Recycling of polyamide 12 based powders in the laser sintering process
The DOI matches its Crossref record; 4 of the 4 references it cites were found in a registry or an index.
Abstract
Purpose: The purpose of this paper is to investigate the polyamide 12 (PA12) powder properties deterioration in the laser sintering (LS) process and propose a methodology for more efficient powder recycling. The main goals are: to recommend a level of input PA2200 powder properties which could guarantee acceptable part quality in the LS process; and selection of the refresh rate in order to minimise the consumption of fresh material. Design/methodology/approach: The paper analyses the LS processing conditions and current recycling practices in relation to the deterioration or ageing of the PA12‐based powders. Samples of new and recycled grades of PA2200 powder were artificially aged in a temperature‐controlled oven and then tested using melt flow rate (MFR) indexer. Also, un‐sintered powder samples collected from different locations within various builds, and different LS machines (EOSINT P700 and Sinterstation® 2500 HiQ) were tested. Findings: The powder exposed at higher temperature and longer time experiences a much higher deterioration rate. The temperature and the time at which the un‐sintered material was exposed are the most influential parameters for the powder aging. It was confirmed that the MFR index is a very sensitive indicator of the changes in the powder properties and provides a relatively fast and inexpensive method of measuring the rate of the powder degradation because of the LS process. The powder located in the periphery and the top of a build has a higher MFR and therefore is less deteriorated. In contrast, powder located in the centre, or in the bottom of a long build has much lower MFR and therefore is less usable. Practical implications: Based on the findings, a methodology for powder recycling is proposed. It allows a better control of the input material properties, a consistent quality of the fabricated parts, and more efficient use of the LS material. Originality/value: The paper provides some useful information for the properties deterioration of PA12‐based powders (PA2200) in relation to the temperature and time at which the material is exposed in the LS.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Rapid Manufacturing: An Industrial Revolution for the Digital Age
(2005) · Wiley eBooks · doi:10.1002/0470033991 · Cited by 679
Kohan, M. I. (1995) · Medical Entomology and Zoology · Cited by 415
Effects of processing on microstructure and properties of SLS Nylon 12
Zarringhalam, H., Hopkinson, N., Kamperman, N. F., & de Vlieger, J. J. (2006) · Materials Science and Engineering: A · doi:10.1016/j.msea.2006.07.084 · Cited by 295 · cited 1×
“recycled powder thermal properties and molecular weight (Zarringhalam et al., 2006).”
BackgroundFaculty of Mechanical Engineering
Zvolenský, P. (2003) · Communications - Scientific letters of the University of Zilina · doi:10.26552/com.c.2003.3.17-26 · Cited by 161
Cited by
Polymers for 3D Printing and Customized Additive Manufacturing
Ligon, S. C., Liska, R., Stampfl, J., Gurr, M., & Mülhaupt, R. (2017) · Chemical Reviews · doi:10.1021/acs.chemrev.7b00074 · Cited by 3,741
3D printing with polymers: Challenges among expanding options and opportunities
Stansbury, J. W., & Idacavage, M. J. (2016) · Dental Materials · doi:10.1016/j.dental.2015.09.018 · Cited by 1,732
Towards energy and resource efficient manufacturing: A processes and systems approach
Duflou, J. R., Sutherland, J. W., Dornfeld, D., Herrmann, C., Jeswiet, J., Kara, S., Hauschild, M., & Kellens, K. (2012) · CIRP Annals · doi:10.1016/j.cirp.2012.05.002 · Cited by 1,164
Laser sintering of polyamides and other polymers
Goodridge, R. D., Tuck, C. J., & Hague, R. J. M. (2012) · Progress in Materials Science · doi:10.1016/j.pmatsci.2011.04.001 · Cited by 835
A Review of 3D Printing Technologies for Soft Polymer Materials
Zhou, L., Fu, J., & He, Y. (2020) · Advanced Functional Materials · doi:10.1002/adfm.202000187 · Cited by 713
Recent developments in polymers/polymer nanocomposites for additive manufacturing
Wu, H., Fahy, W. P., Kim, S., Kim, H., Zhao, N., Pilato, L., Kafi, A., Bateman, S., & Koo, J. H. (2020) · Progress in Materials Science · doi:10.1016/j.pmatsci.2020.100638 · Cited by 531
Sustainability of additive manufacturing: An overview on its energy demand and environmental impact
Peng, T., Kellens, K., Tang, R., Chen, C., & Chen, G. (2018) · Additive Manufacturing · doi:10.1016/j.addma.2018.04.022 · Cited by 426
3D printing: Principles and pharmaceutical applications of selective laser sintering
Awad, A., Fina, F., Goyanes, A., Gaisford, S., & Basit, A. W. (2020) · International Journal of Pharmaceutics · doi:10.1016/j.ijpharm.2020.119594 · Cited by 371
Sutton, A. T., Kriewall, C. S., Leu, M. C., & Newkirk, J. W. (2017) · Virtual and Physical Prototyping · doi:10.1080/17452759.2016.1250605 · Cited by 354
Kellens, K., Baumers, M., Gutowski, T. G., Flanagan, W., Lifset, R., & Duflou, J. R. (2017) · Journal of Industrial Ecology · doi:10.1111/jiec.12629 · Cited by 310
Chatham, C. A., Long, T. E., & Williams, C. B. (2019) · Progress in Polymer Science · doi:10.1016/j.progpolymsci.2019.03.003 · Cited by 305
Addressing sustainability in research on distributed production: an integrated literature review
Kohtala, C. (2015) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2014.09.039 · Cited by 290
Design for sustainable additive manufacturing: A review
Hegab, H., Khanna, N., Monib, N., & Salem, A. (2023) · Sustainable Materials and Technologies · doi:10.1016/j.susmat.2023.e00576 · Cited by 289
Charoo, N. A., Barakh Ali, S. F., Mohamed, E. M., Kuttolamadom, M. A., Ozkan, T., Khan, M. A., & Rahman, Z. (2020) · Drug Development and Industrial Pharmacy · doi:10.1080/03639045.2020.1764027 · Cited by 268
Advances in selective laser sintering of polymers
Han, W., Kong, L., & Xu, M. (2022) · International Journal of Extreme Manufacturing · doi:10.1088/2631-7990/ac9096 · Cited by 254
Polymer recycling in an open-source additive manufacturing context: Mechanical issues
Cruz Sanchez, F. A., Boudaoud, H., Hoppe, S., & Camargo, M. (2017) · Additive Manufacturing · doi:10.1016/j.addma.2017.05.013 · Cited by 243
Research needs and recommendations on environmental implications of additive manufacturing
Rejeski, D., Zhao, F., & Huang, Y. (2018) · Additive Manufacturing · doi:10.1016/j.addma.2017.10.019 · Cited by 233
Advances in powder bed fusion 3D printing in drug delivery and healthcare
Awad, A., Fina, F., Goyanes, A., Gaisford, S., & Basit, A. W. (2021) · Advanced Drug Delivery Reviews · doi:10.1016/j.addr.2021.04.025 · Cited by 232
Characterization of polyamide powders for determination of laser sintering processability
Verbelen, L., Dadbakhsh, S., Van den Eynde, M., Kruth, J.-P., Goderis, B., & Van Puyvelde, P. (2016) · European Polymer Journal · doi:10.1016/j.eurpolymj.2015.12.014 · Cited by 208
Effect of PA12 powder reuse on coalescence behaviour and microstructure of SLS parts
Dadbakhsh, S., Verbelen, L., Verkinderen, O., Strobbe, D., Van Puyvelde, P., & Kruth, J.-P. (2017) · European Polymer Journal · doi:10.1016/j.eurpolymj.2017.05.014 · Cited by 204
Liu, W., Liu, X., Liu, Y., Wang, J., Evans, S., & Yang, M. (2023) · Sustainability · doi:10.3390/su15043827 · Cited by 27
“The literature suggests that coming to the conclusion that AM processes have lower environmental impacts than traditional manufacturing is biased, as data on total waste are missing, and uncertainties exist [22,30].”
Background
Metadata
- Authors
- Dotchev, K., & Yusoff, W.
- Venue
- Rapid Prototyping Journal
- Publisher
- Emerald
- Published
- 2009-05-29
- Volume
- 15
- Issue
- 3
- Pages
- 192-203
- ISSN
- 1355-2546 (ISSN-L)
- OpenAlex
- W2084022694
- Cited by
- 229
- References
- 4
- FWCI
- 8.13
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.