Abstract
The long-term cycling of anode-free Li-metal cells (i.e., cells where the negative electrode is in situ formed by electrodeposition on an electronically conductive matrix of lithium sourced from the positive electrode) using a liquid electrolyte is affected by the formation of an inhomogeneous solid electrolyte interphase (SEI) on the current collector and irregular Li deposition. To circumvent these issues, we report an atomically defective carbon current collector where multivacancy defects induce homogeneous SEI formation on the current collector and uniform Li nucleation and growth to obtain a dense Li morphology. Via simulations and experimental measurements and analyses, we demonstrate the beneficial effect of electron deficiency on the Li hosting behavior of the carbon current collector. Furthermore, we report the results of testing anode-free coin cells comprising a multivacancy defective carbon current collector, a Li x Ni 0.8 Co 0.1 Mn 0.1 -based cathode and a nonaqueous Li-containing electrolyte solution. These cells retain 90% of their initial capacity for over 50 cycles under lean electrolyte conditions.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Raman Spectrum of Graphene and Graphene Layers
Ferrari, A. C., Meyer, J. C., Scardaci, V., Casiraghi, C., Lazzeri, M., Mauri, F., Piscanec, S., Jiang, D., Novoselov, K. S., Roth, S., et al. (2006) · Physical Review Letters · doi:10.1103/physrevlett.97.187401 · Cited by 15,047
Pathways for practical high-energy long-cycling lithium metal batteries
Liu, J., Bao, Z., Cui, Y., Dufek, E. J., Goodenough, J. B., Khalifah, P., Li, Q., Liaw, B. Y., Liu, P., Manthiram, A., et al. (2019) · Nature Energy · doi:10.1038/s41560-019-0338-x · Cited by 3,412
Selective deposition and stable encapsulation of lithium through heterogeneous seeded growth
Yan, K., Lu, Z., Lee, H.-W., Xiong, F., Hsu, P.-C., Li, Y., Zhao, J., Chu, S., & Cui, Y. (2016) · Nature Energy · doi:10.1038/nenergy.2016.10 · Cited by 2,116
Reversible epitaxial electrodeposition of metals in battery anodes
Zheng, J., Zhao, Q., Tang, T., Yin, J., Quilty, C. D., Renderos, G. D., Liu, X., Deng, Y., Wang, L., Bock, D. C., et al. (2019) · Science · doi:10.1126/science.aax6873 · Cited by 1,877
Review on modeling of the anode solid electrolyte interphase (SEI) for lithium-ion batteries
Wang, A., Kadam, S., Li, H., Shi, S., & Qi, Y. (2018) · npj Computational Materials · doi:10.1038/s41524-018-0064-0 · Cited by 1,639
Atomic structure of sensitive battery materials and interfaces revealed by cryo–electron microscopy
Li, Y., Li, Y., Pei, A., Yan, K., Sun, Y., Wu, C.-L., Joubert, L.-M., Chin, R., Koh, A. L., Yu, Y., et al. (2017) · Science · doi:10.1126/science.aam6014 · Cited by 1,547
Non-flammable electrolyte enables Li-metal batteries with aggressive cathode chemistries
Fan, X., Chen, L., Borodin, O., Ji, X., Chen, J., Hou, S., Deng, T., Zheng, J., Yang, C., Liou, S.-C., et al. (2018) · Nature Nanotechnology · doi:10.1038/s41565-018-0183-2 · Cited by 1,371
Asenbauer, J., Eisenmann, T., Kuenzel, M., Kazzazi, A., Chen, Z., & Bresser, D. (2020) · Sustainable Energy & Fuels · doi:10.1039/d0se00175a · Cited by 1,295
Yu, Z., Wang, H., Kong, X., Huang, W., Tsao, Y., Mackanic, D. G., Wang, K., Wang, X., Huang, W., Choudhury, S., et al. (2020) · Nature Energy · doi:10.1038/s41560-020-0634-5 · Cited by 1,228
Production and processing of graphene and 2d crystals
Bonaccorso, F., Lombardo, A., Hasan, T., Sun, Z., Colombo, L., & Ferrari, A. C. (2012) · Materials Today · doi:10.1016/s1369-7021(13)70014-2 · Cited by 1,057
Weber, R., Genovese, M., Louli, A. J., Hames, S., Martin, C., Hill, I. G., & Dahn, J. R. (2019) · Nature Energy · doi:10.1038/s41560-019-0428-9 · Cited by 948
Electrode Degradation in Lithium-Ion Batteries
Pender, J. P., Jha, G., Youn, D. H., Ziegler, J. M., Andoni, I., Choi, E. J., Heller, A., Dunn, B. S., Weiss, P. S., Penner, R. M., et al. (2020) · ACS Nano · doi:10.1021/acsnano.9b04365 · Cited by 873
Zhang, L., Su, Z., Jiang, F., Yang, L., Qian, J., Zhou, Y., Li, W., & Hong, M. (2014) · Nanoscale · doi:10.1039/c4nr00348a · Cited by 814
Anode‐Free Rechargeable Lithium Metal Batteries
Qian, J., Adams, B. D., Zheng, J., Xu, W., Henderson, W. A., Wang, J., Bowden, M. E., Xu, S., Hu, J., & Zhang, J. (2016) · Advanced Functional Materials · doi:10.1002/adfm.201602353 · Cited by 746
Fluorine-donating electrolytes enable highly reversible 5-V-class Li metal batteries
Suo, L., Xue, W., Gobet, M., Greenbaum, S. G., Wang, C., Chen, Y., Yang, W., Li, Y., & Li, J. (2018) · Proceedings of the National Academy of Sciences · doi:10.1073/pnas.1712895115 · Cited by 679
Chen, X., Chen, X.-R., Hou, T.-Z., Li, B.-Q., Cheng, X.-B., Zhang, R., & Zhang, Q. (2019) · Science Advances · doi:10.1126/sciadv.aau7728 · Cited by 610
Self-smoothing anode for achieving high-energy lithium metal batteries under realistic conditions
Niu, C., Pan, H., Xu, W., Xiao, J., Zhang, J.-G., Luo, L., Wang, C., Mei, D., Meng, J., Wang, X., et al. (2019) · Nature Nanotechnology · doi:10.1038/s41565-019-0427-9 · Cited by 589
Graphitized Carbon Fibers as Multifunctional 3D Current Collectors for High Areal Capacity Li Anodes
Zuo, T., Wu, X., Yang, C., Yin, Y., Ye, H., Li, N., & Guo, Y. (2017) · Advanced Materials · doi:10.1002/adma.201700389 · Cited by 579
Wang, J., Huang, W., Pei, A., Li, Y., Shi, F., Yu, X., & Cui, Y. (2019) · Nature Energy · doi:10.1038/s41560-019-0413-3 · Cited by 528
Li metal deposition and stripping in a solid-state battery via Coble creep
Chen, Y., Wang, Z., Li, X., Yao, X., Wang, C., Li, Y., Xue, W., Yu, D., Kim, S. Y., Yang, F., et al. (2020) · Nature · doi:10.1038/s41586-020-1972-y · Cited by 500
Defect-induced plating of lithium metal within porous graphene networks
Mukherjee, R., Thomas, A. V., Datta, D., Singh, E., Li, J., Eksik, O., Shenoy, V. B., & Koratkar, N. (2014) · Nature Communications · doi:10.1038/ncomms4710 · Cited by 436
El Ouatani, L., Dedryvère, R., Siret, C., Biensan, P., Reynaud, S., Iratçabal, P., & Gonbeau, D. (2009) · Journal of The Electrochemical Society · doi:10.1149/1.3029674 · Cited by 352
Lithiophilic LiC6 Layers on Carbon Hosts Enabling Stable Li Metal Anode in Working Batteries
Shi, P., Li, T., Zhang, R., Shen, X., Cheng, X., Xu, R., Huang, J., Chen, X., Liu, H., & Zhang, Q. (2019) · Advanced Materials · doi:10.1002/adma.201807131 · Cited by 352
Fast galvanic lithium corrosion involving a Kirkendall-type mechanism
Lin, D., Liu, Y., Li, Y., Li, Y., Pei, A., Xie, J., Huang, W., & Cui, Y. (2019) · Nature Chemistry · doi:10.1038/s41557-018-0203-8 · Cited by 318
Assegie, A. A., Cheng, J.-H., Kuo, L.-M., Su, W.-N., & Hwang, B.-J. (2018) · Nanoscale · doi:10.1039/c7nr09058g · Cited by 309
Lin, Y.-X., Liu, Z., Leung, K., Chen, L.-Q., Lu, P., & Qi, Y. (2016) · Journal of Power Sources · doi:10.1016/j.jpowsour.2016.01.078 · Cited by 287
Barinov, A., Malcioǧlu, O. B., Fabris, S., Sun, T., Gregoratti, L., Dalmiglio, M., & Kiskinova, M. (2009) · The Journal of Physical Chemistry C · doi:10.1021/jp902051d · Cited by 276
Temperature‐Dependent Nucleation and Growth of Dendrite‐Free Lithium Metal Anodes
Yan, K., Wang, J., Zhao, S., Zhou, D., Sun, B., Cui, Y., & Wang, G. (2019) · Angewandte Chemie International Edition · doi:10.1002/anie.201905251 · Cited by 273
Gadipelli, S., & Guo, Z. X. (2015) · ChemSusChem · doi:10.1002/cssc.201403402 · Cited by 260
Xu, X., Qi, C., Hao, Z., Wang, H., Jiu, J., Liu, J., Yan, H., & Suganuma, K. (2018) · Nano-Micro Letters · doi:10.1007/s40820-017-0154-4 · Cited by 258
A Concentrated Ternary‐Salts Electrolyte for High Reversible Li Metal Battery with Slight Excess Li
Qiu, F., Li, X., Deng, H., Wang, D., Mu, X., He, P., & Zhou, H. (2019) · Advanced Energy Materials · doi:10.1002/aenm.201803372 · Cited by 247
Budevski, E., Staikov, G., & Lorenz, W. J. (1996) · Cited by 233
Computational Screening of Current Collectors for Enabling Anode-Free Lithium Metal Batteries
Pande, V., & Viswanathan, V. (2019) · ACS Energy Letters · doi:10.1021/acsenergylett.9b02306 · Cited by 226
Ju, Z., Nai, J., Wang, Y., Liu, T., Zheng, J., Yuan, H., Sheng, O., Jin, C., Zhang, W., Jin, Z., et al. (2020) · Nature Communications · doi:10.1038/s41467-020-14358-1 · Cited by 224
Hagos, T. T., Thirumalraj, B., Huang, C.-J., Abrha, L. H., Hagos, T. M., Berhe, G. B., Bezabh, H. K., Cherng, J., Chiu, S.-F., Su, W.-N., et al. (2019) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.8b21052 · Cited by 217
Graphitic Carbon Nitride Induced Micro‐Electric Field for Dendrite‐Free Lithium Metal Anodes
Lu, Z., Liang, Q., Wang, B., Tao, Y., Zhao, Y., Lv, W., Liu, D., Zhang, C., Weng, Z., Liang, J., et al. (2019) · Advanced Energy Materials · doi:10.1002/aenm.201803186 · Cited by 216
Lithium intercalation into bilayer graphene
Ji, K., Han, J., Hirata, A., Fujita, T., Shen, Y., Ning, S., Liu, P., Kashani, H., Tian, Y., Ito, Y., et al. (2019) · Nature Communications · doi:10.1038/s41467-018-07942-z · Cited by 207
Engineering stable interfaces for three-dimensional lithium metal anodes
Xie, J., Wang, J., Lee, H. R., Yan, K., Li, Y., Shi, F., Huang, W., Pei, A., Chen, G., Subbaraman, R., et al. (2018) · Science Advances · doi:10.1126/sciadv.aat5168 · Cited by 190
Revealing Principles for Design of Lean-Electrolyte Lithium Metal Anode via In Situ Spectroscopy
Li, H., Chao, D., Chen, B., Chen, X., Chuah, C., Tang, Y., Jiao, Y., Jaroniec, M., & Qiao, S.-Z. (2020) · Journal of the American Chemical Society · doi:10.1021/jacs.9b11774 · Cited by 190
Ganesan, K., Ghosh, S., Gopala Krishna, N., Ilango, S., Kamruddin, M., & Tyagi, A. K. (2016) · Physical Chemistry Chemical Physics · doi:10.1039/c6cp02033j · Cited by 180
Multilayer-graphene-stabilized lithium deposition for anode-Free lithium-metal batteries
Assegie, A. A., Chung, C.-C., Tsai, M.-C., Su, W.-N., Chen, C.-W., & Hwang, B.-J. (2019) · Nanoscale · doi:10.1039/c8nr06980h · Cited by 180
Exploiting Lithium–Ether Co‐Intercalation in Graphite for High‐Power Lithium‐Ion Batteries
Kim, H., Lim, K., Yoon, G., Park, J., Ku, K., Lim, H., Sung, Y., & Kang, K. (2017) · Advanced Energy Materials · doi:10.1002/aenm.201700418 · Cited by 179
Self-citationMechanistic insight into dendrite–SEI interactions for lithium metal electrodes
Hao, F., Verma, A., & Mukherjee, P. P. (2018) · Journal of Materials Chemistry A · doi:10.1039/c8ta07997h · Cited by 169
Laser‐Induced Silicon Oxide for Anode‐Free Lithium Metal Batteries
Chen, W., Salvatierra, R. V., Ren, M., Chen, J., Stanford, M. G., & Tour, J. M. (2020) · Advanced Materials · doi:10.1002/adma.202002850 · Cited by 169
Beyene, T. T., Bezabh, H. K., Weret, M. A., Hagos, T. M., Huang, C.-J., Wang, C.-H., Su, W.-N., Dai, H., & Hwang, B.-J. (2019) · Journal of The Electrochemical Society · doi:10.1149/2.0731908jes · Cited by 162
Zhang, S. S., Fan, X., & Wang, C. (2017) · Electrochimica Acta · doi:10.1016/j.electacta.2017.11.175 · Cited by 159
Wondimkun, Z. T., Beyene, T. T., Weret, M. A., Sahalie, N. A., Huang, C., Thirumalraj, B., Jote, B. A., Wang, D., Su, W.-N. J., Wang, C., et al. (2020) · Journal of Power Sources · doi:10.1016/j.jpowsour.2019.227589 · Cited by 153
Liu, W., Xia, Y., Wang, W., Wang, Y., Jin, J., Chen, Y., Paek, E., & Mitlin, D. (2018) · Advanced Energy Materials · doi:10.1002/aenm.201802918 · Cited by 143
Hot Formation for Improved Low Temperature Cycling of Anode-Free Lithium Metal Batteries
Genovese, M., Louli, A. J., Weber, R., Martin, C., Taskovic, T., & Dahn, J. R. (2019) · Journal of The Electrochemical Society · doi:10.1149/2.0661914jes · Cited by 134
Beyene, T. T., Jote, B. A., Wondimkun, Z. T., Olbasa, B. W., Huang, C., Thirumalraj, B., Wang, C., Su, W.-N. J., Dai, H., & Hwang, B. (2019) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.9b09551 · Cited by 109
Meng, Q., Deng, B., Zhang, H., Wang, B., Zhang, W., Wen, Y., Ming, H., Zhu, X., Guan, Y., Yu, X., et al. (2018) · Energy storage materials · doi:10.1016/j.ensm.2018.06.024 · Cited by 98
Design principles for self-forming interfaces enabling stable lithium-metal anodes
Zhu, Y., Pande, V., Li, L., Wen, B., Pan, M. S., Wang, D., Ma, Z.-F., Viswanathan, V., & Chiang, Y. (2020) · Proceedings of the National Academy of Sciences · doi:10.1073/pnas.2001923117 · Cited by 78
Vilá, R. A., Huang, W., & Cui, Y. (2020) · Cell Reports Physical Science · doi:10.1016/j.xcrp.2020.100188 · Cited by 48
Mamme, M. H., Köhn, C., Deconinck, J., & Ustarroz, J. (2018) · Nanoscale · doi:10.1039/c7nr08529j · Cited by 43
Cited by
Strategies toward the development of high-energy-density lithium batteries
Niu, H., Zhang, N., Lu, Y., Zhang, Z., Li, M., Liu, J., Zhang, N., Song, W., Zhao, Y., & Miao, Z. (2024) · Journal of Energy Storage · doi:10.1016/j.est.2024.111666 · Cited by 327
Anode‐Free Solid‐State Lithium Batteries: A Review
Huang, W., Zhao, C., Wu, P., Yuan, H., Feng, W., Liu, Z., Lu, Y., Sun, S., Fu, Z., Hu, J., et al. (2022) · Advanced Energy Materials · doi:10.1002/aenm.202201044 · Cited by 278
Wu, B., Chen, C., Raijmakers, L. H. J., Liu, J., Danilov, D. L., Eichel, R.-A., & Notten, P. H. L. (2023) · Energy Storage Materials · doi:10.1016/j.ensm.2023.02.036 · Cited by 219
A 110 Wh kg−1 Ah-level anode-free sodium battery at −40°C
Zhu, Q., Yu, D., Chen, J., Cheng, L., Tang, M., Wang, Y., Li, Y., Yang, J., & Wang, H. (2024) · Joule · doi:10.1016/j.joule.2024.01.010 · Cited by 170
Huang, F., Xu, P., Fang, G., & Liang, S. (2024) · Advanced Materials · doi:10.1002/adma.202405310 · Cited by 159
Metadata
- Authors
- Kwon, H., Lee, J.-H., Roh, Y., Baek, J., Shin, D. J., Yoon, J. K., Ha, H. J., Kim, J. Y., & Kim, H.-T.
- Venue
- Nature Communications
- Published
- 2021-09-20
- Volume
- 12
- Issue
- 1
- Pages
- 5537-5537
- ISSN
- 2041-1723 (ISSN-L)
- OpenAlex
- W3199065526
- Cited by
- 257
- References
- 54
- FWCI
- 11.02
- Type
- journal article
- Language
- en
- Open access
- gold
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.