Abstract
Significance: This work represents a first attempt to study the crystallographic texture of Li metal in batteries. X-ray diffraction pole-figure analysis demonstrates that the texture of Li deposition is primarily dependent on the type of additive or cross-over molecule from the cathode side. We find that reversibility of Li, which is phenomenologically influenced by morphology, is fundamentally driven by the texture (crystallographic orientation). Additives in electrolytes and the cross-over molecules from the cathode play crucial roles on the crystallographic texture because they hinder the cathodic process and selectively adsorb/react on different crystal planes. Additives with favorable adsorption and reusability will generate controllable texture, resulting in more uniform morphology and better cycling reversibility.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Li-O2 and Li-S batteries with high energy storage
Bruce, P. G., Freunberger, S. A., Hardwick, L. J., & Tarascon, J.-M. (2012) · Nature Materials · doi:10.1038/nmat3191 · Cited by 9,479
Reviving the lithium metal anode for high-energy batteries
Lin, D., Liu, Y., & Cui, Y. (2017) · Nature Nanotechnology · doi:10.1038/nnano.2017.16 · Cited by 6,763
Shape‐Controlled Synthesis of Metal Nanocrystals: Simple Chemistry Meets Complex Physics?
Xia, Y., Xiong, Y., Lim, B., & Skrabalak, S. E. (2009) · Angewandte Chemie International Edition · doi:10.1002/anie.200802248 · Cited by 5,702 · cited 1×
“The shape of metal crystals is commonly controlled by and strongly dependent on their crystallographic nature (20).”
Electrolytes and Interphases in Li-Ion Batteries and Beyond
Xu, K. (2014) · Chemical Reviews · doi:10.1021/cr500003w · Cited by 5,566 · cited 1×
“Carbonate-based solvents are commonly used in batteries due to their large electrochemical decomposition window, enabling the coupling of Li metal with high-voltage cathodes (34).”
Lithium metal anodes for rechargeable batteries
Xu, W., Wang, J., Ding, F., Chen, X., Nasybulin, E., Zhang, Y., & Zhang, J.-G. (2014) · Energy Environ. Sci. · doi:10.1039/c3ee40795k · Cited by 4,704
High rate and stable cycling of lithium metal anode
Qian, J., Henderson, W. A., Xu, W., Bhattacharya, P., Engelhard, M., Borodin, O., & Zhang, J.-G. (2015) · Nature Communications · doi:10.1038/ncomms7362 · Cited by 2,561
Aurbach, D. (2000) · Journal of Power Sources · doi:10.1016/s0378-7753(00)00431-6 · Cited by 2,130
Selective deposition and stable encapsulation of lithium through heterogeneous seeded growth
Yan, K., Lu, Z., Lee, H.-W., Xiong, F., Hsu, P.-C., Li, Y., Zhao, J., Chu, S., & Cui, Y. (2016) · Nature Energy · doi:10.1038/nenergy.2016.10 · Cited by 2,116
Self-citationA Reversible and Higher-Rate Li-O 2 Battery
Peng, Z., Freunberger, S. A., Chen, Y., & Bruce, P. G. (2012) · Science · doi:10.1126/science.1223985 · Cited by 1,915
Lin, D., Liu, Y., Liang, Z., Lee, H.-W., Sun, J., Wang, H., Yan, K., Xie, J., & Cui, Y. (2016) · Nature Nanotechnology · doi:10.1038/nnano.2016.32 · Cited by 1,798
Self-citation
Cited by
Designing polymers for advanced battery chemistries
Lopez, J., Mackanic, D. G., Cui, Y., & Bao, Z. (2019) · Nature Reviews Materials · doi:10.1038/s41578-019-0103-6 · Cited by 894
Self-citationFluorinated Solid-Electrolyte Interphase in High-Voltage Lithium Metal Batteries
Li, T., Zhang, X.-Q., Shi, P., & Zhang, Q. (2019) · Joule · doi:10.1016/j.joule.2019.09.022 · Cited by 714
Stabilizing metal battery anodes through the design of solid electrolyte interphases
Zhao, Q., Stalin, S., & Archer, L. A. (2021) · Joule · doi:10.1016/j.joule.2021.03.024 · Cited by 629
Critical Review on Low‐Temperature Li‐Ion/Metal Batteries
Zhang, N., Deng, T., Zhang, S., Wang, C., Chen, L., Wang, C., & Fan, X. (2022) · Advanced Materials · doi:10.1002/adma.202107899 · Cited by 604
Moving beyond 99.9% Coulombic efficiency for lithium anodes in liquid electrolytes
Hobold, G. M., Lopez, J., Guo, R., Minafra, N., Banerjee, A., Shirley Meng, Y., Shao-Horn, Y., & Gallant, B. M. (2021) · Nature Energy · doi:10.1038/s41560-021-00910-w · Cited by 547
Uniform High Ionic Conducting Lithium Sulfide Protection Layer for Stable Lithium Metal Anode
Chen, H., Pei, A., Lin, D., Xie, J., Yang, A., Xu, J., Lin, K., Wang, J., Wang, H., Shi, F., et al. (2019) · Advanced Energy Materials · doi:10.1002/aenm.201900858 · Cited by 472
Self-citationZheng, J., Kim, M. S., Tu, Z., Choudhury, S., Tang, T., & Archer, L. A. (2020) · Chemical Society Reviews · doi:10.1039/c9cs00883g · Cited by 466
Effects of Polymer Coatings on Electrodeposited Lithium Metal
Lopez, J., Pei, A., Oh, J. Y., Wang, G.-J. N., Cui, Y., & Bao, Z. (2018) · Journal of the American Chemical Society · doi:10.1021/jacs.8b06047 · Cited by 452
Self-citationGandoman, F. H., Jaguemont, J., Goutam, S., Gopalakrishnan, R., Firouz, Y., Kalogiannis, T., Omar, N., & Van Mierlo, J. (2019) · Applied Energy · doi:10.1016/j.apenergy.2019.113343 · Cited by 436
Zou, P., Sui, Y., Zhan, H., Wang, C., Xin, H. L., Cheng, H.-M., Kang, F., & Yang, C. (2021) · Chemical Reviews · doi:10.1021/acs.chemrev.0c01100 · Cited by 368
Stabilizing Zinc Anode Reactions by Polyethylene Oxide Polymer in Mild Aqueous Electrolytes
Jin, Y., Han, K. S., Shao, Y., Sushko, M. L., Xiao, J., Pan, H., & Liu, J. (2020) · Advanced Functional Materials · doi:10.1002/adfm.202003932 · Cited by 362
Lithium Mechanics: Roles of Strain Rate and Temperature and Implications for Lithium Metal Batteries
LePage, W. S., Chen, Y., Kazyak, E., Chen, K.-H., Sanchez, A. J., Poli, A., Arruda, E. M., Thouless, M. D., & Dasgupta, N. P. (2019) · Journal of The Electrochemical Society · doi:10.1149/2.0221902jes · Cited by 334
Fast lithium growth and short circuit induced by localized-temperature hotspots in lithium batteries
Zhu, Y., Xie, J., Pei, A., Liu, B., Wu, Y., Lin, D., Li, J., Wang, H., Chen, H., Xu, J., et al. (2019) · Nature Communications · doi:10.1038/s41467-019-09924-1 · Cited by 330
Self-citationGunnarsdóttir, A. B., Amanchukwu, C. V., Menkin, S., & Grey, C. P. (2020) · Journal of the American Chemical Society · doi:10.1021/jacs.0c10258 · Cited by 326
Electrochemomechanics of lithium dendrite growth
Jana, A., Woo, S. I., Vikrant, K. S. N., & García, R. E. (2019) · Energy & Environmental Science · doi:10.1039/c9ee01864f · Cited by 318
Luo, D., Zheng, L., Zhang, Z., Li, M., Chen, Z., Cui, R., Shen, Y., Li, G., Feng, R., Zhang, S., et al. (2021) · Nature Communications · doi:10.1038/s41467-020-20339-1 · Cited by 318
Zhang, X., Li, T., Li, B., Zhang, R., Shi, P., Yan, C., Huang, J., & Zhang, Q. (2020) · Angewandte Chemie International Edition · doi:10.1002/anie.201911724 · Cited by 313
Magnetic Field–Suppressed Lithium Dendrite Growth for Stable Lithium‐Metal Batteries
Shen, K., Wang, Z., Bi, X., Ying, Y., Zhang, D., Jin, C., Hou, G., Cao, H., Wu, L., Zheng, G., et al. (2019) · Advanced Energy Materials · doi:10.1002/aenm.201900260 · Cited by 309
High entropy liquid electrolytes for lithium batteries
Wang, Q., Zhao, C., Wang, J., Yao, Z., Wang, S., Kumar, S. G. H., Ganapathy, S., Eustace, S., Bai, X., Li, B., et al. (2023) · Nature Communications · doi:10.1038/s41467-023-36075-1 · Cited by 299
Strategies towards enabling lithium metal in batteries: interphases and electrodes
Horstmann, B., Shi, J., Amine, R., Werres, M., He, X., Jia, H., Hausen, F., Cekic-Laskovic, I., Wiemers-Meyer, S., Lopez, J., et al. (2021) · Energy & Environmental Science · doi:10.1039/d1ee00767j · Cited by 298
Wan, J., Xie, J., Mackanic, D. G., Burke, W., Bao, Z., & Cui, Y. (2018) · Materials Today Nano · doi:10.1016/j.mtnano.2018.12.003 · Cited by 281
Self-citationAhmad, Z., Xie, T., Maheshwari, C., Grossman, J. C., & Viswanathan, V. (2018) · ACS Central Science · doi:10.1021/acscentsci.8b00229 · Cited by 279
Insights into the deposition chemistry of Li ions in nonaqueous electrolyte for stable Li anodes
Wang, Z., Sun, Z., Li, J., Shi, Y., Sun, C., An, B., Cheng, H.-M., & Li, F. (2021) · Chemical Society Reviews · doi:10.1039/d0cs01017k · Cited by 268
Chen, Y., He, Q., Zhao, Y., Zhou, W., Xiao, P., Gao, P., Tavajohi, N., Tu, J., Li, B., He, X., et al. (2023) · Nature Communications · doi:10.1038/s41467-023-43163-9 · Cited by 268
Ultrafast deposition of faceted lithium polyhedra by outpacing SEI formation
Yuan, X., Liu, B., Mecklenburg, M., & Li, Y. (2023) · Nature · doi:10.1038/s41586-023-06235-w · Cited by 265
Self-citationLi2O Solid Electrolyte Interphase: Probing Transport Properties at the Chemical Potential of Lithium
Guo, R., & Gallant, B. M. (2020) · Chemistry of Materials · doi:10.1021/acs.chemmater.0c00333 · Cited by 252
Tortuosity Effects in Lithium-Metal Host Anodes
Chen, H., Pei, A., Wan, J., Lin, D., Vilá, R., Wang, H., Mackanic, D., Steinrück, H.-G., Huang, W., Li, Y., et al. (2020) · Joule · doi:10.1016/j.joule.2020.03.008 · Cited by 249
“To elucidate the mechanisms behind the improved electrochemical performances, we compared the morphology evolution of different bare electrodes without prestored Li after CE test cycling in the commonly used carbonate electrolyte system, as the dendritic Li morphology is more obvious in the carbonate electrolyte syste…”
ResultSelf-citationLithium metal stripping beneath the solid electrolyte interphase
Shi, F., Pei, A., Boyle, D. T., Xie, J., Yu, X., Zhang, X., & Cui, Y. (2018) · Proceedings of the National Academy of Sciences · doi:10.1073/pnas.1806878115 · Cited by 226
“This fast potentiodynamic measurement makes the speed of Li deposition much faster than that of lithium corrosion, such that only the contribution of electron transfer is significant (27, 32).”
BackgroundSelf-citationOnboard early detection and mitigation of lithium plating in fast-charging batteries
Huang, W., Ye, Y., Chen, H., Vilá, R. A., Xiang, A., Wang, H., Liu, F., Yu, Z., Xu, J., Zhang, Z., et al. (2022) · Nature Communications · doi:10.1038/s41467-022-33486-4 · Cited by 224
Self-citationChae, O. B., & Lucht, B. L. (2023) · Advanced Energy Materials · doi:10.1002/aenm.202203791 · Cited by 221
Controlling Li deposition below the interface
Cao, W., Li, Q., Yu, X., & Li, H. (2022) · eScience · doi:10.1016/j.esci.2022.02.002 · Cited by 203
Hierarchical Li electrochemistry using alloy-type anode for high-energy-density Li metal batteries
Cao, J., Shi, Y., Gao, A., Du, G., Dilxat, M., Zhang, Y., Cai, M., Qian, G., Lu, X., Xie, F., et al. (2024) · Nature Communications · doi:10.1038/s41467-024-45613-4 · Cited by 196
“Of specialimportance is that the deposition surface of Li changes to the (110) plane rather than the starting (200) plane, which is conducive to the formation of planar Li morphology 53 – 55 .”
Shangguan, X., Xu, G., Cui, Z., Wang, Q., Du, X., Chen, K., Huang, S., Jia, G., Li, F., Wang, X., et al. (2019) · Small · doi:10.1002/smll.201900269 · Cited by 194
Mechanical properties of metallic lithium: from nano to bulk scales
Fincher, C. D., Ojeda, D., Zhang, Y., Pharr, G. M., & Pharr, M. (2020) · Acta Materialia · doi:10.1016/j.actamat.2019.12.036 · Cited by 187
On the crystallography and reversibility of lithium electrodeposits at ultrahigh capacity
Zhao, Q., Deng, Y., Utomo, N. W., Zheng, J., Biswal, P., Yin, J., & Archer, L. A. (2021) · Nature Communications · doi:10.1038/s41467-021-26143-9 · Cited by 181
Zheng, J., Deng, Y., Yin, J., Tang, T., Garcia‐Mendez, R., Zhao, Q., & Archer, L. A. (2022) · Advanced Materials · doi:10.1002/adma.202106867 · Cited by 172
Problem, Status, and Possible Solutions for Lithium Metal Anode of Rechargeable Batteries
Zhang, S. S. (2018) · ACS Applied Energy Materials · doi:10.1021/acsaem.8b00055 · Cited by 162
Investigation of the temperature-dependent behaviours of Li metal anode
Guo, Y., Li, D., Xiong, R., & Li, H. (2019) · Chemical Communications · doi:10.1039/c9cc04897a · Cited by 49
Metadata
- Authors
- Shi, F., Pei, A., Vailionis, A., Xie, J., Liu, B., Zhao, J., Gong, Y., & Cui, Y.
- Venue
- Proceedings of the National Academy of Sciences
- Published
- 2017-10-30
- Volume
- 114
- Issue
- 46
- Pages
- 12138-12143
- ISSN
- 0027-8424 (ISSN-L)
- 1091-6490
- OpenAlex
- W2766142673
- Cited by
- 283
- References
- 37
- FWCI
- 9.06
- Type
- journal article
- Language
- en
- Open access
- green
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.