Printability and Shape Fidelity of Bioinks in 3D Bioprinting

Open access

Abstract

Three-dimensional bioprinting uses additive manufacturing techniques for the automated fabrication of hierarchically organized living constructs. The building blocks are often hydrogel-based bioinks, which need to be printed into structures with high shape fidelity to the intended computer-aided design. For optimal cell performance, relatively soft and printable inks are preferred, although these undergo significant deformation during the printing process, which may impair shape fidelity. While the concept of good or poor printability seems rather intuitive, its quantitative definition lacks consensus and depends on multiple rheological and chemical parameters of the ink. This review discusses qualitative and quantitative methodologies to evaluate printability of bioinks for extrusion- and lithography-based bioprinting. The physicochemical parameters influencing shape fidelity are discussed, together with their importance in establishing new models, predictive tools and printing methods that are deemed instrumental for the design of next-generation bioinks, and for reproducible comparison of their structural performance.

Overview

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Integrity signals

Registry

Crossref · 10.1021/acs.chemrev.0c00084

Cites

285 of 286 references verified0 citation errors · 0 not checkable

Statistics

Figures

Image 1
CC-BY-NC-ND · From the PDF
Image 2
CC-BY-NC-ND · From the PDF
Image 3
CC-BY-NC-ND · From the PDF
Figure 1 Terminology of cell-free and cell-containing hydrogel inks for bioprinting and the biofabrication window. (A) Distinction between bioinks (cell laden) and biomaterial inks (cell free). In bioinks (left side), single cells, coated cells, and cell aggregates are intrinsic components of the formulation in combination with microcarriers, embedded in microgels, in precursors or physical hydrogels. In biomaterial inks (right side), cells are introduced within the 3D printed biomaterial sca ff old, reducing the biological constraints on the inks. (A) Reproduced with permission from ref 20. Copyright 2018 IOP publishing under CC BY 3.0 (https://creativecommons.org/licenses/by/3.0/). (B) Schematic representation of the biofabrication window, illustrating the relation between shape fi delity and polymer concentration, cross-linking density, and sti ff ness. While sti ff materials generally result in high shape fi delity, indicators of biological performance, such as cell proliferation, migration, and di ff erentiation, are commonly reduced in such highly cross-linked hydrogels. The traditional biofabrication window is the result of a compromise between these opposing requirements. Novel approaches have been recently developed that expand the biofabrication window, enabling high shape fi delity even when printing low sti ff ness materials, enhancing biological competency. (B) Reproduced with permission from ref 21. Copyright 2013 John Wiley and Sons.
Figure 1 Terminology of cell-free and cell-containing hydrogel inks for bioprinting and the biofabrication window. (A) Distinction between bioinks (cell laden) and biomaterial inks (cell free). In bioinks (left side), single cells, coated cells, and cell aggregates are intrinsic components of the formulation in combination with microcarriers, embedded in microgels, in precursors or physical hydrogels. In biomaterial inks (right side), cells are introduced within the 3D printed biomaterial sca ff old, reducing the biological constraints on the inks. (A) Reproduced with permission from ref 20. Copyright 2018 IOP publishing under CC BY 3.0 (https://creativecommons.org/licenses/by/3.0/). (B) Schematic representation of the biofabrication window, illustrating the relation between shape fi delity and polymer concentration, cross-linking density, and sti ff ness. While sti ff materials generally result in high shape fi delity, indicators of biological performance, such as cell proliferation, migration, and di ff erentiation, are commonly reduced in such highly cross-linked hydrogels. The traditional biofabrication window is the result of a compromise between these opposing requirements. Novel approaches have been recently developed that expand the biofabrication window, enabling high shape fi delity even when printing low sti ff ness materials, enhancing biological competency. (B) Reproduced with permission from ref 21. Copyright 2013 John Wiley and Sons.CC-BY-NC-ND · From the PDF
Image 5
CC-BY-NC-ND · From the PDF
Figure 3 Rheological properties a ff ecting printability and shape fi delity. (A) Interplay of rheological properties in extrusion-based printing. (B) Amplitude sweep of a viscoelastic substance represented as a function of the shear stress, illustrating the yield point as the limit of the linear viscoelastic range, and the fl ow point, e.g., the stress at which the viscous modulus G ″ is above the elastic modulus G ′ and therefore fl ow can occur. (C) Elastic recovery test, where G ′ (blue) and G ″ (red) are measured under low deformation (white time interval) and high deformation (gray time interval). The curve represents the idealized behavior of a bioink for good printability and shape retention.
Figure 3 Rheological properties a ff ecting printability and shape fi delity. (A) Interplay of rheological properties in extrusion-based printing. (B) Amplitude sweep of a viscoelastic substance represented as a function of the shear stress, illustrating the yield point as the limit of the linear viscoelastic range, and the fl ow point, e.g., the stress at which the viscous modulus G ″ is above the elastic modulus G ′ and therefore fl ow can occur. (C) Elastic recovery test, where G ′ (blue) and G ″ (red) are measured under low deformation (white time interval) and high deformation (gray time interval). The curve represents the idealized behavior of a bioink for good printability and shape retention.CC-BY-NC-ND · From the PDF
Figure 4 Key aspects to assess printability in the context of extrusion- and lithography-based bioprinting technologies. While the principles (e.g., extrudability, fi lament characterization, rheological requirements) to assess the printability of a given bioink for extrusion-based bioprinting are di ff erent from those needed for lithographic bioprinting, the de fi nition and methods to assess shape fi delity remain comparable across these di ff erent bioprinting platforms.
Figure 4 Key aspects to assess printability in the context of extrusion- and lithography-based bioprinting technologies. While the principles (e.g., extrudability, fi lament characterization, rheological requirements) to assess the printability of a given bioink for extrusion-based bioprinting are di ff erent from those needed for lithographic bioprinting, the de fi nition and methods to assess shape fi delity remain comparable across these di ff erent bioprinting platforms.CC-BY-NC-ND · From the PDF
Figure 5 Schematic summarizing key aspects during bioink development and modi fi cation, including printability assessment. During hydrogel development for 3D bioprinting, a cell friendly gelation mechanism and biomaterial cytocompatibility need to be assessed. When cells, particles, or fi bers are embedded in the biomaterial, a homogeneous distribution before and after gelation is desirable to minimize sedimentation. Degradation and swelling behavior may have an in fl uence on geometrical accuracy. The second step covers the assessment of printability which di ff ers between printing technologies. The concept of printability assessment for extrusion printing includes rheological characterization, extrudability, and fi lament formation as well as shape fi delity. In lithographic printing, rheological requirements, shape fi delity is accompanied by optimization of photocuring depth and light penetration depth. After optimizing printing parameters to meet the printability requirements, the biological performance, including evaluating cell viability, cell proliferation, and cell di ff erentiation, is required. When the bioink is modi fi ed by means of composition, cross-linking mechanism, or photoinitiator, the whole work fl ow should be repeated to ensure a cell friendly environment and optimized conditions to achieve good printability.
Figure 5 Schematic summarizing key aspects during bioink development and modi fi cation, including printability assessment. During hydrogel development for 3D bioprinting, a cell friendly gelation mechanism and biomaterial cytocompatibility need to be assessed. When cells, particles, or fi bers are embedded in the biomaterial, a homogeneous distribution before and after gelation is desirable to minimize sedimentation. Degradation and swelling behavior may have an in fl uence on geometrical accuracy. The second step covers the assessment of printability which di ff ers between printing technologies. The concept of printability assessment for extrusion printing includes rheological characterization, extrudability, and fi lament formation as well as shape fi delity. In lithographic printing, rheological requirements, shape fi delity is accompanied by optimization of photocuring depth and light penetration depth. After optimizing printing parameters to meet the printability requirements, the biological performance, including evaluating cell viability, cell proliferation, and cell di ff erentiation, is required. When the bioink is modi fi ed by means of composition, cross-linking mechanism, or photoinitiator, the whole work fl ow should be repeated to ensure a cell friendly environment and optimized conditions to achieve good printability.CC-BY-NC-ND · From the PDF
Figure 6 Quantitative tests to assess the extrudability, fi lament formation, and shape fi delity of bioink prior to the printing process. (A) Rheological data can be acquired for a speci fi c ink, providing key information on properties necessary to extrude cohesive, stackable fi laments. (Ai) Yield stress measurements correlate with the fl ow initiation step, (Aii) whereas shear-thinning properties of a bioink permit facile extrusion. (Aiii) Depending on the extrusion pressure and the polymer viscosity, droplet, or fi lament formation can occur at the nozzle. (Aiv) Bioinks able to form fi laments and also show a rapid shear recovery after extrusion, can be used for printing and stacking multilayer constructs with improved shape fi delity. 144 (B) Uniformity of each extruded fi lament and thus its shape fi delity compared to the intended design (typically a cylindrical, smooth fi lament) can be assessed via image analysis and correlates with the ability of a viscoelastic bioink to absorb and disperse energy, as quanti fi ed by the loss tangent (tan ( δ )). Higher values of the loss tangent were shown to correlate with better fi lament uniformity. 162 (C) Printed fi laments can experience di ff erent deformations, given their limited mechanical properties, under the action of di ff erent forces, including gravity and surface tension. 78 (Ci) Printing a bioink fi lament on top of an array of pillar placed at increasing distances o ff ers a simple and quanti fi able way to assess sagging of supportfree structures due to gravity (and, in absence of postprinting cross-linking to the viscoelastic properties of the hydrogel ink), as estimated via assessing the de fl ection angle θ . (Cii) Adjacent fi laments in a fi lament fusion test (deposited in a meandering pattern at increasing fi lament distances, f d ) can merge due to the surface tension between the bioink and the collector substrate, as well as between each layer of a bioink. Inks with lower yield stress tend to have longer fused segment length ( f s ) even at higher f d , causing a loss of resolution in the x -y plane. Schematics based on proposals from Paxton et al. 144 (A), Gao et al. 2018 162 (B), and Ribeiro et al. 2017 78 (C).
Figure 6 Quantitative tests to assess the extrudability, fi lament formation, and shape fi delity of bioink prior to the printing process. (A) Rheological data can be acquired for a speci fi c ink, providing key information on properties necessary to extrude cohesive, stackable fi laments. (Ai) Yield stress measurements correlate with the fl ow initiation step, (Aii) whereas shear-thinning properties of a bioink permit facile extrusion. (Aiii) Depending on the extrusion pressure and the polymer viscosity, droplet, or fi lament formation can occur at the nozzle. (Aiv) Bioinks able to form fi laments and also show a rapid shear recovery after extrusion, can be used for printing and stacking multilayer constructs with improved shape fi delity. 144 (B) Uniformity of each extruded fi lament and thus its shape fi delity compared to the intended design (typically a cylindrical, smooth fi lament) can be assessed via image analysis and correlates with the ability of a viscoelastic bioink to absorb and disperse energy, as quanti fi ed by the loss tangent (tan ( δ )). Higher values of the loss tangent were shown to correlate with better fi lament uniformity. 162 (C) Printed fi laments can experience di ff erent deformations, given their limited mechanical properties, under the action of di ff erent forces, including gravity and surface tension. 78 (Ci) Printing a bioink fi lament on top of an array of pillar placed at increasing distances o ff ers a simple and quanti fi able way to assess sagging of supportfree structures due to gravity (and, in absence of postprinting cross-linking to the viscoelastic properties of the hydrogel ink), as estimated via assessing the de fl ection angle θ . (Cii) Adjacent fi laments in a fi lament fusion test (deposited in a meandering pattern at increasing fi lament distances, f d ) can merge due to the surface tension between the bioink and the collector substrate, as well as between each layer of a bioink. Inks with lower yield stress tend to have longer fused segment length ( f s ) even at higher f d , causing a loss of resolution in the x -y plane. Schematics based on proposals from Paxton et al. 144 (A), Gao et al. 2018 162 (B), and Ribeiro et al. 2017 78 (C).CC-BY-NC-ND · From the PDF
Figure 7 Quantitative tests to assess the shape fi delity of a bioink during printing and postfabrication. (Ai) Single fi laments are evaluated on their (Aii) homogeneity based on the fi ber diameter (d 1 , d2, and d 3 ), with identical diameters characterizing a homogeneous fi lament. 163,178 (Bi) Top and side view of 2D planar structures, meaning constructs that predominantly extend along two directions which are signi fi cantly wider than the height of the constructs which are typically composed of 1 -2 layers. Planar structures being evaluated on (Bii) fi lament diameter and merging with focus on the intersection/overlay of two fi laments and (Biii) transversal pore geometry with optimal rectangular pore shape for ideal fi lament stacking (printability index P r = 1). 46,163 (Ci) Top and side view of multilayered constructs illustrating circularity of fi laments. 46,105,140 (Cii) Visual grid as indicator how close the printed structure (green lines) match with the computer designed shape (black lines) post printing. 105 (Ciii) Layer stacking indicating the shape retention of circular fi laments in multilayered constructs is analyzed by comparing the height of the computer designed sample to the height (h 1 and h2). 162,163 Schematics based on proposals from Soltan et al. 2019, Wang et al. 2018 163,178 (A); Ouyang et al. 2016, Soltan et al. 2019 46,163 (B); and Petta el al. 2018, Gao et al. 2018, and Soltan et al. 2019 105,162,163 (C).
Figure 7 Quantitative tests to assess the shape fi delity of a bioink during printing and postfabrication. (Ai) Single fi laments are evaluated on their (Aii) homogeneity based on the fi ber diameter (d 1 , d2, and d 3 ), with identical diameters characterizing a homogeneous fi lament. 163,178 (Bi) Top and side view of 2D planar structures, meaning constructs that predominantly extend along two directions which are signi fi cantly wider than the height of the constructs which are typically composed of 1 -2 layers. Planar structures being evaluated on (Bii) fi lament diameter and merging with focus on the intersection/overlay of two fi laments and (Biii) transversal pore geometry with optimal rectangular pore shape for ideal fi lament stacking (printability index P r = 1). 46,163 (Ci) Top and side view of multilayered constructs illustrating circularity of fi laments. 46,105,140 (Cii) Visual grid as indicator how close the printed structure (green lines) match with the computer designed shape (black lines) post printing. 105 (Ciii) Layer stacking indicating the shape retention of circular fi laments in multilayered constructs is analyzed by comparing the height of the computer designed sample to the height (h 1 and h2). 162,163 Schematics based on proposals from Soltan et al. 2019, Wang et al. 2018 163,178 (A); Ouyang et al. 2016, Soltan et al. 2019 46,163 (B); and Petta el al. 2018, Gao et al. 2018, and Soltan et al. 2019 105,162,163 (C).CC-BY-NC-ND · From the PDF
Figure 8 Use of CT and OCT for visualization of fi laments and pore structure in printed hydrogels for the evaluation of shape fi delity. (A) Use of micro-CT to assess shape fi delity of 3D printed HA-based hydrogel: (a) Optical image of a 3D printed lattice grid overlapped with its 3D CAD model; (b) micro-CT 3D reconstruction of the printed construct, where the color represents the thickness; (c) Strut thickness distribution in the 3D reconstruction; (d) micro-CT crosssection of a 3D printed construct of multiple layers illustrating overlaying accuracy; (e) 3D reconstruction image showing air pockets in red. Scale bars 1 mm. (A). Reproduced with permission from ref 105. Copyright 2018 American Chemical Society. (B) Optical coherence tomography (OCT) imaging of gelatin/alginate hydrogel with di ff erent architectures illustrating (A1, 3) the cross-section; (B1, 3) surface; (C1, 3) hydrogel at 1 mm depth; and (D1, 3) 3D observation of hydrogel matrix. Scale bars 500 μ m, UMP: unde fi ned micropores. (B) Adapted with permission from ref 192. Copyright 2106 The Optical Society.
Figure 8 Use of CT and OCT for visualization of fi laments and pore structure in printed hydrogels for the evaluation of shape fi delity. (A) Use of micro-CT to assess shape fi delity of 3D printed HA-based hydrogel: (a) Optical image of a 3D printed lattice grid overlapped with its 3D CAD model; (b) micro-CT 3D reconstruction of the printed construct, where the color represents the thickness; (c) Strut thickness distribution in the 3D reconstruction; (d) micro-CT crosssection of a 3D printed construct of multiple layers illustrating overlaying accuracy; (e) 3D reconstruction image showing air pockets in red. Scale bars 1 mm. (A). Reproduced with permission from ref 105. Copyright 2018 American Chemical Society. (B) Optical coherence tomography (OCT) imaging of gelatin/alginate hydrogel with di ff erent architectures illustrating (A1, 3) the cross-section; (B1, 3) surface; (C1, 3) hydrogel at 1 mm depth; and (D1, 3) 3D observation of hydrogel matrix. Scale bars 500 μ m, UMP: unde fi ned micropores. (B) Adapted with permission from ref 192. Copyright 2106 The Optical Society.CC-BY-NC-ND · From the PDF
Image 12
CC-BY-NC-ND · From the PDF
Figure 9 Schematic illustration of DLP printing and the e ff ect of overcuring. (A) Schematics of a DLP printing approach, with a particular example using silk derived bioresins. (A) Adapted with permission from ref 263. Copyright 2018 Springer Nature under CC BY 4.0 (https:// creativecommons.org/licenses/by/4.0/). (B) Example of improved printing resolution via addition of a biocompatible food dye as photo absorber to a PVA-MA bioink. CAD design of a cube, (C) overcured print, and (D) printed cube with sharp edges, from the photo absorber-laden bioink. (B -D) Adapted with permission from ref 247. Copyright 2018 IOP publishing under CC BY-NC-ND 3.0 (https://creativecommons.org/licenses/ by-nc-nd/3.0/).
Figure 9 Schematic illustration of DLP printing and the e ff ect of overcuring. (A) Schematics of a DLP printing approach, with a particular example using silk derived bioresins. (A) Adapted with permission from ref 263. Copyright 2018 Springer Nature under CC BY 4.0 (https:// creativecommons.org/licenses/by/4.0/). (B) Example of improved printing resolution via addition of a biocompatible food dye as photo absorber to a PVA-MA bioink. CAD design of a cube, (C) overcured print, and (D) printed cube with sharp edges, from the photo absorber-laden bioink. (B -D) Adapted with permission from ref 247. Copyright 2018 IOP publishing under CC BY-NC-ND 3.0 (https://creativecommons.org/licenses/ by-nc-nd/3.0/).CC-BY-NC-ND · From the PDF
Image 14
CC-BY-NC-ND · From the PDF

Verification

Claims the paper makes

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Claims other papers make about this one

Each is checked against this paper’s own text: does it say what the citing paper says it does?

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

The self-check needs the paper’s full text.

Citations

Cites

Show all 287 references

Research works printed but not linked: 5

  1. Chimene, 2020, Hydrogel Bioink Reinforcement for Additive Manufacturing: A Focused Review of Emerging Strategies, Adv. Mater., 32, 1902026, 10.1002/adma.201902026 · DOI · Paper page
  2. Mezger, 2011, The Rheology Handbook
  3. Petta, 2018, Three-Dimensional Printing of a Tyramine Hyaluronan Derivative with Double Gelation Mechanism for Independent Tuning of Shear Thinning and Postprinting Curing, ACS Biomater. Sci. Eng., 4, 3088, 10.1021/acsbiomaterials.8b00416 · DOI
  4. Kiyotake, 2019, Development and Quantitative Characterization of the Precursor Rheology of Hyaluronic Acid Hydrogels for Bioprinting, Acta Biomater., 95, 176, 10.1016/j.actbio.2019.01.041 · DOI · Paper page
  5. 2015, ASTM52900-15, I.

Cited by

See all 1,359

Metadata

Authors
Schwab, A., Levato, R., D’Este, M., Piluso, S., Eglin, D., & Malda, J.
Affiliations
  • AO Foundation (CH)
  • Utrecht University (NL)
Corresponding author
Malda, Jos
Venue
Chemical Reviews
Published
2020-08-28
Volume
120
Issue
19
Pages
10850-10877
ISSN
  • 0009-2665 (ISSN-L)
  • 1520-6890
OpenAlex
W3082213210
Cited by
1,359
References
287
Citations by year
2026: 305 · 2025: 283 · 2024: 280 · 2023: 202 · 2022: 176 · 2021: 107 · 2020: 6
FWCI
10.29
Type
journal article
Language
en
Open access
Locations
  • Chemical Reviews (publishedVersion, cc-by-nc-nd)
  • PubMed Central (publishedVersion)
  • PubMed (publishedVersion)
  • University of Twente Research Information (publishedVersion, cc-by-nc-nd)
  • HAL (submittedVersion)
  • Utrecht University Repository (Utrecht University) (submittedVersion, other-oa)
  • University of Twente Research Information (submittedVersion, cc-by-nc-nd)
Funders
  • AO Foundation (3D OC)
  • Nederlandse Organisatie voor Wetenschappelijk Onderzoek (024.003.013)
  • ReumaNederland (LLP12, LLP22)
Topics
  • Physical Sciences › Engineering › Biomedical Engineering › 3D Printing in Biomedical Research
  • Physical Sciences › Materials Science › Biomaterials › Hydrogels: synthesis, properties, applications
  • Physical Sciences › Engineering › Industrial and Manufacturing Engineering › Additive Manufacturing and 3D Printing Technologies
Keywords
bioinks, 3D bioprinting, printability, shape fidelity, hydrogels, extrusion-based bioprinting, rheology, physicochemical parameters, prediction model
MeSH terms
Humans, Ink, Tissue Engineering, Bioprinting, Printing, Three-Dimensional

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

How to cite

Cite CoChat for the checks on this page, and the paper for its own findings.

This page
CoChat. (2026). Citation check: Printability and Shape Fidelity of Bioinks in 3D Bioprinting. https://app.cochat.ai/papers/10.1021/acs.chemrev.0c00084
The paper
Schwab, A., Levato, R., D’Este, M., Piluso, S., Eglin, D., & Malda, J. (2020). Printability and Shape Fidelity of Bioinks in 3D Bioprinting. Chemical Reviews. https://doi.org/10.1021/acs.chemrev.0c00084

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.