Review on Research and Development of Abrasive Scratching of Hard Brittle Materials and Its Underlying Mechanisms
Open accessThe DOI matches its Crossref record; 67 of the 67 references it cites were found in a registry or an index.
Abstract
Hard brittle materials such as ceramics and crystals are commonly utilized in various industries, including information technology, mechanical engineering, and semiconductors. These materials, known for their high brittleness and hardness but low fracture toughness, pose challenges in efficient and high-quality machining. Current abrasive machining techniques involve rough grinding, fine grinding, and polishing processes, with the latter being the most time-consuming and accounting for over half of the total machining time. Improving processing parameters in rough and fine grinding can increase machining efficiency, reduce surface and subsurface damage, and improve workpiece quality, ultimately reducing the polishing time. This paper explores the abrasive scratching of hard brittle materials, examining the nucleation and propagation of cracks causing surface and subsurface damage, and the underlying mechanisms. The research provides suggestions for enhancing abrasive machining efficiency and ensuring the surface quality of hard brittle materials.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Figures



![Figure 4 Distribution of the stresses and cracks in the single abrasive Figure 4. Distribution of the stresses and cracks in the single abrasive scratching of fused silica [27].](https://figures.cochat.ai/paper-figures/2ab6f8ad56284cd58784b4adab6d38b6/review-on-research-and-development-of-abrasive-scratching-of-hard-brittle-figure-4.png)

![Figure 6 Effect of temperature on the single abrasive scratching of optical glass: ( a ) microhardnes ( b ) fracture toughness, ( c ) specific grinding force, ( d ) specific grinding energy [14]. Figure 6. Effect of temperature on the single abrasive scratching of optical glass: ( a ) microhardness, ( b ) fracture toughness, ( c ) specific grinding force, ( d ) specific grinding energy [14].](https://figures.cochat.ai/paper-figures/a1d3936fb8564a80a7554d83b1b8ee6d/review-on-research-and-development-of-abrasive-scratching-of-hard-brittle-figure-6.png)
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Elastic/Plastic Indentation Damage in Ceramics: The Median/Radial Crack System
LAWN, B. R., EVANS, A. G., & MARSHALL, D. B. (1980) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1980.tb10768.x · Cited by 2,108
Moving sources of heat and the temperature at sliding contacts
Jaeger, J. C. (1943) · Journal and proceedings of the Royal Society of New South Wales · doi:10.5962/p.360338 · Cited by 1,157
Direct Observation and Analysis of Indentation Cracking in Glasses and Ceramics
Cook, R. F., & Pharr, G. M. (1990) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1990.tb05119.x · Cited by 1,071
Elastic/Plastic Indentation Damage in Ceramics: The Lateral Crack System
MARSHALL, D. B., LAWN, B. R., & EVANS, A. G. (1982) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1982.tb10782.x · Cited by 775
Microfracture beneath point indentations in brittle solids
Lawn, B. R., & Swain, M. V. (1975) · Journal of Materials Science · doi:10.1007/bf00541038 · Cited by 717
Material Removal Mechanisms in Lapping and Polishing
Evans, C. J., Paul, E., Dornfeld, D., Lucca, D. A., Byrne, G., Tricard, M., Klocke, F., Dambon, O., & Mullany, B. A. (2003) · CIRP Annals · doi:10.1016/s0007-8506(07)60207-8 · Cited by 383
Elastic stress fields caused by indenting brittle materials
Yoffe, E. H. (1982) · Philosophical Magazine A · doi:10.1080/01418618208236917 · Cited by 376
Li, C., Piao, Y., Meng, B., Hu, Y., Li, L., & Zhang, F. (2022) · International Journal of Machine Tools and Manufacture · doi:10.1016/j.ijmachtools.2021.103827 · Cited by 315
Molecular dynamics simulation of laser assisted grinding of GaN crystals
Li, C., Hu, Y., Zhang, F., Geng, Y., & Meng, B. (2023) · International Journal of Mechanical Sciences · doi:10.1016/j.ijmecsci.2022.107856 · Cited by 257
A New Analytical Model for Estimation of Scratch‐Induced Damage in Brittle Solids
Jing, X., Maiti, S., & Subhash, G. (2007) · Journal of the American Ceramic Society · doi:10.1111/j.1551-2916.2006.01471.x · Cited by 184
Research works printed but not linked: 6
- 9. Shi, X.K.; Teng, L.; Li, Y.Q. The critical condition of ductile grinding of hard brittle materials. Aviat. Precis. Manuf. Technol. 1996 , 4 , 10-13.
- 27. Wang, W. High Efficiency Controllable Precision Grinding Mechanisms of Fused Silica. Ph.D. Thesis, Shandong University, Jinan, China, 2017.
- 31. Lin, B. Theoretical and Experimental Studies on the Ultra-precision Grinding of Engineering Ceramics. Doctoral Thesis, Tianjin University, Tianjin, China, 1999.
- 44. Zhao, H.H.; Cai, G.Q. Model establishment and mechanism research of chip-formation due to shock under ultra-high speed grinding. China Mech. Eng. 2004 , 12 , 1038-1041.
- 52. Ji, P .J.; Zhang, J.J.; Xie, X.D.; Ying, R.M.; Zhang, L. Review on Wear Characteristics of Artificial Hip Joint and Associated Physical Training. Front. Mater. 2023 , 10 .
- 54. Hahn, R.S. On the nature of the grinding process. In Proceedings of the 3rd International Machine Tool Design & Research Conference, Manchester, UK, 18-20 September 1962; pp. 129-154.
Cited by
Xie, X., Zhang, L., Zhu, L., Li, Y., Hong, T., Yang, W., & Shan, X. (2023) · Coatings · doi:10.3390/coatings13050859 · Cited by 49
Self-citationYang, M., Hao, J., Wu, W., Li, Z., Ma, Y., Zhou, Z., Gao, T., Liu, M., Cui, X., Zhang, Y., et al. (2024) · Tribology International · doi:10.1016/j.triboint.2024.109881 · Cited by 40
Ji, R., Qi, Z., Chen, J., Zhang, L., Lin, K., Lu, S., & Li, Y. (2023) · Crystals · doi:10.3390/cryst13030430 · Cited by 32
Self-citationZhao, X., Gu, K., Zhang, M., Weng, Z., Pan, R., Liu, B., & Wang, J. (2025) · Materials Science and Engineering A · doi:10.1016/j.msea.2025.147919 · Cited by 31
Grinding mechanics of ceramics: from mechanism to modeling
Xu, W., Li, C., Xu, W., Wang, W., Zhang, Y.-B., Yang, M., Cui, X., Li, B.-K., Liu, M.-Z., Gao, T., et al. (2025) · Advances in Manufacturing · doi:10.1007/s40436-025-00553-0 · Cited by 20
“This mechanism is distinguished by the initiation and propagation of cracks [39].”
BHATTACHARYYA, A. S., & Bhattacharyya, K. (2024) · Results in Surfaces and Interfaces · doi:10.1016/j.rsurfi.2024.100196 · Cited by 17
Direct observation of the fracture process on C-plane sapphire by in-situ scratch tests
He, G., Wu, H., Huang, H., & Zhao, H. (2024) · Journal of Materials Research and Technology · doi:10.1016/j.jmrt.2024.07.093 · Cited by 17
Huang, S., Jiang, F., Zhang, T., & Cui, H. (2024) · Materials and Manufacturing Processes · doi:10.1080/10426914.2024.2419102 · Cited by 16
“[10,11] 14] The characteristics, application fields and machining challenges of these materials has been summarized in detail by Zhang et al. [14] With the trend toward miniaturization and precision development of high-end components, micro manufacturing technology has become a focus.”
Wang, Y., Wang, Z., Ni, P., Wang, D., Lu, Y., Lu, H., Guo, S., & Chen, Z. (2023) · Coatings · doi:10.3390/coatings13040758 · Cited by 13
Yuan, H., Yang, W., Zhang, L., & Hong, T. (2023) · Coatings · doi:10.3390/coatings13030581 · Cited by 12
Self-citationThe Polishing of Inner Wall on Medical Device Hole by Shear Thickening Abrasive Flow
Ye, B., Mao, W., Ji, R., Zeng, X., & Zhang, L. (2023) · Coatings · doi:10.3390/coatings13091492 · Cited by 12
Self-citationWang, T., Wang, C., Li, J., Wang, W., Chai, L., & Luo, J. (2024) · International Journal of Refractory Metals and Hard Materials · doi:10.1016/j.ijrmhm.2024.106771 · Cited by 11
Gao, D., Cai, J., Liu, Z., Wang, Z., Guo, X., & Kang, R. (2024) · Ceramics International · doi:10.1016/j.ceramint.2024.12.204 · Cited by 11
Vargas-Arana, C., Leal-Perez, J. E., Flores-Valenzuela, J., Macías, A. H., Mendivil-Escalante, J. M., Yáñez-Limón, J. M., Leal-Zayas, J. C., Hussain, S., & Vargas-Ortiz, R. Á. (2025) · Inorganic Chemistry Communications · doi:10.1016/j.inoche.2025.114263 · Cited by 10
Significant Influence on Residual Bending Strength by Cracks Generation During Grinding of Ceramics
Zhang, J., Sui, T., Lin, B., Lv, B., Li, J., & Zhou, J. (2025) · Chinese Journal of Mechanical Engineering · doi:10.1186/s10033-025-01211-z · Cited by 10
“However, due to the random distribution of abrasives and the complex interaction between workpiece materials and abrasives [14, 15], the effect of coupling between randomly positioned abrasives on damage accumulation and material removal during grinding remains unclear [35, 36].”
Ceramic–Titanium Alloy Artificial Hip Joint Wear Simulation and Experimental Study
Ji, R., Fei, C., Ying, R., & Zhang, L. (2023) · Coatings · doi:10.3390/coatings13081321 · Cited by 10
Self-citationShi, K., Li, H., Kuang, Y., Zhang, Z., Liu, J., & Du, Y. (2026) · Tribology International · doi:10.1016/j.triboint.2026.111868 · Cited by 9
Recent Development of Abrasive Machining Processes Enhanced with Non-Newtonian Fluids
Zhu, L., He, X., Wu, X., Wu, J., & Hong, T. (2024) · Coatings · doi:10.3390/coatings14070779 · Cited by 8
Ductile–brittle indentation fracture transitions in hard coatings
BHATTACHARYYA, A. S., Rajak, A. K., & Bhattacharyya, K. (2024) · Surface Engineering · doi:10.1177/02670844241245797 · Cited by 6
“25,26 σ = σ nHans + σ tBous + σ rBlister (4 a ) A complete brittle failure is evident from the formation of debris and spallation occurring due to the interaction of the radial and lateral cracks.”
Qiao, G., Mao, Y., & Zhen, D. (2025) · Ceramics International · doi:10.1016/j.ceramint.2025.08.397 · Cited by 6
BHATTACHARYYA, A. S., & Bhattacharyya, K. (2024) · Surface Review and Letters · doi:10.1142/s0218625x24501233 · Cited by 5
Wen, D., Shi, Y., Cao, Y., Zhao, J., Ding, W., & Zhao, B. (2025) · The International Journal of Advanced Manufacturing Technology · doi:10.1007/s00170-025-16172-9 · Cited by 3
You, Z., Yuan, H., & Ye, X. (2023) · Coatings · doi:10.3390/coatings13061048 · Cited by 3
On the creation of structured abrasive tools via multiple-pass rotary wire EDM: A geometrical model
Wang, B., Liu, G., Zhao, Y., Wang, B., Bi, Q., Pierce, R. S., Qi, H., Fang, X., & Li, H. (2023) · The International Journal of Advanced Manufacturing Technology · doi:10.1007/s00170-023-11276-6 · Cited by 3
Self-citationAnalytical Modeling of Particle Scratching Process
Chen, S., Sun, M., Fan, Y., Yin, F., Huang, J., & Huang, S. (2025) · Applied Sciences · doi:10.3390/app15105670 · Cited by 1
BHATTACHARYYA, A. S. (2023) · doi:10.22541/au.169945437.79259938/v1
Mathematical Modelling of Mechanical Coating
Bhattacharyya, A. S., Bhattacharyya, K., Kumar, R. P., Dash, R., & Rajak, A. K. (2025) · Materials horizons · doi:10.1007/978-981-96-7484-8_8
Optimizing multidiameter cutting for sustainable abrasive disc production
Pereira, J., Silva, F. J. G., Campilho, R. D. S. G., Sebbe, N. P. V., Martinho, R. P., Pedroso, A. F. V., & Sales-Contini, R. C. M. (2026) · Discover Sustainability · doi:10.1007/s43621-026-03132-w
Discharge location control: electrochemical discharge-assisted grinding of quartz Glass
Chen, J., Tong, H., Li, Y., & Liu, Y. (2026) · Materials and Manufacturing Processes · doi:10.1080/10426914.2026.2698505
“[1] However, their high hardness, brittleness, and non-conductivity make these materials difficult to machine.”
Liu, Z., Zhang, H., Cao, Z., Jiangshan, 罗. L., jin, L., & Sheng, Z. (2026) · SSRN Electronic Journal · doi:10.2139/ssrn.7644246
Liu, Z., Zhang, H., Cao, Z., Jiangshan, 罗. L., jin, L., & Sheng, Z. (2026) · SSRN Electronic Journal · doi:10.2139/ssrn.7644242
Liu, Z., Zhang, H., Cao, Z., Jiangshan, 罗. L., jin, L., & Sheng, Z. (2026) · SSRN Electronic Journal · doi:10.2139/ssrn.7657726
Metadata
- Authors
- Qian, H., Chen, M., Qi, Z., Teng, Q., Qi, H., Zhang, L., & Shan, X.
- Affiliations
- Hangzhou Vocational and Technical College (CN)
- Zhejiang Wanli University (CN)
- Central South University (CN)
- Zhejiang University of Technology (CN)
- Corresponding author
- Shan, Xiaohang
- Venue
- Crystals
- Publisher
- MDPI AG
- Published
- 2023-03-02
- Volume
- 13
- Issue
- 3
- Pages
- 428
- ISSN
- 2073-4352 (ISSN-L)
- OpenAlex
- W4322774631
- Cited by
- 33
- References
- 67
- Citations by year
- 2026: 6 · 2025: 8 · 2024: 9 · 2023: 10
- FWCI
- 2.61
- Type
- journal article
- Language
- en
- Open access
- gold
- doi.org
- Licence
- Locations
- Crystals (publishedVersion, cc-by)
- DOAJ (DOAJ: Directory of Open Access Journals) (submittedVersion, cc-by-sa)
- Funders
- Key Research and Development Program of Zhejiang Province (2021C04011, 51575493)
- National Natural Science Foundation of China (2021C04011, 51575493)
- Topics
- Physical Sciences › Engineering › Industrial and Manufacturing Engineering › Advanced Surface Polishing Techniques
- Physical Sciences › Engineering › Mechanical Engineering › Advanced machining processes and optimization
- Physical Sciences › Engineering › Mechanical Engineering › Erosion and Abrasive Machining
- Keywords
- hard and brittle materials, ceramics, crack nucleation, crack propagation, surface damage, subsurface damage, polishing, rough grinding, fine grinding, machining efficiency, surface quality
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.