Borate–pyran lean electrolyte-based Li-metal batteries with minimal Li corrosion
Open accessThe DOI matches its Crossref record; 45 of the 45 references it cites were found in a registry or an index.
Abstract
Engineering liquid electrolytes for lithium (Li)-metal electrodes has been used to control the morphology of deposited Li in Li-metal batteries (LMBs). However, the Li corrosion problem remains unresolved, hindering the design of lean electrolytes for practical LMBs, which require the electrolyte/capacity (E/C) ratio to be 2 g Ah−1 or lower. Here we report a borate–pyran-based electrolyte to address the chronic Li-corrosion problem. We discovered that the borate–pyran electrolyte transforms large LiF crystallites in the solid–electrolyte interphase into fine crystalline or glassy LiF, which enhances the passivity of the Li/electrolyte interface by minimizing the permeation of electrolyte molecules into the solid–electrolyte interphase. LMBs assembled with the borate–pyran electrolyte, a high-nickel layered oxide cathode (3.83 mAh cm−2) and thin lithium (20 μm) delivered a high initial full-cell-level energy density (>400 Wh kg−1) and operated for 400 cycles with 70% capacity retention at an E/C ratio of 1.92 g Ah−1, 350 cycles with 73% capacity retention at 1.24 g Ah−1 and 200 cycles with 85% retention at 0.96 g Ah−1.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Pathways for practical high-energy long-cycling lithium metal batteries
Liu, J., Bao, Z., Cui, Y., Dufek, E. J., Goodenough, J. B., Khalifah, P., Li, Q., Liaw, B. Y., Liu, P., Manthiram, A., et al. (2019) · Nature Energy · doi:10.1038/s41560-019-0338-x · Cited by 3,412 · cited 1×
“Lithium (Li) metal is the most targeted anode material for rechargeable batteries 1 .”
High rate and stable cycling of lithium metal anode
Qian, J., Henderson, W. A., Xu, W., Bhattacharya, P., Engelhard, M., Borodin, O., & Zhang, J.-G. (2015) · Nature Communications · doi:10.1038/ncomms7362 · Cited by 2,561 · cited 7×
“45 and 46 and Supplementary Note 5).”
InfluentialA review on electrolyte additives for lithium-ion batteries
Zhang, S. S. (2006) · Journal of Power Sources · doi:10.1016/j.jpowsour.2006.07.074 · Cited by 1,831
A Review of Solid Electrolyte Interphases on Lithium Metal Anode
Cheng, X., Zhang, R., Zhao, C., Wei, F., Zhang, J., & Zhang, Q. (2016) · Advanced Science · doi:10.1002/advs.201500213 · Cited by 1,786 · cited 2×
“…SEIs in which desired components (for example, LiF, Li 2 O, Li 2 S and LiN x O y crystallites or organic materials with good physicochemical properties 11,12 ) are uniformly distributed via the preferential decomposition of certain electrolyte species (for example, LiFSI or fluorinated solvents).”
InfluentialReview on modeling of the anode solid electrolyte interphase (SEI) for lithium-ion batteries
Wang, A., Kadam, S., Li, H., Shi, S., & Qi, Y. (2018) · npj Computational Materials · doi:10.1038/s41524-018-0064-0 · Cited by 1,639 · cited 2×
“The SEI structure is determined by the accumulation of insoluble by-products of Li corrosion 13,18,19 .”
Atomic structure of sensitive battery materials and interfaces revealed by cryo–electron microscopy
Li, Y., Li, Y., Pei, A., Yan, K., Sun, Y., Wu, C.-L., Joubert, L.-M., Chin, R., Koh, A. L., Yu, Y., et al. (2017) · Science · doi:10.1126/science.aam6014 · Cited by 1,547 · cited 2×
“20), the average efficiencies of Li plating/stripping in the carbonate and LHCE electrolytes were 88.14% and 99.62%, respectively.”
InfluentialAccurate Determination of Coulombic Efficiency for Lithium Metal Anodes and Lithium Metal Batteries
Adams, B. D., Zheng, J., Ren, X., Xu, W., & Zhang, J. (2018) · Advanced Energy Materials · doi:10.1002/aenm.201702097 · Cited by 1,499 · cited 2×
“27) and small R interface (31 Ω cm −2 after five days; Fig.”
Quantifying inactive lithium in lithium metal batteries
Fang, C., Li, J., Zhang, M., Zhang, Y., Yang, F., Lee, J. Z., Lee, M.-H., Alvarado, J., Schroeder, M. A., Yang, Y., et al. (2019) · Nature · doi:10.1038/s41586-019-1481-z · Cited by 1,413 · cited 5×
“Although the electrolytes can extend the lifespan of Li-metal batteries (LMBs) by regulating the morphology of deposited Li, the constant consumption of the electrolyte by reaction with Li (referred to as Li corrosion) hinders further progress 3 .”
InfluentialYu, Z., Wang, H., Kong, X., Huang, W., Tsao, Y., Mackanic, D. G., Wang, K., Wang, X., Huang, W., Choudhury, S., et al. (2020) · Nature Energy · doi:10.1038/s41560-020-0634-5 · Cited by 1,228 · cited 4×
“The value obtained for the LHCE electrolyte is similar to those of recently reported LHCEs 21 or fluorinated solvent electrolytes 9,10 .”
InfluentialStable cycling of high-voltage lithium metal batteries in ether electrolytes
Jiao, S., Ren, X., Cao, R., Engelhard, M. H., Liu, Y., Hu, D., Mei, D., Zheng, J., Zhao, W., Li, Q., et al. (2018) · Nature Energy · doi:10.1038/s41560-018-0199-8 · Cited by 1,149 · cited 7×
“45 and 46 and Supplementary Note 5).”
InfluentialChen, J., Fan, X., Li, Q., Yang, H., Khoshi, M. R., Xu, Y., Hwang, S., Chen, L., Ji, X., Yang, C., et al. (2020) · Nature Energy · doi:10.1038/s41560-020-0601-1 · Cited by 1,137 · cited 1×
“This correction factor may fluctuate within the range of 0.1 ‒ 0.3 V considering the Li free energy in different electrolyte environments 50,51 .”
InfluentialEnabling High-Voltage Lithium-Metal Batteries under Practical Conditions
Ren, X., Zou, L., Cao, X., Engelhard, M. H., Liu, W., Burton, S. D., Lee, H., Niu, C., Matthews, B. E., Zhu, Z., et al. (2019) · Joule · doi:10.1016/j.joule.2019.05.006 · Cited by 1,092 · cited 2×
“7 and 8); this observation indicates that the restructuring of the preformed LiF can be ascribed to a chemical process of LiBF 4 .”
Carbon-free high-loading silicon anodes enabled by sulfide solid electrolytes
Tan, D. H. S., Chen, Y., Yang, H., Bao, W., Sreenarayanan, B., Doux, J., Li, W., Lu, B., Ham, S., Sayahpour, B., et al. (2021) · Science · doi:10.1126/science.abg7217 · Cited by 1,062
Localized High-Concentration Sulfone Electrolytes for High-Efficiency Lithium-Metal Batteries
Ren, X., Chen, S., Lee, H., Mei, D., Engelhard, M. H., Burton, S. D., Zhao, W., Zheng, J., Li, Q., Ding, M. S., et al. (2018) · Chem · doi:10.1016/j.chempr.2018.05.002 · Cited by 1,024
Weber, R., Genovese, M., Louli, A. J., Hames, S., Martin, C., Hill, I. G., & Dahn, J. R. (2019) · Nature Energy · doi:10.1038/s41560-019-0428-9 · Cited by 948 · cited 2×
“14).”
InfluentialRational solvent molecule tuning for high-performance lithium metal battery electrolytes
Yu, Z., Rudnicki, P. E., Zhang, Z., Huang, Z., Celik, H., Oyakhire, S. T., Chen, Y., Kong, X., Kim, S. C., Xiao, X., et al. (2022) · Nature Energy · doi:10.1038/s41560-021-00962-y · Cited by 937 · cited 4×
“…(>400 Wh kg −1 ) to operate for 400 cycles with 70% capacity retention at an E / C ratio of 1.92 g Ah −1 , 350 cycles with 73% capacity retention at 1.24 g Ah −1 and 200 cycles with 85% retention at 0.96 g Ah −1 , which exceeds the performances of state-of-the-art lean electrolyte LMBs 2,9,17 .”
InfluentialCao, X., Ren, X., Zou, L., Engelhard, M. H., Huang, W., Wang, H., Matthews, B. E., Lee, H., Niu, C., Arey, B. W., et al. (2019) · Nature Energy · doi:10.1038/s41560-019-0464-5 · Cited by 930 · cited 4×
“In particular, recently reported high-concentration electrolytes (HCEs) 5,6 , local high-concentration electrolytes (LHCEs) 7,8 and electrolytes with fluorinated solvents 9,10 have been designed to form SEIs in which desired components (for example, LiF, Li 2 O, Li 2 S and LiN x O y crystallites or organic materials w…”
InfluentialHigh-energy lithium metal pouch cells with limited anode swelling and long stable cycles
Niu, C., Lee, H., Chen, S., Li, Q., Du, J., Xu, W., Zhang, J.-G., Whittingham, M. S., Xiao, J., & Liu, J. (2019) · Nature Energy · doi:10.1038/s41560-019-0390-6 · Cited by 732 · cited 7×
“45 and 46 and Supplementary Note 5).”
InfluentialLithium Metal Anodes with Nonaqueous Electrolytes
Zhang, J.-G., Xu, W., Xiao, J., Cao, X., & Liu, J. (2020) · Chemical Reviews · doi:10.1021/acs.chemrev.0c00275 · Cited by 730
Calendar Aging of Lithium-Ion Batteries: I. Impact of the Graphite Anode on Capacity Fade
Keil, P., Schuster, S. F., Wilhelm, J., Travi, J., Hauser, A., Karl, R. C., & Jossen, A. (2016) · Journal of The Electrochemical Society · doi:10.1149/2.0411609jes · Cited by 669 · cited 2×
“33 and 34 and Supplementary Note 2).”
Steric Effect Tuned Ion Solvation Enabling Stable Cycling of High-Voltage Lithium Metal Battery
Chen, Y., Yu, Z., Rudnicki, P., Gong, H., Huang, Z., Kim, S. C., Lai, J.-C., Kong, X., Qin, J., Cui, Y., et al. (2021) · Journal of the American Chemical Society · doi:10.1021/jacs.1c09006 · Cited by 605 · cited 2×
“25 and 26).”
InfluentialBalancing interfacial reactions to achieve long cycle life in high-energy lithium metal batteries
Niu, C., Liu, D., Lochala, J. A., Anderson, C. S., Cao, X., Gross, M. E., Xu, W., Zhang, J.-G., Whittingham, M. S., Xiao, J., et al. (2021) · Nature Energy · doi:10.1038/s41560-021-00852-3 · Cited by 588 · cited 13×
“Although the electrolytes can extend the lifespan of Li-metal batteries (LMBs) by regulating the morphology of deposited Li, the constant consumption of the electrolyte by reaction with Li (referred to as Li corrosion) hinders further progress 3 .”
InfluentialDiagnosing and correcting anode-free cell failure via electrolyte and morphological analysis
Louli, A. J., Eldesoky, A., Weber, R., Genovese, M., Coon, M., deGooyer, J., Deng, Z., White, R. T., Lee, J., Rodgers, T., et al. (2020) · Nature Energy · doi:10.1038/s41560-020-0668-8 · Cited by 570 · cited 2×
“…(>400 Wh kg −1 ) to operate for 400 cycles with 70% capacity retention at an E / C ratio of 1.92 g Ah −1 , 350 cycles with 73% capacity retention at 1.24 g Ah −1 and 200 cycles with 85% retention at 0.96 g Ah −1 , which exceeds the performances of state-of-the-art lean electrolyte LMBs 2,9,17 .”
InfluentialToward Critical Electrode/Electrolyte Interfaces in Rechargeable Batteries
Yan, C., Xu, R., Xiao, Y., Ding, J., Xu, L., Li, B., & Huang, J. (2020) · Advanced Functional Materials · doi:10.1002/adfm.201909887 · Cited by 510 · cited 1×
“The successful regulation of Li corrosion in liquid electrolytes requires not only a finely passivated interphase but also a high reduction stability of electrolyte molecules and Li + solvates in the liquid electrolyte 18,22–24 .”
An Armored Mixed Conductor Interphase on a Dendrite‐Free Lithium‐Metal Anode
Yan, C., Cheng, X., Yao, Y., Shen, X., Li, B., Li, W., Zhang, R., Huang, J., Li, H., & Zhang, Q. (2018) · Advanced Materials · doi:10.1002/adma.201804461 · Cited by 427 · cited 1×
“15 –17 and Supplementary Note 1).”
The passivity of lithium electrodes in liquid electrolytes for secondary batteries
He, X., Bresser, D., Passerini, S., Baakes, F., Krewer, U., Lopez, J., Mallia, C. T., Shao-Horn, Y., Cekic-Laskovic, I., Wiemers-Meyer, S., et al. (2021) · Nature Reviews Materials · doi:10.1038/s41578-021-00345-5 · Cited by 393 · cited 3×
“The SEI structure is determined by the accumulation of insoluble by-products of Li corrosion 13,18,19 .”
Corrosion of lithium metal anodes during calendar ageing and its microscopic origins
Boyle, D. T., Huang, W., Wang, H., Li, Y., Chen, H., Yu, Z., Zhang, W., Bao, Z., & Cui, Y. (2021) · Nature Energy · doi:10.1038/s41560-021-00787-9 · Cited by 334 · cited 6×
“The SEI structure is determined by the accumulation of insoluble by-products of Li corrosion 13,18,19 .”
InfluentialThe surface energies, surface tensions and surface structure of the alkali halide crystals
Tasker, P. W. (1979) · Philosophical Magazine A · doi:10.1080/01418617908236887 · Cited by 307
Solvating power series of electrolyte solvents for lithium batteries
Su, C.-C., He, M., Amine, R., Rojas, T., Cheng, L., Ngo, A. T., & Amine, K. (2019) · Energy & Environmental Science · doi:10.1039/c9ee00141g · Cited by 252 · cited 1×
“25 and 26).”
Tackling realistic Li+ flux for high-energy lithium metal batteries
Zhang, S., Li, R., Hu, N., Deng, T., Weng, S., Wu, Z., Lu, D., Zhang, H., Zhang, J., Wang, X., et al. (2022) · Nature Communications · doi:10.1038/s41467-022-33151-w · Cited by 246
Liu, Z., Qi, Y., Lin, Y. X., Chen, L., Lu, P., & Chen, L. Q. (2016) · Journal of The Electrochemical Society · doi:10.1149/2.0151605jes · Cited by 243 · cited 1×
“41).”
A negative surface energy for alumina
Łodziana, Z., Topsøe, N.-Y., & Nørskov, J. K. (2004) · Nature Materials · doi:10.1038/nmat1106 · Cited by 218 · cited 2×
“…causing Ostwald ripening, physical or chemical interactions sufficiently strong to offset for the surface energy can result in reverse coarsening in multicomponent systems 34–39 (for example, -OH-adsorbed θ -Al 2 O 3 surfaces in water 34 or oleic-acid-adsorbed Ba 2 F 3 Cl surfaces in alcohol 39 ).”
Chang, Z., Qiao, Y., Yang, H., Deng, H., Zhu, X., He, P., & Zhou, H. (2020) · Energy & Environmental Science · doi:10.1039/d0ee02769c · Cited by 197 · cited 1×
“23).”
Boyle, D. T., Kong, X., Pei, A., Rudnicki, P. E., Shi, F., Huang, W., Bao, Z., Qin, J., & Cui, Y. (2020) · ACS Energy Letters · doi:10.1021/acsenergylett.0c00031 · Cited by 197 · cited 1×
“4d), which typically corresponds to the resistance of SEI 13,29,30 .”
Liu, S., Xia, X., Deng, S., Xie, D., Yao, Z., Zhang, L., Zhang, S., Wang, X., & Tu, J. (2019) · Advanced Materials · doi:10.1002/adma.201806470 · Cited by 177 · cited 1×
“In particular, the large gap in the electrolyte to capacity ( E / C ) ratio between LMBs (>2 g Ah −1 ) 14–16 and Li-ion batteries ( ∼ 1.3 g Ah −1 ) 2 reveals that an excessive amount of electrolyte is used to compensate for the electrolyte consumption of the LMBs, which reduces the advantage of…”
InfluentialRevisiting the t0.5 Dependence of SEI Growth
Attia, P. M., Chueh, W. C., & Harris, S. J. (2020) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/ab8ce4 · Cited by 129
Zuo, X., Fan, C., Liu, J., Xiao, X., Wu, J., & Nan, J. (2013) · Journal of The Electrochemical Society · doi:10.1149/2.066308jes · Cited by 81 · cited 2×
“47–49 and Supplementary Note 6.”
Silicon Anodes with Improved Calendar Life Enabled By Multivalent Additives
Zhang, Y., Li, X., Sivonxay, E., Wen, J., Persson, K. A., Vaughey, J. T., Key, B., & Doğan, F. (2021) · Advanced Energy Materials · doi:10.1002/aenm.202101820 · Cited by 64 · cited 2×
“32), consistent with findings reported in previous work 2 .”
Elastic stresses reverse Ostwald ripening
Rosowski, K. A., Vidal-Henriquez, E., Zwicker, D., Style, R. W., & Dufresne, E. R. (2020) · Soft Matter · doi:10.1039/d0sm00628a · Cited by 58 · cited 1×
“35).”
Synergistic Effect of LiPF6and LiBF4as Electrolyte Salts in Lithium-Ion Cells
Ellis, L. D., Hill, I. G., Gering, K. L., & Dahn, J. R. (2017) · Journal of The Electrochemical Society · doi:10.1149/2.0811712jes · Cited by 54
Nie, M., Madec, L., Xia, J., Hall, D. S., & Dahn, J. R. (2016) · Journal of Power Sources · doi:10.1016/j.jpowsour.2016.08.048 · Cited by 35
Calendar and Cycle Life of Lithium-Ion Batteries Containing Silicon Monoxide Anode
Lu, W., Zhang, L., Qin, Y. F., & Jansen, A. N. (2018) · Journal of The Electrochemical Society · doi:10.1149/2.0631810jes · Cited by 35 · cited 2×
“The corrosion rate for the borate–pyran electrolyte was comparable to that of lithiated Si anodes 31,32 and slightly higher than that of lithi-ated graphite anodes 33 .”
Nucleation and Growth of BaFxCl2−x Nanorods
Xie, T., Li, S., Wang, W., Peng, Q., & Li, Y. (2008) · Chemistry - A European Journal · doi:10.1002/chem.200800363 · Cited by 27
Khan, M. A. S., & Ganguly, B. (2013) · CrystEngComm · doi:10.1039/c3ce26764d · Cited by 23 · cited 1×
“36–38).”
Gal, J., Maria, P., Yáñez, M., & Mó, O. (2021) · Molecules · doi:10.3390/molecules26216659 · Cited by 9 · cited 1×
“45 and 46 and Supplementary Note 5).”
Cited by
The contrast between monovalent and multivalent metal battery anodes
Li, Y., Kumar, S., Yang, G., Lu, J., Yao, Y., Kang, K., & Seh, Z. W. (2025) · Science · doi:10.1126/science.adl5482 · Cited by 171
Metadata
- Authors
- Kwon, H., Kim, H., Hwang, J., Oh, W., Roh, Y., Shin, D., & Kim, H.-T.
- Venue
- Nature Energy
- Published
- 2023-11-23
- Volume
- 9
- Issue
- 1
- Pages
- 57-69
- ISSN
- 2058-7546 (ISSN-L)
- OpenAlex
- W4388939065
- Cited by
- 210
- References
- 45
- FWCI
- 15.39
- Type
- journal article
- Language
- en
- Open access
- hybrid
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.