Oxidative biodegradation mechanisms of biaxially strained poly(etherurethane urea) elastomers
The DOI matches its Crossref record; 3 of the 3 references it cites were found in a registry or an index.
Abstract
As part of ongoing studies in polyurethane biostability and biodegradation, we have investigated an in vitro system to test strained poly(etherurethane urea) (PEUU). Recently, we utilized this system to reproduce in vivo stress cracking in strained Pellethane®. In this study, strained PEUU was tested to determine whether it degrades through a common mechanism with Pellethane® and to further examine the steps involved in this degradation. Biaxially strained PEUU elastomers were treated with an α 2‐macroglobulin (α 2‐Mac) protein solution followed by an oxidative H 2 O 2/CoCl 2 treatment. Characterization of the strained PEUU specimens was performed with attenuated total reflectance‐Fourier transform infrared spectroscopy, scanning electron microscopy (SEM), electron spectroscopy for chemical analysis, and contact angle analysis. The results from these characterization techniques provide conclusive evidence that biodegradation of PEUU and Pellethane® occurs through a common mechanism. Chemical changes to the PEUU include cleavage of the polyether soft segments and urethane linkages, leaving the hard segment domains unaffected. SEM analysis shows that this chain cleavage leads to the development of severe pitting and cracking of the PEUU surface. In addition, the in vitro degradation accurately reproduces the in vivo degradation chemically and physically. This result verifies that the primary species responsible for biodegradation of PEUUs, in vivo, are hydroxyl and/or hydroperoxide radicals. α 2‐Mac pretreatment increases the rate of degradation compared to direct treatment in H 2 O 2/CoCl 2. As the PEUU soft segment chains are cleaved, the degradation products are extracted into the treatment solution or environment. Finally, a new biodegradation mechanism of PEUUs is presented that involves crosslinking of the polyether soft segments. © 1995 John Wiley & Sons, Inc.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Zhao, Q., Topham, N., Anderson, J. M., Hiltner, A., Lodoen, G., & Payet, C. R. (1991) · Journal of Biomedical Materials Research · doi:10.1002/jbm.820250205 · Cited by 318
Self-citationIn vivo biocompatibility studies. I. The cage implant system and a biodegradable hydrogel
Marchant, R., Hiltner, A., Hamlin, C., Rabinovitch, A., Slobodkin, R., & Anderson, J. M. (1983) · Journal of Biomedical Materials Research · doi:10.1002/jbm.820170209 · Cited by 181
Self-citationZhao, Q. H., McNally, A. K., Rubin, K. R., Renier, M., Wu, Y., Rose‐Caprara, V., Anderson, J. M., Hiltner, A., Urbanski, P., & Stokes, K. (1993) · Journal of Biomedical Materials Research · doi:10.1002/jbm.820270311 · Cited by 140
Self-citation
Cited by
On the mechanisms of biocompatibility
Williams, D. F. (2008) · Biomaterials · doi:10.1016/j.biomaterials.2008.04.023 · Cited by 2,772
Degradation and stabilization of polyurethane elastomers
Xie, F., Zhang, T., Bryant, P., Kurusingal, V., Colwell, J. M., & Laycock, B. (2019) · Progress in Polymer Science · doi:10.1016/j.progpolymsci.2018.12.003 · Cited by 722
Santerre, J. P., Woodhouse, K., Laroche, G., & Labow, R. S. (2005) · Biomaterials · doi:10.1016/j.biomaterials.2005.05.079 · Cited by 718
“Anderson [44–49] and Stokes [2] have applied strain into PU systems in order to observe its effect on the end point of EB (i.”
Intraoral aging of orthodontic materials: The picture we miss and its clinical relevance
Eliades, T., & Bourauel, C. (2005) · American Journal of Orthodontics and Dentofacial Orthopedics · doi:10.1016/j.ajodo.2004.09.015 · Cited by 296
Polymeric Systems for Bioprinting
Bedell, M. L., Navara, A. M., Du, Y., Zhang, S., & Mikos, A. G. (2020) · Chemical Reviews · doi:10.1021/acs.chemrev.9b00834 · Cited by 258
Nano-structured polymers enhance bladder smooth muscle cell function
Thapa, A., Miller, D. C., Webster, T. J., & Haberstroh, K. M. (2003) · Biomaterials · doi:10.1016/s0142-9612(03)00123-6 · Cited by 251
“The resulting polymer degradation does not affect the polymer hard segment domain [ 19 ].”
BackgroundSurface Chemistry of Biodegradable Polymers for Drug Delivery Systems
Ha, C.-S., & Gardella, J. A. (2005) · Chemical Reviews · doi:10.1021/cr040419y · Cited by 229
Elastomers for biomedical applications
Yoda, R. (1998) · Journal of Biomaterials Science, Polymer Edition · doi:10.1163/156856298x00046 · Cited by 226
Christenson, E. M., Anderson, J. M., & Hiltner, A. (2004) · Journal of Biomedical Materials Research Part A · doi:10.1002/jbm.a.30067 · Cited by 219
Self-citationSchumann, D. A., Wippermann, J., Klemm, D. O., Kramer, F., Koth, D., Kosmehl, H., Wahlers, T., & Salehi-Gelani, S. (2009) · Cellulose · doi:10.1007/s10570-008-9264-y · Cited by 206
Simmons, A., Hyvarinen, J., Odell, R. A., Martin, D. J., Gunatillake, P. A., Noble, K. R., & Poole-Warren, L. A. (2004) · Biomaterials · doi:10.1016/j.biomaterials.2004.01.004 · Cited by 189
Poly(carbonate urethane) and poly(ether urethane) biodegradation: In vivo studies
Christenson, E. M., Dadsetan, M., Wiggins, M., Anderson, J. M., & Hiltner, A. (2004) · Journal of Biomedical Materials Research Part A · doi:10.1002/jbm.a.30002 · Cited by 185
Self-citationMechanical characterisation of polyurethane elastomer for biomedical applications
Kanyanta, V., & Ivankovic, A. (2010) · Journal of the Mechanical Behavior of Biomedical Materials · doi:10.1016/j.jmbbm.2009.03.005 · Cited by 179
“This is adequately covered in literature (Stokes et al., 1995; Wiggins et al., 2003; Thoma, 1987; Schmidt et al., 1998; Zhao et al., 1990, 1991; Wu et al., 1992; Schubert et al., 1995, 1997).”
BackgroundHydrolytic degradation of poly(carbonate)-urethanes by monocyte-derived macrophages
Labow, R. S., Meek, E., & Santerre, J. P. (2001) · Biomaterials · doi:10.1016/s0142-9612(01)00049-7 · Cited by 108
Synthesis of degradable, biocompatible, and tough block‐copolyesterurethanes
Hirt, T. D., Neuenschwander, P., & Suter, U. W. (1996) · Macromolecular Chemistry and Physics · doi:10.1002/macp.1996.021971221 · Cited by 78
Antioxidant inhibition of poly(carbonate urethane) in vivo biodegradation
Christenson, E. M., Anderson, J. M., & Hiltner, A. (2006) · Journal of Biomedical Materials Research Part A · doi:10.1002/jbm.a.30506 · Cited by 64
Self-citationThe effect of oxidation on the enzyme-catalyzed hydrolytic biodegradation of poly(urethane)s
Labow, R. S., Tang, Y., McCloskey, C. B., & Santerre, J. P. (2002) · Journal of Biomaterials Science Polymer Edition · doi:10.1163/156856202320269148 · Cited by 54
Metadata
- Authors
- Schubert, M. A., Wiggins, M. J., Schaefer, M. P., Hiltner, A., & Anderson, J. M.
- Venue
- Journal of Biomedical Materials Research
- Publisher
- Wiley
- Published
- 1995-03
- Volume
- 29
- Issue
- 3
- Pages
- 337-347
- ISSN
- 0021-9304 (ISSN-L)
- 1097-4636
- OpenAlex
- W2042995201
- Cited by
- 117
- References
- 3
- FWCI
- 3.71
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.