Reversible Cycling of Crystalline Silicon Powder
Open accessAbstract
A method is described in which crystalline silicon can be used as a practical anode material for lithium-ion batteries. Commercial lithium-ion cells are typically charged at a constant current to a fixed voltage and then are held by the charger at constant voltage until the current decreases to a certain value (also known as constant current/constant voltage or CCCV charging). It is first shown that CCCV charging can be used to reversibly cycle crystalline silicon and limit its capacity. A cycling method is then demonstrated in which crystalline silicon is first partially converted to amorphous silicon, in situ, during conditioning cycles. After the conditioning cycles the silicon can be cycled normally, using CCCV cycling limits, with good coulombic efficiency and little overlithiation during the first cycle.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Structural Changes in Silicon Anodes during Lithium Insertion/Extraction
Obrovac, M. N., & Christensen, L. (2004) · Electrochemical and Solid-State Letters · doi:10.1149/1.1652421 · Cited by 1,995
Self-citationIn Situ XRD and Electrochemical Study of the Reaction of Lithium with Amorphous Silicon
Hatchard, T. D., & Dahn, J. R. (2004) · Journal of The Electrochemical Society · doi:10.1149/1.1739217 · Cited by 1,113
Limthongkul, P., Jang, Y.-I., Dudney, N. J., & Chiang, Y. (2003) · Acta Materialia · doi:10.1016/s1359-6454(02)00514-1 · Cited by 511
On the Aggregation of Tin in SnO Composite Glasses Caused by the Reversible Reaction with Lithium
Courtney, I. A., McKinnon, W. R., & Dahn, J. R. (1999) · Journal of The Electrochemical Society · doi:10.1149/1.1391565 · Cited by 391
Enhanced Cycle Life of Si Anode for Li-Ion Batteries by Using Modified Elastomeric Binder
Liu, W., Yang, M., Wu, H., Chiao, S., & Wu, N. (2005) · Electrochemical and Solid-State Letters · doi:10.1149/1.1847685 · Cited by 336
Electrochemically-driven solid-state amorphization in lithium–metal anodes
Limthongkul, P., Jang, Y.-I., Dudney, N. J., & Chiang, Y. (2003) · Journal of Power Sources · doi:10.1016/s0378-7753(03)00303-3 · Cited by 208
Cited by
High-performance lithium battery anodes using silicon nanowires
Chan, C. K., Peng, H., Liu, G., McIlwrath, K., Zhang, X. F., Huggins, R. A., & Cui, Y. (2008) · Nature Nanotechnology · doi:10.1038/nnano.2007.411 · Cited by 6,683
Advanced Materials for Energy Storage
Liu, C., Li, F., Ma, L., & Cheng, H. (2010) · Advanced Materials · doi:10.1002/adma.200903328 · Cited by 4,765
Rechargeable Lithium–Sulfur Batteries
Manthiram, A., Fu, Y., Chung, S.-H., Zu, C., & Su, Y.-S. (2014) · Chemical Reviews · doi:10.1021/cr500062v · Cited by 4,665
Size-Dependent Fracture of Silicon Nanoparticles During Lithiation
Liu, X. H., Zhong, L., Huang, S., Mao, S. X., Zhu, T., & Huang, J. Y. (2012) · ACS Nano · doi:10.1021/nn204476h · Cited by 2,376
Alloy Negative Electrodes for Li-Ion Batteries
Obrovac, M. N., & Chevrier, V. L. (2014) · Chemical Reviews · doi:10.1021/cr500207g · Cited by 2,175
Self-citationA review of the electrochemical performance of alloy anodes for lithium-ion batteries
Zhang, W.-J. (2011) · Journal of Power Sources · doi:10.1016/j.jpowsour.2010.07.020 · Cited by 2,140
High-performance lithium-ion anodes using a hierarchical bottom-up approach
Magasinski, A., Dixon, P., Hertzberg, B., Kvit, A., Ayala, J., & Yushin, G. (2010) · Nature Materials · doi:10.1038/nmat2725 · Cited by 2,044
Li-alloy based anode materials for Li secondary batteries
Park, C.-M., Kim, J.-H., Kim, H., & Sohn, H.-J. (2010) · Chemical Society Reviews · doi:10.1039/b919877f · Cited by 1,703
McDowell, M. T., Lee, S. W., Nix, W. D., & Cui, Y. (2013) · Advanced Materials · doi:10.1002/adma.201301795 · Cited by 1,670
Silicon‐Based Nanomaterials for Lithium‐Ion Batteries: A Review
Su, X., Wu, Q., Li, J., Xiao, X., Lott, A., Lu, W., Sheldon, B. W., & Wu, J. (2014) · Advanced Energy Materials · doi:10.1002/aenm.201300882 · Cited by 1,593
Interconnected Silicon Hollow Nanospheres for Lithium-Ion Battery Anodes with Long Cycle Life
Yao, Y., McDowell, M. T., Ryu, I., Wu, H., Liu, N., Hu, L., Nix, W. D., & Cui, Y. (2011) · Nano Letters · doi:10.1021/nl201470j · Cited by 1,456
Nanostructured silicon for high capacity lithium battery anodes
Szczech, J. R., & Jin, S. (2011) · Energy Environ. Sci. · doi:10.1039/c0ee00281j · Cited by 1,395
Wang, C., Wu, H., Chen, Z., McDowell, M. T., Cui, Y., & Bao, Z. (2013) · Nature Chemistry · doi:10.1038/nchem.1802 · Cited by 1,269
Chen, J., Fan, X., Li, Q., Yang, H., Khoshi, M. R., Xu, Y., Hwang, S., Chen, L., Ji, X., Yang, C., et al. (2020) · Nature Energy · doi:10.1038/s41560-020-0601-1 · Cited by 1,137
Toward Efficient Binders for Li-Ion Battery Si-Based Anodes: Polyacrylic Acid
Magasinski, A., Zdyrko, B., Kovalenko, I., Hertzberg, B., Burtovyy, R., Huebner, C. F., Fuller, T. F., Luzinov, I., & Yushin, G. (2010) · ACS Applied Materials & Interfaces · doi:10.1021/am100871y · Cited by 1,101
Carbon−Silicon Core−Shell Nanowires as High Capacity Electrode for Lithium Ion Batteries
Cui, L.-F., Yang, Y., Hsu, C.-M., & Cui, Y. (2009) · Nano Letters · doi:10.1021/nl901670t · Cited by 1,054
Hu, Y., Demir‐Cakan, R., Titirici, M., Müller, J., Schlögl, R., Antonietti, M., & Maier, J. (2008) · Angewandte Chemie International Edition · doi:10.1002/anie.200704287 · Cited by 968
Designing polymers for advanced battery chemistries
Lopez, J., Mackanic, D. G., Cui, Y., & Bao, Z. (2019) · Nature Reviews Materials · doi:10.1038/s41578-019-0103-6 · Cited by 894
Current Li-Ion Battery Technologies in Electric Vehicles and Opportunities for Advancements
Miao, Y., Hynan, P., von Jouanne, A., & Yokochi, A. (2019) · Energies · doi:10.3390/en12061074 · Cited by 874
Chae, S., Choi, S., Kim, N., Sung, J., & Cho, J. (2020) · Angewandte Chemie International Edition · doi:10.1002/anie.201902085 · Cited by 856
Anisotropic Swelling and Fracture of Silicon Nanowires during Lithiation
Liu, X. H., Zheng, H., Zhong, L., Huang, S., Karki, K., Zhang, L. Q., Liu, Y., Kushima, A., Liang, W. T., Wang, J. W., et al. (2011) · Nano Letters · doi:10.1021/nl201684d · Cited by 809
Nitta, N., & Yushin, G. (2014) · Particle & Particle Systems Characterization · doi:10.1002/ppsc.201300231 · Cited by 724
Xu, C., Lindgren, F., Philippe, B., Gorgoi, M., Björefors, F., Edström, K., & Gustafsson, T. (2015) · Chemistry of Materials · doi:10.1021/acs.chemmater.5b00339 · Cited by 690
Chan, C. K., Ruffo, R., Hong, S. S., & Cui, Y. (2009) · Journal of Power Sources · doi:10.1016/j.jpowsour.2009.01.007 · Cited by 647
Sethuraman, V. A., Chon, M. J., Shimshak, M., Srinivasan, V., & Guduru, P. R. (2010) · Journal of Power Sources · doi:10.1016/j.jpowsour.2010.02.013 · Cited by 626
Prelithiated Silicon Nanowires as an Anode for Lithium Ion Batteries
Liu, N., Hu, L., McDowell, M. T., Jackson, A., & Cui, Y. (2011) · ACS Nano · doi:10.1021/nn2017167 · Cited by 578
Polymers with Tailored Electronic Structure for High Capacity Lithium Battery Electrodes
Liu, G., Xun, S., Vukmirovic, N., Song, X., Olalde‐Velasco, P., Zheng, H., Battaglia, V. S., Wang, L., & Yang, W. (2011) · Advanced Materials · doi:10.1002/adma.201102421 · Cited by 576
Solution-Grown Silicon Nanowires for Lithium-Ion Battery Anodes
Chan, C. K., Patel, R. N., O’Connell, M. J., Korgel, B. A., & Cui, Y. (2010) · ACS Nano · doi:10.1021/nn901409q · Cited by 543
Confronting Issues of the Practical Implementation of Si Anode in High-Energy Lithium-Ion Batteries
Chae, S., Ko, M., Kim, K., Ahn, K., & Cho, J. (2017) · Joule · doi:10.1016/j.joule.2017.07.006 · Cited by 542
Liu, N., Huo, K., McDowell, M. T., Zhao, J., & Cui, Y. (2013) · Scientific Reports · doi:10.1038/srep01919 · Cited by 538
Chiang, Y.-M. (2010) · Science · doi:10.1126/science.1198591 · Cited by 504
Key Parameters Governing the Reversibility of Si/Carbon/CMC Electrodes for Li-Ion Batteries
Bridel, J.-S., Azaïs, T., Morcrette, M., Tarascon, J.-M., & Larcher, D. (2010) · Chemistry of Materials · doi:10.1021/cm902688w · Cited by 499
In situ TEM electrochemistry of anode materials in lithium ion batteries
Liu, X. H., & Huang, J. Y. (2011) · Energy & Environmental Science · doi:10.1039/c1ee01918j · Cited by 496
Research progress on silicon/carbon composite anode materials for lithium-ion battery
Shen, X., Tian, Z., Fan, R., Shao, L., Zhang, D., Cao, G., Kou, L., & Bai, Y. (2018) · Journal of Energy Chemistry · doi:10.1016/j.jechem.2017.12.012 · Cited by 451
Qi, W., Shapter, J. G., Wu, Q., Yin, T., Gao, G., & Cui, D. (2017) · Journal of Materials Chemistry A · doi:10.1039/c7ta05283a · Cited by 445
He, Y., Yu, X., Wang, Y., Li, H., & Huang, X. (2011) · Advanced Materials · doi:10.1002/adma.201102568 · Cited by 438
Recent advancement of SiOx based anodes for lithium-ion batteries
Chen, T., Wu, J., Zhang, Q., & Su, X. (2017) · Journal of Power Sources · doi:10.1016/j.jpowsour.2017.07.073 · Cited by 427
Silicon/Carbon Composite Anode Materials for Lithium-Ion Batteries
Dou, F., Shi, L., Chen, G., & Zhang, D. (2019) · Electrochemical Energy Reviews · doi:10.1007/s41918-018-00028-w · Cited by 419
Ultrafast Electrochemical Lithiation of Individual Si Nanowire Anodes
Liu, X. H., Zhang, L. Q., Zhong, L., Liu, Y., Zheng, H., Wang, J. W., Cho, J.-H., Dayeh, S. A., Picraux, S. T., Sullivan, J. P., et al. (2011) · Nano Letters · doi:10.1021/nl200412p · Cited by 411
Metal hydrides for lithium-ion batteries
Oumellal, Y., Rougier, A., Nazri, G. A., Tarascon, J.-M., & Aymard, L. (2008) · Nature Materials · doi:10.1038/nmat2288 · Cited by 395
Liu, X. H., Huang, S., Picraux, S. T., Li, J., Zhu, T., & Huang, J. Y. (2011) · Nano Letters · doi:10.1021/nl2024118 · Cited by 390
Smith, A. J., Burns, J. C., Trussler, S., & Dahn, J. R. (2010) · Journal of The Electrochemical Society · doi:10.1149/1.3268129 · Cited by 369
Silicon nanowires for Li-based battery anodes: a review
Zamfir, M. R., Nguyen, H. T., Moyen, E., Lee, Y. H., & Pribat, D. (2013) · Journal of Materials Chemistry A · doi:10.1039/c3ta11714f · Cited by 368
In Situ Measurements of Stress-Potential Coupling in Lithiated Silicon
Sethuraman, V. A., Srinivasan, V., Bower, A. F., & Guduru, P. R. (2010) · Journal of The Electrochemical Society · doi:10.1149/1.3489378 · Cited by 364
Cheng, Z., Jiang, H., Zhang, X., Cheng, F., Wu, M., & Zhang, H. (2023) · Advanced Functional Materials · doi:10.1002/adfm.202301109 · Cited by 364
Philippe, B., Dedryvère, R., Gorgoi, M., Rensmo, H., Gonbeau, D., & Edström, K. (2013) · Journal of the American Chemical Society · doi:10.1021/ja403082s · Cited by 343
Synthesis of Ultrathin Si Nanosheets from Natural Clays for Lithium-Ion Battery Anodes
Ryu, J., Hong, D., Choi, S., & Park, S. (2016) · ACS Nano · doi:10.1021/acsnano.5b07977 · Cited by 334
Kim, K., Ma, H., Park, S., & Choi, N.-S. (2020) · ACS Energy Letters · doi:10.1021/acsenergylett.0c00468 · Cited by 314
Improving the cycling stability of silicon nanowire anodes with conducting polymer coatings
Yao, Y., Liu, N., McDowell, M. T., Pasta, M., & Cui, Y. (2012) · Energy & Environmental Science · doi:10.1039/c2ee21437g · Cited by 308
Challenges in Accommodating Volume Change of Si Anodes for Li‐Ion Batteries
Ko, M., Chae, S., & Cho, J. (2015) · ChemElectroChem · doi:10.1002/celc.201500254 · Cited by 305
Structural and electrochemical study of the reaction of lithium with silicon nanowires
Chan, C. K., Ruffo, R., Hong, S. S., Huggins, R. A., & Cui, Y. (2009) · Journal of Power Sources · doi:10.1016/j.jpowsour.2008.12.047 · Cited by 292
Nguyen, C. C., & Lucht, B. L. (2014) · Journal of The Electrochemical Society · doi:10.1149/2.0731412jes · Cited by 281
Low voltage anode materials for lithium-ion batteries
Eftekhari, A. (2017) · Energy Storage Materials · doi:10.1016/j.ensm.2017.01.009 · Cited by 278
Wang, C.-M., Li, X., Wang, Z., Xu, W., Liu, J., Gao, F., Kovarik, L., Zhang, J.-G., Howe, J., Burton, D. J., et al. (2012) · Nano Letters · doi:10.1021/nl204559u · Cited by 277
Solid Electrolyte Interphase Growth and Capacity Loss in Silicon Electrodes
Michan, A. L., Divitini, G., Pell, A. J., Leskes, M., Ducati, C., & Grey, C. P. (2016) · Journal of the American Chemical Society · doi:10.1021/jacs.6b02882 · Cited by 277
Entwistle, J., Rennie, A., & Patwardhan, S. (2018) · Journal of Materials Chemistry A · doi:10.1039/c8ta06370b · Cited by 277
Eshetu, G. G., & Figgemeier, E. (2019) · ChemSusChem · doi:10.1002/cssc.201900209 · Cited by 273
Silicon Nanowire Fabric as a Lithium Ion Battery Electrode Material
Chockla, A. M., Harris, J. T., Akhavan, V. A., Bogart, T. D., Holmberg, V. C., Steinhagen, C., Mullins, C. B., Stevenson, K. J., & Korgel, B. A. (2011) · Journal of the American Chemical Society · doi:10.1021/ja208232h · Cited by 271
Chen, Z., Wang, C., Lopez, J., Lu, Z., Cui, Y., & Bao, Z. (2015) · Advanced Energy Materials · doi:10.1002/aenm.201401826 · Cited by 270
Silicon Inverse‐Opal‐Based Macroporous Materials as Negative Electrodes for Lithium Ion Batteries
Esmanski, A., & Ozin, G. A. (2009) · Advanced Functional Materials · doi:10.1002/adfm.200900306 · Cited by 269
Materials for Rechargeable Lithium-Ion Batteries
Hayner, C. M., Zhao, X., & Kung, H. H. (2012) · Annual Review of Chemical and Biomolecular Engineering · doi:10.1146/annurev-chembioeng-062011-081024 · Cited by 263
High energy density calendered Si alloy/graphite anodes
Du, Z., Dunlap, R. A., & Obrovac, M. N. (2014) · Journal of The Electrochemical Society · doi:10.1149/2.0941410jes · Cited by 107
Self-citation
Metadata
- Authors
- Obrovac, M. N., & Krause, L. J.
- Venue
- Journal of The Electrochemical Society
- Publisher
- The Electrochemical Society
- Published
- 2007
- Volume
- 154
- Issue
- 2
- Pages
- A103
- ISSN
- 0013-4651 (ISSN-L)
- OpenAlex
- W2128922124
- Cited by
- 1,259
- References
- 6
- FWCI
- 22.36
- Type
- journal article
- Language
- en
- Open access
- bronze
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.