Degradation mechanisms of bioresorbable polyesters. Part 2. Effects of initial molecular weight and residual monomer
Open accessThe DOI matches its Crossref record; 11 of the 11 references it cites were found in a registry or an index.
Abstract
This paper presents an understanding of how initial molecular weight and initial monomer fraction affect the degradation of bioresorbable polymers in terms of the underlying hydrolysis mechanisms. A mathematical model was used to analyse the effects of initial molecular weight for various hydrolysis mechanisms including noncatalytic random scission, autocatalytic random scission, noncatalytic end scission or autocatalytic end scission. Different behaviours were identified to relate initial molecular weight to the molecular weight half-life and to the time until the onset of mass loss. The behaviours were validated by fitting the model to experimental data for molecular weight reduction and mass loss of samples with different initial molecular weights. Several publications that consider initial molecular weight were reviewed. The effect of residual monomer on degradation was also analysed, and shown to accelerate the reduction of molecular weight and mass loss. An inverse square root law relationship was found between molecular weight half-life and initial monomer fraction for autocatalytic hydrolysis. The relationship was tested by fitting the model to experimental data with various residual monomer contents.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Hydrolytic degradation of devices based on poly(DL-lactic acid) size-dependence
Grizzi, I., Garreau, H., Li, S., & Vert, M. (1995) · Biomaterials · doi:10.1016/0142-9612(95)93258-f · Cited by 895
Pitt, G. G., Gratzl, M. M., Kimmel, G. L., Surles, J., & Sohindler, A. (1981) · Biomaterials · doi:10.1016/0142-9612(81)90060-0 · Cited by 857
Li, S. M., Garreau, H., & Vert, M. (1990) · Journal of Materials Science: Materials in Medicine · doi:10.1007/bf00700871 · Cited by 733 · cited 1×
“Grizzi, Li, and Vert [20, 21] conducted degradation experiments of 2mm thick poly(DL-lactide-coL-lactide) plates in PBS pH 7.”
MethodDegradation of poly (D,L-lactic acid) microspheres: Effect of molecular weight
Park, T. G. (1994) · Journal of Controlled Release · doi:10.1016/0168-3659(94)90263-1 · Cited by 359 · cited 2×
“One set of experiments that do not fit the expected trends predicted by the model are those of Park [5] which consider 10μm microspheres of poly(DL-lactide).”
BackgroundA phenomenological model for the degradation of biodegradable polymers
Wang, Y., Pan, J., Han, X., Sinka, C., & Ding, L. (2008) · Biomaterials · doi:10.1016/j.biomaterials.2008.04.042 · Cited by 191 · cited 2×
“Simulations are conducted using a more detailed version of a previously developed mathematical model [8-11].”
BackgroundMethodDegradation of poly-L-lactide. Part 2: increased temperature accelerated degradation
Weir, N. A., Buchanan, F. J., Orr, J. F., Farrar, D. F., & Dickson, G. R. (2004) · Proceedings of the Institution of Mechanical Engineers, Part H: Journal of Engineering in Medicine · doi:10.1243/0954411041932809 · Cited by 171
Raman, C., Berkland, C., Kim, K. (., & Pack, D. W. (2005) · Journal of Controlled Release · doi:10.1016/j.jconrel.2004.11.012 · Cited by 166 · cited 6×
“Initial molecular weight significantly affects degradation as has been shown by several experimental publications [1-6].”
BackgroundMethodInfluentialGleadall, A., Pan, J., Kruft, M.-A., & Kellomäki, M. (2014) · Acta Biomaterialia · doi:10.1016/j.actbio.2013.12.039 · Cited by 165 · cited 10×
“effect of residual monomer is analysed by simulations with the mathematical model detailed in part 1 [7].”
BackgroundMethodInfluentialSelf-citationTsuji, H. (2003) · Biomaterials · doi:10.1016/s0142-9612(02)00365-4 · Cited by 145 · cited 1×
“It is often the case that polymer samples show zero mass loss for a long period at the start of degradation [15-18].”
BackgroundA model for simultaneous crystallisation and biodegradation of biodegradable polymers
Han, X., & Pan, J. (2009) · Biomaterials · doi:10.1016/j.biomaterials.2008.10.001 · Cited by 143
Self-citationGleadall, A., Pan, J., & Atkinson, H. (2012) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2012.06.023 · Cited by 67 · cited 1×
“Simulations are conducted using a more detailed version of a previously developed mathematical model [8-11].”
MethodSelf-citation
Cited by
PCL and PCL-based materials in biomedical applications
Malikmammadov, E., Tanir, T. E., Kiziltay, A., Hasirci, V., & Hasirci, N. (2018) · Journal of Biomaterials Science, Polymer Edition · doi:10.1080/09205063.2017.1394711 · Cited by 894
Lifetime prediction of biodegradable polymers
Laycock, B., Nikolić, M., Colwell, J. M., Gauthier, E., Halley, P., Bottle, S., & George, G. (2017) · Progress in Polymer Science · doi:10.1016/j.progpolymsci.2017.02.004 · Cited by 662
Recent advances in polymers and polymer composites for food packaging
Zhang, M., Biesold, G. M., Choi, W., Yu, J., Deng, Y., Silvestre, C., & Lin, Z. (2022) · Materials Today · doi:10.1016/j.mattod.2022.01.022 · Cited by 335
A review on the thermomechanical properties and biodegradation behaviour of polyesters
Larrañaga, A., & Lizundia, E. (2019) · European Polymer Journal · doi:10.1016/j.eurpolymj.2019.109296 · Cited by 257
Joseph, B., Augustine, R., Kalarikkal, N., Thomas, S., Seantier, B., & Grohens, Y. (2019) · Materials Today Communications · doi:10.1016/j.mtcomm.2019.02.009 · Cited by 189
Metadata
- Authors
- Gleadall, A., Pan, J., Kruft, M.-A., & Kellomäki, M.
- Venue
- Acta Biomaterialia
- Publisher
- Elsevier BV
- Published
- 2014-05
- Volume
- 10
- Issue
- 5
- Pages
- 2233-2240
- ISSN
- 1742-7061 (ISSN-L)
- OpenAlex
- W2037368024
- Cited by
- 73
- References
- 11
- FWCI
- 1.75
- Type
- journal article
- Language
- en
- Open access
- green
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.