Improvements in resist performance towards EUV HVM
Open accessThe DOI matches its Crossref record; 21 of the 26 references it cites were found in a registry or an index.
Abstract
Extreme ultraviolet (EUV) lithography with 13.5 nm wavelength is the main option for sub-10nm patterning in the semiconductor industry. We report improvements in resist performance towards EUV high volume manufacturing. A local CD uniformity (LCDU) model is introduced and validated with experimental contact hole (CH) data. Resist performance is analyzed in terms of ultimate printing resolution (R), line width roughness (LWR), sensitivity (S), exposure latitude (EL) and depth of focus (DOF). Resist performance of dense lines at 13 nm half-pitch and beyond is shown by chemical amplified resist (CAR) and non-CAR (Inpria YA Series) on NXE scanner. Resolution down to 10nm half pitch (hp) is shown by Inpria YA Series resist exposed on interference lithography at the Paul Sherrer Institute. Contact holes contrast and consequent LCDU improvement is achieved on a NXE:3400 scanner by decreasing the pupil fill ratio. State-of-the-art imaging meets 5nm node requirements for CHs. A dynamic gas lock (DGL) membrane is introduced between projection optics box (POB) and wafer stage. The DGL membrane will suppress the negative impact of resist outgassing on the projection optics by 100%, enabling a wider range of resist materials to be used. The validated LCDU model indicates that the imaging requirements of the 3nm node can be met with single exposure using a high-NA EUV scanner. The current status, trends, and potential roadblocks for EUV resists are discussed. Our results mark the progress and the improvement points in EUV resist materials to support EUV ecosystem.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
The source backs part of the claim, not all of it — or backs it for a different population, condition or comparison.
In the citing paper
“Most HP values met the industry requirement of LWR being less than 20% of the CD [87].”
From Recent Advances in Metal-Oxide-Based Photoresists for EUV Lithography (2024) · cites this paper as [87]
Experimental — accuracy not yet measuredThe check wasn’t confident either way, so it gives no verdict — never disputed.
In the citing paper
“To prevent issues with the finite thickness of photoresists -such as LWR, pattern collapse and reduced resolution -resist films should ideally decrease in thickness to sub -10 nm, single or few monolayers 12 8 .”
From Extreme ultraviolet lithography (2024) · cites this paper as [128]
Experimental — accuracy not yet measured
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Radiation Chemistry in Chemically Amplified Resists
Kozawa, T., & Tagawa, S. (2010) · Japanese Journal of Applied Physics · doi:10.1143/jjap.49.030001 · Cited by 360
Resist blur and line edge roughness
Gallatin, G. M. (2005) · Optical Microlithography XVIII · doi:10.1117/12.607233 · Cited by 244
Resist Materials and Processes for Extreme Ultraviolet Lithography
Itani, T., & Kozawa, T. (2013) · Japanese Journal of Applied Physics · doi:10.7567/jjap.52.010002 · Cited by 185
Modeling and simulation of chemically amplified electron beam, x-ray, and EUV resist processes
Kozawa, T., Saeki, A., & Tagawa, S. (2004) · Journal of Vacuum Science & Technology B Microelectronics and Nanometer Structures Processing Measurement and Phenomena · doi:10.1116/1.1823435 · Cited by 125
Evaluation of EUV resist materials for use at the 32 nm half-pitch node
Wallow, T., Higgins, C., Brainard, R., Petrillo, K., Montgomery, W., Koay, C.-S., Denbeaux, G., Wood, O., & Wei, Y. (2008) · SPIE Proceedings · doi:10.1117/12.772943 · Cited by 108
Materials challenges for sub-20-nm lithography
Thackeray, J. W. (2011) · Journal of Micro/Nanopatterning Materials and Metrology · doi:10.1117/1.3616067 · Cited by 94
Integrated fab process for metal oxide EUV photoresist
Grenville, A., Anderson, J. T., Clark, B. L., De Schepper, P., Edson, J., Greer, M., Jiang, K., Kocsis, M., Meyers, S. T., Stowers, J. K., et al. (2015) · SPIE Proceedings · doi:10.1117/12.2086006 · Cited by 90
A numeric model for the imaging mechanism of metal oxide EUV resists
Hinsberg, W. D., & Meyers, S. (2017) · SPIE Proceedings · doi:10.1117/12.2260265 · Cited by 66
Stochastic exposure kinetics of extreme ultraviolet photoresists: simulation study
Thackeray, J. W. (2011) · Journal of Micro/Nanolithography, MEMS, and MOEMS · doi:10.1117/1.3631753 · Cited by 56
Metal oxide EUV photoresist performance for N7 relevant patterns and processes
Stowers, J., Anderson, J., Cardineau, B., Clark, B., De Schepper, P., Edson, J., Greer, M., Jiang, K., Kocsis, M., Meyers, S., et al. (2016) · SPIE Proceedings · doi:10.1117/12.2219527 · Cited by 45
Research works printed but not linked: 2
- Pirati, A., "EUV lithograpy performance for manufacturing: status and outlook," Proc. SPIE 97760A, 1-15 (2016).
- Van de Kerkhof, M., "Enabling sub-10nm node lithography: presenting the NXE:3400B EUV," Proc. SPIE, in publication, (2017).
Cited by
Extreme ultraviolet lithography
Kazazis, D., Santaclara, J. G., van Schoot, J., Mochi, I., & Ekinci, Y. (2024) · Nature Reviews Methods Primers · doi:10.1038/s43586-024-00361-z · Cited by 149
Self-citationBlock Copolymer Nanopatterning for Nonsemiconductor Device Applications
Yang, G. G., Choi, H. J., Han, K. H., Kim, J. H., Lee, C. W., Jung, E. I., Jin, H. M., & Kim, S. O. (2022) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.1c22836 · Cited by 102
Merkx, M. J. M., Sandoval, T. E., Hausmann, D. M., Kessels, W. M. M., & Mackus, A. J. M. (2020) · Chemistry of Materials · doi:10.1021/acs.chemmater.9b02992 · Cited by 84
Merkx, M. J. M., Vlaanderen, S., Faraz, T., Verheijen, M. A., Kessels, W. M. M., & Mackus, A. J. M. (2020) · Chemistry of Materials · doi:10.1021/acs.chemmater.0c02370 · Cited by 80
Stochastic printing failures in extreme ultraviolet lithography
De Bisschop, P. (2018) · Journal of Micro/Nanopatterning, Materials, and Metrology · doi:10.1117/1.jmm.17.4.041011 · Cited by 75
High NA EUV lithography: Next step in EUV imaging
van Setten, E., Bottiglieri, G., McNamara, J., van Schoot, J., Troost, K., Zekry, J., Fliervoet, T. F., Hsu, S., Zimmermann, J., Roesch, M., et al. (2019) · Extreme Ultraviolet (EUV) Lithography · doi:10.1117/12.2514952 · Cited by 71
High-numerical aperture extreme ultraviolet scanner for 8-nm lithography and beyond
van Schoot, J., van Setten, E., Rispens, G., Troost, K. Z., Kneer, B., Migura, S., Neumann, J. T., & Kaiser, W. (2017) · Journal of Micro/Nanopatterning, Materials, and Metrology · doi:10.1117/1.jmm.16.4.041010 · Cited by 57
“achievable LCDU is mainly driven by photon shot noise and thus strongly depends on the absolute dose.(42,43) Assuming”
BackgroundSelf-citationStability studies on a sensitive EUV photoresist based on zinc metal oxoclusters
Thakur, N., Tseng, L.-T., Vockenhuber, M., Ekinci, Y., & Castellanos, S. (2019) · Journal of Micro/Nanolithography, MEMS, and MOEMS · doi:10.1117/1.jmm.18.4.043504 · Cited by 52
“8 μm−1.(17,30,31) As a reference value, the theoretical linear absorptivity was calculated for this material.”
BackgroundSelf-citationDeng, J., Bailey, S., Jiang, S., & Ober, C. K. (2022) · Chemistry of Materials · doi:10.1021/acs.chemmater.2c01444 · Cited by 52
Mixed-ligand zinc-oxoclusters: Efficient chemistry for high resolution nanolithography
Thakur, N., Bliem, R., Mochi, I., Vockenhuber, M., Ekinci, Y., & Castellanos, S. (2020) · Journal of Materials Chemistry C · doi:10.1039/d0tc03597a · Cited by 52
Self-citationMechanistic insights in Zr-and Hf-based molecular hybrid EUV photoresists
Wu, L., Baljozovic, M., Portale, G., Kazazis, D., Vockenhuber, M., Jung, T., Ekinci, Y., & Castellanos Ortega, S. (2019) · Journal of Micro/Nanopatterning Materials and Metrology · doi:10.1117/1.jmm.18.1.013504 · Cited by 49
Self-citationStochastic effects in EUV lithography
De Bisschop, P., & Hendrickx, E. (2018) · Extreme Ultraviolet (EUV) Lithography IX · doi:10.1117/12.2300541 · Cited by 38
Effect of Oxygen on Thermal and Radiation-Induced Chemistries in a Model Organotin Photoresist
Frederick, R. T., Diulus, J. T., Hutchison, D. C., Nyman, M., & Herman, G. S. (2019) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.8b16048 · Cited by 42
Diulus, J. T., Frederick, R. T., Li, M., Hutchison, D. C., Olsen, M. R., Lyubinetsky, I., Árnadóttir, L., Garfunkel, E. L., Nyman, M., Ogasawara, H., et al. (2019) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.8b19302 · Cited by 40
Recent Advances in Metal-Oxide-Based Photoresists for EUV Lithography
Hasan, M. W., Deeb, L., Kumaniaev, S., Wei, C., & Wang, K. (2024) · Micromachines · doi:10.3390/mi15091122 · Cited by 35
“Most HP values met the industry requirement of LWR being less than 20% of the CD [87].”
BackgroundEUV Photoresists: A Progress Report and Future Prospects
Lio, A. (2019) · Synchrotron Radiation News · doi:10.1080/08940886.2019.1634431 · Cited by 22
Maas, R., van Lare, C., Rispens, G., & Wuister, S. F. (2018) · Journal of Micro/Nanopatterning Materials and Metrology · doi:10.1117/1.jmm.17.4.041003 · Cited by 28
Self-citationGuruprasad Reddy, P., Kumar, P., Ghosh, S., Pradeep, C. P., Sharma, S. K., & Gonsalves, K. E. (2017) · Materials Chemistry Frontiers · doi:10.1039/c7qm00343a · Cited by 24
Ti, Zr, and Hf-based molecular hybrid materials as EUV photoresists
Castellanos Ortega, S., Wu, L., Baljozovic, M., Portale, G., Kazazis, D., Vockenhuber, M., Ekinci, Y., & Jung, T. (2018) · Extreme Ultraviolet (EUV) Lithography IX · doi:10.1117/12.2297167 · Cited by 14
“[1–4] Ideally, a photoresist should render patterns with line width roughness (LWR) below 20%.[4] However reaching this LWR limit usually requires a dose high enough to allow the shot-noise to be on an acceptable level.”
BackgroundSelf-citationEngineering block copolymer materials for patterning ultra-low dimensions
Cummins, C., Pino, G., Mantione, D., & Fleury, G. (2020) · Molecular Systems Design & Engineering · doi:10.1039/d0me00118j · Cited by 20
Photoresist and stochastic modeling
Hansen, S. G. (2018) · Journal of Micro/Nanopatterning Materials and Metrology · doi:10.1117/1.jmm.17.1.013506 · Cited by 20
“% 1⁄4 20 ILSblðμÞ : (7) The plot shows that the features chosen possess a wide range of dose sensitivities; the low ILS cases are mainly linked to small CD line and trench ends.”
BackgroundOptimization and stability of CD variability in pitch 40 nm contact holes on NXE:3300
Look, L. V., Bekaert, J. P., Frommhold, A., Hendrickx, E., Rispens, G., & Schiffelers, G. (2018) · International Conference on Extreme Ultraviolet Lithography · doi:10.1117/12.2501797 · Cited by 20
Self-citationNandi, S., Khillare, L. D., Kumar, S., Moinuddin, M. G., Chauhan, M. S., Choudhary, S. K., Sharma, S. K., Ghosh, S., & Gonsalves, K. E. (2023) · ACS Applied Nano Materials · doi:10.1021/acsanm.2c04831 · Cited by 20
Fundamental understanding and experimental verification of bright versus dark field imaging
Davydova, N. V., Finders, J. M., McNamara, J., van Setten, E., van Lare, C., Franke, J.-H., Frommhold, A., Capelli, R., Kersteen, G., Verch, A., et al. (2020) · doi:10.1117/12.2573161 · Cited by 18
Self-citationZhao, R., Wang, X., Xu, H., Wei, Y., & He, X. (2024) · Nanoscale · doi:10.1039/d3nr04819e · Cited by 16
Impact of local variability on defect-aware process windows
Maslow, M. J., Yaegashi, H., Frommhold, A., Schiffelers, G., Wählisch, F., Rispens, G., Slachter, B., Yoshida, K., Hara, A., Oikawa, N., et al. (2019) · Extreme Ultraviolet (EUV) Lithography · doi:10.1117/12.2514719 · Cited by 16
Self-citationGong, X., Chen, Z., Wang, D., Xu, R., Huang, X., Zheng, L., Zhang, M., Li, W., Zhao, J., Chen, P., et al. (2025) · Inorganic Chemistry · doi:10.1021/acs.inorgchem.5c00501 · Cited by 15
Photo-electron chemistry of photoresist outgassing upon DUV, VUV, EUV, and BEUV irradiation
Ho, G. H., Lin, H.-M., & Yeh, C.-Y. (2017) · Journal of Photochemistry and Photobiology A Chemistry · doi:10.1016/j.jphotochem.2017.11.027 · Cited by 15
Belete, Z., Bisschop, P. D., Welling, U., & Erdmann, A. A. (2021) · Journal of Micro/Nanopatterning Materials and Metrology · doi:10.1117/1.jmm.20.1.014801 · Cited by 15
“Post exposure bake (PEB) impacts the condensation reaction and, in turn the sensitivity of the photoresist.(20) However, our investigation focuses on the modeling of the stochastic development process for a finished condensation reaction.”
BackgroundNear-field infrared nanoscopic study of EUV- and e-beam-exposed hydrogen silsesquioxane photoresist
Kim, J., Lee, J., Chae, B., Ahn, J., & Lee, S. (2022) · Nano Convergence · doi:10.1186/s40580-022-00345-3 · Cited by 14
Study of molecular layer deposition of zinc-based hybrid film as photoresist
Shan, Y., Wang, X., Zheng, X., Zhao, X., Feng, Z. K., Wang, W., Cheng, Y., Liu, H., Tan, K., Luo, F. C., et al. (2024) · Applied Surface Science · doi:10.1016/j.apsusc.2024.161727 · Cited by 13
Merkx, M. J. M., Tezsevin, I., Yu, P., Janssen, T., Heinemans, R. H. G. M., Lengers, R. J., Chen, J.-R., Jezewski, C. J., Clendenning, S. B., Kessels, W. M. M., et al. (2024) · The Journal of Chemical Physics · doi:10.1063/5.0207496 · Cited by 13
Empirical correlator for stochastic local CD uniformity in extreme ultraviolet lithography
Bisschop, P. D., & Hansen, S. G. (2022) · Journal of Micro/Nanopatterning Materials and Metrology · doi:10.1117/1.jmm.21.3.033201 · Cited by 13
“EQ-TARGET;temp:intralink-;e009;116;293 LWR 1⁄4 ffiffiffi 2 p LER ∝ 1 ILSbl : (9)”
BackgroundWang, D., Gong, X., Xu, R., Zhang, M., Zhou, D., Fan, J., Du, J., Zhao, J., Zhang, J., Chen, P., et al. (2025) · Science China Chemistry · doi:10.1007/s11426-025-2632-y · Cited by 12
Zhao, R., Wang, X., Hu, Z., Xu, H., & He, X. (2023) · Nanoscale · doi:10.1039/d3nr01356a · Cited by 12
Chen, Y., Sun, L., Qi, Z. J., Zhao, S., Goodwin, F. G., Matthew, I., & Plachecki, V. (2017) · Journal of Vacuum Science & Technology B Nanotechnology and Microelectronics Materials Processing Measurement and Phenomena · doi:10.1116/1.4994908 · Cited by 11
Electron beam lithography with negative tone resist for highly integrated silicon quantum bits
Kato, K., Liu, Y., Murakami, S., Morita, Y., & Mori, T. (2021) · Nanotechnology · doi:10.1088/1361-6528/ac201b · Cited by 11
Liu, Z., Chen, J., Yu, T., Zeng, Y. P., Guo, X., Wang, S., Hu, R., Vockenhuber, M., Tian, P., Kazazis, D., et al. (2025) · ACS Applied Electronic Materials · doi:10.1021/acsaelm.5c00273 · Cited by 9
Self-citationSasaki, A., Ishino, M., & Nishikino, M. (2019) · Japanese Journal of Applied Physics · doi:10.7567/1347-4065/ab06bc · Cited by 9
Development of a dynamic gas lock inhibited model for EUV-induced carbon deposition
Hao, M., Teng, S., Liu, J., Xie, Y., Ba, D., Bian, X., Ba, Y., Chen, Z., & Liu, K. (2024) · The Journal of Chemical Physics · doi:10.1063/5.0182717 · Cited by 8
Chauhan, M. S., Palit, K., Choudhary, S. K., Sharma, S. K., & Gonsalves, K. E. (2022) · Journal of Micro/Nanopatterning Materials and Metrology · doi:10.1117/1.jmm.21.4.044603 · Cited by 8
Chemical metrology on latent resist images
van Es, M. H., Tamer, M. S., Bloem, E., Fillinger, L., van Zeijl, E., Maturová, K., van der Donck, J. C. J., Willekers, R. W., Chuang, A., & Maas, D. J. (2023) · Micro and Nano Engineering · doi:10.1016/j.mne.2023.100181 · Cited by 8
Lithographic effects due to particles on high-NA EUV mask pellicle
Devaraj, L., Bottiglieri, G., Erdmann, A. A., Wählisch, F., Kupers, M., van Setten, E., & Fliervoet, T. F. (2019) · European Mask and Lithography Conference (EMLC) · doi:10.1117/12.2534177 · Cited by 8
“Further, the results obtained for NILS can be used to calculate the Local Critical Dimension Uniformity (LCDU), as it is demonstrated to be inversely proportional to NILS [5,6,7].”
MethodInfluentialZhao, R., Wei, Y., Xu, H., & He, X. (2023) · Applied Optics · doi:10.1364/ao.479619 · Cited by 8
Zhao, R., Hu, Z., Wang, X., Tao, P., Wang, Y., Liu, T., Wei, Y., Xu, H., & He, X. (2023) · Applied Optics · doi:10.1364/ao.485006 · Cited by 6
Zhao, R., Wei, Y., Wang, X., He, X., & Xu, H. (2024) · The Journal of Physical Chemistry Letters · doi:10.1021/acs.jpclett.4c01911 · Cited by 6
Roncaglia, A. (2022) · Springer handbooks · doi:10.1007/978-3-030-79827-7_8 · Cited by 6
Impact of mask corner rounding on pitch 40 nm contact hole variability
Look, L. V., Gillijns, W., & Gallagher, E. E. (2021) · International Conference on Extreme Ultraviolet Lithography · doi:10.1117/12.2601850 · Cited by 6
Understanding the Significance of Local Variability in Defect-Aware Process Windows
Maslow, M. J., Yaegashi, H., Frommhold, A., Hara, A., & Cerbu, D. (2019) · IEEE Transactions on Semiconductor Manufacturing · doi:10.1109/tsm.2019.2960090 · Cited by 5
“see an increased LCDU for the new resist compared to the original resist [5].”
BackgroundByeon, J., Kim, D., Kim, S., Ahn, J., Oh, D. S., Yoon, Y. H., Jee, H., Kim, Y., Hwang, C.-C., & Hong, S. (2024) · Materials Today Chemistry · doi:10.1016/j.mtchem.2024.102474 · Cited by 4
Hao, M., Chen, S., Teng, S., Liu, J., Zhang, Y., Xie, Y., Ba, Y., Bian, X., & Liu, K. (2025) · Journal of Industrial and Engineering Chemistry · doi:10.1016/j.jiec.2025.02.013 · Cited by 4
Pattern degradation with larger particles on EUV pellicle
No, H.-R., Lee, S., Oh, H.-K., & Oh, S.-H. (2018) · International Conference on Extreme Ultraviolet Lithography · doi:10.1117/12.2502784 · Cited by 4
“The simulation conditions are summarized in Table 1[8].”
BackgroundParticle on EUV pellicles, impact on LWR
Kupers, M., Rispens, G., Devaraj, L., Bottiglieri, G., van den Hoogenhoff, T., Broman, P., Erdmann, A. A., & Wählisch, F. (2019) · International Conference on Extreme Ultraviolet Lithography · doi:10.1117/12.2537103 · Cited by 4
“Inverting equation (4) and replacing the Dose terms in (5) we get:”
BackgroundSelf-citationReddy, P. G., Moinuddin, M. G., Joseph, A. M., Nandi, S., Ghosh, S., Pradeep, C. P., Sharma, S. K., & Gonsalves, K. E. (2018) · Journal of Photopolymer Science and Technology · doi:10.2494/photopolymer.31.669 · Cited by 4
Predicting stochastic defects across the process window
Frommhold, A., Cerbu, D., Bekaert, J. P., Look, L. V., Maslow, M. J., Rispens, G., & Hendrickx, E. (2019) · International Conference on Extreme Ultraviolet Lithography · doi:10.1117/12.2536898 · Cited by 4
Self-citationNair, V. V., Look, L. V., Aubert, R., & Hendrickx, E. (2020) · doi:10.1117/12.2572993 · Cited by 4
“To further increase its adoption in a production environment, there is also a push towards lower dose, higher sensitivity resists to ensure higher throughput at a reasonable EUV source power([3]).”
BackgroundLCDU decomposition and scaling: mask and resist effects on local MEEF and stochastics
Gustas, D., Borman, S., Oorschot, D., Bekaert, J. P., van Loo, H., Horsten, F., Vaenkatesan, V., Colina, A., & van Rhee, T. (2024) · International Conference on Extreme Ultraviolet Lithography · doi:10.1117/12.3034695 · Cited by 3
“A known model describes the stochastic variability as [7]: , where ILS is the Image Log-Slope, a known lithographic imaging quality metric.”
Near-field infrared spectroscopy: Advanced research method in thin film analysis
Kim, J., Chae, B., & Lee, S. (2024) · Current Applied Physics · doi:10.1016/j.cap.2024.11.002 · Cited by 2
Recent status of resist outgas testing for metal containing resists at EIDEC
Shiobara, E., Mikami, S., & Yamada, K. (2018) · Extreme Ultraviolet (EUV) Lithography · doi:10.1117/12.2297317 · Cited by 2
Characterization of metal resist for EUV lithography using Infrared free electron laser
Toriumi, M., Kawasaki, T., Imai, T., Tsukiyama∥, K., Santillan, J. J., & Itani, T. (2018) · Advances in Patterning Materials and Processes · doi:10.1117/12.2297156 · Cited by 2
Nano metal-oxygen cluster EUV photoresists and their performance influencing factors
Xing, Y., Hu, T., Fang, W., Yin, Y., Gao, L., Liu, W., Ding, X., Jin, H., & Wang, G. (2024) · Scientia Sinica Chimica · doi:10.1360/ssc-2024-0008 · Cited by 1
Jing, 曹. C., & Nan, 林. L. (2025) · Laser & Optoelectronics Progress · doi:10.3788/lop250460 · Cited by 1
Soltani, E. (2023) · theses.fr (ABES) · doi:10.70675/8e05f35eze97ez4166z8ba1z3a38ec2ec341 · Cited by 1
The update of resist outgas testing for metal containing resists at EIDEC
Shiobara, E., & Mikami, S. (2017) · International Conference on Extreme Ultraviolet Lithography · doi:10.1117/12.2280443
Photolithography and surface modification applications of a 172 nanometer xenon microplasma excilamp
Sonoiki, O. (2019) · Illinois Digital Environment for Access to Learning and Scholarship (University of Illinois at Urbana-Champaign)
Highly spatial-resolved chemical metrology on latent resist imagesPreprint
van Es, M. H., Tamer, M. S., Bloem, E., Fillinger, L., van Zeijl, E., Maturová, K., van der Donck, J. C. J., Willekers, R. W., & Maas, D. J. (2022) · Research Square · doi:10.21203/rs.3.rs-1238936/v1
Mask optimization approach for wafer LCDU improvement in ArF lithography
Ichikawa, K., Yoshida, I., Matui, K., Kojima, Y., Nagatomo, T., & Yamana, M. (2023) · SPIE Photomask Technology Conference · doi:10.1117/12.2688551
“𝑴𝑨𝑺𝑲 𝟐 = 𝑳𝒐𝒄𝒂𝒍 𝑴𝑬𝑬𝑭 𝟐 × 𝑴𝒂𝒔𝒌 𝑳𝑪𝑫𝑼 𝟐 (2) ※ Mask LCDU (at wafer scale) Also, the RESIST error can be expressed as Eq.”
Breaking down ADI line edge roughness from a DUV scanner into components
Watson, B., Hemert, T. V., van den Broeke, J. J., Bouma, A., Temchenko, V., Khurana, R., Nair, V. V., Snyder, S. D., Eggleston, M., Taylor, T. L., et al. (2025) · SPIE Optical and EUV Nanolithography · doi:10.1117/12.3051541
Jing, 曹. C., & Nan, 林. L. (2025) · Laser & Optoelectronics Progress · doi:10.3788/lop250506
Onderzoek naar nieuwe materialen voor gebruik in Extreem Ultraviolet Lithografie
Rathore, A. (2021) · Lirias
Zinc Oxoclusters for Extreme Ultraviolet Lithography
Thakur, N. (2022) · ARCNL Institutional Repository (ARCNL)
Xiaowei, 王. W., Zhijun, 张. Z., Ningxia, 尹. Y., Jing, 张. Z., & Shiwei, 张. Z. (2025) · Acta Optica Sinica (Online) · doi:10.3788/aosol250508
Study on the pattern placement error analysis using photo-overlay correction methods
Park, W., Yu, K., Kim, H., Lee, S., Gwak, J., Huh, K., Kim, J., & Park, C. (2026) · SPIE Optical and EUV Nanolithography · doi:10.1117/12.3089996
Resists in modern lithography: from deep ultraviolet to X-rays
Петрова, Д. В., Dzhons, M. M., & Чхало, Н. И. (2026) · Russian Chemical Reviews · doi:10.59761/rcr5199
Byeon, J., Gys, N., Smets, J., Azimi, A., Nulens, L., Fernandes, J., Boullart, L., Kim, D., Dorney, K. M., Gándara-Loe, J., et al. (2026) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.6c16414
Metadata
- Authors
- Yildirim, O., Buitrago, E., Hoefnagels, R., Meeuwissen, M., Wuister, S., Rispens, G., van Oosten, A., Derks, P., Finders, J., Vockenhuber, M., & Ekinci, Y.
- Affiliations
- ASML (Netherlands) (NL)
- Paul Scherrer Institute (CH)
- ASML Netherlands B.V. (Netherlands)
- Venue
- SPIE Proceedings
- Publisher
- SPIE
- Published
- 2017-03-27
- Volume
- 10143
- Pages
- 101430Q
- ISSN
- 0277-786X (ISSN-L)
- OpenAlex
- W2598677901
- Cited by
- 69
- References
- 26
- Citations by year
- 2026: 2 · 2025: 8 · 2024: 11 · 2023: 6 · 2022: 6 · 2021: 3 · 2020: 6 · 2019: 11 · 2018: 11 · 2017: 5
- FWCI
- 12.77
- Type
- conference paper
- Language
- en
- Open access
- bronze
- doi.org
- Locations
- Proceedings of SPIE, the International Society for Optical Engineering/Proceedings of SPIE (publishedVersion)
- DORA PSI (Paul Scherrer Institute) (submittedVersion, other-oa)
- Topics
- Physical Sciences › Engineering › Electrical and Electronic Engineering › Advancements in Photolithography Techniques
- Physical Sciences › Physics and Astronomy › Radiation › Advanced X-ray Imaging Techniques
- Physical Sciences › Physics and Astronomy › Atomic and Molecular Physics, and Optics › Advanced optical system design
- Keywords
- EUV lithography, high-volume manufacturing, line width roughness, exposure latitude, depth of focus, interference lithography, projection optics, 13.5 nm wavelength
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.