The DOI matches its Crossref record; 29 of the 29 references it cites were found in a registry or an index.
Slag and Activator Chemistry Control the Reaction Kinetics of Sodium Metasilicate-Activated Slag Cements
Open accessAbstract
The reaction kinetics of four commercial ground granulated blast furnace slags with varying percentages of MgO (6 to 14 wt.%), activated with four different doses of sodium metasilicate, were evaluated using isothermal calorimetry. The reaction kinetics were strongly dependent on the dose of the alkaline activator used, and the chemical and physical properties of the slag. When using low concentrations of sodium metasilicate as an activator, the MgO content in the slag influences the kinetics of the reaction, while the CaO content plays a more significant role when the concentration of metasilicate is increased. This study elucidated a close relationship between the dose of the alkali-activator and the chemistry of the slag used, although it was not possible to identify a clear correlation between any of the published chemically-based “slag quality moduli” and the calorimetry results, highlighting the complexity of blast furnace slag glass chemistry, and the importance of the physical properties of the slag in defining its reactivity.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Geopolymers and Related Alkali-Activated Materials
Provis, J. L., & Bernal, S. A. (2014) · Annual Review of Materials Research · doi:10.1146/annurev-matsci-070813-113515 · Cited by 1,597
Self-citationAdvances in understanding alkali-activated materials
Provis, J. L., Palomo, A., & Shi, C. (2015) · Cement and Concrete Research · doi:10.1016/j.cemconres.2015.04.013 · Cited by 1,537
Self-citationBen Haha, M., Le Saout, G., Winnefeld, F., & Lothenbach, B. (2011) · Cement and Concrete Research · doi:10.1016/j.cemconres.2010.11.016 · Cited by 1,059
Geopolymers and other alkali activated materials: why, how, and what?
Provis, J. L. (2014) · Materials and Structures · doi:10.1617/s11527-013-0211-5 · Cited by 986
Self-citationHaha, M. B., Lothenbach, B., Le Saout, G., & Winnefeld, F. (2011) · Cement and Concrete Research · doi:10.1016/j.cemconres.2011.05.002 · Cited by 914 · cited 5×
“activated slags with higher slag MgO content reacted more rapidly than those with lower MgO content [15].”
BackgroundResultInfluentialEvolution of binder structure in sodium silicate-activated slag-metakaolin blends
Bernal, S. A., Provis, J. L., Rose, V., & Mejía de Gutierrez, R. (2011) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2010.09.004 · Cited by 786 · cited 1×
“This drives faster dissolution of the slag particles and precipitation of mainly C-(A)-S-H type gels [11,22,23], which have been reported as the main reaction product for the silicate activated slags used in this study, and others of comparable composition [9].”
MethodSelf-citationFactors affecting the strength of alkali-activated slag
Wang, S.-D., Scrivener, K. L., & Pratt, P. L. (1994) · Cement and Concrete Research · doi:10.1016/0008-8846(94)90026-4 · Cited by 716 · cited 2×
“However, silicate-activated slag cements exhibit higher mechanical performance and stability than hydroxide-activated slag cements due to the nature of the reaction products formed [5].”
BackgroundProvis, J. L., & van Deventer, J. S. J. (2009) · Woodhead Publishing Limited eBooks · doi:10.1533/9781845696382 · Cited by 646
Self-citationHaha, M. B., Lothenbach, B., Le Saout, G., & Winnefeld, F. (2012) · Cement and Concrete Research · doi:10.1016/j.cemconres.2011.08.005 · Cited by 580
Incorporation of aluminium in calcium-silicate-hydrates
L’Hôpital, E., Lothenbach, B., Le Saout, G., Kulik, D., & Scrivener, K. (2015) · Cement and Concrete Research · doi:10.1016/j.cemconres.2015.04.007 · Cited by 551 · cited 2×
“The bulk gel chemical compositions are controlled mostly by the availability of CaO, SiO2, and Al2O3 [30,31], which in practice relate to the chemistry of the slag used, the activator dose, and the degree of reaction achieved.”
BackgroundBernal, S. A., San Nicolas, R., Myers, R. J., Mejía de Gutiérrez, R., Puertas, F., van Deventer, J. S. J., & Provis, J. L. (2014) · Cement and Concrete Research · doi:10.1016/j.cemconres.2013.12.003 · Cited by 493 · cited 8×
“activation, the formation of which is closely related to the MgO content in the slag [9] as well as the availability of Al species in the aqueous phase (Figure 7).”
BackgroundMethodResultSelf-citationA calorimetric study of early hydration of alkali-slag cements
Shi, C., & Day, R. L. (1995) · Cement and Concrete Research · doi:10.1016/0008-8846(95)00126-w · Cited by 468 · cited 1×
“For all doses of the sodium metasilicate activator, the heat release curves (Figure 1) exhibited a pre-induction period (first peak) during the first hour of reaction, corresponding to wetting and dissolution of the slag grains [20], and possibly also to the adsorption of some ions onto the surface of the slag grains.”
BackgroundPuertas, F., Fernández-Jiménez, A., & Blanco-Varela, M. T. (2004) · Cement and Concrete Research · doi:10.1016/s0008-8846(03)00254-0 · Cited by 409
Hydration of alkali-activated ground granulated blast furnace slag
Song, S., Sohn, D., Jennings, H. M., & Mason, T. O. (2000) · Journal of Materials Science · doi:10.1023/a:1004742027117 · Cited by 363 · cited 2×
“5 do not facilitate the dissolution and reaction of the slag precursor [12].”
BackgroundAssessing, Understanding and Unlocking Supplementary Cementitious Materials
Snellings, R. (2016) · RILEM Technical Letters · doi:10.21809/rilemtechlett.2016.12 · Cited by 348 · cited 1×
“There have recently been extensive efforts by industry and academia to improve the sustainability of concrete production, and a key focus has been the partial or complete replacement of Portland cement (PC) clinker with supplementary cementitious materials [1].”
Background29Si and 27Al NMR study of alkali-activated slag
Wang, S.-D., & Scrivener, K. L. (2003) · Cement and Concrete Research · doi:10.1016/s0008-8846(02)01044-x · Cited by 328
A thermodynamic model for C-(N-)A-S-H gel: CNASH_ss. Derivation and validation
Myers, R. J., Bernal, S. A., & Provis, J. L. (2014) · Cement and Concrete Research · doi:10.1016/j.cemconres.2014.07.005 · Cited by 312
Self-citationThe Role of Al in Cross‐Linking of Alkali‐Activated Slag Cements
Myers, R. J., Bernal, S. A., Gehman, J. D., van Deventer, J. S. J., & Provis, J. L. (2015) · Journal of the American Ceramic Society · doi:10.1111/jace.13360 · Cited by 287 · cited 2×
“% of activator, the degree of reaction in the simulations was set to be 61% at 72 h after mixing, adopted from the experimental observations in a previous study [19], where slag with a similar chemical composition was used.”
MethodResultSelf-citationEffect of activator mix on the hydration and strength behaviour of alkali-activated slag cements
Fernandez-Jimenez, A., & Puertas, F. (2003) · Advances in Cement Research · doi:10.1680/adcr.15.3.129.36623 · Cited by 285 · cited 4×
“The identification of this pre-induction period is consistent with several previous observations of sodium silicate activated slag cements [8,11].”
BackgroundMethodResultInfluentialA comparative review of the aqueous corrosion of glasses, crystalline ceramics, and metals
Frankel, G. S., Vienna, J. D., Lian, J., Scully, J. R., Gin, S., Ryan, J. V., Wang, J., Kim, S. H., Windl, W., & Du, J. (2018) · npj Materials Degradation · doi:10.1038/s41529-018-0037-2 · Cited by 276 · cited 1×
“However, the presence of sulfide or other redox-active components is generally believed to increase, rather than decrease, the dissolution rates of solids [21], so it is not very clear how such a mechanism would take place from a chemical perspective.”
BackgroundThermodynamic modelling of alkali-activated slag cements
Myers, R. J., Lothenbach, B., Bernal, S. A., & Provis, J. L. (2015) · Applied Geochemistry · doi:10.1016/j.apgeochem.2015.06.006 · Cited by 240 · cited 4×
“The Truesdell–Jones form of the extended Debye–Hückel equation was used to calculate the aqueous-phase activity coefficients, and solid solution models for alkali-substituted calcium aluminate silicate hydrate gels (CNASH_ss) and for hydroxylated hydrotalcite (MgAl-OH-LDH_ss) were used; these are all described in deta…”
BackgroundMethodResultSelf-citationTemperature and activator effect on early-age reaction kinetics of alkali-activated slag binders
Gebregziabiher, B. S., Thomas, R. J., & Peethamparan, S. (2016) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2016.03.098 · Cited by 207 · cited 1×
“Additionally, previous observations have shown that an increased sodium silicate modulus (SiO2/Na2O ratio) results in a greater cumulative heat release [25].”
BackgroundSome factors affecting early hydration of alkali-slag cements
Shi, C., & Day, R. L. (1996) · Cement and Concrete Research · doi:10.1016/s0008-8846(96)85031-9 · Cited by 187 · cited 1×
“This drives faster dissolution of the slag particles and precipitation of mainly C-(A)-S-H type gels [11,22,23], which have been reported as the main reaction product for the silicate activated slags used in this study, and others of comparable composition [9].”
MethodKinetic study on hydration of alkali-activated slag
Huanhai, Z., Xuequan, W., Xu, Z., & Mingshu, T. (1993) · Cement and Concrete Research · doi:10.1016/0008-8846(93)90062-e · Cited by 151 · cited 1×
“The pH of the activating solution plays an important role in the initial dissolution and polycondensation of silicate and aluminate species in alkali-activated slag cements [11,12]; activating solutions with a high pH promote slag dissolution [13], while those with pH values lower than 9.”
BackgroundInfluence of slag composition on the hydration of alkali-activated slags
Winnefeld, F., Haha, M. B., Saoût, G. L., Costoya, M., Ko, S., & Lothenbach, B. (2014) · Journal of Sustainable Cement-Based Materials · doi:10.1080/21650373.2014.955550 · Cited by 126 · cited 1×
“[26] was adopted in this study to identify any potential correlation between the chemical composition of the slag, the initial precipitation of the reaction products, and the extent of the reaction of the slag.”
MethodSurface Chemistry of Calcium Aluminosilicate Glasses
Snellings, R. (2014) · Journal of the American Ceramic Society · doi:10.1111/jace.13263 · Cited by 108 · cited 1×
“Congruent dissolution of slag was assumed as the initial alkalinity of the system would be much higher than pH 12 [29].”
BackgroundFlyunt, R., Schuchmann, M. N., & von Sonntag, C. (2001) · Chemistry - A European Journal · doi:10.1002/1521-3765(20010216)7:4<858::aid-chem858>3.0.co;2-n · Cited by 99
Solubility and Aging of Calcium Silicate Hydrates in Alkaline Solutions at 25°C
Macphee, D. E., Luke, K., Glasser, F. P., & Lachowski, E. E. (1989) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1989.tb06189.x · Cited by 81
Navrotsky, A., & Tian, Z.-R. (2001) · Chemistry - A European Journal · doi:10.1002/1521-3765(20010216)7:4<769::aid-chem769>3.0.co;2-j · Cited by 55
Research works printed but not linked: 2
- Osborn, E.F., Roeder, P.L., and Ulmer, G.C. (1969). Part I—Phase equilibria at solidus temperatures in the quaternary system CaO-MgO-Al2O3-SiO2 and their bearing on optimun composition of blast furnace slag and on slag properties. Bulletin of the Earth and Mineral Sciences Experiment Station, The Pennsylvania State University.
- Smolczyk, H.G. (July, January 30). Slag structure and identification of slags. Proceedings of the 7th International Congress on the Chemistry of Cement, Paris, France.
Cited by
Recent progress in low-carbon binders
Shi, C., Qu, B., & Provis, J. L. (2019) · Cement and Concrete Research · doi:10.1016/j.cemconres.2019.05.009 · Cited by 714
Self-citationLi, L., Xie, J., Zhang, B., Feng, Y., & Yang, J. (2023) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2023.130389 · Cited by 160
Luukkοnen, T., Sreenivasan, H., Abdollahnejad, Z., Yliniemi, J., Kantola, A. M., Telkki, V., Kinnunen, P., & Illikainen, M. (2019) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2019.117354 · Cited by 152
A Review of Durability and Strength Characteristics of Alkali-Activated Slag Concrete
Mohamed, O. A. (2019) · Materials · doi:10.3390/ma12081198 · Cited by 162
“In general, the high pH of the alkaline activator promotes dissolution of GGBS, which drives chemical reaction and strength development [14].”
BackgroundPalomo, A., Maltseva, O., García-Lodeiro, I., & Fernández‐Jiménez, A. (2021) · Frontiers in Chemistry · doi:10.3389/fchem.2021.705475 · Cited by 130
Metadata
- Authors
- Criado, M., Walkley, B., Ke, X., Provis, J. L., & Bernal, S. A.
- Affiliations
- Instituto de Ciencias de La Construcción Eduardo Torroja (ES)
- University of Sheffield (GB)
- University of Bath (GB)
- University of Leeds (GB)
- Corresponding author
- Provis, John L.
- Bernal, Susan A.
- Venue
- Sustainability
- Publisher
- MDPI AG
- Published
- 2018-12-11
- Volume
- 10
- Issue
- 12
- Pages
- 4709
- ISSN
- 2071-1050 (ISSN-L)
- OpenAlex
- W2905264317
- Cited by
- 63
- References
- 28
- Citations by year
- 2026: 6 · 2025: 2 · 2024: 2 · 2023: 14 · 2022: 14 · 2021: 8 · 2020: 9 · 2019: 8
- FWCI
- 5.62
- Type
- journal article
- Language
- en
- Open access
- gold
- dx.doi.org
- Licence
- Locations
- Sustainability (publishedVersion, cc-by)
- White Rose Research Online (University of Leeds, The University of Sheffield, University of York) (acceptedVersion)
- RePEc: Research Papers in Economics (submittedVersion)
- DIGITAL.CSIC (Spanish National Research Council (CSIC)) (submittedVersion, cc-by)
- DOAJ (DOAJ: Directory of Open Access Journals) (submittedVersion, cc-by-sa)
- Funders
- FP7 Ideas: European Research Council (StG 335928)
- Engineering and Physical Sciences Research Council (EP/P013171/1, EP/R001642/1)
- Topics
- Physical Sciences › Engineering › Civil and Structural Engineering › Concrete and Cement Materials Research
- Physical Sciences › Engineering › Building and Construction › Materials Engineering and Processing
- Physical Sciences › Materials Science › Materials Chemistry › Magnesium Oxide Properties and Applications
- Keywords
- ground granulated blast furnace slag, sodium metasilicate, alkali-activated slag, reaction kinetics, MgO content, CaO content, slag reactivity, isothermal calorimetry
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).