Accelerated in vitro degradation properties of polylactic acid/phosphate glass fibre composites
The DOI matches its Crossref record; 41 of the 41 references it cites were found in a registry or an index.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“This plateau in wet weight of the scaffolds was a result of the balance between water uptake and mass loss [38].”
From In vitro degradation and mechanical properties of PLA-PCL copolymer unit cell scaffolds generated by two-photon polymerization (2016) · cites this paper as [38]
In the citing paper
“In contrast, a second phase of increase in the scaffold weights was seen after 25 and 6 d of degradation at 50 and 65 °C respectively, which was a consequence of imbalance between water uptake and mass loss (i.e.mass loss due to hydrolytic degradation became dominant) [38].”
From In vitro degradation and mechanical properties of PLA-PCL copolymer unit cell scaffolds generated by two-photon polymerization (2016) · cites this paper as [38]
In the citing paper
“Therefore, validated accelerated degradation studies are an attractive research tool [38] to explore the influence of the physico-chemical factors as well as other influences such as initiators and polymer blends.”
From In vitro degradation and mechanical properties of PLA-PCL copolymer unit cell scaffolds generated by two-photon polymerization (2016) · cites this paper as [38]
In the citing paper
“Arrhenius relation has been conducted for the change in several parameters of biodegradable polymers such as molecular weight, breaking strength, viscosity and mass loss [34,38,49,71,72].”
From In vitro degradation and mechanical properties of PLA-PCL copolymer unit cell scaffolds generated by two-photon polymerization (2016) · cites this paper as [38]
Citations
Cites
Li, S. M., Garreau, H., & Vert, M. (1990) · Journal of Materials Science: Materials in Medicine · doi:10.1007/bf00700871 · Cited by 733
Li, S. (1999) · Journal of Biomedical Materials Research · doi:10.1002/(sici)1097-4636(1999)48:3<246::aid-jbm7>3.0.co;2-x · Cited by 671
Degradability of Polymers for Implantable Biomedical Devices
Lyu, S., & Untereker, D. (2009) · International Journal of Molecular Sciences · doi:10.3390/ijms10094033 · Cited by 538
Li, S., Garreau, H., & Vert, M. (1990) · Journal of Materials Science: Materials in Medicine · doi:10.1007/bf00701077 · Cited by 488
Orthopaedic applications for PLA‐PGA biodegradable polymers
Athanasiou, K., Agrawal, C., Barber, F., & Burkhart, S. (1998) · Arthroscopy · doi:10.1016/s0749-8063(98)70099-4 · Cited by 487
Further investigations on the hydrolytic degradation of poly (DL-lactide)
Li, S., & McCarthy, S. (1999) · Biomaterials · doi:10.1016/s0142-9612(97)00226-3 · Cited by 301
Hakkarainen, M., Albertsson, A.-C., & Karlsson, S. (1996) · Polymer Degradation and Stability · doi:10.1016/0141-3910(96)00009-2 · Cited by 249
Kinetics and Time−Temperature Equivalence of Polymer Degradation
Lyu, Schley, J., Loy, B., Lind, D., Hobot, C., Sparer, R., & Untereker, D. (2007) · Biomacromolecules · doi:10.1021/bm070313n · Cited by 237
The use of accelerated ageing procedures to predict the long term strength of GRC composites
Litherland, K. L., Oakley, D. R., & Proctor, B. A. (1981) · Cement and Concrete Research · doi:10.1016/0008-8846(81)90117-4 · Cited by 235
Biodegradation of poly(l-lactide)
Tokiwa, Y., & Jarerat, A. (2004) · Biotechnology Letters · doi:10.1023/b:bile.0000025927.31028.e3 · Cited by 191
Degradation of poly-L-lactide. Part 1: in vitro and in vivo physiological temperature degradation
Weir, N. A., Buchanan, F. J., Orr, J. F., & Dickson, G. R. (2004) · Proceedings of the Institution of Mechanical Engineers, Part H: Journal of Engineering in Medicine · doi:10.1243/0954411041932782 · Cited by 182
Degradation of poly-L-lactide. Part 2: increased temperature accelerated degradation
Weir, N. A., Buchanan, F. J., Orr, J. F., Farrar, D. F., & Dickson, G. R. (2004) · Proceedings of the Institution of Mechanical Engineers, Part H: Journal of Engineering in Medicine · doi:10.1243/0954411041932809 · Cited by 171
Effects of Temperature and pH on the Degradation of Poly(lactic acid) Brushes
Xu, L., Crawford, K., & Gorman, C. B. (2011) · Macromolecules · doi:10.1021/ma2000948 · Cited by 167
Fundamentals of Fibre Reinforced Composite Materials
Bunsell, A. R., & Renard, J. (2005) · CRC Press eBooks · doi:10.1201/9781420056969 · Cited by 167
Absorbable polyglycolide devices in trauma and bone surgery
Ashammakhi, N., & Rokkanen, P. (1997) · Biomaterials · doi:10.1016/s0142-9612(96)00107-x · Cited by 166
Fundamentals of Fibre Reinforced Composite Materials
Bunsell, A. R., & Renard, J. (2005) · Materials Today · doi:10.1016/s1369-7021(05)71085-3 · Cited by 139
Claes, L. E., Ignatius, A. A., Rehm, K. E., & Scholz, C. (1996) · Biomaterials · doi:10.1016/0142-9612(95)00327-4 · Cited by 123
Elevated temperature degradation of a 50:50 copolymer of PLA-PGA
Agrawal, C. M., Huang, D., Schmitz, J. P., & Athanasiou, K. A. (1997) · Tissue Engineering · doi:10.1089/ten.1997.3.345 · Cited by 120
Navarro, M., Ginebra, M., Planell, J. A., Barrias, C. C., & Barbosa, M. A. (2005) · Acta Biomaterialia · doi:10.1016/j.actbio.2005.03.004 · Cited by 119
Antheunis, H., van der Meer, J.-C., de Geus, M., Heise, A., & Koning, C. E. (2010) · Biomacromolecules · doi:10.1021/bm100125b · Cited by 116
In vitro hydrolysis of poly(l-lactide) crystalline residues as extended-chain crystallites
Tsuji, H., & Ikarashi, K. (2004) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2004.03.004 · Cited by 96
Yuan, X., Mak, A. F. T., & Yao, K. (2002) · Polymer Degradation and Stability · doi:10.1016/s0141-3910(01)00203-8 · Cited by 88
On the determination of polymer crystallinity for a thermoplastic PPS composite by thermal analysis
Lee, T. H., Boey, F. Y. C., & Khor, K. A. (1995) · Composites Science and Technology · doi:10.1016/0266-3538(94)00070-0 · Cited by 79
Felfel, R. M., Ahmed, I., Parsons, A. J., Haque, P., Walker, G. S., & Rudd, C. D. (2010) · Journal of Biomaterials Applications · doi:10.1177/0885328210384532 · Cited by 78
Self-citationDeng, M., Zhou, J., Chen, G., Burkley, D., Xu, Y., Jamiolkowski, D., & Barbolt, T. (2005) · Biomaterials · doi:10.1016/j.biomaterials.2004.09.067 · Cited by 75
Han, X., Pan, J., Buchanan, F., Weir, N. A., & Farrar, D. F. (2010) · Acta Biomaterialia · doi:10.1016/j.actbio.2010.05.015 · Cited by 72
Accelerated hydrolytic degradation of Poly(l-lactide)/Poly(d-lactide) stereocomplex up to late stage
Tsuji, H., & Tsuruno, T. (2010) · Polymer Degradation and Stability · doi:10.1016/j.polymdegradstab.2010.01.008 · Cited by 67
E-Glass/Vinylester Composites in Aqueous Environments: Effects on Short-Beam Shear Strength
Karbhari, V. M. (2004) · Journal of Composites for Construction · doi:10.1061/(asce)1090-0268(2004)8:2(148 · Cited by 66
Degradation rate of Bioresorbable Materials: Prediction and Evaluation
Buchanan, F. (2008) · Cited by 64
Tsuji, H., & Ikarashi, K. (2004) · Biomacromolecules · doi:10.1021/bm034523l · Cited by 62
Felfel, R. M., Ahmed, I., Parsons, A. J., Walker, G. S., & Rudd, C. D. (2011) · Journal of the mechanical behavior of biomedical materials/Journal of mechanical behavior of biomedical materials · doi:10.1016/j.jmbbm.2011.05.016 · Cited by 57
Self-citationLee, W.-K., Iwata, T., & Gardella, J. A. (2005) · Langmuir · doi:10.1021/la051137b · Cited by 51
The influence of temperature on the degradation rate of lactosorb copolymer
Pietrzak, W. S., Kumar, M., & Eppley, B. L. (2003) · Journal of Craniofacial Surgery · doi:10.1097/00001665-200303000-00008 · Cited by 44
A study on in vitro degradation behavior of a poly(glycolide-co-l-lactide) monofilament
Deng, M., Chen, G., Burkley, D., Zhou, J., Jamiolkowski, D., Xu, Y., & Vetrecin, R. (2008) · Acta Biomaterialia · doi:10.1016/j.actbio.2008.03.011 · Cited by 41
Kline, G. M., & Axilrod, B. M. (1936) · Industrial & Engineering Chemistry · doi:10.1021/ie50322a010 · Cited by 25
Straub, A., Slivka, M. A., & SCHWARTZ, P. L. (1997) · Composites Science and Technology · doi:10.1016/s0266-3538(96)00146-7 · Cited by 23
The Design and Analysis of Laminated Degradable Composite Bone Plates for Fracture Fixation
Zimmerman, M. C., Alexander, H., Parsons, J. R., & Bajpai, P. K. (1991) · ACS symposium series · doi:10.1021/bk-1991-0457.ch010 · Cited by 22
Chin, J. W., Hughes, W. P., & Signor, A. W. (2001) · Cited by 18
Degradation Properties of Co-Continuous Calcium−Phosphate−Polyester Composites
Ehrenfried, L. M., Farrar, D. F., & Cameron, R. E. (2009) · Biomacromolecules · doi:10.1021/bm900397d · Cited by 17
Design Optimisation of Carbon Fibre Epoxy Composites Operating in Humid Atmospheres
Korkees, F. (2010) · Cited by 6
Cited by
Biodegradable Polymers as the Pivotal Player in the Design of Tissue Engineering Scaffolds
Zhang, F., & King, M. W. (2020) · Advanced Healthcare Materials · doi:10.1002/adhm.201901358 · Cited by 309
3D printed bone tissue regenerative PLA/HA scaffolds with comprehensive performance optimizations
Zhang, B., Wang, L., Song, P., Pei, X., Sun, H., Wu, L., Zhou, C., Wang, K., Fan, Y., & Zhang, X. (2021) · Materials & Design · doi:10.1016/j.matdes.2021.109490 · Cited by 285
3D-printed biodegradable gyroid scaffolds for tissue engineering applications
Germain, L., Fuentes, C. A., van Vuure, A. W., des Rieux, A., & Dupont-Gillain, C. (2018) · Materials & Design · doi:10.1016/j.matdes.2018.04.037 · Cited by 127
Zhao, C., Wu, H., Ni, J., Zhang, S., & Zhang, X. (2017) · Composites Science and Technology · doi:10.1016/j.compscitech.2017.04.037 · Cited by 114
Preparation and properties of polylactic acid-tea polyphenol-chitosan composite membranes
Ye, J., Wang, S., Lan, W., Qin, W., & Liu, Y. (2018) · International Journal of Biological Macromolecules · doi:10.1016/j.ijbiomac.2018.05.080 · Cited by 112
“The density of the composite membrane reduces significantly with the addition of TP and CS; the interaction between the three materials and the intense agitation destroy the original compact structure of the PLA membrane [24,36].”
Background
Metadata
- Authors
- Felfel, R. M., Hossain, K. M. Z., Parsons, A. J., Rudd, C. D., & Ahmed, I.
- Affiliations
- University of Nottingham (GB)
- Corresponding author
- Felfel, Reda M.
- Venue
- Journal of Materials Science
- Published
- 2015-03-11
- Volume
- 50
- Issue
- 11
- Pages
- 3942-3955
- ISSN
- 0022-2461 (ISSN-L)
- 1573-4803
- OpenAlex
- W2049467772
- Cited by
- 61
- References
- 41
- Citations by year
- 2026: 5 · 2025: 5 · 2024: 7 · 2023: 3 · 2022: 3 · 2021: 12 · 2020: 7 · 2019: 5 · 2018: 6 · 2017: 5 · 2016: 3
- FWCI
- 1.69
- Type
- journal article
- Language
- en
- Open access
- closed
- Licence
- www.springer.com/tdm (tdm)
- Locations
- Journal of Materials Science (publishedVersion)
- ResearchOnline at James Cook University (James Cook University) (submittedVersion)
- Funders
- Engineering and Physical Sciences Research Council (EP/K029592/1)
- Topics
- Physical Sciences › Materials Science › Biomaterials › biodegradable polymer synthesis and properties
- Physical Sciences › Engineering › Biomedical Engineering › Bone Tissue Engineering Materials
- Physical Sciences › Materials Science › Biomaterials › Magnesium Alloys: Properties and Applications
- Keywords
- polylactic acid, phosphate glass fiber, biodegradable composites, in vitro degradation, phosphate buffered saline, crystallinity, flexural strength, molecular weight distribution, activation energy of degradation, Arrhenius kinetics, unidirectional fibers, tipping points
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.