 236.93 mW/cm² under the same condition.
  • Under 70 °C and 100% RH OCV durability testing, OCV decays were 0.08 V for SPEEK-51, 0.242 V for SPEEK-62, and 0.141 V for Nafion-212, corresponding to decay rates of 1.33, 4.03, and 2.35 mV h−1, respectively.

## Methods

  • SPEEK membranes were prepared from PEEK by sulfonation in concentrated sulfuric acid at 55 °C for 1.5–4 h, yielding membranes labeled SPEEK-34, 43, 51, 62, 72 based on DS.
  • The paper characterized membranes using FTIR, SEM, tensile testing, swelling ratio and water uptake, TGA, acid–base titration for IEC/DS, proton conductivity by impedance spectroscopy, Fenton oxidative stability tests, and PEMFC single-cell tests/OCV durability tests.
  • Single-cell MEAs were fabricated by hot pressing SPEEK membranes with productized GDEs, then tested at 70, 75, and 80 °C under 100% RH, and OCV durability was tested at 70 °C and 50% RH.

## Limitations

  • The paper explicitly notes that SPEEK-34 was not further discussed because its proton conductivity was below 60 mS/cm, and its poor solubility in DMF made membrane preparation difficult.
  • The text indicates that the results are based on a small set of membrane DS values; this is evident from the study design, but the paper does not present broader sampling or replication details here.
  • The text makes evident that some performance conclusions depend on specific testing conditions (for example, 100% RH, 50% RH, and selected temperatures), so generalization beyond those conditions is not directly established in the provided text.

Model-written summary. Check it against the paper before relying on it.

Integrity signals

Registry

Crossref · 10.3390/polym17162181

Cites

60 of 60 references verified0 citation errors · 0 not checkable

Statistics

Nothing to recompute.

Figures

Figure 1 (a) Structural diagrammatic sketch of PEM conductivity testing fixture. (b) Electrochemical impedance spectroscopy (EIS) measurement system of membrane.
Figure 1 (a) Structural diagrammatic sketch of PEM conductivity testing fixture. (b) Electrochemical impedance spectroscopy (EIS) measurement system of membrane.CC BY · PubMed Central
Figure 2 (a) MEAs after hot press at 120 °C under 3 MPa for 5 min; (b) single cell with MEAs; (c) hot press equipment; (d) PEMFC single-cell test system.
Figure 2 (a) MEAs after hot press at 120 °C under 3 MPa for 5 min; (b) single cell with MEAs; (c) hot press equipment; (d) PEMFC single-cell test system.CC BY · PubMed Central
Figure 3 The FTIR spectrum of SPEEK membranes with different DS values and pristine PEEK powder.
Figure 3 The FTIR spectrum of SPEEK membranes with different DS values and pristine PEEK powder.CC BY · PubMed Central
Figure 4 The top view morphology of various SPEEK PEMs: (a) SPEEK-43, (b) SPEEK-51, (c) SPEEK-62, (d) SPEEK-72.
Figure 4 The top view morphology of various SPEEK PEMs: (a) SPEEK-43, (b) SPEEK-51, (c) SPEEK-62, (d) SPEEK-72.CC BY · PubMed Central
Figure 5 The TG curves of SPEEK-43, SPEEK-51, SPEEK-62, and SPEEK-72.
Figure 5 The TG curves of SPEEK-43, SPEEK-51, SPEEK-62, and SPEEK-72.CC BY · PubMed Central
Figure 6 Proton transfer mechanism of SPEEK membrane.
Figure 6 Proton transfer mechanism of SPEEK membrane.CC BY · PubMed Central
Figure 7 (a) Proton conductivity of SPEEK-34, SPEEK-43, SPEEK-51, SPEEK-62, SPEEK-72, and Nafion-212 membranes; (b) Nyquist diagram of SPEEK-51 at different temperatures (24–80 °C); (c) Nyquist diagram of SPEEK-62 at different temperatures (24–80 °C).
Figure 7 (a) Proton conductivity of SPEEK-34, SPEEK-43, SPEEK-51, SPEEK-62, SPEEK-72, and Nafion-212 membranes; (b) Nyquist diagram of SPEEK-51 at different temperatures (24–80 °C); (c) Nyquist diagram of SPEEK-62 at different temperatures (24–80 °C).CC BY · PubMed Central
Figure 8 Visible crack formation time, complete mechanical disintegration time, and WC when visible crack formed for SPEEK membranes with various DS.
Figure 8 Visible crack formation time, complete mechanical disintegration time, and WC when visible crack formed for SPEEK membranes with various DS.CC BY · PubMed Central
Figure 9 PEMFC performance of MEAs prepared by (a) SPEEK-51 membrane; (b) SPEEK-62 membrane; (c) Nafion-212 membrane at various temperatures; (d) PEMFC performance of MEAs assembled with different PEMs under 80 °C and under 100% RH condition; (e) PEMFC performance of MEAs assembled with different PEMs under 70 °C and 50% RH condition; (f) OCV curve of the SPEEK-51, SPEEK-62, and Nafion-212 under 80 °C and 100% RH.
Figure 9 PEMFC performance of MEAs prepared by (a) SPEEK-51 membrane; (b) SPEEK-62 membrane; (c) Nafion-212 membrane at various temperatures; (d) PEMFC performance of MEAs assembled with different PEMs under 80 °C and under 100% RH condition; (e) PEMFC performance of MEAs assembled with different PEMs under 70 °C and 50% RH condition; (f) OCV curve of the SPEEK-51, SPEEK-62, and Nafion-212 under 80 °C and 100% RH.CC BY · PubMed Central

Verification

Claims the paper makes

0 Valid · 0 Not valid · 10 Not checked · 40 Own results and interpretations

24 more claims

Create a free account to see all 50 claims and to verify the 1 reference still open.

See all claims — free account
  • It may state two separate claims as one. 16
  • Probably not a substantial claim. 5

Create a free account to see these claims.

Citations

Cites

Cited by

See all 28

Metadata

Authors
Song, Y., Guo, Z., Yin, J., Liu, M., Tolj, I., Grigoriev, S. A., Ge, M., & Sun, C.
Affiliations
  • Harbin Institute of Technology (CN)
  • Beijing Normal-Hong Kong Baptist University (CN)
  • Shenzhen University (CN)
  • University of Split (HR)
  • National Research University “Moscow Power Engineering Institute”, 14, Krasnokazarmennaya St., Moscow 111250, Russia
Corresponding author
  • Yin, Jiayi
  • Sun, Chuanyu
Venue
Polymers
Publisher
MDPI AG
Published
2025-08-09
Volume
17
Issue
16
Pages
2181
ISSN
2073-4360 (ISSN-L)
OpenAlex
W4413200649
Cited by
28
References
60
Citations by year
2026: 25 · 2025: 3
FWCI
6.22
Type
journal article
Language
en
Open access
Locations
  • Polymers (publishedVersion, cc-by)
  • Europe PMC (PubMed Central) (publishedVersion, cc-by)
  • PubMed Central (publishedVersion, cc-by)
  • PubMed (publishedVersion)
Funders
  • 2023 Youth Talent Introduction Scientific Research Startup Fee (AUGA2160100623, AUGA2160501723, 2024A1515010711, UICR0700117-25, ZJ2023023)
  • 2023 Support Funds for Talent Introduction in Heilongjiang Province (AUGA2160100623, AUGA2160501723, 2024A1515010711, UICR0700117-25, ZJ2023023)
  • GuangDong Basic and Applied Basic Research Foundation (AUGA2160100623, AUGA2160501723, 2024A1515010711, UICR0700117-25, ZJ2023023)
  • UIC research fund (AUGA2160100623, AUGA2160501723, 2024A1515010711, UICR0700117-25, ZJ2023023)
  • Priority Postdoctoral Projects in Zhejiang Province (AUGA2160100623, AUGA2160501723, 2024A1515010711, UICR0700117-25, ZJ2023023)
Topics
  • Physical Sciences › Engineering › Electrical and Electronic Engineering › Fuel Cells and Related Materials
  • Physical Sciences › Chemical Engineering › Filtration and Separation › Membrane-based Ion Separation Techniques
  • Physical Sciences › Materials Science › Materials Chemistry › Advancements in Solid Oxide Fuel Cells
Keywords
sulfonated poly(ether ether ketone), SPEEK membranes, degree of sulfonation, proton exchange membrane fuel cells, membrane durability, chemical stability, thermal stability, proton conductivity, swelling ratio, water absorption, power density

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

A language model drew the claims from the paper on 2026-10-10, under version 3 of the claim definition (model deepseek-v4.1-flash, prompt extract-v3).

A second model labelled each claim on 2026-10-10 (model jev-1.13-20260917, definition revision gold-guideline-v0.2).

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.