Handheld Co-Axial Bioprinting: Application to in situ surgical cartilage repair

Open access

Abstract

Three-dimensional (3D) bioprinting is driving major innovations in the area of cartilage tissue engineering. Extrusion-based 3D bioprinting necessitates a phase change from a liquid bioink to a semi-solid crosslinked network achieved by a photo-initiated free radical polymerization reaction that is known to be cytotoxic. Therefore, the choice of the photocuring conditions has to be carefully addressed to generate a structure stiff enough to withstand the forces phisiologically applied on articular cartilage, while ensuring adequate cell survival for functional chondral repair. We recently developed a handheld 3D printer called “Biopen”. To progress towards translating this freeform biofabrication tool into clinical practice, we aimed to define the ideal bioprinting conditions that would deliver a scaffold with high cell viability and structural stiffness relevant for chondral repair. To fulfill those criteria, free radical cytotoxicity was confined by a co-axial Core/Shell separation. This system allowed the generation of Core/Shell GelMa/HAMa bioscaffolds with stiffness of 200KPa, achieved after only 10 seconds of exposure to 700 mW/cm 2 of 365 nm UV-A, containing >90% viable stem cells that retained proliferative capacity. Overall, the Core/Shell handheld 3D bioprinting strategy enabled rapid generation of high modulus bioscaffolds with high cell viability, with potential for in situ surgical cartilage engineering.

Overview

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Integrity signals

Registry

Crossref · 10.1038/s41598-017-05699-x

Cites

33 of 33 references verified0 citation errors · 0 not checkable

Statistics

Figures

Figure 1 The LAP photo-initiator is able to generate crosslinked hydrogels with the highest modulus values at shortest exposure time (10 s). Compressive modulus (kPa) relative to mechanical properties of GelMa/HAMa, where crosslinking was obtained with three different PIs: Lithium-acylphosphinate (LAP); IRGACURE2959 (IRGA), and VA086 with different photocuring times. The moduli reached by LAP dependent crosslinking are several fold higher respect to the other PIs tested. IRGACURE2959 and VA086 do not achieve the moduli of LAP, even with longer exposure times. Error bars represent standard error of the mean between three replicates. The calculated statistical significance (p < 0.05) was obtained by unpaired t test.
Figure 1 The LAP photo-initiator is able to generate crosslinked hydrogels with the highest modulus values at shortest exposure time (10 s). Compressive modulus (kPa) relative to mechanical properties of GelMa/HAMa, where crosslinking was obtained with three different PIs: Lithium-acylphosphinate (LAP); IRGACURE2959 (IRGA), and VA086 with different photocuring times. The moduli reached by LAP dependent crosslinking are several fold higher respect to the other PIs tested. IRGACURE2959 and VA086 do not achieve the moduli of LAP, even with longer exposure times. Error bars represent standard error of the mean between three replicates. The calculated statistical significance (p < 0.05) was obtained by unpaired t test.CC BY · PubMed Central
Figure 2 Higher concentration of LAP photoinitiator favour higher storage modulus. In situ photo-rheometry of GelMa/HAMa hydrogels incorporating LAP during the crosslinking reaction. Each plot shows storage modulus as a function of time with the UV light (365 nm, 100 mW/cm2) switched on at 100 s. (A) Storage modulus as a function of continuous UV exposure time for four concentrations of LAP (0.005% = open squares, 0.01% = light grey squares, 0.05% = grey squares and 0.1% = black squares). Both the reaction rate and the final storage modulus are impacted by LAP concentration. Low concentrations produce slow reactions resulting in low modulus hydrogels. The two highest LAP concentrations (0.05% and 0.1%) achieve comparable final modulus (~70 kPa), although the 0.05% concentration requires much longer exposure time to achieve this. (B) Effect of dark polymerization. GelMa/HAMa hydrogels incorporating 0.1% LAP were exposed to continuous UV exposure (thick black line) or single bursts of short times (10 s, 2 s and 1 s). The arrows indicate the point at which the UV light was switched off for the continuous exposure (100 s). During light exposure, all hydrogels follow similar crosslinking kinetics, however after the light turns off dark polymerization can continue for many minutes. In the case of the 10 s exposed hydrogel, the dark polymerization is sufficient to match the material crosslinked with a (much longer) continuous exposure.
Figure 2 Higher concentration of LAP photoinitiator favour higher storage modulus. In situ photo-rheometry of GelMa/HAMa hydrogels incorporating LAP during the crosslinking reaction. Each plot shows storage modulus as a function of time with the UV light (365 nm, 100 mW/cm2) switched on at 100 s. (A) Storage modulus as a function of continuous UV exposure time for four concentrations of LAP (0.005% = open squares, 0.01% = light grey squares, 0.05% = grey squares and 0.1% = black squares). Both the reaction rate and the final storage modulus are impacted by LAP concentration. Low concentrations produce slow reactions resulting in low modulus hydrogels. The two highest LAP concentrations (0.05% and 0.1%) achieve comparable final modulus (~70 kPa), although the 0.05% concentration requires much longer exposure time to achieve this. (B) Effect of dark polymerization. GelMa/HAMa hydrogels incorporating 0.1% LAP were exposed to continuous UV exposure (thick black line) or single bursts of short times (10 s, 2 s and 1 s). The arrows indicate the point at which the UV light was switched off for the continuous exposure (100 s). During light exposure, all hydrogels follow similar crosslinking kinetics, however after the light turns off dark polymerization can continue for many minutes. In the case of the 10 s exposed hydrogel, the dark polymerization is sufficient to match the material crosslinked with a (much longer) continuous exposure.CC BY · PubMed Central
Figure 3 Cell cytotoxicity induced by PI and UV irradiated PI. ADSCs cultured in 2D and assayed along 7 days in culture with a metabolic test (Cell Titer-Blue®) to measure the cytotoxicity induced by cell exposure to UV light alone (UV), LAP on its own (LAP) and UV exposed LAP (LAP-UV) compared to untreated cells (CNTRL). Error bars represent standard error of the mean between three replicates. The calculated statistical significance was obtained by unpaired t test and calculated versus CNTRL. At day 7 statistics is calculated also for LAP-UV versus LAP.
Figure 3 Cell cytotoxicity induced by PI and UV irradiated PI. ADSCs cultured in 2D and assayed along 7 days in culture with a metabolic test (Cell Titer-Blue®) to measure the cytotoxicity induced by cell exposure to UV light alone (UV), LAP on its own (LAP) and UV exposed LAP (LAP-UV) compared to untreated cells (CNTRL). Error bars represent standard error of the mean between three replicates. The calculated statistical significance was obtained by unpaired t test and calculated versus CNTRL. At day 7 statistics is calculated also for LAP-UV versus LAP.CC BY · PubMed Central
Figure 4 Core/Shell 3D printing by co-axial extrusion. (A) Schematic representation of the 3D co-axial handheld printer. (B) Schematic representation of the co-axial nozzle. (C) Picture of the cartridges dedicated to Core and Shell loading in the printer, with relative magnification of the nozzle during co-axial deposition. (D) Representative 3D rendered confocal images of Core/Shell printed sample labeled with fluorescent beads. The Shell (GelMa/HAMa plus LAP 0.1%) is shown in red channel, while the Core (GelMa/HAMa) is shown in green channel. z-stacks were acquired every 10 µm and 3D rendering was performed with NIS elements software using the Alpha-blending algorithm. A Nikon Plan Fluor 10x DIC L N1 NA0.3 objective lens was used. The panel shows the same image representative of 3D rendered of superimposed green and red channels in three different orientations.
Figure 4 Core/Shell 3D printing by co-axial extrusion. (A) Schematic representation of the 3D co-axial handheld printer. (B) Schematic representation of the co-axial nozzle. (C) Picture of the cartridges dedicated to Core and Shell loading in the printer, with relative magnification of the nozzle during co-axial deposition. (D) Representative 3D rendered confocal images of Core/Shell printed sample labeled with fluorescent beads. The Shell (GelMa/HAMa plus LAP 0.1%) is shown in red channel, while the Core (GelMa/HAMa) is shown in green channel. z-stacks were acquired every 10 µm and 3D rendering was performed with NIS elements software using the Alpha-blending algorithm. A Nikon Plan Fluor 10x DIC L N1 NA0.3 objective lens was used. The panel shows the same image representative of 3D rendered of superimposed green and red channels in three different orientations.CC BY · PubMed Central
Figure 5 The co-axial printing produces 3D printed samples with high cell viability. (A,B) Representative 3D rendered confocal images of ADSCs Core/Shell (co-axial) and mono-axial bioprinted samples stained with Calcein-AM (live cells, green channel). The samples were labeled with fluorescent beads for identification of the Shell (GelMa/HAMa plus LAP 0.1%, cyan channel). Mono-axial samples were also labelled with fluorescent beads for analysis (GelMa/HAMa plus LAP 0.1% and ADSCs, cyan channel). z-stacks were acquired every 10 μm and 3D rendering was performed with NIS elements software using the Alpha-blending algorithm. Images show representative 3D rendered of single and superimposed (merge) cyan and green channels of confocal single 2D z-stacks. (C) The graph shows the quantification of Calcein-AM stained ADSCs to measure cytotoxicity over time in culture right after UV irradiation in co-axial (Core/Shell) and mono-axial 3D printed samples, and in 2D monolayer. The co-axial approach demonstrates higher cell viability and proliferation compared to mono-axial samples and 2D at 7 days post irradiation exposure. Error bars represent standard error of the mean between three replicates. Statistical significance (p < 0.05) was determined by One way Anova test with Dennett’s correction. (D) The graph shows the quantification of live and dead staining performed with Calcein-AM (live cells, green lines) and SYTOX (dead cells, red lines) to measure cytotoxicity over time in culture in both Core/Shell (co-axial, solid line) printed and mono-axial (dotted line) samples. The Core/Shell approach demonstrates significantly higher cell viability and proliferation compared to mono-axial samples at 10 days. Error bars represent standard error of the mean between three replicates. Statistical significance (p < 0.05) was determined by unpaired t test.
Figure 5 The co-axial printing produces 3D printed samples with high cell viability. (A,B) Representative 3D rendered confocal images of ADSCs Core/Shell (co-axial) and mono-axial bioprinted samples stained with Calcein-AM (live cells, green channel). The samples were labeled with fluorescent beads for identification of the Shell (GelMa/HAMa plus LAP 0.1%, cyan channel). Mono-axial samples were also labelled with fluorescent beads for analysis (GelMa/HAMa plus LAP 0.1% and ADSCs, cyan channel). z-stacks were acquired every 10 μm and 3D rendering was performed with NIS elements software using the Alpha-blending algorithm. Images show representative 3D rendered of single and superimposed (merge) cyan and green channels of confocal single 2D z-stacks. (C) The graph shows the quantification of Calcein-AM stained ADSCs to measure cytotoxicity over time in culture right after UV irradiation in co-axial (Core/Shell) and mono-axial 3D printed samples, and in 2D monolayer. The co-axial approach demonstrates higher cell viability and proliferation compared to mono-axial samples and 2D at 7 days post irradiation exposure. Error bars represent standard error of the mean between three replicates. Statistical significance (p < 0.05) was determined by One way Anova test with Dennett’s correction. (D) The graph shows the quantification of live and dead staining performed with Calcein-AM (live cells, green lines) and SYTOX (dead cells, red lines) to measure cytotoxicity over time in culture in both Core/Shell (co-axial, solid line) printed and mono-axial (dotted line) samples. The Core/Shell approach demonstrates significantly higher cell viability and proliferation compared to mono-axial samples at 10 days. Error bars represent standard error of the mean between three replicates. Statistical significance (p < 0.05) was determined by unpaired t test.CC BY · PubMed Central
Figure 6 The Core/Shell design allows cells to proliferate. (A) Representative 3D rendered confocal images of ADSCs bioprinted samples stained with Calcein-AM (live cells, green channel) at day 1 and day 15 after printing. The Core/Shell samples were generated by labeling with fluorescent beads the Shell (GelMa/HAMa plus LAP 0.1%, cyan channel). z-stacks were acquired every 10 μm and 3D rendering was performed with NIS elements software using the Alpha-blending algorithm. A Nikon Plan Fluor 10x DIC L N1 NA0.3 objective lens was used. Images show representative 3D rendered of superimposed (merge) cyan and green channels of confocal single 2D z-stacks. (B) The graph shows the representation of the percentages of the same area occupied by cells (Cells percentage) and Shell (Shell percentage). (C) Fluorescence images of 10 μm cryosections obtained from the cryopreserved bioprinted samples. The cyan channel represents the labeled Shell, while cells have been stained with DAPI before imaging. A fluorescent Olympus IX70 inverted microscope with a SPOT Diagnostic RT-Slider camera and SPOT Diagnostic software was used. Olimpus 4X UPlanFL NA0.13, 10X CPlanFL RC NA0.3 and 20X LCPlanFL RC2 NA0.4 objective lenses were used.
Figure 6 The Core/Shell design allows cells to proliferate. (A) Representative 3D rendered confocal images of ADSCs bioprinted samples stained with Calcein-AM (live cells, green channel) at day 1 and day 15 after printing. The Core/Shell samples were generated by labeling with fluorescent beads the Shell (GelMa/HAMa plus LAP 0.1%, cyan channel). z-stacks were acquired every 10 μm and 3D rendering was performed with NIS elements software using the Alpha-blending algorithm. A Nikon Plan Fluor 10x DIC L N1 NA0.3 objective lens was used. Images show representative 3D rendered of superimposed (merge) cyan and green channels of confocal single 2D z-stacks. (B) The graph shows the representation of the percentages of the same area occupied by cells (Cells percentage) and Shell (Shell percentage). (C) Fluorescence images of 10 μm cryosections obtained from the cryopreserved bioprinted samples. The cyan channel represents the labeled Shell, while cells have been stained with DAPI before imaging. A fluorescent Olympus IX70 inverted microscope with a SPOT Diagnostic RT-Slider camera and SPOT Diagnostic software was used. Olimpus 4X UPlanFL NA0.13, 10X CPlanFL RC NA0.3 and 20X LCPlanFL RC2 NA0.4 objective lenses were used.CC BY · PubMed Central
Figure 7 Core/Shell printing facilitates a layer by layer deposition of cell-laden hydrogels with structural integrity. Representative epifluorescent image of Calciein-AM (green channel) stained cells after 7 days from printing. The Shell and the Core has been differently labeled with fluorescent beads (cyan channel for Shell, violet channel for Core) to estimate the compartmentalization. An epifluorescent Olympus IX70 inverted microscope with a SPOT Diagnostic RT-Slider camera and SPOT Diagnostic software was used with an Olimpus 4X UPlanFL NA0.13 objective lens.
Figure 7 Core/Shell printing facilitates a layer by layer deposition of cell-laden hydrogels with structural integrity. Representative epifluorescent image of Calciein-AM (green channel) stained cells after 7 days from printing. The Shell and the Core has been differently labeled with fluorescent beads (cyan channel for Shell, violet channel for Core) to estimate the compartmentalization. An epifluorescent Olympus IX70 inverted microscope with a SPOT Diagnostic RT-Slider camera and SPOT Diagnostic software was used with an Olimpus 4X UPlanFL NA0.13 objective lens.CC BY · PubMed Central

Verification

Claims the paper makes

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Claims other papers make about this one

Each is checked against this paper’s own text: does it say what the citing paper says it does?

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

The self-check needs the paper’s full text.

Citations

Cites

Show all 33 references

Cited by

See all 227

Metadata

Authors
Duchi, S., Onofrillo, C., O’Connell, C. D., Blanchard, R., Augustine, C., Quigley, A. F., Kapsa, R. M. I., Pivonka, P., Wallace, G., Di Bella, C., & Choong, P. F. M.
Affiliations
  • The University of Melbourne (AU)
  • University of Wollongong (AU)
Venue
Scientific Reports
Published
2017-07-19
Volume
7
Issue
1
Pages
5837-5837
ISSN
2045-2322 (ISSN-L)
OpenAlex
W2734455281
Cited by
219
References
33
Citations by year
2026: 11 · 2025: 19 · 2024: 22 · 2023: 30 · 2022: 29 · 2021: 39 · 2020: 28 · 2019: 19 · 2018: 22
FWCI
8.50
Type
journal article
Language
en
Open access
Licence
Locations
  • Scientific Reports (publishedVersion, cc-by)
  • Europe PMC (PubMed Central) (publishedVersion, cc-by)
  • PubMed Central (publishedVersion, cc-by)
  • PubMed (publishedVersion)
  • QUT ePrints (Queensland University of Technology) (submittedVersion, cc-by)
  • Research Online (University of Wollongong) (submittedVersion)
  • RMIT Research Repository (RMIT University Library) (submittedVersion)
  • DOAJ (DOAJ: Directory of Open Access Journals) (submittedVersion, cc-by-sa)
  • Figshare (submittedVersion, cc-by)
  • Minerva Access (University of Melbourne) (submittedVersion, cc-by)
Funders
  • Arthritis Australia
  • Australian Research Council (140100012, CE140100012)
Topics
  • Physical Sciences › Engineering › Biomedical Engineering › 3D Printing in Biomedical Research
  • Physical Sciences › Materials Science › Biomaterials › Hydrogels: synthesis, properties, applications
  • Health Sciences › Medicine › Surgery › Tissue Engineering and Regenerative Medicine
Keywords
3D bioprinting, cartilage tissue engineering, gelatin methacryloyl, Hamas, radical polymerization, photocuring, cytotoxicity, scaffold stiffness, stem cell viability, articular cartilage
MeSH terms
Animals, Cartilage, Articular, Cell Survival, Light, Methacrylates, Regeneration, Sheep, Cell Death, Hydrogel, Polyethylene Glycol Dimethacrylate, Cell Proliferation, Tissue Scaffolds, Elastic Modulus, Bioprinting

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

How to cite

Cite CoChat for the checks on this page, and the paper for its own findings.

This page
CoChat. (2026). Citation check: Handheld Co-Axial Bioprinting: Application to in situ surgical cartilage repair. https://app.cochat.ai/papers/10.1038/s41598-017-05699-x
The paper
Duchi, S., Onofrillo, C., O’Connell, C. D., Blanchard, R., Augustine, C., Quigley, A. F., Kapsa, R. M. I., Pivonka, P., Wallace, G., Di Bella, C., & Choong, P. F. M. (2017). Handheld Co-Axial Bioprinting: Application to in situ surgical cartilage repair. Scientific Reports. https://doi.org/10.1038/s41598-017-05699-x

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.