The DOI matches its Crossref record; 85 of the 85 references it cites were found in a registry or an index.
Corrosion of Additively Manufactured Alloys: A Review
Open accessAbstract
Additive manufacturing (AM), often termed 3D printing, has recently emerged as a mainstream means of producing metallic components from a variety of metallic alloys. The numerous benefits of AM include net shape manufacturing, efficient use of material, suitability to low volume production runs, and the ability to explore alloy compositions not previously accessible to conventional casting. The process of AM, which is nominally performed using laser (or electron) based local melting, has a definitive role in the resultant alloy microstructure. Herein, the corrosion of alloys prepared by AM using laser and electron-based methods, relating the corrosion performance to the microstructural features influenced by AM processing, are reviewed. Such features include unique porosity, grain structures, dislocation networks, residual stress, solute segregation, and surface roughness. Correlations between reported results and deficiencies in present understanding are highlighted.
Overview
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Additive manufacturing of metallic components – Process, structure and properties
DebRoy, T., Wei, H. L., Zuback, J. S., Mukherjee, T., Elmer, J. W., Milewski, J. O., Beese, A. M., Wilson-Heid, A., De, A., & Zhang, W. (2018) · Progress in Materials Science · doi:10.1016/j.pmatsci.2017.10.001 · Cited by 8,805
Metal Additive Manufacturing: A Review
Frazier, W. E. (2014) · Journal of Materials Engineering and Performance · doi:10.1007/s11665-014-0958-z · Cited by 5,984
Additive manufacturing of metals
Herzog, D., Seyda, V., Wycisk, E., & Emmelmann, C. (2016) · Acta Materialia · doi:10.1016/j.actamat.2016.07.019 · Cited by 4,759
Laser additive manufacturing of metallic components: materials, processes and mechanisms
Gu, D. D., Meiners, W., Wissenbach, K., & Poprawe, R. (2012) · International Materials Reviews · doi:10.1179/1743280411y.0000000014 · Cited by 3,197
3D printing of high-strength aluminium alloys
Martin, J. H., Yahata, B. D., Hundley, J. M., Mayer, J. A., Schaedler, T. A., & Pollock, T. M. (2017) · Nature · doi:10.1038/nature23894 · Cited by 2,950
Khairallah, S. A., Anderson, A. T., Rubenchik, A., & King, W. E. (2016) · Acta Materialia · doi:10.1016/j.actamat.2016.02.014 · Cited by 2,766
The metallurgy and processing science of metal additive manufacturing
Sames, W. J., List, F. A., Pannala, S., Dehoff, R. R., & Babu, S. S. (2016) · International Materials Reviews · doi:10.1080/09506608.2015.1116649 · Cited by 2,529
Residual stresses in selective laser sintering and selective laser melting
Mercelis, P., & Kruth, J. (2006) · Rapid Prototyping Journal · doi:10.1108/13552540610707013 · Cited by 2,015
Wire + Arc Additive Manufacturing
Williams, S., Martina, F., Addison, A. C., Ding, J., Pardal, G., & Colegrove, P. A. (2015) · Materials Science and Technology · doi:10.1179/1743284715y.0000000073 · Cited by 1,971
Metal Additive Manufacturing: A Review of Mechanical Properties
Lewandowski, J. J., & Seifi, M. (2016) · Annual Review of Materials Research · doi:10.1146/annurev-matsci-070115-032024 · Cited by 1,722
Metal Fabrication by Additive Manufacturing Using Laser and Electron Beam Melting Technologies
Murr, L. E., Gaytan, S. M., Ramirez, D. A., Martinez, E., Hernandez, J., Amato, K. N., Shindo, P. W., Medina, F. R., & Wicker, R. B. (2012) · Journal of Materials Science & Technology · doi:10.1016/s1005-0302(12)60016-4 · Cited by 1,686
Xu, W., Brandt, M., Sun, S., Elambasseril, J., Liu, Q., Latham, K., Xia, K., & Qian, M. (2015) · Acta Materialia · doi:10.1016/j.actamat.2014.11.028 · Cited by 1,245
Shamsaei, N., Yadollahi, A., Bian, L., & Thompson, S. M. (2015) · Additive Manufacturing · doi:10.1016/j.addma.2015.07.002 · Cited by 1,108
Gong, H., Rafi, K., Gu, H., Starr, T., & Stucker, B. (2014) · Additive Manufacturing · doi:10.1016/j.addma.2014.08.002 · Cited by 1,038
Liverani, E., Toschi, S., Ceschini, L., & Fortunato, A. (2017) · Journal of Materials Processing Technology · doi:10.1016/j.jmatprotec.2017.05.042 · Cited by 990
Gorsse, S., Hutchinson, C., Gouné, M., & Banerjee, R. (2017) · Science and Technology of Advanced Materials · doi:10.1080/14686996.2017.1361305 · Cited by 920
Jia, Q., & Gu, D. (2014) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2013.09.171 · Cited by 905
Szklarska‐Śmiałowska, Z. (1986) · Cited by 862
Gokuldoss, P. K., Kolla, S., & Eckert, J. (2017) · Materials · doi:10.3390/ma10060672 · Cited by 804
Wang, Z., Palmer, T. A., & Beese, A. M. (2016) · Acta Materialia · doi:10.1016/j.actamat.2016.03.019 · Cited by 789
Ryan, M. P., Williams, D. E., Chater, R. J., Hutton, B. M., & McPhail, D. S. (2002) · Nature · doi:10.1038/415770a · Cited by 760
Cherry, J. A., Davies, H. M., Mehmood, S., Lavery, N. P., Brown, S. G. R., & Sienz, J. (2015) · The International Journal of Advanced Manufacturing Technology · doi:10.1007/s00170-014-6297-2 · Cited by 755
Selective laser melting of stainless steel 316L with low porosity and high build rates
Sun, Z., Tan, X., Tor, S. B., & Yeong, W. Y. (2016) · Materials & Design · doi:10.1016/j.matdes.2016.05.035 · Cited by 714
Xu, W., Lui, E. W., Pateras, A., Qian, M., & Brandt, M. (2017) · Acta Materialia · doi:10.1016/j.actamat.2016.12.027 · Cited by 687
Shipley, H., McDonnell, D., Culleton, M., Coull, R., Lupoi, R., O’Donnell, G. E., & Trimble, D. (2018) · International Journal of Machine Tools and Manufacture · doi:10.1016/j.ijmachtools.2018.01.003 · Cited by 617
Formation of metastable cellular microstructures in selective laser melted alloys
Prashanth, K. G., & Eckert, J. (2016) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2016.12.209 · Cited by 597
Dehoff, R. R., Kirka, M. M., Sames, W. J., Bilheux, H., Tremsin, A. S., Lowe, L. E., & Babu, S. S. (2015) · Materials Science and Technology · doi:10.1179/1743284714y.0000000734 · Cited by 555
Suryawanshi, J., Prashanth, K. G., Scudino, S., Eckert, J., Prakash, O., & Ramamurty, U. (2016) · Acta Materialia · doi:10.1016/j.actamat.2016.06.009 · Cited by 549
A study on the residual stress during selective laser melting (SLM) of metallic powder
Liu, Y., Yang, Y., & Wang, D. (2016) · The International Journal of Advanced Manufacturing Technology · doi:10.1007/s00170-016-8466-y · Cited by 534
Ziętala, M., Durejko, T., Polański, M., et al. (2016) · Materials Science and Engineering A · doi:10.1016/j.msea.2016.09.028 · Cited by 503
Takaichi, A., Suyalatu, Nakamoto, T., Joko, N., Nomura, N., Tsutsumi, Y., Migita, S., Doi, H., Kurosu, S., Chiba, A., et al. (2013) · Journal of the mechanical behavior of biomedical materials/Journal of mechanical behavior of biomedical materials · doi:10.1016/j.jmbbm.2013.01.021 · Cited by 489
Oxides, porosity and fatigue performance of AlSi10Mg parts produced by selective laser melting
Ming, T., & Pistorius, P. C. (2016) · International Journal of Fatigue · doi:10.1016/j.ijfatigue.2016.06.002 · Cited by 487
Tucho, W. M., Lysne, V. H., Austbø, H., Sjolyst-Kverneland, A., & Hansen, V. (2018) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2018.01.098 · Cited by 482
Murr, L. E., Martinez, E., Amato, K. N., Gaytan, S. M., Hernandez, J., Ramirez, D. A., Shindo, P. W., Medina, F., & Wicker, R. B. (2012) · Journal of Materials Research and Technology · doi:10.1016/s2238-7854(12)70009-1 · Cited by 470
Practical considerations and capabilities for laser assisted direct metal deposition
Lewis, G. K., & Schlienger, E. (2000) · Materials & Design (1980-2015) · doi:10.1016/s0261-3069(99)00078-3 · Cited by 449
Effects of processing parameters on tensile properties of selective laser melted 304 stainless steel
Guan, K., Wang, Z., Gao, M., Li, X., & Zeng, X. (2013) · Materials & Design · doi:10.1016/j.matdes.2013.03.056 · Cited by 423
Guo, P., Zou, B., Huang, C., & Gao, H. (2016) · Journal of Materials Processing Technology · doi:10.1016/j.jmatprotec.2016.09.005 · Cited by 413
Sander, G., Thomas, S., Cruz, V., Jurg, M., Birbilis, N., Gao, X., Brameld, M., & Hutchinson, C. R. (2017) · Journal of The Electrochemical Society · doi:10.1149/2.0551706jes · Cited by 398
Self-citationAdditively manufactured biodegradable porous magnesium
Li, Y., Zhou, J., Pavanram, P., Leeflang, M. A., Fockaert, L. I., Pouran, B., Tümer, N., Schröder, K.-U., Mol, J. M. C., Weinans, H., et al. (2018) · Acta Biomaterialia · doi:10.1016/j.actbio.2017.12.008 · Cited by 396
On the enhanced corrosion resistance of a selective laser melted austenitic stainless steel
Chao, Q., Cruz, V., Thomas, S., Birbilis, N., Collins, P., Taylor, A., Hodgson, P. D., & Fabijanic, D. (2017) · Scripta Materialia · doi:10.1016/j.scriptamat.2017.07.037 · Cited by 387
Self-citationDefining the tensile properties of Al-12Si parts produced by selective laser melting
Prashanth, K. G., Scudino, S., & Eckert, J. (2017) · Acta Materialia · doi:10.1016/j.actamat.2016.12.044 · Cited by 382
Stewart, J., & Williams, D. E. (1992) · Corrosion Science · doi:10.1016/0010-938x(92)90074-d · Cited by 367
Chen, X., Li, J., Cheng, X., Wang, H., & Huang, Z. (2018) · Materials Science and Engineering: A · doi:10.1016/j.msea.2017.10.002 · Cited by 340
Lou, X., Andresen, P. L., & Rebak, R. B. (2018) · Journal of Nuclear Materials · doi:10.1016/j.jnucmat.2017.11.036 · Cited by 310
Wang, R., Zhang, K., Davies, C., & Wu, X. (2017) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2016.10.138 · Cited by 306
Metallic additive manufacturing: state-of-the-art review and prospects
Vayre, B., Vignat, F., & Villeneuve, F. (2012) · Mechanics & Industry · doi:10.1051/meca/2012003 · Cited by 294
Sliding Wear Characteristics and Corrosion Behaviour of Selective Laser Melted 316L Stainless Steel
Sun, Y., Moroz, A., & Alrbaey, K. (2014) · Journal of Materials Engineering and Performance · doi:10.1007/s11665-013-0784-8 · Cited by 286
Control of melt pool temperature and deposition height during direct metal deposition process
Song, L., Bagavath-Singh, V., Dutta, B., & Mazumder, J. (2012) · The International Journal of Advanced Manufacturing Technology · doi:10.1007/s00170-011-3395-2 · Cited by 283
Microstructure and Corrosion Resistance of Laser Additively Manufactured 316L Stainless Steel
Trelewicz, J. R., Halada, G. P., Donaldson, O. K., & Manogharan, G. P. (2016) · JOM · doi:10.1007/s11837-016-1822-4 · Cited by 274
A review on powder bed fusion technology of metal additive manufacturing
Bhavar, V., Kattire, P., Patil, V., Khot, S., Gujar, K., & Singh, R. (2017) · Additive Manufacturing Handbook · doi:10.1201/9781315119106-15 · Cited by 258
Wang, D., Liu, Y., Yang, Y., & Xiao, D. (2016) · Rapid Prototyping Journal · doi:10.1108/rpj-06-2015-0078 · Cited by 254
316L Stainless Steel with Gradient Porosity Fabricated by Selective Laser Melting
Li, R., Liu, J., Shi, Y., Du, M., & Xie, Z. (2010) · Journal of Materials Engineering and Performance · doi:10.1007/s11665-009-9535-2 · Cited by 247
Tian, Y., McAllister, D., Colijn, H., Mills, M., Farson, D., Nordin, M., & Babu, S. (2014) · Metallurgical and Materials Transactions A · doi:10.1007/s11661-014-2370-6 · Cited by 241
Mani, M., Lane, B. M., Donmez, M. A., Feng, S. C., & Moylan, S. P. (2017) · International Journal of Production Research · doi:10.1080/00207543.2016.1223378 · Cited by 225
Corrosion Behavior of Additive Manufactured Ti-6Al-4V Alloy in NaCl Solution
Yang, J., Yang, H., Yu, H., Wang, Z., & Zeng, X. (2017) · Metallurgical and Materials Transactions A · doi:10.1007/s11661-017-4087-9 · Cited by 219
Industrial Additive Manufacturing: A manufacturing systems perspective
Eyers, D. R., & Potter, A. T. (2017) · Computers in Industry · doi:10.1016/j.compind.2017.08.002 · Cited by 215
A three dimensional model for direct laser metal powder deposition and rapid prototyping
Labudovic, M., Hu, D., & Kovacevic, R. (2003) · Journal of Materials Science · doi:10.1023/a:1021153513925 · Cited by 212
Corrosion Behaviour of Selective Laser Melted Ti-TiB Biocomposite in Simulated Body Fluid
Chen, Y., Zhang, J., Dai, N., Qin, P., Attar, H., & Zhang, L.-C. (2017) · Electrochimica Acta · doi:10.1016/j.electacta.2017.02.112 · Cited by 207
Anisotropic response of Ti-6Al-4V alloy fabricated by 3D printing selective laser melting
Chen, L. Y., Huang, J. C., Lin, C., Pan, C., Chen, S. Y., Yang, T.-J., Lin, D. Y., Lin, H. K., & Jang, J. S. C. (2016) · Materials Science and Engineering A · doi:10.1016/j.msea.2016.11.061 · Cited by 182
Lou, X., Song, M., Emigh, P. W., Othon, M. A., & Andresen, P. L. (2017) · Corrosion Science · doi:10.1016/j.corsci.2017.09.017 · Cited by 174
Zhao, B., Wang, H., Qiao, N., Wang, C., & Hu, M. (2017) · Materials Science and Engineering: C · doi:10.1016/j.msec.2016.07.045 · Cited by 169
Gu, H., Gong, H., Pal, D., Rafi, K., Starr, T. L., & Stucker, B. E. (2013) · doi:10.26153/tsw/15572 · Cited by 166
Wang, P., Sin, W., Nai, M., & Wei, J. (2017) · Materials · doi:10.3390/ma10101121 · Cited by 164
Guo, S., Lu, Y., Wu, S., Liu, L., He, M., Zhao, C., Gan, Y., Lin, J., Luo, J., Xu, X., et al. (2017) · Materials Science and Engineering: C · doi:10.1016/j.msec.2016.11.126 · Cited by 163
Influence of energy density on metallurgy and properties in metal additive manufacturing
Yusuf, S. M., & Gao, N. (2017) · Materials Science and Technology · doi:10.1080/02670836.2017.1289444 · Cited by 163
Murr, L. E. (2018) · Metallography Microstructure and Analysis · doi:10.1007/s13632-018-0433-6 · Cited by 156
Xie, F., He, X., Cao, S., Mei, M., & Qu, X. (2013) · Electrochimica Acta · doi:10.1016/j.electacta.2013.04.105 · Cited by 154
Corrosion Properties of Powder Bed Fusion Additively Manufactured 17-4 PH Stainless Steel
Schaller, R. F., Taylor, J. M., Rodelas, J., & Schindelholz, E. J. (2017) · CORROSION · doi:10.5006/2365 · Cited by 146
Zhai, Y., Galarraga, H., & Lados, D. A. (2015) · Procedia Engineering · doi:10.1016/j.proeng.2015.08.007 · Cited by 144
Effect of heat treatment on corrosion resistance of DMLS AlSi10Mg alloy
Cabrini, M., Lorenzi, S., Pastore, T., Pellegrini, S., Ambrosio, E. P., Calignano, F., Manfredi, D., Pavese, M., & Fino, P. (2016) · Electrochimica Acta · doi:10.1016/j.electacta.2016.04.157 · Cited by 143
Wang, P., Tan, X., Nai, M. L. S., Tor, S. B., & Wei, J. (2016) · Materials & Design · doi:10.1016/j.matdes.2016.01.093 · Cited by 140
Laser rapid solidification improves corrosion behavior of Mg-Zn-Zr alloy
Shuai, C., Yang, Y., Wu, P., Lin, X., Liu, Y., Zhou, Y., Feng, P., Liu, X., & Peng, S. (2016) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2016.09.019 · Cited by 130
Microstructure and corrosion behavior of laser processed NiTi alloy
Marattukalam, J. J., Singh, A. K., Datta, S., Das, M., Balla, V. K., Bontha, S., & Kalpathy, S. K. (2015) · Materials Science and Engineering C · doi:10.1016/j.msec.2015.07.067 · Cited by 124
Gong, X., Cui, Y., Wei, D., Liu, B., Liu, R., Nie, Y., & Li, Y. (2017) · Corrosion Science · doi:10.1016/j.corsci.2017.08.008 · Cited by 121
Review on Powder-Based Electron Beam Additive Manufacturing Technology
Gong, X., Anderson, T., & Chou, K. (2012) · doi:10.1115/isfa2012-7256 · Cited by 116
Lou, X., Othon, M. A., & Rebak, R. B. (2017) · Corrosion Science · doi:10.1016/j.corsci.2017.08.023 · Cited by 114
Stoudt, M. R., Ricker, R. E., Lass, E. A., & Levine, L. E. (2017) · JOM · doi:10.1007/s11837-016-2237-y · Cited by 97
Xu, Y., Lu, Y., Sundberg, K. L., Liang, J., & Sisson, R. D. (2017) · Journal of Materials Engineering and Performance · doi:10.1007/s11665-017-2710-y · Cited by 90
Additive Manufacturing of Titanium Alloys for Orthopedic Applications: A Materials Science Viewpoint
Majumdar, T., Eisenstein, N., Frith, J. E., Cox, S. C., & Birbilis, N. (2018) · Advanced Engineering Materials · doi:10.1002/adem.201800172 · Cited by 85
Self-citationInvestigations on heat regulation of additive manufacturing processes for metal structures
Zaeh, M. F., & Ott, M. (2011) · CIRP Annals · doi:10.1016/j.cirp.2011.03.109 · Cited by 61
Surface characterisation and corrosion behaviour of oxide layer for SLMed-316L stainless steel
Harun, W. S. W., Asri, R. I. M., Romlay, F. R. M., Sharif, S., Jan, N. H. M., & Tsumori, F. (2018) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2018.03.233 · Cited by 52
Shang, Y., Yuan, Y., Li, D., et al. (2017) · The International Journal of Advanced Manufacturing Technology · doi:10.1007/s00170-017-0525-5 · Cited by 51
Bhattacharya, S., Dinda, G. P., Dasgupta, A. K., et al. (2011) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2011.03.091 · Cited by 50
Mahamood, R. M., & Akinlabi, E. T. (2017) · Materials Science · doi:10.1007/s11003-017-0046-2 · Cited by 16
Hot Corrosion of Ti–Re Alloys Fabricated by Selective Laser Melting
Majchrowicz, K., Pakieła, Z., Moszczyńska, D., Kurzynowski, T., & Chlebus, E. (2017) · Oxidation of Metals · doi:10.1007/s11085-017-9825-2 · Cited by 14
Cited by
Additive manufacturing of steels: a review of achievements and challenges
Haghdadi, N., Laleh, M., Moyle, M., & Primig, S. (2021) · Journal of Materials Science · doi:10.1007/s10853-020-05109-0 · Cited by 622
Additive manufacturing of heat exchangers in aerospace applications: a review
Careri, F., Khan, R. H. U., Todd, C., & Attallah, M. M. (2023) · Applied Thermal Engineering · doi:10.1016/j.applthermaleng.2023.121387 · Cited by 320
Mukherjee, T., Elmer, J. W., Wei, H. L., Lienert, T. J., Zhang, W., Kou, S., & DebRoy, T. (2023) · Progress in Materials Science · doi:10.1016/j.pmatsci.2023.101153 · Cited by 267
The passivity of selective laser melted 316L stainless steel
Kong, D., Dong, C., Ni, X., Zhang, L., Luo, H., Li, R., Wang, L., Man, C., & Li, X. (2020) · Applied Surface Science · doi:10.1016/j.apsusc.2019.144495 · Cited by 253
Metadata
- Authors
- Sander, G., Tan, J., Balan, P., Gharbi, O., Feenstra, D. R., Singer, L., Thomas, S., Kelly, R. G., Scully, J. R., & Birbilis, N.
- Venue
- Corrosion
- Published
- 2018-10-01
- Volume
- 74
- Issue
- 12
- Pages
- 1318-1350
- ISSN
- 0010-9312 (ISSN-L)
- 1938-159X
- DOI
- 10.5006/2926
- OpenAlex
- W2895269473
- Cited by
- 344
- References
- 85
- FWCI
- 15.99
- Type
- journal article
- Language
- en
- Open access
- green
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.