The effects of chlorides, hydrogen chloride, and sulfur dioxide in the oxidation of steels below deposits
The DOI matches its Crossref record; 18 of the 18 references it cites were found in a registry or an index.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“The alkali chlorides initiate chlorine-induced corrosion on boiler steels under thermodynamically favourable conditions, followed by active oxidation by chlorine.”
From High Temperature Corrosion Resistant and Anti-slagging Coatings for Boilers: A Review (2024) · cites this paper as [14]
In the citing paper
“Despite the presence of corrosive sulphur dioxide (SO2), it was reported that SO2 was unable to diffuse through the oxidation scale to react with the boiler steel surface underneath unless there are cracks in the metal oxide scale [14].”
From High Temperature Corrosion Resistant and Anti-slagging Coatings for Boilers: A Review (2024) · cites this paper as [14]
In the citing paper
“The results of this study show that despite the presence of large amounts of Cl detected in some samples there is no indication of the active oxidation mechanism, driven by gaseous transport of Cl2(g) and MeClx(g), whereas the transport of O2(g) is prohibited, which has been suggested in literature.29”
From High-Temperature Corrosion Behavior of Superheater Materials at 600 °C: Insights from Laboratory and Field Exposures (2025) · cites this paper as [29]
Citations
Cites
(2006) · Electrochemistry and Corrosion Science · doi:10.1007/1-4020-7860-9_10 · Cited by 1,814
Stott, F. H. (1982) · Corrosion Science · doi:10.1016/0010-938x(82)90037-3 · Cited by 394
Whitney Award Lecture—1986: Chemistry and Electrochemistry of the Hot Corrosion of Metals
Rapp, R. A. (1986) · Corrosion · doi:10.5006/1.3583026 · Cited by 188
Ignition of nickel in environments containing oxygen and chlorine
Lee, Y. Y., & McNallan, M. J. (1987) · Metallurgical Transactions A · doi:10.1007/bf02668559 · Cited by 118
Einfluß von Chloriden auf die Oxidation des 2¼ Cr‐1 Mo‐Stahls
Reese, E., & Grabke, H. J. (1992) · Materials and Corrosion · doi:10.1002/maco.19920431202 · Cited by 70
Self-citationThe rate of chlorination of metals and oxides: Part I. Fe, Ni, and Sn in chlorine
Fruehan, R. J. (1972) · Metallurgical Transactions · doi:10.1007/bf02644233 · Cited by 62
Bramhoff, D., Grabke, H. J., Reese, E., & Schmidt, H. P. (1990) · Materials and Corrosion · doi:10.1002/maco.19900410602 · Cited by 55
Self-citationEinfluß von Natriumchlorid auf die Oxidation von hochlegierten Chrom‐ und Chrom‐Nickel‐Stählen
Reese, E., & Grabke, H. J. (1993) · Materials and Corrosion · doi:10.1002/maco.19930440204 · Cited by 55
Self-citationReinhold, K., & Häuffe, K. (1977) · Journal of The Electrochemical Society · doi:10.1149/1.2133445 · Cited by 47
Hochtemperaturkorrosion von Nickel in Chlor und Chlor‐Sauerstoffgemischen
Häuffe, K., & Hinrichs, J. (1970) · Materials and Corrosion · doi:10.1002/maco.19700211111 · Cited by 45
Research works printed but not linked: 2
- Bruce, 1969, J. Inst. Met., 97, 140
- M. Spiegel and H. J. Grabke, Werkstoffe u. Korr. (in press).
Cited by
Items 301–400 of 531
Initial Oxidation of a 9%CrMo- and a 12%CrMoV-Steel
Grabke, H. J., Tökei, Z., & Ostwald, C. (2004) · steel research international · doi:10.1002/srin.200405925 · Cited by 11
Self-citationPrevention of Superheater Corrosion in the Combustion of Biofuels
Salmenoja, K., & Mäkelä, K. (2000) · NACE CORROSION Conference · doi:10.5006/c2000-00238 · Cited by 10
Liu, X., Duan, Y., Chen, Q., Long, L., Lv, G., Huang, Q., & Jiang, X. (2022) · ACS Omega · doi:10.1021/acsomega.2c02722 · Cited by 10
High-Temperature Corrosion Characterization of Ni-Al Laser Cladding: The Effect of Al Content and Fe
Wang, X., Liu, Z., Cheng, K., Li, J., Ning, H., & Mao, J. (2024) · Journal of Thermal Spray Technology · doi:10.1007/s11666-024-01782-8 · Cited by 9
“It has been demonstrated that Cl 2 can react with metal group elements to produce the corresponding metal chlorides (Ref 39, 52, 53).”
Wu, S., Hu, Y., Chen, D., Wu, N., Zhao, X., Liu, Z., Zhang, R., Tang, Y., & Feng, Y. (2024) · Waste Management · doi:10.1016/j.wasman.2024.05.026 · Cited by 9
Wang, X., Fu, K., Ren, X., Xue, Y., & Luan, B. (2025) · Surfaces and Interfaces · doi:10.1016/j.surfin.2025.107190 · Cited by 16
Park, J. H., Lee, D.-H., Han, K.-H., Shin, J.-S., Bae, D.-H., Shim, T.-E., Lee, J. H., & Shun, D. (2019) · Fuel · doi:10.1016/j.fuel.2018.09.020 · Cited by 9
Hjörnhede, A., Sotkovszki, P., & Nylund, A. (2006) · Materials and Corrosion · doi:10.1002/maco.200503911 · Cited by 9
Phase Stability Diagrams for High Temperature Corrosion Processes
Ramos-Hernández, J. J., Porcayo-Calderón, J., Salinas-Bravo, V. M., Arrieta-González, C. D., Gonzalez-Rodriguez, J. G., & Martinez-Gomez, L. (2013) · Mathematical Problems in Engineering · doi:10.1155/2013/542061 · Cited by 9
Effect of Saline Environment on LCF Behavior of Inconel 718 at 550 °C
Mahobia, G. S., Paulose, N., Sreekanth, K., Mannan, S. L., Rao, G. S., & Singh, V. (2014) · Journal of Materials Engineering and Performance · doi:10.1007/s11665-014-1278-z · Cited by 9
Investigating corrosion memory: The influence of previous boiler operation on current corrosion rate
Paz, M. D., Zhao, D., Karlsson, S., Liske, J., & Jonsson, T. (2016) · Fuel Processing Technology · doi:10.1016/j.fuproc.2016.09.018 · Cited by 9
Okoro, S. C., Montgomery, M., Frandsen, F., & Pantleon, K. (2017) · Surface and Coatings Technology · doi:10.1016/j.surfcoat.2017.03.068 · Cited by 9
Innovative Production Technology of High Quality Pellets for Power Plants
Mudryk, K., Wróbel, M., Jewiarz, M., Pelczar, G., & Dyjakon, A. (2018) · Springer proceedings in energy · doi:10.1007/978-3-319-72371-6_69 · Cited by 9
Roshith, P., & Arivarasu, M. (2019) · Materials Research Express · doi:10.1088/2053-1591/ab61ab · Cited by 9
Improved oxidation and hot corrosion resistance of the NiSiAlY alloy at 750 ℃
Yu, M., Cui, T., Zhou, D., Li, R., Pu, J., & Li, C. (2021) · Materials Today Communications · doi:10.1016/j.mtcomm.2021.102939 · Cited by 15
Yan, M., Yang, Y., Jiang, J., Zheng, R., Ma, Y., Khalid, M., & Wibowo, H. (2022) · Waste Disposal & Sustainable Energy · doi:10.1007/s42768-022-00110-6 · Cited by 9
“The increase in Cl observed in Table 5 could be the result of the gradual infiltration of chloride molten salt into the matrix of the materials[44, 45].”
BackgroundCai, Y., Nguyen, T. D., Zhang, J., Gleeson, B. T., & Young, D. J. (2022) · Corrosion Science · doi:10.1016/j.corsci.2022.110822 · Cited by 9
High-Temperature Corrosion of A210-C Carbon Steel in Simulated Coal-Combustion Atmospheres
Peng, X., Liu, K., Pan, W., & Riley, J. T. (2003) · Oxidation of Metals · doi:10.1023/a:1024621514635 · Cited by 9
Hot Corrosion Mechanism of Steels Exposed to Heavy Metal Chlorides and Sulphates in SO2 Environment
Viitala, H., & Taskinen, P. A. (2016) · Oxidation of Metals · doi:10.1007/s11085-016-9634-z · Cited by 10
Standard liquid fuel for industrial boilers from used wood
Lindfors, C., Oasmaa, A., Välimäki, A., Ohra‐aho, T., Punkkinen, H., Bajamundi, C., & Onarheim, K. (2019) · Biomass and Bioenergy · doi:10.1016/j.biombioe.2019.105265 · Cited by 13
Effect of Chloride Content in Ash in Oxidation Kinetics of Ni-Based and Fe-Based Alloys
Schaal, E., David, N., Panteix, P., Rapin, C., Brossard, J.-M., & Maad, F. (2015) · Oxidation of Metals · doi:10.1007/s11085-015-9556-1 · Cited by 9
Pettersson, C., Svensson, J. E., & Johansson, L. G. (2006) · Materials science forum · doi:10.4028/www.scientific.net/msf.522-523.539 · Cited by 9
Ruiz-Cabañas, F. J., Prieto, C., Madina, V., Fernández, A. I., & Cabeza, L. F. (2019) · Journal of Energy Storage · doi:10.1016/j.est.2019.100922 · Cited by 9
Local reactions between NaCl and KCl particles and metal surfaces
Cha, S. C., & Spiegel, M. (2005) · Corrosion Engineering Science and Technology The International Journal of Corrosion Processes and Corrosion Control · doi:10.1179/174327805x66317 · Cited by 11
Self-citationBroström, M. (2010) · DiVA at Umeå University (Umeå University) · Cited by 21
Hu, Y. L., Jia, H., Zhang, X., Yang, X., Liu, B., Jiayu, X., Gao, Y., Ding, Y., & Zhang, D. (2024) · Journal of Materials Research and Technology · doi:10.1016/j.jmrt.2024.06.141 · Cited by 9
Kaczmarczyk, R., & Gurgul, S. (2024) · Energies · doi:10.3390/en17133223 · Cited by 10
Wang, X., Ji, Z., Gan, M., Fan, X., Sun, Z., Liu, L., Li, J., & Yu, D. (2025) · Engineering Failure Analysis · doi:10.1016/j.engfailanal.2025.109265 · Cited by 8
Investigation on corrosion behaviors of stainless steel in solar salt using cellular automata model
Zhang, R., Zhang, C., Zhang, C., Wu, Y., Li, C. S., & Lu, Y. (2025) · Solar Energy Materials and Solar Cells · doi:10.1016/j.solmat.2025.113435 · Cited by 8
Xie, Y. G., Chen, X., Wu, Y., Zhang, C., & Ma, C. (2025) · Journal of Energy Storage · doi:10.1016/j.est.2025.118404 · Cited by 8
Wang, Y., Liu, W., Zhou, M., Yang, W., Wang, D., Wang, Y., & Duan, L. (2025) · Fuel · doi:10.1016/j.fuel.2025.137170 · Cited by 9
Failure Analysis and Improvement Measures of Grate Bars Used in Iron Ore Pelletizing Plant
Sekhar, C., Moon, A. P., Dwarapudi, S., Kadhe, D. M., Gupta, N., Kundu, S., Mondal, A., Paul, I., & Singh, U. (2021) · Journal of Materials Engineering and Performance · doi:10.1007/s11665-021-05835-9 · Cited by 8
Viklund, P., Kassman, H., & Åmand, L.-E. (2014) · Materials and Corrosion · doi:10.1002/maco.201307162 · Cited by 11
Chlorine Corrosion Degradation of Low Alloyed Ferritic Steels in Temperature Range 450–550 °C
Dudziak, T. P., Jura, K., & Rutkowska, J. (2016) · Oxidation of Metals · doi:10.1007/s11085-016-9617-0 · Cited by 8
Krumm, L., & Galetz, M. C. (2020) · Materials and Corrosion · doi:10.1002/maco.201911091 · Cited by 8
Migration pattern of chlorine during co-pyrolysis for herb residue and coal
Guo, Z., Guo, F., Miao, Z., Guo, Y., Zhao, X., Liu, H., Wu, J., & Zhang, Y. (2021) · Journal of environmental chemical engineering · doi:10.1016/j.jece.2021.105196 · Cited by 8
Liu, X., Chen, Q., Long, L., Meng, X., Lv, G., Huang, Q., & Jiang, X. (2021) · Waste Disposal & Sustainable Energy · doi:10.1007/s42768-021-00087-8 · Cited by 8
“1 3 gas were previously confirmed to accelerate the oxidation of metals [3].”
BackgroundInfluentialCorrosion Behavior of High-Cr–Ni Materials in Biomass Incineration Atmospheres
Wei, L., Wang, S., Liu, G., Hao, W., Liang, K., Yang, X., & Diao, W. (2022) · ACS Omega · doi:10.1021/acsomega.2c01223 · Cited by 8
Ma, W., Zeng, S., & Wenga, T. (2024) · Corrosion Science · doi:10.1016/j.corsci.2024.112128 · Cited by 8
High temperature alloy chloridation at 850°C
Chevalier, S., Ched’homme, S., Bekaddour, A., Amilain‐Basset, K., & Buisson, L. (2007) · Materials and Corrosion · doi:10.1002/maco.200604013 · Cited by 11
Chevalier, S., Ched’homme, S., Bekaddour, A., Amilain‐Basset, K., & Buisson, L. (2007) · Materials and Corrosion · doi:10.1002/maco.200604012 · Cited by 8
Krumm, L., & Galetz, M. C. (2017) · Oxidation of Metals · doi:10.1007/s11085-017-9749-x · Cited by 8
A computational thermodynamic and kinetic study of chlorine binding to the Zr(0001) surface
Samin, A. J., & Taylor, C. D. (2017) · Colloids and Surfaces A Physicochemical and Engineering Aspects · doi:10.1016/j.colsurfa.2017.11.075 · Cited by 8
KCl‐induced corrosion of Ni‐based alloys containing 35–45 wt% Cr
Malede, Y. C., Simon, J. P., Jonsson, T., Montgomery, M., Dahl, K. V., & Hald, J. (2019) · Materials and Corrosion · doi:10.1002/maco.201810658 · Cited by 8
Li, K., Zeng, Y., & Luo, J. (2020) · International journal of greenhouse gas control · doi:10.1016/j.ijggc.2020.103108 · Cited by 9
Effect of High Temperature Hot Corrosion on the Compression Creep Behavior of 12Cr1MoV Alloys
He, J., & Xiong, W. (2017) · High Temperature Materials and Processes · doi:10.1515/htmp-2016-0027 · Cited by 8
Simulation of road salt corrosion in austenitic alloys for automotive exhaust systems
Antoni, L., Bousquet, R., & Davidson, J. H. (2003) · Materials at High Temperatures · doi:10.1179/mht.2003.065 · Cited by 8
“2/3 Fe3O4 + 2 NaCl (g) + 2/3 O2 → 2 NaFeO2 + Cl2 (2)”
BackgroundInfluentialErosion corrosion properties of HVOF coatings for municipal solid waste incinerator protection
Guilemany, J. M., Torrell, M., & Miguel, J. R. (2008) · Corrosion Engineering Science and Technology The International Journal of Corrosion Processes and Corrosion Control · doi:10.1179/174327807x234651 · Cited by 8
Maj, I., Niesporek, K., Matus, K., Miccio, F., Mazzocchi, M., & Łój, P. (2024) · Energies · doi:10.3390/en17081854 · Cited by 8
Czech, T., Marchewicz, A., Sobczyk, A. T., Krupa, A., Gazda, M., & Jaworek, A. (2024) · Applied Sciences · doi:10.3390/app14177616 · Cited by 9
Laboratory studies on the ageing behaviour of waste incineration superheater ash deposits
Balint, R., Niemi, J., Hayashi, S., & Lehmusto, J. (2025) · Energy · doi:10.1016/j.energy.2025.135359 · Cited by 7
Alloy degradation in a co-firing biomass CFB vortex finder application at 880 °C
Hagman, H., Boström, D., Lundberg, M., & Backman, R. (2019) · Corrosion Science · doi:10.1016/j.corsci.2019.01.038 · Cited by 7
Liu, X., Duan, Y., Zheng, L., Long, L., Khalid, Z., Huang, Q., & Jiang, X. (2023) · Journal of Material Cycles and Waste Management · doi:10.1007/s10163-023-01812-7 · Cited by 8
“This process is called “active oxidation” [18].”
High Temperature Degradation of Co Based Superalloy in Incinerator Environment
Mudgal, D., Verma, P. K., Singh, S. P., & Prakash, S. (2012) · Advanced materials research · doi:10.4028/www.scientific.net/amr.585.542 · Cited by 7
Identification and 3D Reconstruction of Cr5S6 Precipitates Along Grain Boundaries in Fe13Cr
Nützmann, K., Wollschläger, N., Rockenhäuser, C., Kranzmann, A., & Stephan‐Scherb, C. (2018) · JOM · doi:10.1007/s11837-018-2940-y · Cited by 7
Effect of Temperature on Corrosion Behaviour of Fe–Cr Alloys in Wet CO2 With and Without HCl Gases
Aye, K. K., Cai, Y., Zhang, J., & Young, D. J. (2022) · Oxidation of Metals · doi:10.1007/s11085-021-10092-1 · Cited by 7
“The active oxidation process [7] is one of volatilisation of metal oxides as chlorides, for example”
BackgroundField test of superheater corrosion in a CFB waste boiler: Part II – Scale formation characteristics
Andersson, P., & Norell, M. (2005) · Materials and Corrosion · doi:10.1002/maco.200403853 · Cited by 7
Talus, A., Alipour, Y., Norling, R., & Henderson, P. (2016) · Materials and Corrosion · doi:10.1002/maco.201508693 · Cited by 7
Zapote Seed (Pouteria mammosa L.) Valorization for Thermal Energy Generation in Tropical Climates
Perea-Moreno, M.-Á., Hernández-Escobedo, Q., Rueda-Martínez, F., & Perea-Moreno, A.-J. (2020) · Sustainability · doi:10.3390/su12104284 · Cited by 7
“The ash is considered an indicator of the efficiency of the biofuel because the more residue it leaves when burned, the greater the problems of clogging and corrosion in the installation [37].”
BackgroundHot waste-to-energy flue gas treatment using an integrated fluidised bed reactor
Bianchini, A., Pellegrini, M., & Saccani, C. (2008) · Waste Management · doi:10.1016/j.wasman.2008.09.007 · Cited by 7
“The corrosion behaviour of materials normally used in the superheater has been elucidated through several specific tests (Dechema, 1991; Grabke et al., 1995; Kawahara, 2002; Persson et al., 2007).”
MethodFouling in biomass fired boilers
Sandberg, J. (2007) · DiVA (Mälardalen University College) · Cited by 10
Decomposition of SO2 on Ni(111) Surface and the Effect of Metal Doping: A First-Principles Study
Liu, L., Zhang, C., Wang, W., Li, G., & Zhu, B. (2023) · Molecules · doi:10.3390/molecules28186739 · Cited by 6
“SO 2 is an important raw material that produces bulk chemicals, and it is also a major air pollutant, which kills lives [1], erodes metals [2–4], and poisons catalysts [5–7].”
BackgroundSingh, M. K., Mahobia, G. S., Sinha, O. P., & Singh, V. (2019) · Materials Research Express · doi:10.1088/2053-1591/ab3547 · Cited by 6
Lindmark, H., Jonsson, T., & Liske, J. (2024) · Corrosion Science · doi:10.1016/j.corsci.2024.111843 · Cited by 8
Corrosion in Complex Environments
Young, D. J. (2016) · Elsevier eBooks · doi:10.1016/b978-0-08-100101-1.00012-1 · Cited by 9
Kingsbery, P., & Stephan‐Scherb, C. (2022) · Materials and Corrosion · doi:10.1002/maco.202112901 · Cited by 6
Li, H., Wang, X., Feng, X., Yang, X., Tang, J., & Gong, J. (2022) · Materials and Corrosion · doi:10.1002/maco.202213323 · Cited by 6
Benalia, S., Tesfaye, F., Lindberg, D., Sibarani, D., Hupa, L., Chartrand, P., & Robelin, C. (2023) · Journal of Physical and Chemical Reference Data · doi:10.1063/5.0154609 · Cited by 6
Exposure of 304L and 310S in chlorinating gasification environments
Elger, R., Lindberg, F., Norling, R., & Pettersson, R. F. A. (2015) · Materials at High Temperatures · doi:10.1179/0960340914z.00000000059 · Cited by 6
Elevated temperature molten salt corrosion study of SS304L austenitic boiler steel
Mahajan, S., & Chhibber, R. (2020) · Sadhana · doi:10.1007/s12046-020-01416-z · Cited by 6
Martinez, F. D., Morar, N. I., Kothari, M., Gibson, G. J., Leggett, J., Mason-Flucke, J., Nicholls, J. R., Castelluccio, G. M., & Gray, S. (2020) · The minerals, metals & materials series · doi:10.1007/978-3-030-51834-9_73 · Cited by 7
Roshith, P., & Arivarasu, M. (2022) · Welding International · doi:10.1080/09507116.2022.2089608 · Cited by 7
Effect of service exposure on KCl corrosion attack of AISI 347H FG steel
Malede, Y. C., Dahl, K. V., Montgomery, M., Grumsen, F. B., & Hald, J. K. (2019) · Journal of Materials Science · doi:10.1007/s10853-019-03863-4 · Cited by 6
Zhu, M. F., Zeng, S., Sharif, A. A., Cao, B., Zhang, H., & Wang, M. (2020) · Materialwissenschaft und Werkstofftechnik · doi:10.1002/mawe.201900016 · Cited by 6
Pfrang-Stotz, G., Reichelt, J., Bergfeldt, B., & Seifert, H. (2007) · Environmental Engineering Science · doi:10.1089/ees.2007.0128 · Cited by 6
Fouling and corrosion of bed nozzles in a bubbling fluidized-bed power boiler
Prescott, R., Kish, J. R., & Singbeil, D. (2006) · Journal of Failure Analysis and Prevention · doi:10.1361/154770206x117531 · Cited by 6
Corrosion of High-Alloy Superheater Tubes in a Coastal Biomass Power Boiler
Kish, J. R., Reid, C., Singbeil, D., & Seguin, R. (2008) · CORROSION · doi:10.5006/1.3278479 · Cited by 6
Mechanisms of simultaneous oxidation-chloridation of austenitic stainless steels by NaCl in air
Kwon, J.-W., Lee, Y.-Y., & Lee, Y.-D. (2000) · Materials at High Temperatures · doi:10.1179/mht.2000.17.2.021 · Cited by 6
Effect of High-Temperature Corrosion on the Service Life of P91 Piping in Biomass Co-firing
O’Hagan, C. P., Barrett, R. A., Leen, S. B., & Monaghan, R. F. D. (2016) · Journal of Pressure Vessel Technology · doi:10.1115/1.4032648 · Cited by 6
“The released chlorine is also now free to restart the cycle or is itself converted to HCl in the high moisture flue gas [22] (R5).”
BackgroundSsenteza, V., Jonsson, T., Nockert, J., & Liske, J. (2024) · High Temperature Corrosion of Materials · doi:10.1007/s11085-024-10265-8 · Cited by 5
Hu, Q., Geng, S., Niu, X., Wang, J., Huang, Y., & Wang, F. (2025) · Corrosion Science · doi:10.1016/j.corsci.2025.113000 · Cited by 7
Chen, Z., Dong, A., Zhang, Z., & Pan, Y. (2025) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2025.185387 · Cited by 6
Prediction of biomass corrosiveness over different coatings in fluidized bed combustion
Contreras, M. L., Benito, M., & Bahillo, A. (2022) · International journal of energy and environmental engineering · doi:10.1007/s40095-022-00544-y · Cited by 7
“[47] gave the basis for understanding this mechanism.”
BackgroundVerma, R., Kaushal, G., & Bala, N. (2023) · Journal of Thermal Spray Technology · doi:10.1007/s11666-023-01569-3 · Cited by 6
Corrosion Behavior of 45 Steel in Molten Nitrate Salts with 3wt% Impurities at 773.15K
Hu, Y., Han, Y., Qin, Y., & Zhou, H. (2018) · IOP Conference Series Materials Science and Engineering · doi:10.1088/1757-899x/394/3/032117 · Cited by 5
Verma, R., & Kaushal, G. (2022) · Journal of Thermal Spray Technology · doi:10.1007/s11666-022-01445-6 · Cited by 6
Sosnowska, M., Dudyński, M., Kardaś, D., Klein, M., & Kwiatkowski, K. (2015) · Fuel Processing Technology · doi:10.1016/j.fuproc.2015.08.014 · Cited by 5
The potential of SO2 for reducing corrosion in WtE plants
Hunsinger, H., & Andersson, S. (2014) · Journal of Material Cycles and Waste Management · doi:10.1007/s10163-014-0271-9 · Cited by 6
Izzuddin, H., Hayashi, S., Yoneda, S., Kogin, T., Ishikawa, E., & Noguchi, M. (2020) · MATERIALS TRANSACTIONS · doi:10.2320/matertrans.mt-m2020156 · Cited by 5
Środa, S., Baxter, D. J., & Arponen, M. (2005) · Materials and Corrosion · doi:10.1002/maco.200503880 · Cited by 5
Lichti, K. A., Levi, T. P., Swann, S. J., Ferguson, S. L., & McIlhone, P. G. H. (1999) · Materials at High Temperatures · doi:10.1179/mht.1999.010 · Cited by 5
Pu, J., Su, X., Zhang, X., Liu, X., Ma, D., Hu, Z., Dai, G., & Wang, X. (2026) · Fuel · doi:10.1016/j.fuel.2026.139118 · Cited by 4
Chlorine-Induced Stress Corrosion Cracking of Single Crystal Superalloys at 550 °C
Martinez, F. D., Dawson, K., Tatlock, G. J., Leggett, J., Gibson, G. J., Mason-Flucke, J., Nicholls, J. R., Syed, A. U., Morar, N. I., & Gray, S. (2024) · High Temperature Corrosion of Materials · doi:10.1007/s11085-024-10282-7 · Cited by 4
Chen, S., Zhao, W.-C., Fan, Y., Wang, X., Guan, X., Guo, Z., Yan, Y., Zhang, Z., & Li, L. (2024) · Engineering Failure Analysis · doi:10.1016/j.engfailanal.2024.109204 · Cited by 5
Jiang, Y., Li, S., Huang, D., Bao, Z., Wang, J., Zhu, S., & Wang, F. (2025) · Journal of Material Science and Technology · doi:10.1016/j.jmst.2025.01.077 · Cited by 4
Zhang, S., He, J., Wang, D., Wang, Y., & Duan, L. (2025) · Chemical Engineering Science · doi:10.1016/j.ces.2025.122231 · Cited by 6
Fouling as a Result of Corrosion
Speight, J. G. (2015) · Elsevier eBooks · doi:10.1016/b978-0-12-800777-8.00017-6 · Cited by 4
Pan, T. J., Y.F. Lin, Hu, J., & Zeng, C. (2009) · High Temperature Materials and Processes · doi:10.1515/htmp.2009.28.4.233 · Cited by 4
Brossard, J.-M., Maad, F., Chartier, J., Chavrot, R., & Kawahara, Y. (2017) · Oxidation of Metals · doi:10.1007/s11085-017-9767-8 · Cited by 4
Corrosion behavior of NO6600 alloy in molten chloride salts
Hu, Y., Qin, Y., & Zhou, H. (2018) · IOP Conference Series Materials Science and Engineering · doi:10.1088/1757-899x/394/3/032125 · Cited by 4
Metadata
- Authors
- Grabke, H. J., Reese, E., & Spiegel, M.
- Affiliations
- Max Planck Society (DE)
- Max-Planck-Institut für Nachhaltige Materialien (DE)
- Venue
- Corrosion Science
- Publisher
- Elsevier BV
- Published
- 1995-07
- Volume
- 37
- Issue
- 7
- Pages
- 1023-1043
- ISSN
- 0010-938X (ISSN-L)
- OpenAlex
- W2009404226
- Semantic Scholar
- 05bb362b695843876fd8e1b7dd9b4098b1046c52
- Cited by
- 537
- References
- 18
- Citations by year
- 2026: 25 · 2025: 32 · 2024: 36 · 2023: 24 · 2022: 24 · 2021: 28 · 2020: 28 · 2019: 41 · 2018: 29 · 2017: 26 · 2016: 28 · 2015: 26 · 2014: 26 · 2013: 14 · 2012: 15
- FWCI
- 4.71
- Type
- journal article
- Language
- en
- Open access
- closed
- Licence
- www.elsevier.com/tdm/userlicense/1.0/ (tdm)
- Locations
- Corrosion Science (publishedVersion)
- Max Planck Institute for Plasma Physics (submittedVersion)
- Topics
- Physical Sciences › Materials Science › Surfaces, Coatings and Films › High-Temperature Coating Behaviors
- Physical Sciences › Materials Science › Materials Chemistry › Corrosion Behavior and Inhibition
- Physical Sciences › Energy › Fuel Technology › Chemical Looping and Thermochemical Processes
- Keywords
- steel oxidation, active oxidation, scale deposits, chloride, hydrogen chloride, sulfur dioxide, fly ash deposits, sodium chloride, low-alloy steel, high-alloy steels, iron(II) chloride, rate-determining step, scale/metal interface, thermogravimetric analysis
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.