Lithium Plating Mechanism, Detection, and Mitigation in Lithium-Ion Batteries
Integrity signals
Registry
Cites
Statistics
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
It is possible to avoid Li plating by selecting anodes with higher potential than graphite such as metal oxides or alloy anodes.
“It is possible to avoid Li plating by selecting anodes with higher potential than graphite such as metal oxides or alloy anodes [170].”
From Review on Low-Temperature Electrolytes for Lithium-Ion and Lithium Metal Batteries (2023) · cites this paper as [170]
Cites
Modeling of Galvanostatic Charge and Discharge of the Lithium/Polymer/Insertion Cell
Doyle, M., Fuller, T. F., & Newman, J. (1993) · Journal of The Electrochemical Society · doi:10.1149/1.2221597 · Cited by 4,328 · cited 3× · see citing works
“Newman [204] and co-workers introduced the first battery physics-based model.”
BackgroundMethodInfluentialAgeing mechanisms in lithium-ion batteries
Vetter, J., Novák, P., Wagner, M. R., Veit, C., Möller, K.-C., Besenhard, J. O., Winter, M., Wohlfahrt-Mehrens, M., Vogler, C., & Hammouche, A. (2005) · Journal of Power Sources · doi:10.1016/j.jpowsour.2005.01.006 · Cited by 3,987 · see citing works
Degradation diagnostics for lithium ion cells
Birkl, C. R., Roberts, M. R., McTurk, E., Bruce, P. G., & Howey, D. A. (2017) · Journal of Power Sources · doi:10.1016/j.jpowsour.2016.12.011 · Cited by 1,945 · cited 3× · see citing works
“Furthermore, the active mass of the cathode is reduced due to transition metal dissolution, structural disordering, and electrode particle cracking [27, 34,36,37].”
BackgroundJaguemont, J., Boulon, L., & Dubé, Y. (2016) · Applied Energy · doi:10.1016/j.apenergy.2015.11.034 · Cited by 1,188 · see citing works
Synthesize battery degradation modes via a diagnostic and prognostic model
Dubarry, M., Truchot, C., & Liaw, B. Y. (2012) · Journal of Power Sources · doi:10.1016/j.jpowsour.2012.07.016 · Cited by 1,065 · see citing works
Han, X., Ouyang, M., Lu, L., Li, J., Zheng, Y., & Li, Z. (2014) · Journal of Power Sources · doi:10.1016/j.jpowsour.2013.11.029 · Cited by 822 · cited 11× · see citing works
“As mentioned earlier, the most common modes of degradation in the literature are LLI and LAM, where LAM can be further divided into four types based on the affected electrode and the degree of lithiation: loss of active material on the delithiated negative electrode (LAMdeNE), loss of active material on the delithiate…”
BackgroundInfluentialSelf-citationArora, P., Doyle, M., & White, R. E. (1999) · Journal of The Electrochemical Society · doi:10.1149/1.1392512 · Cited by 586 · cited 25× · see citing works
“In order to control these parameters, the internal states of LiBs are needed (Fig.”
BackgroundInfluentialFactors Limiting Li<sup>+</sup>Charge Transfer Kinetics in Li-Ion Batteries
Jow, T. R., Delp, S. A., Allen, J. L., Jones, J.-P., & Smart, M. C. (2018) · Journal of The Electrochemical Society · doi:10.1149/2.1221802jes · Cited by 437 · see citing works
Kim, N., Chae, S., Ma, J., Ko, M., & Cho, J. (2017) · Nature Communications · doi:10.1038/s41467-017-00973-y · Cited by 434 · cited 3× · see citing works
“A hybrid anode was developed which consists of an edge-plane activated graphite and Si nanolayer (SEAG), where the activated edge-plane increases the site reaction [217].”
BackgroundMethodInfluentialStudies on Charging Lithium-Ion Cells at Low Temperatures
Fan, J., & Tan, S. (2006) · Journal of The Electrochemical Society · doi:10.1149/1.2190029 · Cited by 211 · cited 1× · see citing works
“This process affects the voltage plateau signal due to variations in the overall potential of the anode electrode during relaxation and discharging after a charging step [48,59,152].”
BackgroundEcker, M., Shafiei Sabet, P., & Sauer, D. U. (2017) · Applied Energy · doi:10.1016/j.apenergy.2017.08.034 · Cited by 181 · see citing works
Flagged first, then by citations
Cited by
Sorted by citations
Health prognostics for lithium-ion batteries: mechanisms, methods, and prospects
Che, Y., Hu, X., Lin, X., Guo, J., & Teodorescu, R. (2023) · Energy & Environmental Science · doi:10.1039/d2ee03019e · Cited by 421 · see citing works
Self-citationThermal state monitoring of lithium-ion batteries: Progress, challenges, and opportunities
Zheng, Y.-S., Che, Y., Hu, X.-S., Sui, X., Stroe, D., & Teodorescu, R. (2023) · Progress in Energy and Combustion Science · doi:10.1016/j.pecs.2023.101120 · Cited by 258 · see citing works
Self-citationWang, Y.-J., Zhang, X.-C., & Chen, Z.-H. (2022) · Applied Energy · doi:10.1016/j.apenergy.2022.118832 · Cited by 256 · see citing works
Liao, Y., Zhang, H.-Y., Peng, Y.-F., Hu, Y., Liang, J.-D., Gong, Z., Wei, Y.-M., & Yang, Y. (2024) · Advanced Energy Materials · doi:10.1002/aenm.202304295 · Cited by 224 · see citing works
Elmahallawy, M., Elfouly, T., Alouani, A. T., & Massoud, A. M. (2022) · IEEE Access · doi:10.1109/access.2022.3221137 · Cited by 260 · see citing works
Battery Safety: Machine Learning-Based Prognostics
Zhao, J., Feng, X., Pang, Q., Fowler, M., Lian, Y., Ouyang, M., & Burke, A. F. (2024) · Progress in Energy and Combustion Science · doi:10.1016/j.pecs.2023.101142 · Cited by 216 · see citing works
Battery safety: Fault diagnosis from laboratory to real world
Zhao, J.-Y., Feng, X.-N., Tran, M.-K., Fowler, M., Ouyang, M., & Burke, A. F. (2024) · Journal of Power Sources · doi:10.1016/j.jpowsour.2024.234111 · Cited by 215 · see citing works
Challenges and recent progress in fast-charging lithium-ion battery materials
He, J., Meng, J., & Huang, Y. (2023) · Journal of Power Sources · doi:10.1016/j.jpowsour.2023.232965 · Cited by 167 · see citing works
Battery Degradation in Electric and Hybrid Electric Vehicles: A Survey Study
Timilsina, L., Badr, P. R., Hoang, P. H., Özkan, G., Papari, B., & Edrington, C. S. (2023) · IEEE Access · doi:10.1109/access.2023.3271287 · Cited by 201 · see citing works
Liu, K., Peng, Q., Che, Y., Zheng, Y., Li, K., Teodorescu, R., Widanage, W. D., & Barai, A. (2022) · Advances in Applied Energy · doi:10.1016/j.adapen.2022.100117 · Cited by 172 · see citing works
“Furthermore, charging batteries at low temperatures can trigger lithium plating, which renders accelerated battery degradation and can lead to inter short-circuit [ 9 , 63 ].”
BackgroundA review on thermal management of battery packs for electric vehicles
Maiorino, A., Cilenti, C., Petruzziello, F., & Aprea, C. (2024) · Applied Thermal Engineering · doi:10.1016/j.applthermaleng.2023.122035 · Cited by 147
Mama, M., Solai, E., Capurso, T., Danlos, A., & Khelladi, S. (2025) · Energy Conversion and Management · doi:10.1016/j.enconman.2024.119223 · Cited by 138 · see citing works
“This can lead to reduced capacity, altered SEI composition, volume expansion, and potentially hazardous dendrite formation leading to internal short circuits [57].”
Progress and challenges of prelithiation technology for lithium‐ion battery
Huang, Z.-Y., Deng, Z., Zhong, Y., Xu, M.-K., Li, S., Liu, X.-T., Zhou, Y., Huang, K., Shen, Y., & Huang, Y. (2022) · Carbon Energy · doi:10.1002/cey2.256 · Cited by 138 · see citing works
Advances on two-phase heat transfer for lithium-ion battery thermal management
Lin, X.-W., Li, Y.-B., Wu, W.-T., Zhou, Z.-F., & Chen, B. (2024) · Renewable & Sustainable Energy Reviews · doi:10.1016/j.rser.2023.114052 · Cited by 135 · see citing works
Self-citationXiong, R., Tian, J., Shen, W., Lu, J., & Sun, F. (2022) · Journal of Energy Chemistry · doi:10.1016/j.jechem.2022.09.045 · Cited by 148 · see citing works
Overview of multi-stage charging strategies for Li-ion batteries
Tahir, M. U., Sangwongwanich, A., Stroe, D., & Blaabjerg, F. (2023) · Journal of Energy Chemistry · doi:10.1016/j.jechem.2023.05.023 · Cited by 130 · see citing works
Review on Low-Temperature Electrolytes for Lithium-Ion and Lithium Metal Batteries
Tan, S., Shadike, Z., Cai, X., Lin, R., Kludze, A., Borodin, O., Lucht, B. L., Wang, C., Hu, E., Xu, K., et al. (2023) · Electrochemical Energy Reviews · doi:10.1007/s41918-023-00199-1 · Cited by 118 · see citing works
Xiao, H., Jiaqiang, E., Tian, S., Huang, Y., & Song, X. (2024) · Energy · doi:10.1016/j.energy.2024.131093 · Cited by 124 · see citing works
Wang, Y.-Y., Lai, X., Chen, Q.-W., Han, X.-B., Lu, L.-G., Ouyang, M.-G., & Zheng, Y.-J. (2024) · Energy Storage Materials · doi:10.1016/j.ensm.2024.103430 · Cited by 109 · see citing works
Liu, X.-H., Zhang, L., Yu, H.-Q., Wang, J., Li, J.-F., Yang, K., Zhao, Y.-L., Wang, H.-Z., Wu, B., Brandon, N., et al. (2022) · Advanced Energy Materials · doi:10.1002/aenm.202200889 · Cited by 104 · see citing works
Self-citationDu, X.-H., Meng, J.-H., Amirat, Y., Gao, F., & Benbouzid, M. (2024) · Journal of Energy Chemistry · doi:10.1016/j.jechem.2024.04.005 · Cited by 101 · see citing works
Peng, Y.-F., Ding, M.-F., Zhang, K., Zhang, H.-Y., Hu, Y., Lin, Y., Hu, W.-X., Liao, Y., Tang, S.-J., Liang, J.-D., et al. (2024) · ACS Energy Letters · doi:10.1021/acsenergylett.4c02898 · Cited by 95
A review of improvements on electric vehicle battery
Koech, A. K., Mwandila, G., & Mulolani, F. (2024) · Heliyon · doi:10.1016/j.heliyon.2024.e34806 · Cited by 101 · see citing works
“Charging batteries at low temperatures is associated with the occurrence of Li plating due to the slow Li-ion transit in the electrolyte, resulting in substantial overpotential at relatively low currents [43,197].”
BackgroundLi, A. G., West, A. C., & Preindl, M. (2022) · Applied Energy · doi:10.1016/j.apenergy.2022.119030 · Cited by 93 · see citing works
Aging behavior and mechanisms of lithium-ion battery under multi-aging path
Liu, J., Zhou, L., Zhang, Y., Wang, J., & Wang, Z. (2023) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2023.138678 · Cited by 87 · see citing works
Ding, S., Li, Y., Dai, H., Wang, L., & He, X. (2023) · Advanced Energy Materials · doi:10.1002/aenm.202301452 · Cited by 67 · see citing works
In Situ/Operando Imaging Techniques for Next-Generation Battery Analysis
Cho, B.-K., Jung, S.-Y., Park, S.-J., Hyun, J., & Yu, S.-H. (2024) · ACS Energy Letters · doi:10.1021/acsenergylett.4c01098 · Cited by 79 · see citing works
Lin, Y., Hu, W.-X., Ding, M.-F., Hu, Y., Peng, Y.-F., Liang, J.-D., Wei, Y.-M., Fu, A., Lin, J., & Yang, Y. (2024) · Advanced Energy Materials · doi:10.1002/aenm.202400894 · Cited by 76 · see citing works
Electric Vehicle Batteries: Status and Perspectives of Data-Driven Diagnosis and Prognosis
Zhao, J., & Burke, A. F. (2022) · Batteries · doi:10.3390/batteries8100142 · Cited by 82 · see citing works
“The objectives would be to identify cells exhibiting abnormal behavior indicating self-discharge [58], internal short circuit [59], external short circuit [60] lithium plating [61], oxygen release of the charged electrodes [62] and expansion force [63] at the cell level, and inconsistency information at the pack level…”
BackgroundRahman, M. M., Nisar, U., Abouimrane, A., Belharouak, I., & Amin, R. (2025) · Electrochemical Energy Reviews · doi:10.1007/s41918-025-00249-w · Cited by 73 · see citing works
“The low lithiation potential of graphite makes it more prone to lithium plating under high current densities [151].”
Zhou, H., Fear, C., Carter, R. E., Love, C., & Mukherjee, P. P. (2024) · Energy Storage Materials · doi:10.1016/j.ensm.2024.103214 · Cited by 72 · see citing works
Li-ion battery degradation modes diagnosis via Convolutional Neural Networks
Costa, N., Sánchez, L., Anseán, D., & Dubarry, M. (2022) · Journal of Energy Storage · doi:10.1016/j.est.2022.105558 · Cited by 81 · see citing works
Yu, H., Zhang, H., Zhang, Z., & Yang, S. (2025) · eTransportation · doi:10.1016/j.etran.2025.100420 · Cited by 73 · see citing works
Townsend, A. K., & Gouws, R. (2022) · Energies · doi:10.3390/en15134930 · Cited by 87 · see citing works
Advances in thermal management systems for Li-Ion batteries: A review
Amer, M. M., Shouman, M. A., Salem, M. S., Kannan, A. M., & Hamed, A. M. (2024) · Thermal Science and Engineering Progress · doi:10.1016/j.tsep.2024.102714 · Cited by 68 · see citing works
Lithium-ion battery lifetime extension: A review of derating methods
Ruan, H., Barreras, J., Engstrom, T., Merla, Y., Millar, R., & Wu, B. (2023) · Journal of Power Sources · doi:10.1016/j.jpowsour.2023.232805 · Cited by 67 · see citing works
Influence of lithium plating on lithium-ion battery aging at high temperature
Liu, J.-L., Zhang, Y., Bai, J.-L., Zhou, L.-F., & Wang, Z.-R. (2023) · Electrochimica Acta · doi:10.1016/j.electacta.2023.142362 · Cited by 66 · see citing works
Han, X.-B., Mao, S.-Y., Wang, Y., Lu, Y., Wang, D.-P., Sun, Y.-K., Zheng, Y.-J., Feng, X.-N., Lu, L.-G., Hua, J.-F., et al. (2025) · Nature Communications · doi:10.1038/s41467-025-58818-y · Cited by 65 · see citing works
“…dendritic morphology, and low-rate stripping helps to avoid dendrite fracture, both methods are anticipated to result in higher capacity retention 28,29 , we set up control groups for low-rate plating and low-rate stripping, without resting and with a total time increment of 10 hours, to…”
Battery impedance spectrum prediction from partial charging voltage curve by machine learning
Guo, J., Che, Y., Pedersen, K., & Stroe, D. (2023) · Journal of Energy Chemistry · doi:10.1016/j.jechem.2023.01.004 · Cited by 64 · see citing works
Tian, Y., Lin, C., Chen, X., Yu, X., Xiong, R., & Zhang, Q. (2023) · Social Science Research Network · doi:10.2139/ssrn.4310538 · Cited by 63
Operando visualisation of lithium plating by ultrasound imaging of battery cells
Wasylowski, D., Ditler, H., Sonnet, M., Falkenstein, T., Leogrande, L., Ronge, E., Blömeke, A., Würsig, A., Ringbeck, F., & Sauer, D. (2024) · Nature Communications · doi:10.1038/s41467-024-54319-6 · Cited by 61
Extremely Fast-Charging Batteries: Principle, Strategies, Detection, and Prediction.
Liu, H., Zhao, L.-Y., Ye, Y., Yang, X.-T., Zhang, Y., Li, Q., Li, R.-X., Liu, H., Huang, B., Wu, F., et al. (2025) · Chemical Reviews · doi:10.1021/acs.chemrev.5c00203 · Cited by 57 · see citing works
Nondestructive Analysis of Commercial Batteries.
Zuo, W.-H., Liu, R., Cai, J.-Y., Hu, Y., Almazrouei, M., Liu, X., Cui, T., Jia, X., Apodaca, E., Alami, J., et al. (2024) · Chemical Reviews · doi:10.1021/acs.chemrev.4c00566 · Cited by 56 · see citing works
Zhao, J., Han, X., Wu, Y., Wang, Z., & Burke, A. F. (2024) · Journal of Energy Chemistry · doi:10.1016/j.jechem.2024.11.011 · Cited by 62 · see citing works
Duan, X., Li, B., Li, J.-N., Gao, X., Wang, L.-B., & Xu, J. (2023) · Advanced Energy Materials · doi:10.1002/aenm.202203767 · Cited by 55 · see citing works
Self-citationAssessment of the calendar aging of lithium-ion batteries for a long-term—Space missions
Ali, H., Beltran, H., Lindsey, N., & Pecht, M. G. (2023) · Frontiers in Energy Research · doi:10.3389/fenrg.2023.1108269 · Cited by 53 · see citing works
“In addition, lithium plating is also significantly affected by the electrolyte composition (Lin et al., 2021).”
BackgroundInsight Understanding of External Pressure on Lithium Plating in Commercial Lithium‐Ion Batteries
Yu, H.-Q., Wang, L., Zhang, Z., Li, Y., Yang, S., & He, X.-M. (2024) · Advanced Functional Materials · doi:10.1002/adfm.202406966 · Cited by 52 · see citing works
Polat, H., Hosseinabadi, F., Hasan, M. M., Chakraborty, S., Geury, T., Baghdadi, M. E., Wilkins, S., & Hegazy, O. (2023) · Batteries · doi:10.3390/batteries9020121 · Cited by 54 · see citing works
Electrode and Electrolyte Design Strategies Toward Fast‐Charging Lithium‐Ion Batteries
Li, J.-W., Guo, C.-Y., Tao, L.-J., Meng, J.-S., Xu, X.-M., Liu, F., & Wang, X.-P. (2024) · Advanced Functional Materials · doi:10.1002/adfm.202409097 · Cited by 51
Self-citationZhou, H., Alujjage, A. S. J., Terese, M., Fear, C., Joshi, T., Rikka, V., Jeevarajan, J., & Mukherjee, P. P. (2025) · Applied Energy · doi:10.1016/j.apenergy.2024.124465 · Cited by 50 · see citing works
Ding, S., Wang, L., Dai, H.-F., & He, X.-M. (2024) · Energy Storage Materials · doi:10.1016/j.ensm.2024.103998 · Cited by 48 · see citing works
Lipu, M. S. H., Rahman, M. S. A., Islam, Z. U., Rahman, T., Rahman, M. S., Meraj, S. T., Hossain, M. S. B., & Mansor, M. (2025) · Journal of Energy Storage · doi:10.1016/j.est.2025.116629 · Cited by 41 · see citing works
Effect of the Formation Rate on the Stability of Anode-Free Lithium Metal Batteries
Kim, S., Didwal, P. N., Fiates, J., Dawson, J. A., Weatherup, R., & Volder, M. D. D. (2024) · ACS Energy Letters · doi:10.1021/acsenergylett.4c02258 · Cited by 47
Localized lithium plating under mild cycling conditions in high-energy lithium-ion batteries
Smith, A. J., Fang, Y., Mikheenkova, A., Ekström, H., Svens, P., Ahmed, I., Lacey, M., Lindbergh, G., Furó, I., & Lindström, R. (2023) · Journal of Power Sources · doi:10.1016/j.jpowsour.2023.233118 · Cited by 46 · see citing works
Smart Battery Technology for Lifetime Improvement
Teodorescu, R., Sui, X., Vilsen, S. B., Bharadwaj, P., Kulkarni, A., & Stroe, D. (2022) · Batteries · doi:10.3390/batteries8100169 · Cited by 45 · see citing works
“Moreover, noise suppression methods were used to pre-process the SOH data, improving not just the accuracy but also the speed of the fuzzy entropy-based feature extraction [32,33].”
MethodEarly warning of lithium-ion battery thermal runaway based on gas sensors
Song, Y., Jiang, X., Lyu, N., Lu, H., Zhang, D., Li, H., & Jin, Y. (2025) · eTransportation · doi:10.1016/j.etran.2025.100502 · Cited by 42 · see citing works
Michelini, E., Höschele, P., Heindl, S. F., Erker, S., & Ellersdorfer, C. (2023) · Batteries · doi:10.3390/batteries9040218 · Cited by 43 · see citing works
Mei, W., Zhang, Y., Li, Y., Zhuo, P., Chu, Y., Chen, Y., Jiang, L.-H., Zhou, H., Sun, J.-H., & Wang, Q.-S. (2024) · Energy Storage Materials · doi:10.1016/j.ensm.2024.103193 · Cited by 42
Multi-factor aging in Lithium Iron phosphate batteries: Mechanisms and insights
Xiong, R., Wang, P., Jia, Y.-B., Shen, W.-X., & Sun, F.-C. (2025) · Applied Energy · doi:10.1016/j.apenergy.2024.125250 · Cited by 41 · see citing works
Monitoring and control of internal temperature in power batteries: A comprehensive review
Guo, X., Yang, Y., Shi, C., Xu, M., Liu, Y., & Zou, D. (2025) · Energy storage materials · doi:10.1016/j.ensm.2025.104051 · Cited by 28 · see citing works
Methods for Quantifying Expansion in Lithium-Ion Battery Cells Resulting from Cycling: A Review
Krause, T., Nusko, D., Bauermann, L. P., Vetter, M., Schäfer, M., & Holly, C. (2024) · Energies · doi:10.3390/en17071566 · Cited by 41 · see citing works
Thermal safety focus and early warning of lithium-ion batteries: A systematic review
Liu, Z., Han, K., Zhang, Q., & Li, M. (2025) · Journal of Energy Storage · doi:10.1016/j.est.2025.115944 · Cited by 43 · see citing works
Aging mechanisms of NMC811/Si-Graphite Li-ion batteries
Laakso, E., Efimova, S., Colalongo, M., Kauranen, P., Lahtinen, K., Napolitano, E., Ruiz, V., Moškon, J., Gaberšček, M., Park, J., et al. (2024) · Journal of Power Sources · doi:10.1016/j.jpowsour.2024.234159 · Cited by 40 · see citing works
“Lithium plating causes capacity loss, impedance rise, and serious safety hazards due to dendrite upgrowth which can cause short circuit in the battery [26].”
BackgroundYang, L.-Y., Cao, J., Liang, W.-H., Wang, Y.-K., & Wu, D.-Y. (2022) · ACS Applied Materials and Interfaces · doi:10.1021/acsami.2c00390 · Cited by 40
State-of-the-art review of degradation mechanisms of commercial lithium-ion batteries
Jeon, D. H., Kim, S., & Hempelmann, R. (2025) · Journal of Power Sources · doi:10.1016/j.jpowsour.2025.237242 · Cited by 39 · see citing works
Multi-objective optimization for multi-stage constant current charging for Li-ion batteries
Tahir, M. U., Sangwongwanich, A., Stroe, D., & Blaabjerg, F. (2024) · Journal of Energy Storage · doi:10.1016/j.est.2024.111313 · Cited by 39
Composition and Explosibility of Gas Emissions from Lithium-Ion Batteries Undergoing Thermal Runaway
Amano, K. A., Hahn, S.-K., Butt, N., Vorwerk, P., Gimadieva, E., Tschirschwitz, R., Rappsilber, T., & Krause, U. (2023) · Batteries · doi:10.3390/batteries9060300 · Cited by 39
“al, lithium plating forms lithium dendrite, which penetrates the separator and causes an internal short circuit [37].”
BackgroundZhang, G.-X., Wei, X.-Z., Wang, X.-Y., Chen, S., Zhu, J.-G., & Dai, H.-F. (2024) · Nano Energy · doi:10.1016/j.nanoen.2024.109621 · Cited by 37 · see citing works
Revealing how internal sensors in a smart battery impact the local graphite lithiation mechanism
Olgo, A., Genies, S., Franchi, R., Septet, C., Jacquet, Q., Berrod, Q., Palm, R., Chenevier, P., Villemin, E., Villevieille, C., et al. (2024) · Nature Communications · doi:10.1038/s41467-024-54656-6 · Cited by 36
“For instance, Li-plating occurs on the graphite electrode at high current rates and/or low temperatures 21,22 , leading to increased internal temperature, gas evolution, and fi nally, thermal runaway 17,23 .”
Vashisht, S., Rajat, & Rakshit, D. (2024) · eTransportation · doi:10.1016/j.etran.2024.100381 · Cited by 34 · see citing works
Challenges and Issues Facing Ultrafast-Charging Lithium-Ion Batteries
Mehrizi, A. A., Yeganehdoust, F., Reddy, A. K. M. R., & Zaghib, K. (2025) · Batteries · doi:10.3390/batteries11060209 · Cited by 35 · see citing works
Zhu, G., Chen, J., Liu, X., Sun, T., Lai, X., Zheng, Y., Guo, Y., & Bhagat, R. (2024) · Green Energy and Intelligent Transportation · doi:10.1016/j.geits.2024.100167 · Cited by 35 · see citing works
Han, U., Jun, Y., Choi, H., & Lee, H. (2023) · International Communications in Heat and Mass Transfer · doi:10.1016/j.icheatmasstransfer.2023.107128 · Cited by 35 · see citing works
Lin, C.-P., Xu, J., Hou, J.-Y., Jiang, D., Liang, Y., Zhang, X.-G., Li, E., & Mei, X.-S. (2023) · Energy Storage Materials · doi:10.1016/j.ensm.2023.102967 · Cited by 35 · see citing works
Arif, N., Mekhilef, S., Seyedmahmoudian, M., & Stojcevski, A. (2026) · Journal of Energy Storage · doi:10.1016/j.est.2026.121270 · Cited by 34 · see citing works
Miao, J.-H. (2023) · Electrochem · doi:10.3390/electrochem4020013 · Cited by 34
“However, electrode polarization is increased at high charge rate due to relatively slow intercalation or electrode reaction, and results in larger overpotentials, making the anode (graphite in most cases) more prone to Li plating in parallel with intercalation [83].”
BackgroundQu, J., Xie, Z., Bicket, I., Yuan, H., Zuin, L., Andelic, M., Qu, W., Botton, G., & Liu, H.-S. (2025) · ACS Nano · doi:10.1021/acsnano.5c07347 · Cited by 33
Zhang, D., Wang, Z., Liu, P., She, C., Wang, Q., Zhou, L., & Qin, Z. (2024) · Energy · doi:10.1016/j.energy.2024.130773 · Cited by 25 · see citing works
Graphene nanonetwork embedded with polyaniline nanoparticles as anode of Li-ion battery
Fu, H.-Y., Gao, B., Qiao, Y., Zhu, W.-H., Liu, Z., Wei, G., Feng, Z., & Kamali, A. R. (2023) · Chemical Engineering Journal · doi:10.1016/j.cej.2023.146936 · Cited by 32 · see citing works
Jordan, S. M., Schreiber, C., Parhizi, M., & Shah, K. (2024) · Applied Energy · doi:10.1016/j.apenergy.2024.122746 · Cited by 30 · see citing works
“Additionally, battery efficiency also reduces at low temperatures due to sluggish electrolyte transport and slower reaction kinetics, increasing overall cell resistance [3].”
BackgroundZhu, C., Sun, L., Chen, C., Tian, J., Shen, W., & Xiong, R. (2023) · Electrochimica Acta · doi:10.1016/j.electacta.2023.142588 · Cited by 30 · see citing works
Khot, M., Shaik, R. S., Touseef, W., & Kiani, A. (2023) · Scientific Reports · doi:10.1038/s41598-023-34274-w · Cited by 29 · see citing works
Insights into the Enhanced Reversibility of Graphite Anode Upon Fast Charging Through Li Reservoir.
Qian, J., Zhu, T.-Y., Huang, D., Liu, G., & Tong, W. (2022) · ACS Nano · doi:10.1021/acsnano.2c05428 · Cited by 29
Liu, W., Hu, X.-S., Lin, X.-K., Yang, X.-G., Song, Z., Foley, A., & Couture, J. (2022) · eTransportation · doi:10.1016/j.etran.2022.100195 · Cited by 29 · see citing works
Self-citationStudy on Lithium-Ion Battery Degradation Caused by Side Reactions in Fast-Charging Process
Gao, Z.-H., Xie, H.-C., Yu, H.-Q., Ma, B., Liu, X.-H., & Chen, S.-Y. (2022) · Frontiers in Energy Research · doi:10.3389/fenrg.2022.905710 · Cited by 29 · see citing works
Sharma, A. (2023) · International Journal of Production Research · doi:10.1080/00207543.2023.2180308 · Cited by 28 · see citing works
“Similarly, charging a battery back in cold temperatures (below 32 ◦ F) can cause lithium plating, which is the deposition of metallic lithium on anode (Lin et al. 2021).”
BackgroundJohn, J., Kudva, G., & Jayalakshmi, N. S. (2024) · IEEE Access · doi:10.1109/access.2024.3396164 · Cited by 28 · see citing works
“2) LITHIUM PLATING [37], [38] Lithium plating is the phenomenon where lithium instead of intercalating into the anode crystal gets deposited on the anode surface.”
BackgroundPradhan, A., Badam, R., Miyairi, R., Takamori, N., & Matsumi, N. (2023) · ACS Materials Letters · doi:10.1021/acsmaterialslett.2c00999 · Cited by 27
Kumar, K., Rithvik, G., Mittal, G., Arya, R., Sharma, T. K., & Pareek, K. (2024) · Journal of Energy Storage · doi:10.1016/j.est.2024.112580 · Cited by 27 · see citing works
Swelling Mechanisms, Diagnostic Applications, and Mitigation Strategies in Lithium-Ion Batteries
Maddipatla, S., Rauf, H., Osterman, M., Arshad, N., & Pecht, M. G. (2025) · Batteries · doi:10.3390/batteries11100356 · Cited by 26 · see citing works
LiF-Rich Solid Electrolyte Interphase Formation by Establishing Sacrificial Layer on the Separator.
Jin, H.-D., Pyo, S., Seo, H., Cho, J., Han, J., Han, J., Yun, H., Kim, H., Lee, J., Min, B., et al. (2024) · Small · doi:10.1002/smll.202401928 · Cited by 26
Sun, K., Li, X., Zhang, Z.-J., Xiao, X., Gong, L.-L., & Tan, P. (2023) · ACS Applied Materials and Interfaces · doi:10.1021/acsami.3c07098 · Cited by 26 · see citing works
Tian, Y., Lin, C., Li, H., Du, J.-Y., & Xiong, R. (2022) · EcoMat · doi:10.1002/eom2.12280 · Cited by 26 · see citing works
Xu, H., Zhang, G., Zhang, J.-T., Zhang, J.-Y., Wu, H.-W., Jiang, L.-Q., Jiang, W.-Z., Liu, J., & Peng, K. (2025) · International Journal of Electrochemical Science · doi:10.1016/j.ijoes.2025.101027 · Cited by 25
“When the internal stress within the anode active material exceeds its mechanical stability limit, it causes structural breakage, agglomeration, and material shedding [46]. sodium clusters form, followed by the deposition of sodium dendrites [47,48].”
Wan, Z., Pannala, S., Solbrig, C. E., Garrick, T. R., Stefanopoulou, A., & Siegel, J. B. (2025) · eTransportation · doi:10.1016/j.etran.2025.100416 · Cited by 25
Battery Prognostics and Health Management: AI and Big Data
Li, D., Nan, J.-R., Burke, A. F., & Zhao, J.-Y. (2024) · World Electric Vehicle Journal · doi:10.3390/wevj16010010 · Cited by 25 · see citing works
“Recent advancements have refined these models to include intricate phenomena, such as the evolution of interfacial layers [70], metallic deposition [71], material degradation [72], and changes in resistance over time [73].”
Yang, Z.-Z., Charalambous, H., Trask, S., Montoya, A. T., Jansen, A., Wiaderek, K., & Bloom, I. (2022) · Journal of Power Sources · doi:10.1016/j.jpowsour.2022.232119 · Cited by 25
Understanding thermal and mechanical effects on lithium plating in lithium-ion batteries
Qiu, Y., Zhang, X.-X., Usubelli, C., Mayer, D., Linder, C., & Christensen, J. (2022) · Journal of Power Sources · doi:10.1016/j.jpowsour.2022.231632 · Cited by 25 · see citing works
“As lithium ions accumulate at the interface between the anode and the electrolyte due to poor transport, the surface concentration in the active material particles tends toward its maximum [22–24].”
BackgroundLiu, K.-L., Zhao, S., Wang, Y., Li, K., Wang, J., Sun, Y.-J., Wu, Q.-W., & Peng, Q. (2025) · Advances in Applied Energy · doi:10.1016/j.adapen.2025.100247 · Cited by 24 · see citing works
Yang, L.-Z., Liu, F., Li, F.-Z., Chen, Z., Wang, J., Gao, L., Xiao, F., Sun, J.-H., & Romagnoli, A. (2024) · Aerospace Traffic and Safety · doi:10.1016/j.aets.2024.12.005 · Cited by 24
- Authors
- Lin, X., Khosravinia, K., Hu, X., Li, J., & Lu, W.
- Affiliations
- Ontario Tech University (CA)
- Chongqing University (CN)
- Massachusetts Institute of Technology (US)
- University of Michigan (US)
- Corresponding author
- Lin, Xianke
- Hu, Xiaosong
- Venue
- Progress in Energy and Combustion Science
- Publisher
- Elsevier BV
- Published
- 2021-11
- Volume
- 87
- Pages
- 100953
- ISSN
- 0360-1285 (ISSN-L)
- OpenAlex
- W3188626832
- Cited by
- 490
- References
- 0
- Citations by year
- 2026: 122 · 2025: 155 · 2024: 108 · 2023: 72 · 2022: 31 · 2021: 2
- FWCI
- 17.29
- Type
- journal article
- Language
- en
- Open access
- closed
- Licence
- Locations
- Progress in Energy and Combustion Science (publishedVersion)
- Funders
- American Society of Mechanical Engineers
- NSERC (RGPIN-2018-05471)
- University of Ontario Institute of Technology
- National Science Foundation
- National Natural Science Foundation of China (51875054, U1864212)
- Topics
- Physical Sciences › Engineering › Automotive Engineering › Advanced Battery Technologies Research
- Physical Sciences › Engineering › Electrical and Electronic Engineering › Advancements in Battery Materials
- Physical Sciences › Engineering › Electrical and Electronic Engineering › Advanced Battery Materials and Technologies
- Keywords
- lithium plating, lithium-ion batteries, lithium dendrites, fast charging, low-temperature charging, graphite anode, battery degradation, internal short circuit, charging protocols
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review