Crack deflection processes—I. Theory
The DOI matches its Crossref record; 7 of the 7 references it cites were found in a registry or an index.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Stochastic Problems in Physics and Astronomy
Chandrasekhar, S. (1943) · Reviews of Modern Physics · doi:10.1103/revmodphys.15.1 · Cited by 8,470
Lawn, B. (1993) · Cambridge University Press eBooks · doi:10.1017/cbo9780511623127 · Cited by 4,759
Slightly curved or kinked cracks
Cotterell, B., & Rice, J. R. (1980) · International Journal of Fracture · doi:10.1007/bf00012619 · Cited by 1,876
Deighton, M. (1976) · Physics Bulletin · doi:10.1088/0031-9112/27/5/044 · Cited by 1,039
The interaction of a crack front with a second-phase dispersion
Lange, F. F. (1970) · Philosophical Magazine · doi:10.1080/14786437008221068 · Cited by 538
The strength of brittle materials containing second phase dispersions
Evans, A. G. (1972) · Philosophical magazine · doi:10.1080/14786437208220346 · Cited by 348
Self-citationAverage nearest-neighbor distances between uniformly distributed finite particles
Bansal, P. P., & Ardell, A. J. (1972) · Metallography · doi:10.1016/0026-0800(72)90048-1 · Cited by 176
Cited by
Fu, S.-Y., Feng, X.-Q., Lauke, B., & Mai, Y.-W. (2008) · Composites Part B: Engineering · doi:10.1016/j.compositesb.2008.01.002 · Cited by 3,549
Microstructural Design of Toughened Ceramics
Becher, P. F. (1991) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1991.tb06872.x · Cited by 997
Strong, tough and stiff bioinspired ceramics from brittle constituents
Bouville, F., Maire, E., Meille, S., Van de Moortèle, B., Stevenson, A. J., & Deville, S. (2014) · Nature Materials · doi:10.1038/nmat3915 · Cited by 959
Toughening mechanisms of nanoparticle-modified epoxy polymers
Johnsen, B. B., Kinloch, A. J., Mohammed, R. D., Taylor, A. C., & Sprenger, S. (2007) · Polymer · doi:10.1016/j.polymer.2006.11.038 · Cited by 942
Fracture and Fatigue in Graphene Nanocomposites
Reif, J., Rafiee, J., Srivastava, I., Wang, Z., Song, H., Yu, Z., & Koratkar, N. (2010) · Small · doi:10.1002/smll.200901480 · Cited by 907
Ritchie, R. O. (1988) · Materials Science and Engineering: A · doi:10.1016/0025-5416(88)90547-2 · Cited by 874
On the Mechanistic Origins of Toughness in Bone
Launey, M. E., Buehler, M. J., & Ritchie, R. O. (2010) · Annual Review of Materials Research · doi:10.1146/annurev-matsci-070909-104427 · Cited by 741
Evans, A. G., & Cannon, R. M. (1986) · Acta Metallurgica · doi:10.1016/0001-6160(86)90052-0 · Cited by 632
Self-citationThe true toughness of human cortical bone measured with realistically short cracks
Koester, K. J., Ager, J. W., & Ritchie, R. O. (2008) · Nature Materials · doi:10.1038/nmat2221 · Cited by 558
Pearson, R. A., & Yee, A. F. (1991) · Journal of Materials Science · doi:10.1007/bf01184979 · Cited by 537
SWANSON, P. L., FAIRBANKS, C. J., LAWN, B. R., MAI, Y., & HOCKEY, B. J. (1987) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1987.tb04982.x · Cited by 534
Impressive Fatigue Life and Fracture Toughness Improvements in Graphene Oxide/Epoxy Composites
Bortz, D. R., Heras, E. G., & Martin-Gullon, I. (2012) · Macromolecules · doi:10.1021/ma201563k · Cited by 514
THE THEORY OF SUBCRITICAL CRACK GROWTH WITH APPLICATIONS TO MINERALS AND ROCKS
Atkinson, B. K., & Meredith, P. G. (1987) · Fracture Mechanics of Rock · doi:10.1016/b978-0-12-066266-1.50009-0 · Cited by 446
Zirconia-toughened alumina (ZTA) ceramics
Wang, J., & Stevens, R. (1989) · Journal of Materials Science · doi:10.1007/bf02385721 · Cited by 426
Shin, M. K., Lee, B., Kim, S. H., Lee, J. A., Spinks, G. M., Gambhir, S., Wallace, G. G., Kozlov, M. E., Baughman, R. H., & Kim, S. J. (2012) · Nature Communications · doi:10.1038/ncomms1661 · Cited by 423
Preparation, mechanical and anti-friction performance of MXene/polymer composites
Zhang, H., Wang, L., Chen, Q., Li, P., Zhou, A., Cao, X., & Hu, Q. (2016) · Materials & Design · doi:10.1016/j.matdes.2015.12.084 · Cited by 410
Hsieh, T. H., Kinloch, A. J., Masania, K., Sohn Lee, J., Taylor, A. C., & Sprenger, S. (2010) · Journal of Materials Science · doi:10.1007/s10853-009-4064-9 · Cited by 391
Toughening mechanisms in thermoplastic-modified epoxies: 1. Modification using poly(phenylene oxide)
Pearson, R. A., & Yee, A. F. (1993) · Polymer · doi:10.1016/0032-3861(93)90051-b · Cited by 380
Mechanical, Thermal, and Electrical Properties of Graphene-Epoxy Nanocomposites—A Review
Atif, R., Shyha, I., & Inam, F. (2016) · Polymers · doi:10.3390/polym8080281 · Cited by 360
Graphene and graphene derivatives toughening polymers: Toward high toughness and strength
Wang, J., Jin, X., Li, C., Wang, W., Wu, H., & Guo, S. (2019) · Chemical Engineering Journal · doi:10.1016/j.cej.2019.03.229 · Cited by 333
Biomineralization: Integrating mechanism and evolutionary history
Gilbert, P. U. P. A., Bergmann, K. D., Boekelheide, N., Tambutté, S., Mass, T., Marin, F., Adkins, J. F., Erez, J., Gilbert, B., Knutson, V., et al. (2022) · Science Advances · doi:10.1126/sciadv.abl9653 · Cited by 327
Wang, J., Cheng, Q., Lin, L., & Jiang, L. (2014) · ACS Nano · doi:10.1021/nn406428n · Cited by 325
Twisting cracks in Bouligand structures
Suksangpanya, N., Yaraghi, N. A., Kisailus, D., & Zavattieri, P. (2017) · Journal of the Mechanical Behavior of Biomedical Materials · doi:10.1016/j.jmbbm.2017.06.010 · Cited by 294
Surface roughness profile and its effect on coating adhesion and corrosion protection: A review
Croll, S. G. (2020) · Progress in Organic Coatings · doi:10.1016/j.porgcoat.2020.105847 · Cited by 288
Patterning by controlled cracking
Nam, K. H., Park, I. H., & Ko, S. H. (2012) · Nature · doi:10.1038/nature11002 · Cited by 270
Crystallization toughening of a model glass-ceramic
Serbena, F. C., Mathias, I., Foerster, C. E., & Zanotto, E. D. (2015) · Acta Materialia · doi:10.1016/j.actamat.2014.12.007 · Cited by 222
Effective toughness of heterogeneous media
Hossain, M. Z., Hsueh, C.-J., Bourdin, B., & Bhattacharya, K. (2014) · Journal of the Mechanics and Physics of Solids · doi:10.1016/j.jmps.2014.06.002 · Cited by 220
“Consequently, there is an extensive literature on the fracture toughness of composite materials, e.g. (Bower and Ortiz, 1991; Cox and Yang, 2006; Evans and Faber, 1981; Faber and Evans, 1983, 1983; Gao and Rice, 1989; Hutchinson and Suo, 1992; Suresh, 1985).”
BackgroundR-curve behaviour of Al2O3 ceramics
Vekinis, G., Ashby, M. F., & Beaumont, P. W. R. (1990) · Acta Metallurgica et Materialia · doi:10.1016/0956-7151(90)90188-m · Cited by 220
In Situ Toughened Silicon Carbide with Al‐B‐C Additions
Cao, J. J., MoberlyChan, W. J., De Jonghe, L. C., Gilbert, C. J., & Ritchie, R. O. (1996) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1996.tb08145.x · Cited by 213
3D Printing of Biomimetic Composites with Improved Fracture Toughness
Jia, Z., & Wang, L. (2018) · SSRN Electronic Journal · doi:10.2139/ssrn.3300049 · Cited by 211
Biomimetic architected materials with improved dynamic performance
Jia, Z., Yu, Y., Hou, S., & Wang, L. (2019) · Journal of the Mechanics and Physics of Solids · doi:10.1016/j.jmps.2018.12.015 · Cited by 195
The roles of toughness and cohesive strength on crack deflection at interfaces
PARMIGIANI, J., & THOULESS, M. (2006) · Journal of the Mechanics and Physics of Solids · doi:10.1016/j.jmps.2005.09.002 · Cited by 191
“Deflection along interfaces in these materials results in toughening by crack bridging, frictional pull-out, or crack deflection [10] [11] (Fig.”
BackgroundWu, K., Song, Z., Zhang, S., Ni, Y., Cai, S., Gong, X., He, L., & Yu, S.-H. (2020) · Proceedings of the National Academy of Sciences · doi:10.1073/pnas.2000639117 · Cited by 189
Crack interaction with microstructure
Kumar, S., & Curtin, W. A. (2007) · Materials Today · doi:10.1016/s1369-7021(07)70207-9 · Cited by 180
Mechanistic aspects of the fracture toughness of elk antler bone
Launey, M. E., Chen, P.-Y., McKittrick, J., & Ritchie, R. O. (2010) · Acta Biomaterialia · doi:10.1016/j.actbio.2009.11.026 · Cited by 180
“Linear-elastic calculations using crack-deflection mechanics [49] show that for inplane deviations of the crack path, the resulting fracture toughness can be increased by up to a factor of two compared to that for an undeflected crack; where the crack twists out-of-plane, this increase can be significantly higher (fac…”
Zimmermann, E. A., Gludovatz, B., Schaible, E., Busse, B., & Ritchie, R. O. (2014) · Biomaterials · doi:10.1016/j.biomaterials.2014.03.066 · Cited by 163
Brittle fracture in disordered materials: A spring network model
Curtin, W. A., & Scher, H. (1990) · Journal of Materials Research · doi:10.1557/jmr.1990.0535 · Cited by 163
Crystal orientation, toughening mechanisms and a mimic of nacre
Feng, Q. L., Cui, F. Z., Pu, G., Wang, R. Z., & Li, H. D. (2000) · Materials Science and Engineering: C · doi:10.1016/s0928-4931(00)00138-7 · Cited by 158
Metadata
- Authors
- Faber, K. T., & Evans, A. G.
- Venue
- Acta Metallurgica
- Publisher
- Elsevier BV
- Published
- 1983-04
- Volume
- 31
- Issue
- 4
- Pages
- 565-576
- ISSN
- 0001-6160 (ISSN-L)
- OpenAlex
- W1986428572
- Cited by
- 1,444
- References
- 7
- FWCI
- 38.43
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.