Two electrolyte decomposition pathways at nickel-rich cathode surfaces in lithium-ion batteries
Open accessAbstract
NMR and operando gas measurements show that at low potentials, EC is dehydrogenated to VC, whereas at high potentials, EC is chemically oxidised to CO 2, CO and H 2 O, where the water that is formed induces secondary decomposition reactions.
Overview
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Fulmer, G. R., Miller, A. J. M., Sherden, N. H., Gottlieb, H. E., Nudelman, A., Stoltz, B. M., Bercaw, J. E., & Goldberg, K. I. (2010) · Organometallics · doi:10.1021/om100106e · Cited by 4,050
Performance and cost of materials for lithium-based rechargeable automotive batteries
Schmuch, R., Wagner, R., Hörpel, G., Placke, T., & Winter, M. (2018) · Nature Energy · doi:10.1038/s41560-018-0107-2 · Cited by 3,233
Noh, H.-J., Youn, S., Yoon, C. S., & Sun, Y.-K. (2013) · Journal of Power Sources · doi:10.1016/j.jpowsour.2013.01.063 · Cited by 2,302
Ryu, H.-H., Park, K.-J., Yoon, C. S., & Sun, Y.-K. (2018) · Chemistry of Materials · doi:10.1021/acs.chemmater.7b05269 · Cited by 1,629
Lin, F., Markus, I. M., Nordlund, D., Weng, T.-C., Asta, M. D., Xin, H. L., & Doeff, M. M. (2014) · Nature Communications · doi:10.1038/ncomms4529 · Cited by 1,481
Jung, R., Metzger, M., Maglia, F., Stinner, C., & Gasteiger, H. A. (2017) · Journal of The Electrochemical Society · doi:10.1149/2.0021707jes · Cited by 1,350
Zhan, C., Wu, T., Lu, J. B., & Amine, K. (2017) · Energy & Environmental Science · doi:10.1039/c7ee03122j · Cited by 1,006
Prospect and Reality of Ni‐Rich Cathode for Commercialization
Kim, J., Lee, H., Cha, H., Yoon, M., Park, M., & Cho, J. (2017) · Advanced Energy Materials · doi:10.1002/aenm.201702028 · Cited by 933
Thermal Decomposition of LiPF[sub 6]-Based Electrolytes for Lithium-Ion Batteries
Campion, C. L., Li, W., & Lucht, B. L. (2005) · Journal of The Electrochemical Society · doi:10.1149/1.2083267 · Cited by 827
Differential voltage analyses of high-power, lithium-ion cells
Bloom, I., Jansen, A. N., Abraham, D. P., Knuth, J., Jones, S. A., Battaglia, V. S., & Henriksen, G. L. (2005) · Journal of Power Sources · doi:10.1016/j.jpowsour.2004.07.021 · Cited by 585
Chemical Reactivity of PF[sub 5] and LiPF[sub 6] in Ethylene Carbonate/Dimethyl Carbonate Solutions
Sloop, S. E., Pugh, J. K., Wang, S., Kerr, J. B., & Kinoshita, K. (2001) · Electrochemical and Solid-State Letters · doi:10.1149/1.1353158 · Cited by 577
Analysis of Vinylene Carbonate Derived SEI Layers on Graphite Anode
Ota, H., Sakata, Y., Inoue, A., & Yamaguchi, S. (2004) · Journal of The Electrochemical Society · doi:10.1149/1.1785795 · Cited by 553
Wandt, J., Freiberg, A. T. S., Ogrodnik, A., & Gasteiger, H. A. (2018) · Materials Today · doi:10.1016/j.mattod.2018.03.037 · Cited by 496
Gilbert, J. A., Shkrob, I. A., & Abraham, D. P. (2017) · Journal of The Electrochemical Society · doi:10.1149/2.1111702jes · Cited by 493
Electrolyte Oxidation Pathways in Lithium-Ion Batteries
Rinkel, B. L. D., Hall, D. S., Temprano, I., & Grey, C. P. (2020) · Journal of the American Chemical Society · doi:10.1021/jacs.0c06363 · Cited by 455
Self-citationZhang, Y., Katayama, Y., Tatara, R., Giordano, L., Yu, Y., Fraggedakis, D., Sun, J. G., Maglia, F., Jung, R., Bazant, M. Z., et al. (2020) · Energy & Environmental Science · doi:10.1039/c9ee02543j · Cited by 452
Mahne, N., Schafzahl, B., Leypold, C., Leypold, M., Grumm, S., Leitgeb, A., Strohmeier, G. A., Wilkening, M., Fontaine, O., Kramer, D., et al. (2017) · Nature Energy · doi:10.1038/nenergy.2017.36 · Cited by 446
Zheng, H., Sun, Q., Liu, G., Song, X., & Battaglia, V. S. (2012) · Journal of Power Sources · doi:10.1016/j.jpowsour.2012.01.122 · Cited by 433
Dubarry, M., Svoboda, V., Hwu, R., & Yann Liaw, B. (2006) · Electrochemical and Solid-State Letters · doi:10.1149/1.2221767 · Cited by 427
Renfrew, S. E., & McCloskey, B. D. (2017) · Journal of the American Chemical Society · doi:10.1021/jacs.7b08461 · Cited by 409
Origin of H2Evolution in LIBs: H2O Reduction vs. Electrolyte Oxidation
Metzger, M., Strehle, B., Solchenbach, S., & Gasteiger, H. A. (2016) · Journal of The Electrochemical Society · doi:10.1149/2.1151605jes · Cited by 405
Tasaki, K., Goldberg, A., Lian, J.-J., Walker, M., Timmons, A., & Harris, S. J. (2009) · Journal of The Electrochemical Society · doi:10.1149/1.3239850 · Cited by 370
Thermal stability of lithium-ion battery electrolytes
Ravdel, B., Abraham, K. M., Gitzendanner, R., DiCarlo, J., Lucht, B., & Campion, C. (2003) · Journal of Power Sources · doi:10.1016/s0378-7753(03)00257-x · Cited by 352
Electrochemical and Infrared Studies of the Reduction of Organic Carbonates
Zhang, X., Kostecki, R., Richardson, T. J., Pugh, J. K., & Ross, P. N. (2001) · Journal of The Electrochemical Society · doi:10.1149/1.1415547 · Cited by 351
Predicting and Extending the Lifetime of Li-Ion Batteries
Burns, J. C., Kassam, A., Sinha, N. N., Downie, L. E., Solnickova, L., Way, B. M., & Dahn, J. R. (2013) · Journal of The Electrochemical Society · doi:10.1149/2.060309jes · Cited by 321
Degradation mechanism of alkyl carbonate solvents used in lithium-ion cells during initial charging
Yoshida, H., Fukunaga, T., Hazama, T., Terasaki, M., Mizutani, M., & Yamachi, M. (1997) · Journal of Power Sources · doi:10.1016/s0378-7753(97)02635-9 · Cited by 316
Electrochemical Oxidation of Lithium Carbonate Generates Singlet Oxygen
Mahne, N., Renfrew, S. E., McCloskey, B. D., & Freunberger, S. A. (2018) · Angewandte Chemie International Edition · doi:10.1002/anie.201802277 · Cited by 314
Intrinsic Origins of Crack Generation in Ni-rich LiNi0.8Co0.1Mn0.1O2 Layered Oxide Cathode Material
Lim, J.-M., Hwang, T., Kim, D., Park, M.-S., Cho, K., & Cho, M. (2017) · Scientific Reports · doi:10.1038/srep39669 · Cited by 305
Dedryvère, R., Foix, D., Franger, S., Patoux, S., Daniel, L., & Gonbeau, D. (2010) · The Journal of Physical Chemistry C · doi:10.1021/jp1026509 · Cited by 301
Wandt, J., Freiberg, A., Thomas, R., Gorlin, Y., Siebel, A., Jung, R., Gasteiger, H. A., & Tromp, M. (2016) · Journal of Materials Chemistry A · doi:10.1039/c6ta08865a · Cited by 297
Jin, Y., Kneusels, N.-J. H., Magusin, P. C. M. M., Kim, G., Castillo-Martínez, E., Marbella, L. E., Kerber, R. N., Howe, D. J., Paul, S., Liu, T., et al. (2017) · Journal of the American Chemical Society · doi:10.1021/jacs.7b06834 · Cited by 291
Self-citationElectrochemical Reduction of Carbon Dioxide to Formic Acid
Lu, X., Leung, D. Y. C., Wang, H., Leung, M. K. H., & Xuan, J. (2014) · ChemElectroChem · doi:10.1002/celc.201300206 · Cited by 279
Xing, L., Li, W., Wang, C., Gu, F., Xu, M., Tan, C., & Yi, J. (2009) · The Journal of Physical Chemistry B · doi:10.1021/jp9074064 · Cited by 272
Dubarry, M., Truchot, C., Liaw, B. Y., Gering, K., Sazhin, S., Jamison, D., & Michelbacher, C. (2011) · Journal of Power Sources · doi:10.1016/j.jpowsour.2011.08.078 · Cited by 265
Guéguen, A., Streich, D., He, M., Mendez, M., Chesneau, F. F., Novák, P., & Berg, E. J. (2016) · Journal of The Electrochemical Society · doi:10.1149/2.0981606jes · Cited by 265
Origin of Carbon Dioxide Evolved during Cycling of Nickel-Rich Layered NCM Cathodes
Hatsukade, T., Schiele, A., Hartmann, P., Brezesinski, T., & Janek, J. (2018) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.8b13158 · Cited by 256
Ashbrook, S. E., & Smith, M. E. (2006) · Chemical Society Reviews · doi:10.1039/b514051j · Cited by 228
Quantification of PF5 and POF3 from Side Reactions of LiPF6 in Li-Ion Batteries
Solchenbach, S., Metzger, M., Egawa, M., Beyer, H., & Gasteiger, H. A. (2018) · Journal of The Electrochemical Society · doi:10.1149/2.0481813jes · Cited by 222
Pritzl, D., Teufl, T., Freiberg, A. T. S., Strehle, B., Sicklinger, J., Sommer, H., Hartmann, P., & Gasteiger, H. A. (2019) · Journal of The Electrochemical Society · doi:10.1149/2.1351915jes · Cited by 216
Identification of the Source of Evolved Gas in Li-Ion Batteries Using [sup 13]C-labeled Solvents
Onuki, M., Kinoshita, S., Sakata, Y., Yanagidate, M., Otake, Y., Ue, M., & Deguchi, M. (2008) · Journal of The Electrochemical Society · doi:10.1149/1.2969947 · Cited by 211
Electrocatalytic transformation of HF impurity to H2 and LiF in lithium-ion batteries
Strmcnik, D., Castelli, I. E., Connell, J. G., Haering, D., Zorko, M., Martins, P., Lopes, P. P., Genorio, B., Østergaard, T., Gasteiger, H. A., et al. (2018) · Nature Catalysis · doi:10.1038/s41929-018-0047-z · Cited by 207
Solchenbach, S., Hong, G., Freiberg, A. T. S., Jung, R., & Gasteiger, H. A. (2018) · Journal of The Electrochemical Society · doi:10.1149/2.0511814jes · Cited by 205
Jung, R., Strobl, P., Maglia, F., Stinner, C., & Gasteiger, H. A. (2018) · Journal of The Electrochemical Society · doi:10.1149/2.1261811jes · Cited by 202
Singlet Oxygen Reactivity with Carbonate Solvents Used for Li-Ion Battery Electrolytes
Freiberg, A. T. S., Roos, M. K., Wandt, J., de Vivie-Riedle, R., & Gasteiger, H. A. (2018) · The Journal of Physical Chemistry A · doi:10.1021/acs.jpca.8b08079 · Cited by 189
Bernhard, R., Metzger, M., & Gasteiger, H. A. (2015) · Journal of The Electrochemical Society · doi:10.1149/2.0191510jes · Cited by 186
Survey of Gas Expansion in Li-Ion NMC Pouch Cells
Self, J., Aiken, C. P., Petibon, R., & Dahn, J. R. (2015) · Journal of The Electrochemical Society · doi:10.1149/2.0081506jes · Cited by 166
Burns, J. C., Petibon, R., Nelson, K. J., Sinha, N. N., Kassam, A., Way, B. M., & Dahn, J. R. (2013) · Journal of The Electrochemical Society · doi:10.1149/2.031310jes · Cited by 165
Imhof, R., & Novák, P. (1999) · Journal of The Electrochemical Society · doi:10.1149/1.1391829 · Cited by 163
Gas Evolution in Operating Lithium-Ion Batteries Studied In Situ by Neutron Imaging
Michalak, B., Sommer, H., Mannes, D., Kaestner, A., Brezesinski, T., & Janek, J. (2015) · Scientific Reports · doi:10.1038/srep15627 · Cited by 161
Operando Monitoring of Early Ni-mediated Surface Reconstruction in Layered Lithiated Ni–Co–Mn Oxides
Streich, D., Erk, C., Guéguen, A., Müller, P., Chesneau, F.-F., & Berg, E. J. (2017) · The Journal of Physical Chemistry C · doi:10.1021/acs.jpcc.7b02303 · Cited by 161
Mechanism of Gases Generation during Lithium-Ion Batteries Cycling
Galushkin, N. Е., Yazvinskaya, N. N., & Galushkin, D. N. (2019) · Journal of The Electrochemical Society · doi:10.1149/2.0041906jes · Cited by 158
Hydrolysis of Ethylene Carbonate with Water and Hydroxide under Battery Operating Conditions
Metzger, M., Strehle, B., Solchenbach, S., & Gasteiger, H. A. (2016) · Journal of The Electrochemical Society · doi:10.1149/2.0411607jes · Cited by 157
Zhuang, G. V., & Ross, P. N. (2003) · Electrochemical and Solid-State Letters · doi:10.1149/1.1575594 · Cited by 153
Capacity and power fading mechanism identification from a commercial cell evaluation
Dubarry, M., Svoboda, V., Hwu, R., & Liaw, B. Y. (2007) · Journal of Power Sources · doi:10.1016/j.jpowsour.2006.10.046 · Cited by 152
Schwenke, K. U., Solchenbach, S., Demeaux, J., Lucht, B. L., & Gasteiger, H. A. (2019) · Journal of The Electrochemical Society · doi:10.1149/2.0821910jes · Cited by 151
Bernhard, R., Meini, S., & Gasteiger, H. A. (2014) · Journal of The Electrochemical Society · doi:10.1149/2.013404jes · Cited by 150
Singlet oxygen-mediated selective C–H bond hydroperoxidation of ethereal hydrocarbons
Sagadevan, A., Hwang, K. C., & Su, M. (2017) · Nature Communications · doi:10.1038/s41467-017-01906-5 · Cited by 148
Zafeiratos, S., Dintzer, T., Teschner, D., Blume, R., Hävecker, M., Knop‐Gericke, A., & Schlögl, R. (2009) · Journal of Catalysis · doi:10.1016/j.jcat.2009.11.013 · Cited by 140
Ota, H., Sakata, Y., Otake, Y., Shima, K., Ue, M., & Yamaki, J. (2004) · Journal of The Electrochemical Society · doi:10.1149/1.1798411 · Cited by 138
Quantifying, Understanding and Evaluating the Effects of Gas Consumption in Lithium-Ion Cells
Ellis, L. D., Allen, J. P., Thompson, L., Harlow, J. E., Stone, W. J., Hill, I. G., & Dahn, J. R. (2017) · Journal of The Electrochemical Society · doi:10.1149/2.0191714jes · Cited by 138
Mixed solvent electrolyte for high voltage lithium metal secondary cells
Hayashi, K., Nemoto, Y., Tobishima, S., & Yamaki, J. (1999) · Electrochimica Acta · doi:10.1016/s0013-4686(98)00374-0 · Cited by 136
Tebbe, J. L., Fuerst, T. F., & Musgrave, C. B. (2016) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.6b06157 · Cited by 128
Ryu, H., Park, G., Yoon, C. S., & Sun, Y. (2018) · Small · doi:10.1002/smll.201803179 · Cited by 126
Transition Metal Dissolution and Degradation in NMC811-Graphite Electrochemical Cells
Ruff, Z. M., Xu, C., & Grey, C. P. (2021) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/ac0359 · Cited by 113
Self-citationStrehle, B., Solchenbach, S., Metzger, M., Schwenke, K. U., & Gasteiger, H. A. (2017) · Journal of The Electrochemical Society · doi:10.1149/2.1001712jes · Cited by 111
Anodic oxidation of propylene carbonate and ethylene carbonate on graphite electrodes
Arakawa, M., & Yamaki, J. (1995) · Journal of Power Sources · doi:10.1016/0378-7753(94)02078-h · Cited by 93
Xiong, D. J., Ellis, L. D., Petibon, R., Hynes, T., Liu, Q. Q., & Dahn, J. R. (2016) · Journal of The Electrochemical Society · doi:10.1149/2.1091702jes · Cited by 93
Oxidation of Ethylene Carbonate on Li Metal Oxide Surfaces
Østergaard, T., Giordano, L., Castelli, I. E., Maglia, F., Antonopoulos, B. K., Shao‐Horn, Y., & Rossmeisl, J. (2018) · The Journal of Physical Chemistry C · doi:10.1021/acs.jpcc.8b01713 · Cited by 82
LiPO2F2 as an Electrolyte Additive in Li[Ni0.5Mn0.3Co0.2]O2/Graphite Pouch Cells
Ma, L., Ellis, L., Glazier, S. L., Ma, X.-W., Liu, Q.-Q., Li, J., & Dahn, J. (2018) · Journal of The Electrochemical Society · doi:10.1149/2.0381805jes · Cited by 74
Metzger, M., Sicklinger, J., Haering, D., Kavakli, C., Stinner, C., Marino, C., & Gasteiger, H. A. (2015) · Journal of The Electrochemical Society · doi:10.1149/2.0461507jes · Cited by 73
Free Energy for Protonation Reaction in Lithium-Ion Battery Cathode Materials
Benedek, R., Thackeray, M. M., & van de Walle, A. (2008) · Chemistry of Materials · doi:10.1021/cm703042r · Cited by 71
High-Throughput in Situ Pressure Analysis of Lithium-Ion Batteries
Schiele, A., Hatsukade, T., Berkes, B. B., Hartmann, P., Brezesinski, T., & Janek, J. (2017) · Analytical Chemistry · doi:10.1021/acs.analchem.7b01760 · Cited by 69
Selective lithium extraction from brines by chemical reaction with battery materials
Intaranont, N., García-Aráez, N., Hector, A. L., Milton, J. A., & Owen, J. R. (2014) · Journal of Materials Chemistry A · doi:10.1039/c4ta01101e · Cited by 59
Nuclear magnetic resonance spectra of glycolaldehyde
Collins, G. C. S., & George, W. O. (1971) · Journal of the Chemical Society B Physical Organic · doi:10.1039/j29710001352 · Cited by 56
Ma, L., Ellis, L. D., Glazier, S., Ma, X., & Dahn, J. R. (2018) · Journal of The Electrochemical Society · doi:10.1149/2.0661809jes · Cited by 55
Assessing the Oxidation Behavior of EC:DMC Based Electrolyte on Non-Catalytically Active Surface
Azcarate, I., Yin, W., Méthivier, C., Ribot, F. O., Laberty‐Robert, C., & Grimaud, A. (2020) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/ab8f57 · Cited by 51
Transition-Metal Dissolution from NMC-Family Oxides: A Case Study
Morin, H., GRACZYK, D. G., Tsai, Y., Lopykinski, S. J., Iddir, H. H., Garcia, J. C., Rago, N. L. D., Trask, S. E., Flores, L., Son, S., et al. (2020) · ACS Applied Energy Materials · doi:10.1021/acsaem.9b02277 · Cited by 46
The Selective Oxidation of Methanol on Iron Molybdate Catalysts
Bowker, M., Holroyd, R., House, M. P., Bracey, R., Bamroongwongdee, C., Shannon, M. D., & Carley, A. F. (2008) · Topics in Catalysis · doi:10.1007/s11244-008-9058-3 · Cited by 45
Factors influencing the quantum yields for rose bengal formation of singlet oxygen
Gottschalk, P., Pączkowski, J., & Neckers, D. C. (1986) · Journal of Photochemistry · doi:10.1016/0047-2670(86)87059-9 · Cited by 39
Pérez-Rodríguez, S., Fitch, S. D. S., Bartlett, P. N., & García-Aráez, N. (2021) · ChemSusChem · doi:10.1002/cssc.202102182 · Cited by 21
Metadata
- Authors
- Rinkel, B. L. D., Vivek, J. P., Garcia-Araez, N., & Grey, C. P.
- Venue
- Energy & Environmental Science
- Publisher
- Royal Society of Chemistry (RSC)
- Published
- 2022
- Volume
- 15
- Issue
- 8
- Pages
- 3416-3438
- ISSN
- 1754-5692 (ISSN-L)
- 1754-5706
- OpenAlex
- W4285283202
- Cited by
- 326
- References
- 80
- FWCI
- 15.66
- Type
- journal article
- Language
- en
- Open access
- hybrid
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.