Reliability Challenges for CMOS Technology Qualifications With Hafnium Oxide/Titanium Nitride Gate Stacks
The DOI matches its Crossref record; 19 of the 19 references it cites were found in a registry or an index.
Abstract
It has been demonstrated that the introduction of HfO2/ TiN gate stacks into CMOS technologies provides the means to continue with traditional device gate length scaling. However, the introduction of HfO2as a new gate dielectric and TiN as a metallic gate electrode into the gate stack of FETs brings about new challenges for understanding reliability physics and qualification. This contribution summarizes recent advances in the understanding of charge trapping and defect generation in HfO2/ TiN gate stacks. This paper relates the electrical properties to the chemical/physical properties of the high-epsiv dielectric and discusses test procedures specifically tailored to quantify gate stack reliability of HfO2/TiN gate stacks.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Band offsets of wide-band-gap oxides and implications for future electronic devices
Robertson, J. (2000) · Journal of Vacuum Science & Technology B: Microelectronics and Nanometer Structures Processing, Measurement, and Phenomena · doi:10.1116/1.591472 · Cited by 2,312 · cited 1×
“The widths of the band gap and the band alignments are drawn to scale based on literature data [ 16 ].”
MethodHigh dielectric constant gate oxides for metal oxide Si transistors
Robertson, J. (2006) · Reports on Progress in Physics · doi:10.1088/0034-4885/69/2/r02 · Cited by 1,726 · cited 2×
“(Right Panel) Calculated energy levels for oxygen vacancies in various charge states. (After [25] and [ 26 ].)”
BackgroundMistry, K., Chau, R., Choi, C.-H., Ding, G., Fischer, K., Ghani, T., Grover, R., Han, W., Hanken, D., Hattendorf, M., et al. (2007) · 2007 IEEE International Electron Devices Meeting · doi:10.1109/iedm.2007.4418914 · Cited by 854
Fischetti, M. V., Neumayer, D. A., & Cartier, E. A. (2001) · Journal of Applied Physics · doi:10.1063/1.1405826 · Cited by 747
Self-citationDegraeve, R., Groeseneken, G., Bellens, R., Ogier, J. L., Depas, M., Roussel, P. J., & Maes, H. E. (1998) · IEEE Transactions on Electron Devices · doi:10.1109/16.662800 · Cited by 656 · cited 1×
“The first process is referred to as Soft Breakdown (SBD), and it is attributed to the formation of a percolation path between the two electrodes [ 48 ]‐[50].”
BackgroundPercolation models for gate oxide breakdown
Stathis, J. H. (1999) · Journal of Applied Physics · doi:10.1063/1.371590 · Cited by 542
Review on high-k dielectrics reliability issues
Ribes, G., Mitard, J., Denais, M., Bruyere, S., Monsieur, F., Parthasarathy, C., Vincent, E., & Ghibaudo, G. (2005) · IEEE Transactions on Device and Materials Reliability · doi:10.1109/tdmr.2005.845236 · Cited by 533 · cited 2×
“In the case of NBTI, the power-law dependence has been explained by a hydrogen release process via multivibrational excitation [ 36 ].”
BackgroundMethodDielectric breakdown mechanisms in gate oxides
Lombardo, S., Stathis, J. H., Linder, B. P., Pey, K. L., Palumbo, F., & Tung, C. H. (2005) · Journal of Applied Physics · doi:10.1063/1.2147714 · Cited by 456
The negative bias temperature instability in MOS devices: A review
Stathis, J. H., & Zafar, S. (2006) · Microelectronics Reliability · doi:10.1016/j.microrel.2005.08.001 · Cited by 427 · cited 2×
“Several recent review articles cover various reliability issues [ 6 ]‐[9].”
BackgroundOrigin of the threshold voltage instability in SiO2/HfO2 dual layer gate dielectrics
Kerber, A., Cartier, E., Pantisano, L., Degraeve, R., Kauerauf, T., Kim, Y., Hou, A., Groeseneken, G., Maes, H. E., & Schwalke, U. (2003) · IEEE Electron Device Letters · doi:10.1109/led.2003.808844 · Cited by 362 · cited 3×
“Electron trapping has been attributed to defects in the IL (oxygen deficiency-related defect precursors) [22], defects at the interface between the two dielectrics [21], defects in the HfO2 layer [ 23 ], and defects at”
MethodResultInfluentialSelf-citationNew physics-based analytic approach to the thin-oxide breakdown statistics
Sune, J. (2001) · IEEE Electron Device Letters · doi:10.1109/55.924847 · Cited by 290 · cited 1×
“The first process is referred to as Soft Breakdown (SBD), and it is attributed to the formation of a percolation path between the two electrodes [48]‐[ 50 ].”
BackgroundThreshold voltage instabilities in high-/spl kappa/ gate dielectric stacks
Zafar, S., Kumar, A., Gusev, E., & Cartier, E. (2005) · IEEE Transactions on Device and Materials Reliability · doi:10.1109/tdmr.2005.845880 · Cited by 272
Self-citationCarrier transport in HfO/sub 2//metal gate MOSFETs: physical insight into critical parameters
Cassé, M., Thevenod, L., Guillaumot, B., Tosti, L., Martín, F., Mitard, J., Weber, O., Andrieu, F., ERNST, T. P., Reimbold, G., et al. (2006) · IEEE Transactions on Electron Devices · doi:10.1109/ted.2006.870888 · Cited by 147 · cited 6×
“The data showing much lower mobility numbers ([21]) were measured on nFETs fabricated in a lowtemperature process, and the mobility reduction was attributed to remote Coulomb scattering due to charges in the gate stack, possibly located at the interface between the two dielectrics [ 21 ].”
BackgroundMethodInfluentialMonsieur, F., Vincent, E., Roy, D., Bruyere, S., Vildeuil, J. C., Pananakakis, G., & Ghibaudo, G. (2003) · IEEE International Reliability Physics Symposium proceedings · doi:10.1109/relphy.2002.996609 · Cited by 123 · cited 2×
“The second process, PBD, describes the phase of local dielectric wear-out by growth of the perculation path until HBD is formed [ 43 ], [44], [51].”
BackgroundReliability screening of high-k dielectrics based on voltage ramp stress
Kerber, A., Pantisano, L., Veloso, A., Groeseneken, G., & Kerber, M. (2007) · Microelectronics Reliability · doi:10.1016/j.microrel.2007.01.030 · Cited by 100 · cited 3×
“A recent study introduced a VRS methodology to evaluate dielectric reliability [47], [ 63 ].”
MethodInfluentialSelf-citationRole of oxygen vacancies in V/sub FB//V/sub t/ stability of pFET metals on HfO/sub 2/
Cartier, E., McFeely, F. R., Narayanan, V., Jamison, P. C., Linder, B. P., Copel, M., Paruchuri, V. K., Basker, V. S., Haight, R., Lim, D., et al. (2005) · Symposium on VLSI Technology · doi:10.1109/.2005.1469279 · Cited by 91
Self-citationA novel approach to characterization of progressive breakdown in high-k/metal gate stacks
Pagano, R., Lombardo, S. A., Palumbo, F., Kirsch, P. D., Krishnan, S. A., Young, C. D., Choi, R., Bersuker, G. I., & Stathis, J. H. (2008) · Microelectronics Reliability · doi:10.1016/j.microrel.2008.07.071 · Cited by 37 · cited 1×
“Preliminary evidence of PBD occurrence with HK/MG stacks was reported in [57] and in a detailed SILC analysis for nFETs with HK/MG stacks [ 58 ].”
MethodTime-dependent dielectric breakdown in poly-Si CVD HfO/sub 2/ gate stack
Lee, S. J., Lee, C. H., Choi, C., & Kwong, D. (2003) · IEEE International Reliability Physics Symposium proceedings · doi:10.1109/relphy.2002.996671 · Cited by 22 · cited 1×
“In the case of HfO2 gate dielectrics with poly-Si electrodes, preliminary evidence for PBD occurrence has been presented [36], [ 52 ], [53].”
BackgroundKim, Y. H., Onishi, K., Kang, C. S., Choi, R., Cho, H.-J., Nieh, R., Han, J. H., Krishnan, S., Shahriar, A., & Lee, J. C. (2003) · Technical digest - International Electron Devices Meeting/Technical digest · doi:10.1109/iedm.2002.1175918 · Cited by 18 · cited 1×
“In the case of HfO2 gate dielectrics with poly-Si electrodes, preliminary evidence for PBD occurrence has been presented [36], [52], [ 53 ].”
Background
Cited by
Enhancing ferroelectricity in dopant-free hafnium oxide
Pal, A., Narasimhan, V. K., Weeks, S., Littau, K., Pramanik, D., & Chiang, T. (2017) · Applied Physics Letters · doi:10.1063/1.4973928 · Cited by 225
Metadata
- Authors
- Kerber, A., & Cartier, E. A.
- Venue
- IEEE Transactions on Device and Materials Reliability
- Published
- 2009-06
- Volume
- 9
- Issue
- 2
- Pages
- 147-162
- ISSN
- 1530-4388 (ISSN-L)
- 1558-2574
- OpenAlex
- W2152664452
- Cited by
- 189
- References
- 19
- FWCI
- 9.77
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.