Abstract
The growing demand for lithium-ion batteries will result in an increasing flow of spent batteries, which must be recycled to prevent environmental and health problems, while helping to mitigate the raw materials dependence and risks of shortage and promoting a circular economy. Combining pyrometallurgical and hydrometallurgical recycling approaches has been the focus of recent studies, since it can bring many advantages. In this work, the effects of incineration on the leaching efficiency of metals from EV LIBs were evaluated. The thermal process was applied as a pre-treatment for the electrode material, aiming for carbothermic reduction of the valuable metals by the graphite contained in the waste. Leaching efficiencies above 70% were obtained for Li, Mn, Ni and Co after 60 min of leaching even when using 0.5 M sulfuric acid, which can be linked to the formation of more easily leachable compounds during the incineration process. When the incineration temperature was increased (600-700 °C), the intensity of graphite signals decreased and other oxides were identified, possibly due to the increase in oxidative conditions. Higher leaching efficiencies of Mn, Ni, Co, and Li were reached at lower temperatures of incineration (400-500 °C) and at higher leaching times, which could be related to the partial carbothermic reduction of the metals.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
CRC Handbook of Chemistry and Physics
(2016) · CRC Press eBooks · doi:10.1201/9781315380476 · Cited by 13,921
Lithium-ion batteries. A look into the future
Scrosati, B., Hassoun, J., & Sun, Y.-K. (2011) · Energy & Environmental Science · doi:10.1039/c1ee01388b · Cited by 2,595 · cited 1×
“Nowadays, LIBs (lithium-ion batteries) are the technology of choice to power portable electronic devices and are also the most promising option to power electric vehicles (EV) and energy storage systems, due to characteristics including small volume, lightweight, high battery voltage, high energy density, long chargin…”
BackgroundLithium ion secondary batteries; past 10 years and the future
Nishi, Y. (2001) · Journal of Power Sources · doi:10.1016/s0378-7753(01)00887-4 · Cited by 1,074 · cited 2×
“Nowadays, LIBs (lithium-ion batteries) are the technology of choice to power portable electronic devices and are also the most promising option to power electric vehicles (EV) and energy storage systems, due to characteristics including small volume, lightweight, high battery voltage, high energy density, long chargin…”
BackgroundMeshram, P., Pandey, B. D., & Mankhand, T. R. (2014) · Hydrometallurgy · doi:10.1016/j.hydromet.2014.10.012 · Cited by 982 · cited 4×
“This could be related to an inefficient decomposition of LiPF6, which was suggested by Lombardo et al. (2020), based on the concentration of P in samples incinerated under the same conditions.”
BackgroundInfluentialRecycling of spent lithium-ion batteries in view of lithium recovery: A critical review
Liu, C., Lin, J., Cao, H., Zhang, Y., & Sun, Z. (2019) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2019.04.304 · Cited by 789 · cited 1×
“Vacuum pyrolysis is also combined with carbothermic reduction to enhance lithium recycling efficiency (Liu et al., 2019).”
BackgroundLithium-ion rechargeable batteries with LiCoO2 and carbon electrodes: the LiCoO2/C system
OZAWA, K. (1994) · Solid State Ionics · doi:10.1016/0167-2738(94)90411-1 · Cited by 776 · cited 3×
“Shin et al. (2005) observed a negative effect on the leaching efficiency of cobalt after incineration at 900 C, which was attributed to the surface of lithium cobalt oxide being covered with molten aluminum, hindering the leaching process.”
BackgroundThe Current Move of Lithium Ion Batteries Towards the Next Phase
Kim, T., Park, J., Chang, S. K., Choi, S., Ryu, J. H., & Song, H. (2012) · Advanced Energy Materials · doi:10.1002/aenm.201200028 · Cited by 742 · cited 1×
“Nowadays, LIBs (lithium-ion batteries) are the technology of choice to power portable electronic devices and are also the most promising option to power electric vehicles (EV) and energy storage systems, due to characteristics including small volume, lightweight, high battery voltage, high energy density, long chargin…”
BackgroundHigh-Performance Anode Materials for Rechargeable Lithium-Ion Batteries
Lu, J., Chen, Z., Pan, F., Cui, Y., & Amine, K. (2018) · Electrochemical Energy Reviews · doi:10.1007/s41918-018-0001-4 · Cited by 695
Li, J., Wang, G., & Xu, Z. (2016) · Journal of Hazardous Materials · doi:10.1016/j.jhazmat.2015.09.050 · Cited by 579 · cited 1×
“A detailed review of processes currently employed for recycling LIBs from mobility appliances was recently published by Mossali et al. (2020). Hydrometallurgy is considered a more suitable technology than pyrometallurgy from an environmental and health point of view.”
BackgroundMossali, E., Picone, N., Gentilini, L., Rodrìguez, O., Pérez, J. M., & Colledani, M. (2020) · Journal of Environmental Management · doi:10.1016/j.jenvman.2020.110500 · Cited by 574
Cited by
Recycling of spent lithium-ion batteries for a sustainable future: recent advancements
Biswal, B. K., Zhang, B., Thi Minh Tran, P., Zhang, J., & Balasubramanian, R. (2024) · Chemical Society Reviews · doi:10.1039/d3cs00898c · Cited by 436
Windisch-Kern, S., Gerold, E., Nigl, T., Jandric, A., Altendorfer, M., Rutrecht, B., Scherhaufer, S., Raupenstrauch, H., Pomberger, R., Antrekowitsch, H., et al. (2022) · Waste Management · doi:10.1016/j.wasman.2021.11.038 · Cited by 284
Recycling of cathode material from spent lithium-ion batteries: Challenges and future perspectives
Raj, T., Chandrasekhar, K., Kumar, A. N., Sharma, P., Pandey, A., Jang, M., Jeon, B.-H., Varjani, S., & Kim, S.-H. (2022) · Journal of Hazardous Materials · doi:10.1016/j.jhazmat.2022.128312 · Cited by 271
Yu, X., Yu, S., Yang, Z., Gao, H., Xu, P., Cai, G., Rose, S., Brooks, C., Liu, P., & Chen, Z. (2022) · Energy Storage Materials · doi:10.1016/j.ensm.2022.06.017 · Cited by 218
“well as increasing recovery efficiency [14].”
Preprocessing of spent lithium-ion batteries for recycling: Need, methods, and trends
Ali, H., Khan, H. A., & Pecht, M. (2022) · Renewable and Sustainable Energy Reviews · doi:10.1016/j.rser.2022.112809 · Cited by 202
Jiao, M., Zhang, Q., Ye, C., Liu, Z., Zhong, X., Wang, J., Li, C., Dai, L., Zhou, G., & Cheng, H.-M. (2022) · Proceedings of the National Academy of Sciences · doi:10.1073/pnas.2202202119 · Cited by 196
Roadmap for a sustainable circular economy in lithium-ion and future battery technologies
Harper, G. D. J., Kendrick, E., Anderson, P. A., Mrozik, W., Christensen, P., Lambert, S., Greenwood, D., Das, P. K., Ahmeid, M., Milojevic, Z., et al. (2023) · Journal of Physics: Energy · doi:10.1088/2515-7655/acaa57 · Cited by 137
Huang, J., Dong, X., Chen, J., & Zeng, A. (2023) · Resources Policy · doi:10.1016/j.resourpol.2023.103504 · Cited by 33
Sustainable Development Goals and End-of-Life Electric Vehicle Battery: Literature Review
Akram, M. N., & Abdul-Kader, W. (2023) · Batteries · doi:10.3390/batteries9070353 · Cited by 32
“2021 [99] This study focused on the recovery of cobalt from LIB leachate in hydroxide form.”
Background
Metadata
- Authors
- Vieceli, N., Casasola, R., Lombardo, G., Ebin, B., & Petranikova, M.
- Venue
- Waste Management
- Publisher
- Elsevier BV
- Published
- 2021-04
- Volume
- 125
- Pages
- 192-203
- ISSN
- 0956-053X (ISSN-L)
- OpenAlex
- W3133940810
- Cited by
- 161
- References
- 35
- FWCI
- 9.93
- Type
- journal article
- Language
- en
- Open access
- hybrid
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.