Sequential Crystallization and Multicrystalline Morphology in PE- b -PEO- b -PCL- b -PLLA Tetrablock Quarterpolymers

Open access

Abstract

small-angle X-ray scattering/wide-angle X-ray scattering (SAXS/WAXS), and atomic force microscopy (AFM). The direct comparison of the results obtained with these different techniques allows the precise identification of the crystallization sequence of the blocks upon cooling from the melt. SAXS indicated that Q1 is melt miscible, while Q2 is weakly segregated in the melt but breaks out during crystallization. According to WAXS and DSC results, the blocks follow a sequence as they crystallize: PLLA first, then PE, then PCL, and finally PEO in the case of the Q1 quarterpolymer; in Q2, the PLLA block is not able to crystallize due to its low isotacticity. Although the temperatures at which the PEO and PCL blocks and the PE and PLLA blocks crystallize overlap, the analysis of the intensity changes measured by WAXS and PLOM experiments allows identifying each of the crystallization processes. The quarterpolymer Q1 remarkably self-assembles during crystallization into tetracrystalline banded spherulites, where four types of different lamellae coexist. Nanostructural features arising upon sequential crystallization are found to have a relevant impact on the mechanical properties. Nanoindentation measurements show that storage modulus and hardness of the Q1 quarterpolymer significantly deviate from those of the stiff PE and PLLA blocks, approaching typical values of compliant PEO and PCL. Results are mainly attributed to the low crystallinity of the PE and PLLA blocks. Moreover, the Q2 copolymer exhibits inferior mechanical properties than Q1, and this can be related to the PE block within Q1 that has thinner crystal lamellae according to its much lower melting point.

Overview

CoChat Summary

TL;DR

Two novel PE-b-PEO-b-PCL-b-PLLA tetrablock quarterpolymers were synthesized and characterized, showing sequential crystallization of up to four blocks and, for Q1, tetracrystalline banded spherulites. Q1 crystallizes PLLA, PE, PCL, and PEO sequentially, whereas Q2’s PLLA block does not crystallize due to low isotacticity, yielding tricrystalline microspherulites and lower mechanical properties.

Key findings

  • Q1 (PE187.1-b-PEO3715.1-b-PCL2610.4-b-PLLA197.6) is melt-miscible by SAXS; WAXS/DSC show crystallization sequence PLLA at 84 °C, PE at 82 °C, PCL at 42 °C, and PEO at 24 °C, forming tetracrystalline banded spherulites with Maltese crosses and negative signs.
  • Q2 (PE299.5-b-PEO268.8-b-PCL237.6-b-PLLA227.3) is weakly segregated in the melt by SAXS with breakout crystallization; PLLA does not crystallize (84% isotactic tetrads), and the sequence is PE at 104 °C, PCL at 32 °C, and PEO at 20 °C, giving tricrystalline microspherulites.
  • Nanoindentation shows both quarterpolymers have low storage modulus and hardness (E′ ≤ 1 GPa, H ≤ 50 MPa), attributed to low PE and PLLA crystallinity; Q2 is inferior to Q1, related to thinner PE lamellae/lower PE melting point. Q1 crystallinity estimates include PE 7% and PLLA 4% (Table S9).
  • SAXS indicates Q1 has no diffraction peaks in the melt, while Q2 shows a sharp low-q peak and weak second-order reflection consistent with lamellar phase segregation in the melt.

Methods

  • Q1 and Q2 were synthesized by one-pot polyhomologation plus ring-opening polymerization using a catalyst-switch strategy (organic/metal for Q1, organic/organic for Q2); corresponding triblock, diblock, and homopolymer precursors were also studied.
  • Characterization used nonisothermal DSC, PLOM, simultaneous in situ SAXS/WAXS at ALBA, AFM, and nanoindentation; most cooling/heating experiments were at 20 °C/min, and WAXS normalized intensity versus temperature was used to assign block crystallization.
  • Nanoindentation used dynamic testing at 400 nm depth, with at least 50 indents averaged for E′ and H; AFM samples were spin-coated thin films cooled from the melt at 50 or 20 °C/min.

Limitations

  • Stated: overlapping PE/PLLA and PEO/PCL crystallization and melting transitions make individual crystallinity estimation difficult; AFM cannot clearly distinguish lamellae of the different blocks; PEO spherulites approached millimeter scale, so average E′ and H values were meaningless.
  • Stated: experimental determination of χ for terpolymers or quarterpolymers has not been reported, so segregation-strength estimates are approximate and based on literature solubility parameters.
  • Evident: conclusions rest on only two quarterpolymers and mostly 20 °C/min thermal protocols, so generality across compositions and cooling rates is limited; cooling-rate variation was not systematically explored except in AFM sample preparation.

Model-written summary. Check it against the paper before relying on it.

Integrity signals

Registry

Crossref · 10.1021/acs.macromol.1c01186

Cites

67 of 67 references verified0 citation errors · 0 not checkable

Statistics

Nothing to recompute.

Figures

Scheme 1 Synthesis of Tetracrystalline Quarterpolymer PE-b-PEO-b-PCL-b-PLLA by a Combination of Polyhomologation and the ″Catalyst Switch″ Strategy54
Scheme 1 Synthesis of Tetracrystalline Quarterpolymer PE-b-PEO-b-PCL-b-PLLA by a Combination of Polyhomologation and the ″Catalyst Switch″ Strategy54CC BY · PubMed Central
Figure 1 SAXS patterns of (Q1) PE187.1-b-PEO3715.1-b-PCL2610.4-b-PLLA197.6 and (Q2) PE299.5-b-PEO268.8-b-PCL237.6-b-PLLA227.3at (a) molten state at 180 °C indicating a lamellar structure in the melt by 1:2 q position of the scattering peaks and (b) room temperature of 25 °C.
Figure 1 SAXS patterns of (Q1) PE187.1-b-PEO3715.1-b-PCL2610.4-b-PLLA197.6 and (Q2) PE299.5-b-PEO268.8-b-PCL237.6-b-PLLA227.3at (a) molten state at 180 °C indicating a lamellar structure in the melt by 1:2 q position of the scattering peaks and (b) room temperature of 25 °C.CC BY · PubMed Central
Figure 2 DSC cooling scans at 20 °C/min for tetrablock quarterpolymers (a) PE187.1-b-PEO3715.1-b-PCL2610.4-b-PLLA197.6 (Q1) and (b) PE299.5-b-PEO268.8-b-PCL237.6-b-PLLA227.3 (Q2) with arrows indicating transitions for each block (violet for PE, green for PLLA, blue for PCL, and red for PEO) and close-ups to better identify crystallization peaks.
Figure 2 DSC cooling scans at 20 °C/min for tetrablock quarterpolymers (a) PE187.1-b-PEO3715.1-b-PCL2610.4-b-PLLA197.6 (Q1) and (b) PE299.5-b-PEO268.8-b-PCL237.6-b-PLLA227.3 (Q2) with arrows indicating transitions for each block (violet for PE, green for PLLA, blue for PCL, and red for PEO) and close-ups to better identify crystallization peaks.CC BY · PubMed Central
Figure 3 DSC heating scans at 20 °C/min for (a) PE187.1-b-PEO3715.1-b-PCL2610.4-b-PLLA197.6 (Q1) and (b) PE299.5-b-PEO268.8-b-PCL237.6-b-PLLA227.3 (Q2), with arrows indicating transitions for each block (violet for PE, green for PLLA, blue for PCL, and red for PEO) and a close-up to better identify melting peaks.
Figure 3 DSC heating scans at 20 °C/min for (a) PE187.1-b-PEO3715.1-b-PCL2610.4-b-PLLA197.6 (Q1) and (b) PE299.5-b-PEO268.8-b-PCL237.6-b-PLLA227.3 (Q2), with arrows indicating transitions for each block (violet for PE, green for PLLA, blue for PCL, and red for PEO) and a close-up to better identify melting peaks.CC BY · PubMed Central
Figure 4 WAXS patterns taken during cooling from the melt at 20 °C/min for (a) PE187.1-b-PEO3715.1-b-PCL2610.4-b-PLLA197.6 (Q1) and (b) PE299.5-b-PEO268.8-b-PCL237.6-b-PLLA227.3 (Q2) at different temperatures with arrows indicating transitions for each block (violet for PE, green for PLLA, blue for PCL, and red for PEO) and the corresponding (hkl) planes of the blocks.
Figure 4 WAXS patterns taken during cooling from the melt at 20 °C/min for (a) PE187.1-b-PEO3715.1-b-PCL2610.4-b-PLLA197.6 (Q1) and (b) PE299.5-b-PEO268.8-b-PCL237.6-b-PLLA227.3 (Q2) at different temperatures with arrows indicating transitions for each block (violet for PE, green for PLLA, blue for PCL, and red for PEO) and the corresponding (hkl) planes of the blocks.CC BY · PubMed Central
Figure 5 Normalized WAXS intensities as a function of the temperature of the indicated block reflections for (a) PE187.1-b-PEO3715.1-b-PCL2610.4-b-PLLA197.6 (Q1) and (b) PE299.5-b-PEO268.8-b-PCL237.6-b-PLLA227.3 (Q2) with colored data points and lines (violet for PE, green for PLLA, blue for PCL, and red for PEO) to follow the crystallization of each block. Empty data points represent the molten state of the corresponding block in the samples.
Figure 5 Normalized WAXS intensities as a function of the temperature of the indicated block reflections for (a) PE187.1-b-PEO3715.1-b-PCL2610.4-b-PLLA197.6 (Q1) and (b) PE299.5-b-PEO268.8-b-PCL237.6-b-PLLA227.3 (Q2) with colored data points and lines (violet for PE, green for PLLA, blue for PCL, and red for PEO) to follow the crystallization of each block. Empty data points represent the molten state of the corresponding block in the samples.CC BY · PubMed Central
Figure 6 PLOM micrographs taken upon cooling from the melt at 20 °C/min with colored boxes indicating the crystallization of each of the blocks (violet for PE, green for PLLA, blue for PCL, and red for PEO) for the tetrablock quarterpolymer PE187.1-b-PEO3715.1-b-PCL2610.4-b-PLLA197.6 (Q1): (a) molten state at 95 °C; (b) PLLA at 88 °C; (c) PLLA and PE at 80 °C; (d) PLLA and PE at 45 °C; (e) PLLA, PE, and PCL at 40 °C; (f) PLLA, PE, PCL, and PEO at 34 °C; (g) PLLA, PE, PCL, and PEO at 30 °C; and (h) PLLA, PE, PCL, and PEO at 0 °C.
Figure 6 PLOM micrographs taken upon cooling from the melt at 20 °C/min with colored boxes indicating the crystallization of each of the blocks (violet for PE, green for PLLA, blue for PCL, and red for PEO) for the tetrablock quarterpolymer PE187.1-b-PEO3715.1-b-PCL2610.4-b-PLLA197.6 (Q1): (a) molten state at 95 °C; (b) PLLA at 88 °C; (c) PLLA and PE at 80 °C; (d) PLLA and PE at 45 °C; (e) PLLA, PE, and PCL at 40 °C; (f) PLLA, PE, PCL, and PEO at 34 °C; (g) PLLA, PE, PCL, and PEO at 30 °C; and (h) PLLA, PE, PCL, and PEO at 0 °C.CC BY · PubMed Central
Figure 7 PLOM intensity measurements corresponding to the micrographs of Figure 6 as a function of temperature indicating (a) melt and the progressive crystallization upon cooling of the (b) PLLA block, (c) PE block, (d) PCL block, and (e) PEO block for the tetrablock quarterpolymer PE187.1-b-PEO3715.1-b-PCL2610.4-b-PLLA197.6 (Q1), with colored data points and lines (green for PLLA, violet for PE, blue for PCL, and red for PEO) to follow the crystallization of each block. Empty data points represent the molten state of the sample.
Figure 7 PLOM intensity measurements corresponding to the micrographs of Figure 6 as a function of temperature indicating (a) melt and the progressive crystallization upon cooling of the (b) PLLA block, (c) PE block, (d) PCL block, and (e) PEO block for the tetrablock quarterpolymer PE187.1-b-PEO3715.1-b-PCL2610.4-b-PLLA197.6 (Q1), with colored data points and lines (green for PLLA, violet for PE, blue for PCL, and red for PEO) to follow the crystallization of each block. Empty data points represent the molten state of the sample.CC BY · PubMed Central
Figure 8 PLOM micrograph of the tetrablock quarterpolymer PE187.1-b-PEO3715.1-b-PCL2610.4-b-PLLA197.6 (Q1) (a) after isothermally crystallizing the sample at 88 °C during 40 min (a temperature at which only the PLLA block can crystallize) and (b) at room temperature after cooling the sample at 20 °C/min, allowing the crystallization of the other three blocks within the PLLA spherulites so that tetracrystalline spherulites are formed.
Figure 8 PLOM micrograph of the tetrablock quarterpolymer PE187.1-b-PEO3715.1-b-PCL2610.4-b-PLLA197.6 (Q1) (a) after isothermally crystallizing the sample at 88 °C during 40 min (a temperature at which only the PLLA block can crystallize) and (b) at room temperature after cooling the sample at 20 °C/min, allowing the crystallization of the other three blocks within the PLLA spherulites so that tetracrystalline spherulites are formed.CC BY · PubMed Central
Figure 9 PLOM intensity measurements as a function of temperature with micrographs of cooling from the melt at 20 °C/min at the indicated temperatures with colored arrows and data points indicating the crystallization of each block for the tetrablock quarterpolymer PE299.5-b-PEO268.8-b-PCL237.6-b-PLLA227.3 (Q2) (violet for PE, blue for PCL, and red for PEO).
Figure 9 PLOM intensity measurements as a function of temperature with micrographs of cooling from the melt at 20 °C/min at the indicated temperatures with colored arrows and data points indicating the crystallization of each block for the tetrablock quarterpolymer PE299.5-b-PEO268.8-b-PCL237.6-b-PLLA227.3 (Q2) (violet for PE, blue for PCL, and red for PEO).CC BY · PubMed Central
Figure 10 AFM micrographs of the tetrablock quarterpolymer PE187.1-b-PEO3715.1-b-PCL2610.4-b-PLLA197.6 (Q1) observed at 25 °C with close-ups of the indicated regions enclosed by a red box, applying two different thermal protocols: (a) cooling from the melt at 50 °C/min and (b) cooling from the melt at 20 °C/min.
Figure 10 AFM micrographs of the tetrablock quarterpolymer PE187.1-b-PEO3715.1-b-PCL2610.4-b-PLLA197.6 (Q1) observed at 25 °C with close-ups of the indicated regions enclosed by a red box, applying two different thermal protocols: (a) cooling from the melt at 50 °C/min and (b) cooling from the melt at 20 °C/min.CC BY · PubMed Central
Figure 11 AFM micrographs of the tetrablock quarterpolymer PE299.5-b-PEO268.8-b-PCL237.6-b-PLLA227.3 (Q2) observed at 25 °C with close-ups of the indicated regions enclosed by a red box, using 20 °C/min as the cooling rate in the preparation of the sample.
Figure 11 AFM micrographs of the tetrablock quarterpolymer PE299.5-b-PEO268.8-b-PCL237.6-b-PLLA227.3 (Q2) observed at 25 °C with close-ups of the indicated regions enclosed by a red box, using 20 °C/min as the cooling rate in the preparation of the sample.CC BY · PubMed Central
Figure 12 Lamellar thickness histogram obtained from the analysis of AFM micrographs shown in Figure 11.
Figure 12 Lamellar thickness histogram obtained from the analysis of AFM micrographs shown in Figure 11.CC BY · PubMed Central
Figure 13 Storage modulus and hardness values (penetration depth = 400 nm) for the homopolymers, the two tetrablock quarterpolymers, the precursors including PE7.1, and one triblock copolymer with high PLLA content.
Figure 13 Storage modulus and hardness values (penetration depth = 400 nm) for the homopolymers, the two tetrablock quarterpolymers, the precursors including PE7.1, and one triblock copolymer with high PLLA content.CC BY · PubMed Central

Verification

Claims the paper makes

0 Valid · 1 Not valid · 5 Not checked · 96 Own results and interpretations

31 more claims

Create a free account to see all 102 claims and every source verdict.

See all claims — free account
  • It may state two separate claims as one. 59
  • Probably not a substantial claim. 11
  • The quote only partly states this claim. 1

Create a free account to see these claims.

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

Each contradiction between two passages listed here was confirmed by an independent check.

3 of 3

Citations

Cites

Research works printed but not linked: 4

  1. Van Horn R. M., 2018, Polym. Cryst., 1, e10039
  2. Bao J., 2020, J. Polym. Sci., 1
  3. Palacios J. K., 2016, R. Soc. Chem. Adv., 6, 4739
  4. Palacios J. K., 2017, Macromolecules, 50, 7261

Cited by

See all 16

Metadata

Authors
Matxinandiarena, E., Múgica, A., Tercjak, A., Ladelta, V., Zapsas, G., Hadjichristidis, N., Cavallo, D., Flores, A., & Müller, A. J.
Affiliations
  • University of the Basque Country (ES)
  • King Abdullah University of Science and Technology (SA)
  • University of Genoa (IT)
  • Consejo Superior de Investigaciones Científicas (ES)
  • Ikerbasque (ES)
Corresponding author
Müller, Alejandro J.
Venue
Macromolecules
Published
2021-07-23
Volume
54
Issue
15
Pages
7244-7257
ISSN
  • 0024-9297 (ISSN-L)
  • 1520-5835
OpenAlex
W3185076943
Cited by
16
References
67
Citations by year
2026: 2 · 2025: 5 · 2024: 2 · 2023: 2 · 2022: 5
FWCI
0.80
Type
journal article
Language
en
Open access
Locations
  • Macromolecules (publishedVersion, cc-by)
  • PubMed Central (publishedVersion, cc-by)
  • PubMed (publishedVersion)
  • Communities in ADDI (University of the Basque Country) (submittedVersion, other-oa)
  • DIGITAL.CSIC (Spanish National Research Council (CSIC)) (submittedVersion)
  • Hispana (submittedVersion, other-oa)
  • CINECA IRIS Institutial Research Information System (University of Genoa) (submittedVersion)
  • King Abdullah University of Science and Technology Repository (King Abdullah University of Science and Technology) (submittedVersion, other-oa)
Funders
  • Ministerio de Econom??a y Competitividad (MAT2017-83014-C2-1-P, MAT2017-88382-P)
  • Eusko Jaurlaritza (IT1309-19)
  • Horizon 2020 Framework Programme (778092)
  • Abraham Lincoln Brigade Archives (u2020084441)
  • BIODEST project
Topics
  • Physical Sciences › Materials Science › Polymers and Plastics › Polymer crystallization and properties
  • Physical Sciences › Materials Science › Materials Chemistry › Block Copolymer Self-Assembly
  • Physical Sciences › Materials Science › Biomaterials › biodegradable polymer synthesis and properties
Keywords
sequential crystallization, block copolymers, poly(ethylene-alt-propylene), poly(ethylene oxide), polycaprolactone, poly(L-lactic acid), banded spherulites, lamellar thickness, melt miscibility, isotacticity, mechanical properties, storage modulus, hardness, nanoindentation, crystallization sequence

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

The claim verdicts this report counts are experimental: their accuracy is not yet measured.

A language model drew the claims from the paper on 2026-10-10, under version 3 of the claim definition (model deepseek-v4.1-flash, prompt extract-v3).

A second model labelled each claim on 2026-10-10 (model jev-1.13-20260917, definition revision gold-guideline-v0.2).

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.