Student or educator? Sign up with your school email and get 6 months of Pro free.
CoChat

The DOI matches its Crossref record; 41 of the 41 references it cites were found in a registry or an index; 3 of the 17 sources its claims cite were checked for support.

Silver Nanowire Aerogel Support Promotes Stable Hydrogen Evolution Reaction at High Current Density

Zuo, Chunyan, Tao, Guohua, Zhong, Liubiao, Zhang, Gaowei, Liu, Bu, Qiu, Yejun · 2024 · ACS Applied Materials & Interfaces

Abstract

The stability of electrocatalysts during the hydrogen evolution reaction (HER) is vital for efficient production of hydrogen energy. Herein, we demonstrate that silver nanowire aerogel-based support (AABS) could facilitate the construction of HER catalysts with extraordinary long-term stability. A full nanostructure catalyst of nickel phosphide based formed on AABS (Ni 2 P–Ni 5 P 4 @AABS) was prepared to achieve an overpotential of 687 mV (without iR compensation) for HER at the current density of 1 A cm –2 in 0.5 M H 2 SO 4 . Excitingly, the stable HER performance was kept for 42 days during the long-term stability (i–t) test at high current density (0.5–1 A cm –2 ). The excellent HER performance of the Ni 2 P–Ni 5 P 4 @AABS catalyst is attributed to rapid electron transport pathways, numerous more accessible active sites, and support induced enhanced catalytic activity. The support effect was highlighted by a proposed phenomenological two-channel model for electron transport, which provides fresh insights into the design strategy for energy storage and delivery.

Overview

CoChat Summary

TL;DR

A silver nanowire aerogel-based support (AABS) was used to build a Ni₂P–Ni₅P₄ HER electrocatalyst that requires 687 mV overpotential (without iR compensation) at 1 A cm⁻² in 0.5 M H₂SO₄ and holds stable performance for 42 days at 0.5–1 A cm⁻². The authors attribute the performance to rapid electron transport, more accessible active sites, and a support-induced effect captured by a proposed two-channel electron-transport model.

Key findings

  • Ni₂P–Ni₅P₄@AABS achieved an overpotential of 687 mV at 1000 mA cm⁻² in 0.5 M H₂SO₄ without iR compensation, reported as the lowest among Ni–P-type catalysts on microsized supports without iR compensation (Table S1).
  • In 1 M KOH, the catalyst showed an overpotential of 267 mV at 200 mA cm⁻², lower than Ni₂P–Ni₅P₄ on Ni foam, Cu foam, and Ag foam; solution resistance was Rs ∼ 0.33 Ω.
  • Long-term stability (i–t) held for 42 days at high current density (0.5–1 A cm⁻²) without degradation; performance actually improved over time, with current density rising at 434 mV until the workstation limit was reached at 27–28 days, then continuing at 326 mV.
  • Tafel slopes were 88, 103, and 121 mV dec⁻¹ for Ni₂P–Ni₅P₄ on AABS, NF, and CuF, respectively. Fitted parameters gave j₀ of 0.8 (AABS), 0.015 (NF), 0.0035 (CuF) mA cm⁻², and R₀ of 0.52, 1.10, 1.45 Ω.

Methods

  • Catalyst prepared by electrodeposition of Ni on AABS (30 mA cm⁻², 30 min, room temperature) followed by phosphidation with NaH₂PO₂·H₂O at 350 °C for 1 h under Ar; control samples made identically on Ni foam, Ag foam, and Cu foam.
  • Characterization by SEM, HRTEM/EDS, XRD, XPS (with depth profiling), and ICP (Ni:P ≈ 5:9).
  • Electrochemical testing (LSV at 5 mV s⁻¹, CV over 10,000 cycles at 50 mV s⁻¹, EIS from 0.01 Hz to 100 kHz) in 1 M KOH (CHE760E, graphite rod counter) and 0.5 M H₂SO₄ (Gamry Interface 1010E, Pt sheet counter), all without iR compensation; a phenomenological two-channel model (eqs 1–2) fitted LSV data with six parameters.

Limitations

  • The paper notes the 42-day stability test was run under air conditions, so oxidation may occur, especially at the high temperature caused by the running high current density; it also notes the catalyst was polluted by the Pt sheet counter electrode during the long-term test (prominent Pt 4f peak), though a carbon-rod comparison showed no appreciable difference for AABS.
  • The authors state that the risk of structural collapse of nanostructured supports is more severe than for conventional micrometer-size supports, and that the observed performance enhancement during stability testing is not fully due to Pt contamination, with surface morphology changes and new-phase (Ni₂P₂O₇) formation as other contributors.
  • Evident from the text: the two-channel model is described as "phenomenological" and its parameters are fitted rather than independently derived; the 42-day test was interrupted by a workstation shutdown and a power-off on day 41, so the durability record is not fully continuous.

Model-written summary. Check it against the paper before relying on it.

Integrity signals

Registry

Crossref · 10.1021/acsami.4c12131

Cites

41 of 41 references verified0 citation errors · 0 not checkable

Statistics

Nothing to recompute.

Verification

Claims the paper makes

2 Valid · 1 Not valid · 8 Not checked · 43 Own results and interpretations

19 more claims

Create a free account to see all 54 claims and to verify the 1 reference still open.

See all claims — free account
  • It may state two separate claims as one. 23
  • Probably not a substantial claim. 8

Create a free account to see these claims.

Citations

Cites

Metadata

Authors
Zuo, C., Tao, G., Zhong, L., Zhang, G., Liu, B., & Qiu, Y.
Affiliations
  • Harbin Institute of Technology (CN)
  • Peking University (CN)
  • Lingnan Normal University (CN)
Corresponding author
  • Tao, Guohua
  • Qiu, Yejun
Venue
ACS Applied Materials & Interfaces
Published
2024-10-09
Volume
16
Issue
42
Pages
57091-57098
ISSN
  • 1944-8244 (ISSN-L)
  • 1944-8252
OpenAlex
W4403275785
Cited by
1
References
36
Citations by year
2025: 1
FWCI
0.07
Type
journal article
Language
en
Open access
closed
Locations
  • ACS Applied Materials & Interfaces (publishedVersion)
  • PubMed (publishedVersion)
Funders
National Natural Science Foundation of China (51471005, 51971080)
Topics
  • Physical Sciences › Energy › Renewable Energy, Sustainability and the Environment › Electrocatalysts for Energy Conversion
  • Physical Sciences › Energy › Renewable Energy, Sustainability and the Environment › CO2 Reduction Techniques and Catalysts
  • Physical Sciences › Materials Science › Materials Chemistry › Hydrogen Storage and Materials
Keywords
hydrogen evolution reaction, electrocatalyst support, nickel phosphide, catalyst stability, high current density, electron transport, two-channel model, catalyst support effects, hydrogen production

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

The claim verdicts this report counts are experimental: their accuracy is not yet measured.

A language model drew the claims from the paper on 2026-10-11, under version 3 of the claim definition (model deepseek-v4.1-flash, prompt extract-v3).

A second model labelled each claim on 2026-10-11 (model jev-1.13-20260917, definition revision gold-guideline-v0.2).

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.