CoChat

Quantifying the fragmentation of polypropylene upon exposure to accelerated weathering

Open access
Meides, Nora, Mauel, Anika, Menzel, Teresa, Altstädt, Volker, Ruckdäschel, Holger, Senker, Jürgen, Strohriegl, Peter · 2022 · Microplastics and Nanoplastics
Cited by 68

The DOI matches its Crossref record; 12 of the 12 references it cites were found in a registry or an index.

Abstract

Polymers are omnipresent in our everyday lives. For specific applications, their properties can be extensively modified by various types of additives, e.g., processing stabilizers, antioxidants, UV-stabilizers, flame retardants, and plasticizers. While several additives are nowadays considered to be toxic or persistent in the environment, quantitative data characterizing plastic fragmentation and microplastic formation have not yet been discussed in detail. Here, we present a long-term, laboratory-controlled accelerated weathering study on polypropylene (PP) particles with and without processing stabilizers. We were able to identify the stabilizers as Irgafos® 168, and Irganox® 1010. For both PP sample sets, we monitored the degradation using a combination of various analytical methods, such as gel permeation chromatography, particle size distributions, scanning electron microscopy, solid-state 13 C magic-angle spinning NMR and liquid-state 1 H, 13 C, 31 P NMR spectroscopy, differential scanning calorimetry and matrix-assisted laser desorption ionization time of flight mass spectrometry. The stabilizers prevent degradation by simulated solar radiation for about 350 h. Then, degradation sets in rapidly, leading to an exponential decrease in molecular weight and particle size, accompanied by an increase in crystallinity and the formation of oxygen-containing functional groups. After 3200 h, representing approximately 2 years of outdoor weathering, both PP samples exhibit comparable characteristics and sizes, regardless if a stabilizer was initially present. During degradation, an extremely large number of 100,000 daughter particles (4 µm) are formed and released from one MP particle of 192 µm diameter. Their physical properties and chemical composition have largely changed, resulting in a very low molecular weight and a hydrophilic character. These particles no longer resemble pristine PP. We thus expect them to be more prone to biodegradation compared to the starting material.

Overview

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Integrity signals

Registry

Crossref · 10.1186/s43591-022-00042-2

Cites

12 of 12 references verified0 citation errors · 0 not checkable

Statistics

Verification

Claims the paper makes

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

The self-check needs the paper’s full text.

Citations

Cites

Show all 12 references

Research works printed but not linked: 48

  1. Bishop G, Styles D, Lens PNL. Recycling of European plastic is a pathway for plastic debris in the ocean. Environ Int. 2020;142: 105893. · DOI · Paper page
  2. Chen HL, Nath TK, Chong S, Foo V, Gibbins C, Lechner AM. The plastic waste problem in Malaysia: management, recycling and disposal of local and global plastic waste. SN Applied Sciences. 2021;3(4):1–15. · DOI · Paper page
  3. Andrady AL. Microplastics in the marine environment. Mar Pollut Bull. 2011;62(8):1596–605. · DOI · Paper page
  4. Meides N, Menzel T, Poetzschner B, Löder MGJ, Mansfeld U, Strohriegl P, et al. Reconstructing the Environmental Degradation of Polystyrene by Accelerated Weathering. Environ Sci Technol. 2021;55(12):7930–8. · DOI · Paper page
  5. Wu X, Liu P, Shi H, Wang H, Huang H, Shi Y, et al. Photo aging and fragmentation of polypropylene food packaging materials in artificial seawater. Water Research. 2021;188:116456. · DOI · Paper page
  6. Duan J, Bolan N, Li Y, Ding S, Atugoda T, Vithanage M, et al. Weathering of microplastics and interaction with other coexisting constituents in terrestrial and aquatic environments. Water Research. 2021;196:117011. · DOI · Paper page
  7. Kumar M, Xiong X, He M, Tsang DCW, Gupta J, Khan E, et al. Microplastics as pollutants in agricultural soils. Environ Pollut. 2020;265(Pt A): 114980. · DOI · Paper page
  8. Zweifel H. Principles of oxidative degradation. In: Stabilization of Polymeric Materials. Springer; 1998. p. 1–40. · DOI
  9. Kirstein IV, Kirmizi S, Wichels A, Garin-Fernandez A, Erler R, Löder M et al. Dangerous hitchhikers? Evidence for potentially pathogenic Vibrio spp. on microplastic particles. Marine Environmental Research 2016; 120:1–8. Available from: URL: https://www.sciencedirect.com/science/article/pii/S014111361630112X. · DOI · Paper page
  10. Imhof HK, Ivleva NP, Schmid J, Niessner R, Laforsch C. Contamination of beach sediments of a subalpine lake with microplastic particles. Curr Biol. 2013;23(19):R867–8.
  11. Imhof HK, Rusek J, Thiel M, Wolinska J, Laforsch C. Do microplastic particles affect Daphnia magna at the morphological, life history and molecular level? PLoS ONE. 2017;12(11): e0187590. · DOI · Paper page
  12. Hwang J, Choi D, Han S, Choi J, Hong J. An assessment of the toxicity of polypropylene microplastics in human derived cells. Sci Total Environ. 2019;684:657–69. · DOI · Paper page
  13. Engler RE. The Complex Interaction between Marine Debris and Toxic Chemicals in the Ocean. Environ Sci Technol. 2012;46(22):12302–15. · DOI · Paper page
  14. Barrick A, Champeau O, Chatel A, Manier N, Northcott G, Tremblay LA. Plastic additives: challenges in ecotox hazard assessment. PeerJ. 2021;9: e11300. · DOI · Paper page
  15. Blázquez-Blázquez E, Cerrada ML, Benavente R, Pérez E. Identification of Additives in Polypropylene and Their Degradation under Solar Exposure Studied by Gas Chromatography-Mass Spectrometry. ACS Omega. 2020;5(16):9055–63. · DOI
  16. Biale G, La Nasa J, Mattonai M, Corti A, Vinciguerra V, Castelvetro V, et al. A systematic study on the degradation products generated from artificially aged microplastics. Polymers. 2021;13(12):1997. · DOI
  17. Shi Y, Qin J, Tao Y, Jie G, Wang J. Natural weathering severity of typical coastal environment on polystyrene: Experiment and modeling. Polym Testing. 2019;76:138–45. · DOI
  18. Grause G, Chien M-F, Inoue C. Changes during the weathering of polyolefins. Polymer degradation and stability 2020:109364. · DOI · Paper page
  19. Da Costa JP, Nunes AR, Santos PSM, Girao AV, Duarte AC, Rocha-Santos T. Degradation of polyethylene microplastics in seawater: Insights into the environmental degradation of polymers. Journal of Environmental Science and Health, Part A. 2018;53(9):866–75. · DOI · Paper page
  20. Ojeda T, Freitas A, Birck K, Dalmolin E, Jacques R, Bento F, et al. Degradability of linear polyolefins under natural weathering. Polym Degrad Stab. 2011;96(4):703–7. · DOI · Paper page
  21. Khelassi A, Belhaneche-Bensemra N. Investigation of pro-oxidant agents’ effects on the ageing of polypropylene bags. Int J Environ Stud. 2020;77(2):264–74. · DOI
  22. Andrady AL, Koongolla B. Degradation and Fragmentation of Microplastics. In: Plastics and the Ocean. John Wiley & Sons, Ltd; 2022. p. 227–68. · DOI
  23. Efimova I, Bagaeva M, Bagaev A, Kileso A, Chubarenko IP. Secondary Microplastics Generation in the Sea Swash Zone With Coarse Bottom Sediments: Laboratory Experiments. Front Mar Sci. 2018;5:313. · DOI · Paper page
  24. Al-Malaika S. Oxidative degradation and stabilisation of polymers. Int Mater Rev. 2003;48(3):165–85. · DOI
  25. Carlsson DJ, Wiles DM. The Photooxidative Degradation of Polypropylene. Part I. Photooxidation and Photoinitiation Processes. Journal of Macromolecular Science, Part C: Polymer Reviews 1976; 14(1):65–106. · DOI · Paper page
  26. Allen NS, Chirinos-Padron A, Henman TJ. Photoinitiated oxidation of polypropylene: a review. Prog Org Coat. 1985;13(2):97–122. · doi:10.1016/0033-0655(85)80020-0
  27. Mattsson K, Björkroth F, Karlsson T, Hassellöv M. Nanofragmentation of Expanded Polystyrene Under Simulated Environmental Weathering (Thermooxidative Degradation and Hydrodynamic Turbulence). Front Mar Sci. 2021;7:1252. · DOI
  28. Born MP, Brüll C. From model to nature - A review on the transferability of marine (micro-) plastic fragmentation studies. Sci Total Environ. 2022;811: 151389. · DOI
  29. Johnson RL, Schmidt-Rohr K. Quantitative solid-state 13C NMR with signal enhancement by multiple cross polarization. J Magn Reson. 2014;239:44–9. · DOI · Paper page
  30. Mauel A, Pötzschner B, Meides N, Siegel R, Strohriegl P, Senker J. Quantification of photooxidative defects in weathered microplastics using 13 C multiCP NMR spectroscopy. RSC Adv. 2022;12(18):10875–85. · DOI
  31. Canopoli L, Coulon F, Wagland ST. Degradation of excavated polyethylene and polypropylene waste from landfill. Sci Total Environ. 2020;698: 134125. · DOI · Paper page
  32. Dong M, Zhang Q, Xing X, Chen W, She Z, Luo Z. Raman spectra and surface changes of microplastics weathered under natural environments. Sci Total Environ. 2020;739: 139990. · DOI · Paper page
  33. Fernández-González V, Andrade-Garda JM, López-Mahía P, Muniategui-Lorenzo S. Impact of weathering on the chemical identification of microplastics from usual packaging polymers in the marine environment. Anal Chim Acta. 2021;1142:179–88. · DOI · Paper page
  34. Veeman WS. Carbon-13 chemical shift anisotropy. Prog Nucl Magn Reson Spectrosc. 1984;16:193–235. · doi:10.1016/0079-6565(84)80006-0
  35. Schwarzinger C, Gabriel S, Beißmann S, Buchberger W. Quantitative Analysis of Polymer Additives with MALDI-TOF MS Using an Internal Standard Approach. J Am Soc Mass Spectrom. 2012;23(6):1120–5. · doi:10.1007/s13361-012-0367-1
  36. Fouyer K, Lavastre O, Rondeau D. Direct monitoring of the role played by a stabilizer in a solid sample of polymer using direct analysis in real time mass spectrometry: the case of Irgafos 168 in polyethylene. Anal Chem. 2012;84(20):8642–9. · doi:10.1021/ac301759q
  37. Maier R-D, Schiller M. Handbuch Kunststoff Additive. Carl Hanser Verlag GmbH Co KG; 2016. · doi:10.3139/9783446432918.fm
  38. Hronský V, Koval'aková M, Vrábel P, Uhrínová M, Olčák D. Estimation of the Degree of Crystallinity of Partially Crystalline Polypropylenes Using 13 C NMR. Acta Physica Polonica, A 2014; 125(6). · doi:10.12693/aphyspola.126.409
  39. Li J, Yang R, Yu J, Liu Y. Natural photo-aging degradation of polypropylene nanocomposites. Polym Degrad Stab. 2008;93(1):84–9. · doi:10.1016/j.polymdegradstab.2007.10.022
  40. Craig IH, White JR, Kin PC. Crystallization and chemi-crystallization of recycled photo-degraded polypropylene. Polymer. 2005;46(2):505–12. · doi:10.1016/j.polymer.2004.11.019
  41. Mowery DM, Assink RA, Derzon DK, Klamo SB, Clough RL, Bernstein R. Solid-state 13C NMR investigation of the oxidative degradation of selectively labeled polypropylene by thermal aging and γ-irradiation. Macromolecules. 2005;38(12):5035–46. · DOI
  42. Mowery DM, Clough RL, Assink RA. Identification of oxidation products in selectively labeled polypropylene with solid-state 13C NMR techniques. Macromolecules. 2007;40(10):3615–23. · DOI
  43. Wool RP. Self-healing materials: a review. Soft Matter. 2008;4(3):400–18. · DOI · Paper page
  44. Rajakumar K, Sarasvathy V, Thamarai Chelvan A, Chitra R, Vijayakumar CT. Natural Weathering Studies of Polypropylene. J Polym Environ. 2009;17(3):191. · DOI · Paper page
  45. Xu C, Zhang B, Gu C, Shen C, Yin S, Aamir M et al. Are we underestimating the sources of microplastic pollution in terrestrial environment? Journal of Hazardous Materials 2020:123228. · DOI · Paper page
  46. Völkl M, Jérôme V, Weig A, Jasinski J, Meides N, Strohriegl P, et al. Pristine and artificially-aged polystyrene microplastic particles differ in regard to cellular response. J Hazard Mater. 2022;435: 128955. · DOI
  47. Yu X, Lang M, Huang D, Yang C, Ouyang Z, Guo X. Photo-transformation of microplastics and its toxicity to Caco-2 cells. Sci Total Environ. 2022;806:150954. · DOI
  48. Bridson JH, Gaugler EC, Smith DA, Northcott GL, Gaw S. Leaching and extraction of additives from plastic pollution to inform environmental risk: A multidisciplinary review of analytical approaches. Journal of Hazardous Materials 2021; 414:125571. Available from: https://www.sciencedirect.com/science/article/pii/S0304389421005343. · DOI · Paper page

Cited by

See all 68

Metadata

Authors
Meides, N., Mauel, A., Menzel, T., Altstädt, V., Ruckdäschel, H., Senker, J., & Strohriegl, P.
Venue
Microplastics and Nanoplastics
Published
2022-09-21
Volume
2
Issue
1
ISSN
2662-4966 (ISSN-L)
OpenAlex
W4296713570
Cited by
68
References
12
FWCI
2.41
Type
journal article
Language
en
Open access
gold
Licence
Funders
Universität Bayreuth

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

How to cite

Cite CoChat for the checks on this page, and the paper for its own findings.

This page
CoChat. (2026). Citation check: Quantifying the fragmentation of polypropylene upon exposure to accelerated weathering. https://app.cochat.ai/papers/10.1186/s43591-022-00042-2
The paper
Meides, N., Mauel, A., Menzel, T., Altstädt, V., Ruckdäschel, H., Senker, J., & Strohriegl, P. (2022). Quantifying the fragmentation of polypropylene upon exposure to accelerated weathering. Microplastics and Nanoplastics. https://doi.org/10.1186/s43591-022-00042-2

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.