Substrate strain tunes operando geometric distortion and oxygen reduction activity of CuN2C2 single-atom sites
Open accessThe DOI matches its Crossref record; 51 of the 51 references it cites were found in a registry or an index.
Abstract
Single-atom catalysts are becoming increasingly significant to numerous energy conversion reactions. However, their rational design and construction remain quite challenging due to the poorly understood structure–function relationship. Here we demonstrate the dynamic behavior of CuN 2 C 2 site during operando oxygen reduction reaction, revealing a substrate-strain tuned geometry distortion of active sites and its correlation with the activity. Our best CuN 2 C 2 site, on carbon nanotube with 8 nm diameter, delivers a sixfold activity promotion relative to graphene. Density functional theory and X-ray absorption spectroscopy reveal that reasonable substrate strain allows the optimized distortion, where Cu bonds strongly with the oxygen species while maintaining intimate coordination with C/N atoms. The optimized distortion facilitates the electron transfer from Cu to the adsorbed O, greatly boosting the oxygen reduction activity. This work uncovers the structure–function relationship of single-atom catalysts in terms of carbon substrate, and provides guidance to their future design and activity promotion.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Grimme, S., Antony, J., Ehrlich, S., & Krieg, H. (2010) · The Journal of Chemical Physics · doi:10.1063/1.3382344 · Cited by 59,686
Separable dual-space Gaussian pseudopotentials
Goedecker, S., Teter, M., & Hutter, J. (1996) · Physical Review B · doi:10.1103/physrevb.54.1703 · Cited by 7,479
VandeVondele, J., Krack, M., Mohamed, F., Parrinello, M., Chassaing, T., & Hutter, J. (2005) · Computer Physics Communications · doi:10.1016/j.cpc.2004.12.014 · Cited by 5,822
Chemistry of Single-Walled Carbon Nanotubes
Niyogi, S., Hamon, M. A., Hu, H., Zhao, B., Bhowmik, P., Sen, R., Itkis, M. E., & Haddon, R. C. (2002) · Accounts of Chemical Research · doi:10.1021/ar010155r · Cited by 1,556
Jiang, H., Gu, J., Zheng, X., Liu, M., Qiu, X., Wang, L., Li, W., Chen, Z., Ji, X., & Li, J. (2019) · Energy & Environmental Science · doi:10.1039/c8ee03276a · Cited by 1,399
Isolated Diatomic Ni‐Fe Metal–Nitrogen Sites for Synergistic Electroreduction of CO2
Ren, W., Tan, X., Yang, W., Jia, C., Xu, S., Wang, K., Smith, S. C., & Zhao, C. (2019) · Angewandte Chemie International Edition · doi:10.1002/anie.201901575 · Cited by 1,036
Isolated Ni single atoms in graphene nanosheets for high-performance CO2 reduction
Jiang, K., Siahrostami, S., Zheng, T., Hu, Y., Hwang, S., Stavitski, E., Peng, Y., Dynes, J., Gangisetty, M., Su, D., et al. (2018) · Energy & Environmental Science · doi:10.1039/c7ee03245e · Cited by 1,024
Zhang, J., Zhao, Y., Chen, C., Huang, Y.-C., Dong, C.-L., Chen, C.-J., Liu, R.-S., Wang, C., Yan, K., Li, Y., et al. (2019) · Journal of the American Chemical Society · doi:10.1021/jacs.9b09352 · Cited by 989
Chen, Y., Ji, S., Zhao, S., Chen, W., Dong, J., Cheong, W.-C., Shen, R., Wen, X., Zheng, L., Rykov, A. I., et al. (2018) · Nature Communications · doi:10.1038/s41467-018-07850-2 · Cited by 977
Chemistry of the Fullerenes: The Manifestation of Strain in a Class of Continuous Aromatic Molecules
Haddon, R. C. (1993) · Science · doi:10.1126/science.261.5128.1545 · Cited by 932
Jiao, L., Wan, G., Zhang, R., Zhou, H., Yu, S., & Jiang, H. (2018) · Angewandte Chemie International Edition · doi:10.1002/anie.201803262 · Cited by 860
Sun, Y., Silvioli, L., Sahraie, N. R., Ju, W., Li, J., Zitolo, A., Li, S., Bagger, A., Arnarson, L., Wang, X., et al. (2019) · Journal of the American Chemical Society · doi:10.1021/jacs.9b05576 · Cited by 825
Jiang, R., Li, L., Sheng, T., Hu, G., Chen, Y., & Wang, L. (2018) · Journal of the American Chemical Society · doi:10.1021/jacs.8b07294 · Cited by 797
Han, X., Ling, X., Yu, D., Xie, D., Li, L., Peng, S., Zhong, C., Zhao, N., Deng, Y., & Hu, W. (2019) · Advanced Materials · doi:10.1002/adma.201905622 · Cited by 741
Gao, J., Yang, H. B., Huang, X., Hung, S.-F., Cai, W., Jia, C., Miao, S., Chen, H. M., Yang, X., Huang, Y., et al. (2020) · Chem · doi:10.1016/j.chempr.2019.12.008 · Cited by 734
Li, Z., Chen, Y., Ji, S., Tang, Y., Chen, W., Li, A., Zhao, J., Xiong, Y., Wu, Y., Gong, Y., et al. (2020) · Nature Chemistry · doi:10.1038/s41557-020-0473-9 · Cited by 715
Self-citationMun, Y., Lee, S., Kim, K., Kim, S., Lee, S., Han, J. W., & Lee, J. (2019) · Journal of the American Chemical Society · doi:10.1021/jacs.8b13543 · Cited by 710
Cao, L., Luo, Q., Chen, J., Wang, L., Lin, Y., Wang, H., Liu, X., Shen, X., Zhang, W., Liu, W., et al. (2019) · Nature Communications · doi:10.1038/s41467-019-12886-z · Cited by 687
Self-citationXiao, M., Chen, Y., Zhu, J., Zhang, H., Zhao, X., Gao, L., Wang, X., Zhao, J., Ge, J., Jiang, Z., et al. (2019) · Journal of the American Chemical Society · doi:10.1021/jacs.9b08362 · Cited by 638
Cheng, Y., Zhao, S., Johannessen, B., Veder, J., Saunders, M., Rowles, M. R., Cheng, M., Liu, C., Chisholm, M. F., De Marco, R., et al. (2018) · Advanced Materials · doi:10.1002/adma.201706287 · Cited by 614
Single-atom Rh/N-doped carbon electrocatalyst for formic acid oxidation
Xiong, Y., Dong, J., Huang, Z.-Q., Xin, P., Chen, W., Wang, Y., Li, Z., Jin, Z., Xing, W., Zhuang, Z., et al. (2020) · Nature Nanotechnology · doi:10.1038/s41565-020-0665-x · Cited by 610
Self-citationReduction of CuO and Cu2O with H2: H Embedding and Kinetic Effects in the Formation of Suboxides
Kim, J. Y., Rodriguez, J. A., Hanson, J. C., Frenkel, A. I., & Lee, P. L. (2003) · Journal of the American Chemical Society · doi:10.1021/ja0301673 · Cited by 592
Tang, C., Jiao, Y., Shi, B., Liu, J., Xie, Z., Chen, X., Zhang, Q., & Qiao, S. (2020) · Angewandte Chemie International Edition · doi:10.1002/anie.202003842 · Cited by 575
Self-citationZitolo, A., Ranjbar-Sahraie, N., Mineva, T., Li, J., Jia, Q., Stamatin, S., Harrington, G. F., Lyth, S. M., Krtil, P., Mukerjee, S., et al. (2017) · Nature Communications · doi:10.1038/s41467-017-01100-7 · Cited by 563
Li, J., Zhang, H., Samarakoon, W., Shan, W., Cullen, D. A., Karakalos, S., Chen, M., Gu, D., More, K. L., Wang, G., et al. (2019) · Angewandte Chemie International Edition · doi:10.1002/anie.201909312 · Cited by 558
Self-citationHou, Y., Qiu, M., Kim, M. G., Liu, P., Nam, G., Zhang, T., Zhuang, X., Yang, B., Cho, J., Chen, M., et al. (2019) · Nature Communications · doi:10.1038/s41467-019-09394-5 · Cited by 539
Chen, W., Pei, J., He, C., Wan, J., Ren, H., Zhu, Y., Wang, Y., Dong, J., Tian, S., Cheong, W., et al. (2017) · Angewandte Chemie International Edition · doi:10.1002/anie.201710599 · Cited by 519
Ji, D., Fan, L., Li, L., Peng, S., Yu, D., Song, J., Ramakrishna, S., & Guo, S. (2019) · Advanced Materials · doi:10.1002/adma.201808267 · Cited by 461
Ferrero, G. A., Preuss, K., Marinovic, A., Jorge, A. B., Mansor, N., Brett, D. J. L., Fuertes, A. B., Sevilla, M., & Titirici, M.-M. (2016) · ACS Nano · doi:10.1021/acsnano.6b01247 · Cited by 428
Wan, J., Zhao, Z., Shang, H., Peng, B., Chen, W., Pei, J., Zheng, L., Dong, J., Cao, R., Sarangi, R., et al. (2020) · Journal of the American Chemical Society · doi:10.1021/jacs.0c02229 · Cited by 422
Wang, P., Ren, Y., Wang, R., Zhang, P., Ding, M., Li, C., Zhao, D., Qian, Z., Zhang, Z., Zhang, L., et al. (2020) · Nature Communications · doi:10.1038/s41467-020-15416-4 · Cited by 394
Zang, W., Yang, T., Zou, H., Xi, S., Zhang, H., Liu, X., Kou, Z., Du, Y., Feng, Y. P., Shen, L., et al. (2019) · ACS Catalysis · doi:10.1021/acscatal.9b02944 · Cited by 393
Boosting Oxygen Reduction Catalysis with Fe–N4 Sites Decorated Porous Carbons toward Fuel Cells
Yang, Z., Wang, Y., Zhu, M., Li, Z., Chen, W., Wei, W., Yuan, T., Qu, Y., Xu, Q., Zhao, C., et al. (2019) · ACS Catalysis · doi:10.1021/acscatal.8b04381 · Cited by 374
Chai, G.-L., Hou, Z., Shu, D.-J., Ikeda, T., & Terakura, K. (2014) · Journal of the American Chemical Society · doi:10.1021/ja502646c · Cited by 323
Shen, H., Gracia-Espino, E., Ma, J., Tang, H., Mamat, X., Wagberg, T., Hu, G., & Guo, S. (2017) · Nano Energy · doi:10.1016/j.nanoen.2017.03.027 · Cited by 314
High-Density Planar-like Fe2N6 Structure Catalyzes Efficient Oxygen Reduction
Zhang, N., Zhou, T., Ge, J., Lin, Y., Du, Z., Zhong, C., Wang, W., Jiao, Q., Yuan, R., Tian, Y., et al. (2020) · Matter · doi:10.1016/j.matt.2020.06.026 · Cited by 297
Opening of Bottleneck Pores for the Improvement of Nitrogen Doped Carbon Electrocatalysts
Pampel, J., & Fellinger, T. (2016) · Advanced Energy Materials · doi:10.1002/aenm.201502389 · Cited by 251
Gupta, S., Qiao, L., Zhao, S., Xu, H., Lin, Y., Devaguptapu, S. V., Wang, X., Swihart, M. T., & Wu, G. (2016) · Advanced Energy Materials · doi:10.1002/aenm.201601198 · Cited by 248
Gong, L., Zhang, H., Wang, Y., Luo, E., Li, K., Gao, L., Wang, Y., Wu, Z., Jin, Z., Ge, J., et al. (2020) · Angewandte Chemie International Edition · doi:10.1002/anie.202004534 · Cited by 242
Chai, G.-L., & Guo, Z.-X. (2016) · Chemical Science · doi:10.1039/c5sc03695j · Cited by 229
Lei, C., Chen, H., Cao, J., Yang, J., Qiu, M., Xia, Y., Yuan, C., Yang, B., Li, Z., Zhang, X., et al. (2018) · Advanced Energy Materials · doi:10.1002/aenm.201801912 · Cited by 221
Self-citationPore-Edge Tailoring of Single-Atom Iron–Nitrogen Sites on Graphene for Enhanced CO2 Reduction
Pan, F., Li, B., Sarnello, E., Fei, Y., Feng, X., Gang, Y., Xiang, X., Fang, L., Li, T., Hu, Y. H., et al. (2020) · ACS Catalysis · doi:10.1021/acscatal.0c02499 · Cited by 205
High loading single-atom Cu dispersed on graphene for efficient oxygen reduction reaction
Han, G., Zheng, Y., Zhang, X., Wang, Z., Gong, Y., Du, C., Banis, M. N., Yiu, Y.-M., Sham, T.-K., Gu, L., et al. (2019) · Nano Energy · doi:10.1016/j.nanoen.2019.104088 · Cited by 194
Self-citationWang, Y., Yuan, H., Li, Y., & Chen, Z. (2015) · Nanoscale · doi:10.1039/c5nr00302d · Cited by 191
Hydronium-Induced Switching between CO2 Electroreduction Pathways
Seifitokaldani, A., Gabardo, C. M., Burdyny, T., Dinh, C.-T., Edwards, J. P., Kibria, M. G., Bushuyev, O. S., Kelley, S. O., Sinton, D., & Sargent, E. H. (2018) · Journal of the American Chemical Society · doi:10.1021/jacs.7b13542 · Cited by 179
Single‐Atomic‐Co Electrocatalysts with Self‐Supported Architecture toward Oxygen‐Involved Reaction
Xie, W., Song, Y., Li, S., Li, J., Yang, Y., Liu, W., Shao, M., & Wei, M. (2019) · Advanced Functional Materials · doi:10.1002/adfm.201906477 · Cited by 131
Self-citationSun, Y., Du, C., An, M., Du, L., Tan, Q., Liu, C., Gao, Y., & Yin, G. (2015) · Journal of Power Sources · doi:10.1016/j.jpowsour.2015.09.046 · Cited by 95
Self-citationAnia, C. O., Seredych, M., Rodríguez-Castellón, E., & Bandosz, T. J. (2014) · Applied Catalysis B: Environmental · doi:10.1016/j.apcatb.2014.08.022 · Cited by 93
Shin, D., Sinthika, S., Choi, M., Thapa, R., & Park, N. (2014) · ACS Catalysis · doi:10.1021/cs501153p · Cited by 49
Wang, H., Grabstanowicz, L. R., Barkholtz, H. M., Rebollar, D., Kaiser, Z. B., Zhao, D., Chen, B., & Liu, D. (2019) · ACS Energy Letters · doi:10.1021/acsenergylett.9b01740 · Cited by 47
Zhao, L., Guo, S. L., Liu, H., Zhu, H., Yuan, S., & Guo, W. (2018) · ACS Applied Nano Materials · doi:10.1021/acsanm.8b01466 · Cited by 45
Cited by
Zhao, Y., Adiyeri Saseendran, D. P., Huang, C., Triana, C. A., Marks, W. R., Chen, H., Zhao, H., & Patzke, G. R. (2023) · Chemical Reviews · doi:10.1021/acs.chemrev.2c00515 · Cited by 802
Understanding the structure-performance relationship of active sites at atomic scale
Li, R., & Wang, D. (2022) · Nano Research · doi:10.1007/s12274-022-4371-x · Cited by 537
Strain enhances the activity of molecular electrocatalysts via carbon nanotube supports
Su, J., Musgrave, C. B., Song, Y., Huang, L., Liu, Y., Li, G., Xin, Y., Xiong, P., Li, M. M.-J., Wu, H., et al. (2023) · Nature Catalysis · doi:10.1038/s41929-023-01005-3 · Cited by 468
Tailoring of Active Sites from Single to Dual Atom Sites for Highly Efficient Electrocatalysis
Zhang, H., Jin, X., Lee, J.-M., & Wang, X. (2022) · ACS Nano · doi:10.1021/acsnano.2c06827 · Cited by 226
Zhang, D., Li, Y., Wang, P., Qu, J., Li, Y., & Zhan, S. (2023) · Nature Communications · doi:10.1038/s41467-023-39228-4 · Cited by 217
Metadata
- Authors
- Han, G., Zhang, X., Liu, W., Zhang, Q., Wang, Z., Cheng, J., Yao, T., Gu, L., Du, C., Gao, Y., & Yin, G.
- Venue
- Nature Communications
- Published
- 2021-11-03
- Volume
- 12
- Issue
- 1
- Pages
- 6335-6335
- ISSN
- 2041-1723 (ISSN-L)
- OpenAlex
- W3208806365
- Cited by
- 222
- References
- 51
- FWCI
- 5.90
- Type
- journal article
- Language
- en
- Open access
- gold
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.