Hydration Characteristics and Microstructure of Alkali-Activated Slag Concrete: A Review
Open accessAbstract
Alkali-activated slag concrete (AASC) is a new green building material. The amount of CO2 produced by AASC is 1/5th of that produced by ordinary Portland cement concrete (OPCC). In addition, AASC promotes the reuse of slag and other wastes and saves resources. Furthermore, the scope of use of slag has been expanded. The progress of the research on the hydration characteristics, microstructure, interfacial transition zone, and pore structure of AASC based on the relevant literatures was analyzed and summarized in this study. The influences of the slag composition, the type and dosage of the alkali activator, and the curing conditions on the hydration characteristics and the microstructure of the AASC were discussed. Relatively few research results on the microstructure of AASC are available, and the relevant conclusions are not completely consistent. Moreover, there are many constraints on the development of AASC (e.g., complex composition of raw materials of slag, large shrinkage deformation, and low fluidity). Therefore, further research is required.
Overview
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Run the check — free, no account needed. It reads the open-access text and checks the sources it cites.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Carbon dioxide equivalent (CO2-e) emissions: A comparison between geopolymer and OPC cement concrete
Turner, L. K., & Collins, F. G. (2013) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2013.01.023 · Cited by 2,411
Geopolymers and Related Alkali-Activated Materials
Provis, J. L., & Bernal, S. A. (2014) · Annual Review of Materials Research · doi:10.1146/annurev-matsci-070813-113515 · Cited by 1,597
Advances in understanding alkali-activated materials
Provis, J. L., Palomo, A., & Shi, C. (2015) · Cement and Concrete Research · doi:10.1016/j.cemconres.2015.04.013 · Cited by 1,537
On the Development of Fly Ash-Based Geopolymer Concrete
(2004) · ACI Materials Journal · doi:10.14359/13485 · Cited by 1,254
Influence of nano-SiO2 addition on properties of hardened cement paste as compared with silica fume
Qing, Y., Zenan, Z., Deyu, K., & Rongshen, C. (2007) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2005.09.001 · Cited by 1,242
Alkali-Activated Cements and Concretes
Shi, C., Krivenko, P. V., & Roy, D. (2006) · Taylor & Francis eBooks · doi:10.4324/9780203390672 · Cited by 1,164
A review: The comparison between alkali-activated slag (Si + Ca) and metakaolin (Si + Al) cements
Li, C., Sun, H., & Li, L. (2010) · Cement and Concrete Research · doi:10.1016/j.cemconres.2010.03.020 · Cited by 1,108
Richardson, I. G. (2004) · Cement and Concrete Research · doi:10.1016/j.cemconres.2004.05.034 · Cited by 1,082
Bernal, S. A., Provis, J. L., Walkley, B., San Nicolas, R., Gehman, J. D., Brice, D. G., Kilcullen, A. R., Duxson, P., & van Deventer, J. S. J. (2013) · Cement and Concrete Research · doi:10.1016/j.cemconres.2013.06.007 · Cited by 1,019
Hydration products of alkali activated slag cement
Wang, S.-D., & Scrivener, K. L. (1995) · Cement and Concrete Research · doi:10.1016/0008-8846(95)00045-e · Cited by 997
Alkali-activated binders: A review
Pacheco-Torgal, F., Castro-Gomes, J., & Jalali, S. (2008) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2007.10.015 · Cited by 989
Haha, M. B., Lothenbach, B., Le Saout, G., & Winnefeld, F. (2011) · Cement and Concrete Research · doi:10.1016/j.cemconres.2011.05.002 · Cited by 914
Alkali Activated Materials: State-of-the-Art Report, RILEM TC 224-AAM
(2014) · RILEM State-of-the-Art Reports · doi:10.1007/978-94-007-7672-2 · Cited by 906
A model for the C-A-S-H gel formed in alkali-activated slag cements
Puertas, F., Palacios, M., Manzano, H., Dolado, J. S., Rico, A., & Rodríguez, J. (2011) · Journal of the European Ceramic Society · doi:10.1016/j.jeurceramsoc.2011.04.036 · Cited by 898
Evolution of binder structure in sodium silicate-activated slag-metakaolin blends
Bernal, S. A., Provis, J. L., Rose, V., & Mejía de Gutierrez, R. (2011) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2010.09.004 · Cited by 786
Carbon dioxide reduction potential in the global cement industry by 2050
Miller, S. A., John, V. M., Pacca, S. A., & Horvath, A. (2018) · Cement and Concrete Research · doi:10.1016/j.cemconres.2017.08.026 · Cited by 757
Factors affecting the strength of alkali-activated slag
Wang, S.-D., Scrivener, K. L., & Pratt, P. L. (1994) · Cement and Concrete Research · doi:10.1016/0008-8846(94)90026-4 · Cited by 716
Sodium silicate-based, alkali-activated slag mortars
Brough, A. R., & Atkinson, A. (2002) · Cement and Concrete Research · doi:10.1016/s0008-8846(02)00717-2 · Cited by 694
Alkali-activated cements Opportunities and challenges
Roy, D. M. (1999) · Cement and Concrete Research · doi:10.1016/s0008-8846(98)00093-3 · Cited by 608
Fernández-Jiménez, A., Palomo, J. G., & Puertas, F. (1999) · Cement and Concrete Research · doi:10.1016/s0008-8846(99)00154-4 · Cited by 598
Resistance of alkali-activated slag concrete to acid attack
Bakharev, T., Sanjayan, J. G., & Cheng, Y.-B. (2003) · Cement and Concrete Research · doi:10.1016/s0008-8846(03)00125-x · Cited by 586
Haha, M. B., Lothenbach, B., Le Saout, G., & Winnefeld, F. (2012) · Cement and Concrete Research · doi:10.1016/j.cemconres.2011.08.005 · Cited by 580
Myers, R. J., Bernal, S. A., San Nicolas, R., & Provis, J. L. (2013) · Langmuir · doi:10.1021/la4000473 · Cited by 579
Alonso, S., & Palomo, A. (2001) · Materials Letters · doi:10.1016/s0167-577x(00)00212-3 · Cited by 542
Effect of binder content on the performance of alkali-activated slag concretes
Bernal, S. A., Mejía de Gutiérrez, R., Pedraza, A. L., Provis, J. L., Rodriguez, E. D., & Delvasto, S. (2011) · Cement and Concrete Research · doi:10.1016/j.cemconres.2010.08.017 · Cited by 537
Bernal, S. A., San Nicolas, R., Myers, R. J., Mejía de Gutiérrez, R., Puertas, F., van Deventer, J. S. J., & Provis, J. L. (2014) · Cement and Concrete Research · doi:10.1016/j.cemconres.2013.12.003 · Cited by 493
Fernández‐Jiménez, A., Puertas, F., Sobrados, I., & Sanz, J. (2003) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.2003.tb03481.x · Cited by 481
Alkali activation of Australian slag cements
Bakharev, T., Sanjayan, J. G., & Cheng, Y.-B. (1999) · Cement and Concrete Research · doi:10.1016/s0008-8846(98)00170-7 · Cited by 474
Alkali-activated slag cement and concrete: a review of properties and problems
Wang, S.-D., Pu, X.-C., Scrivener, K. L., & Pratt, P. L. (1995) · Advances in Cement Research · doi:10.1680/adcr.1995.7.27.93 · Cited by 474
Bernal, S. A., de Gutierrez, R. M., Provis, J. L., & Rose, V. (2010) · Cement and Concrete Research · doi:10.1016/j.cemconres.2010.02.003 · Cited by 473
A calorimetric study of early hydration of alkali-slag cements
Shi, C., & Day, R. L. (1995) · Cement and Concrete Research · doi:10.1016/0008-8846(95)00126-w · Cited by 468
Shrinkage characteristics of alkali-activated fly ash/slag paste and mortar at early ages
Lee, N. K., Jang, J. G., & Lee, H. K. (2014) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2014.07.007 · Cited by 462
Sulfate attack on alkali-activated slag concrete
Bakharev, T., Sanjayan, J. G., & Cheng, Y.-B. (2002) · Cement and Concrete Research · doi:10.1016/s0008-8846(01)00659-7 · Cited by 456
Richardson, I. G., Brough, A. R., Groves, G. W., & Dobson, C. M. (1994) · Cement and Concrete Research · doi:10.1016/0008-8846(94)90002-7 · Cited by 449
Effects of dosage and modulus of water glass on early hydration of alkali–slag cements
Krizan, D., & Zivanovic, B. (2002) · Cement and Concrete Research · doi:10.1016/s0008-8846(01)00717-7 · Cited by 444
Abdalqader, A. F., Jin, F., & Al-Tabbaa, A. (2016) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2015.12.010 · Cited by 444
Low carbon and low embodied energy materials in buildings: A review
Cabeza, L. F., Barreneche, C., Miró, L., Morera, J. M., Bartolí, E., & Inés Fernández, A. (2013) · Renewable and Sustainable Energy Reviews · doi:10.1016/j.rser.2013.03.017 · Cited by 417
Greening of the Concrete Industry for Sustainable Development
Mehta, P. K. (2002) · ACI Concrete International · Cited by 410
Very early-age reaction kinetics and microstructural development in alkali-activated slag
Gebregziabiher, B. S., Thomas, R., & Peethamparan, S. (2015) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2014.09.001 · Cited by 393
Hydration mechanisms of super sulphated slag cement
Gruskovnjak, A., Lothenbach, B., Winnefeld, F., Figi, R., Ko, S.-C., Adler, M., & Mäder, U. (2008) · Cement and Concrete Research · doi:10.1016/j.cemconres.2008.03.004 · Cited by 378
The percolation of pore space in the cement paste/aggregate interfacial zone of concrete
Scrivener, K. L., & Nemati, K. M. (1996) · Cement and Concrete Research · doi:10.1016/0008-8846(95)00185-9 · Cited by 368
Hydration of alkali-activated ground granulated blast furnace slag
Song, S., Sohn, D., Jennings, H. M., & Mason, T. O. (2000) · Journal of Materials Science · doi:10.1023/a:1004742027117 · Cited by 363
Effect of elevated temperature curing on properties of alkali-activated slag concrete
Bakharev, T., Sanjayan, J. G., & Cheng, Y.-B. (1999) · Cement and Concrete Research · doi:10.1016/s0008-8846(99)00143-x · Cited by 349
Hydration of alkali-activated slag: comparison with ordinary Portland cement
Gruskovnjak, A., Lothenbach, B., Holzer, L., Figi, R., & Winnefeld, F. (2006) · Advances in Cement Research · doi:10.1680/adcr.2006.18.3.119 · Cited by 349
Hydration and properties of sodium sulfate activated slag
Rashad, A. M., Bai, Y., Basheer, P. A. M., Milestone, N. B., & Collier, N. C. (2013) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2012.12.010 · Cited by 335
Role of carbonates in the chemical evolution of sodium carbonate-activated slag binders
Bernal, S. A., Provis, J. L., Myers, R. J., San Nicolas, R., & van Deventer, J. S. J. (2015) · Materials and Structures · doi:10.1617/s11527-014-0412-6 · Cited by 334
Zhang, P., Wang, K., Li, Q., Wang, J., & Ling, Y. (2020) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2020.120896 · Cited by 334
A study on the setting characteristics of sodium silicate-activated slag pastes
Chang, J. J. (2003) · Cement and Concrete Research · doi:10.1016/s0008-8846(02)01096-7 · Cited by 330
Ke, X., Bernal, S. A., & Provis, J. L. (2016) · Cement and Concrete Research · doi:10.1016/j.cemconres.2015.11.012 · Cited by 328
27 Al and 29 Si Solid-State NMR Characterization of Calcium-Aluminosilicate-Hydrate
Pardal, X., Brunet, F., Charpentier, T., Pochard, I., & Nonat, A. (2012) · Inorganic Chemistry · doi:10.1021/ic202124x · Cited by 328
Microcracking and strength development of alkali activated slag concrete
Collins, F., & Sanjayan, J. G. (2001) · Cement and Concrete Composites · doi:10.1016/s0958-9465(01)00003-8 · Cited by 316
Mechanical and microstructural properties of heat cured alkali-activated slag mortars
Aydın, S., & Baradan, B. (2011) · Materials & Design (1980-2015) · doi:10.1016/j.matdes.2011.10.005 · Cited by 305
Effect of activator mix on the hydration and strength behaviour of alkali-activated slag cements
Fernandez-Jimenez, A., & Puertas, F. (2003) · Advances in Cement Research · doi:10.1680/adcr.15.3.129.36623 · Cited by 285
Hydration Products and Reactivity of Blast‐Furnace Slag Activated by Various Alkalis
Escalante‐García, J. I., Fuentes, A. F., Gorokhovsky, A., Fraire‐Luna, P. E., & Mendoza‐Suarez, G. (2003) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.2003.tb03623.x · Cited by 284
Effects of nano-TiO2 on strength, shrinkage and microstructure of alkali activated slag pastes
Yang, L. Y., Jia, Z. J., Zhang, Y. M., & Dai, J. G. (2015) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2014.11.009 · Cited by 267
Rashad, A. M., Bai, Y., Basheer, M., Collier, N. C., & Milestone, N. B. (2011) · Cement and Concrete Research · doi:10.1016/j.cemconres.2011.10.007 · Cited by 262
Živica, V. (2007) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2006.07.002 · Cited by 262
The hydration of slag, part 1: reaction models for alkali-activated slag
Chen, W., & Brouwers, H. J. H. (2007) · Journal of Materials Science · doi:10.1007/s10853-006-0873-2 · Cited by 260
Cao, R., Zhang, S., Banthia, N., Zhang, Y., & Zhang, Z. (2020) · Composites Part B: Engineering · doi:10.1016/j.compositesb.2020.107840 · Cited by 254
Self-citationChithiraputhiran, S., & Neithalath, N. (2013) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2013.03.061 · Cited by 250
Li, N., Shi, C., & Zhang, Z. (2019) · Composites Part B: Engineering · doi:10.1016/j.compositesb.2019.04.024 · Cited by 249
Self-citationEffect of Carbonation on Alkali‐Activated Slag Paste
Palacios, M., & Puertas, F. (2006) · Journal of the American Ceramic Society · doi:10.1111/j.1551-2916.2006.01214.x · Cited by 236
Alkali activation of a slag at ambient and elevated temperatures
Altan, E., & Erdoğan, S. T. (2011) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2011.08.003 · Cited by 232
Gijbels, K., Pontikes, Y., Samyn, P., Schreurs, S., & Schroeyers, W. (2020) · Cement and Concrete Research · doi:10.1016/j.cemconres.2020.106054 · Cited by 230
Alkali-activated slag cements: Kinetic studies
Fernández-Jiménez, A., & Puertas, F. (1997) · Cement and Concrete Research · doi:10.1016/s0008-8846(97)00040-9 · Cited by 227
Activation of blast furnace slag by a new method
Bellmann, F., & Stark, J. (2009) · Cement and Concrete Research · doi:10.1016/j.cemconres.2009.05.012 · Cited by 225
Rothstein, D., Thomas, J. J., Christensen, B. J., & Jennings, H. M. (2002) · Cement and Concrete Research · doi:10.1016/s0008-8846(02)00855-4 · Cited by 221
Renaudin, G., Russias, J., Leroux, F., Cau-dit-Coumes, C., & Frizon, F. (2009) · Journal of Solid State Chemistry · doi:10.1016/j.jssc.2009.09.024 · Cited by 220
Temperature and activator effect on early-age reaction kinetics of alkali-activated slag binders
Gebregziabiher, B. S., Thomas, R. J., & Peethamparan, S. (2016) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2016.03.098 · Cited by 207
Tan, H., Deng, X., He, X., Zhang, J., Zhang, X., Su, Y., & Yang, J. (2019) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2019.01.012 · Cited by 206
Hu, X., Shi, C., Shi, Z., & Zhang, L. (2019) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2019.103392 · Cited by 206
Alkali-activated Portland blast-furnace slag cement: Mechanical properties and hydration
Angulo-Ramírez, D. E., Mejía de Gutiérrez, R., & Puertas, F. (2017) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2017.02.092 · Cited by 198
The evolution of interfacial transition zone in alkali-activated fly ash-slag concrete
Fang, G., & Zhang, M. (2020) · Cement and Concrete Research · doi:10.1016/j.cemconres.2019.105963 · Cited by 196
Ravikumar, D., & Neithalath, N. (2012) · Thermochimica Acta · doi:10.1016/j.tca.2012.07.010 · Cited by 191
Some factors affecting early hydration of alkali-slag cements
Shi, C., & Day, R. L. (1996) · Cement and Concrete Research · doi:10.1016/s0008-8846(96)85031-9 · Cited by 187
Structural evolution of an alkali sulfate activated slag cement
Mobasher, N., Bernal, S. A., & Provis, J. L. (2016) · Journal of Nuclear Materials · doi:10.1016/j.jnucmat.2015.11.016 · Cited by 186
Compressive strength of rice husk ash based geopolymer: The effect of alkaline activator
Kaur, K., Singh, J., & Kaur, M. (2018) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2018.02.200 · Cited by 169
Hydration of alkali-activated slag: thermodynamic modelling
Lothenbach, B., & Gruskovnjak, A. (2007) · Advances in Cement Research · doi:10.1680/adcr.2007.19.2.81 · Cited by 166
Influence of compaction on the interfacial transition zone and the permeability of concrete
Leemann, A., Münch, B., Gasser, P., & Holzer, L. (2006) · Cement and Concrete Research · doi:10.1016/j.cemconres.2006.02.010 · Cited by 165
Ćwirzeń, A., & Penttala, V. (2005) · Cement and Concrete Research · doi:10.1016/j.cemconres.2004.06.009 · Cited by 161
Effect of alkali contents, moduli and curing time on engineering properties of alkali activated slag
Fang, S., Lam, S. S. E., Li, B., & Wu, B. (2020) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2020.118799 · Cited by 153
Deir, E., Gebregziabiher, B. S., & Peethamparan, S. (2013) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2013.11.010 · Cited by 152
Kinetic study on hydration of alkali-activated slag
Huanhai, Z., Xuequan, W., Xu, Z., & Mingshu, T. (1993) · Cement and Concrete Research · doi:10.1016/0008-8846(93)90062-e · Cited by 151
World cement production and environmental implications
Uwasu, M., Hara, K., & Yabar, H. (2014) · Environmental Development · doi:10.1016/j.envdev.2014.02.005 · Cited by 148
Jiang, D., Li, X., Lv, Y., Li, C., Jiang, W., Liu, Z., Xu, J., Zhou, Y., & Dan, J. (2021) · Cement and Concrete Research · doi:10.1016/j.cemconres.2021.106581 · Cited by 148
Distinctive microstructural features of aged sodium silicate-activated slag concretes
Nicolas, R. S., Bernal, S. A., de Gutiérrez, R. M., van Deventer, J. S. J., & Provis, J. L. (2014) · Cement and Concrete Research · doi:10.1016/j.cemconres.2014.07.008 · Cited by 137
Gu, Y.-M., Fang, Y., You, D., Gong, Y., & Zhu, C. (2015) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2014.12.068 · Cited by 131
Internal curing by superabsorbent polymers in alkali-activated slag
Li, Z., Wyrzykowski, M., Dong, H., Granja, J. L., Azenha, M., Lura, P., & Ye, G. (2020) · Cement and Concrete Research · doi:10.1016/j.cemconres.2020.106123 · Cited by 123
Effect of slag chemistry on the hydration of alkali-activated blast-furnace slag
Tänzer, R., Buchwald, A., & Stephan, D. A. (2014) · Materials and Structures · doi:10.1617/s11527-014-0461-x · Cited by 117
Fernández‐Jiménez, A., Puertas, F., & Arteaga, A. (1998) · Journal of Thermal Analysis and Calorimetry · doi:10.1023/a:1010172204297 · Cited by 111
29 Si and 27 Al MAS‐NMR of NaOH‐Activated Blast‐Furnace Slag
Schilling, P. J., Butler, L. G., Roy, A. D., & Eaton, H. C. (1994) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.1994.tb04606.x · Cited by 111
Effect of nano-silica on hydration, microstructure of alkali-activated slag
Wang, J., Du, P., Zhou, Z., Xu, D., Xie, N., & Cheng, X. Y. (2019) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2019.05.158 · Cited by 111
Rakhimova, N. R., Rakhimov, R. Z., Наумкина, Н. И., Хузин, А. Ф., & Osin, Y. N. (2016) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2016.06.015 · Cited by 107
Zhang, Y. J., Zhao, Y. L., Li, H. H., & Xu, D. L. (2008) · Journal of Materials Science · doi:10.1007/s10853-008-3028-9 · Cited by 99
Ye, H., Fu, C., & Yang, G. (2019) · Cement and Concrete Composites · doi:10.1016/j.cemconcomp.2019.05.011 · Cited by 95
Häkkinen, T. (1993) · Cement and Concrete Research · doi:10.1016/0008-8846(93)90106-j · Cited by 93
Wei, X., Li, D., Ming, F., Cheng-song, Y., Chen, L., & Liu, Y. (2020) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2020.121811 · Cited by 85
Brough, A. R., & Atkinson, A. (2000) · Cement and Concrete Research · doi:10.1016/s0008-8846(00)00254-4 · Cited by 84
Alkaline activation of synthetic aluminosilicate glass
García-Lodeiro, I., Fernández‐Jiménez, A., Peña, P., & Palomo, A. (2013) · Ceramics International · doi:10.1016/j.ceramint.2013.10.146 · Cited by 83
Bonk, F. A., Schneider, J., Cincotto, M. A., & Panepucci, H. C. (2003) · Journal of the American Ceramic Society · doi:10.1111/j.1151-2916.2003.tb03545.x · Cited by 79
Manjunath, R., Narasimhan, M. C., Umesh, K. M., Kumar, S., & Bharathi, U. K. B. (2018) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2018.11.242 · Cited by 72
Vázquez‐Rowe, I., Ziegler-Rodríguez, K., Laso, J., Quispe, I., García, R. A., & Kahhat, R. F. (2018) · Resources Conservation and Recycling · doi:10.1016/j.resconrec.2018.12.017 · Cited by 72
Ju, C., Liu, Y., Jia, M., Yu, K., Yu, Z., & Yang, Y. (2020) · Journal of Building Engineering · doi:10.1016/j.jobe.2020.101561 · Cited by 60
Bai, Y., Collier, N. C., Milestone, N. B., & Yang, C. H. (2011) · Journal of Nuclear Materials · doi:10.1016/j.jnucmat.2011.04.011 · Cited by 59
Hu, X., Shi, C., Liu, X., et al. (2020) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2020.119982 · Cited by 53
Sakulich, A. R., Anderson, E. M., Schauer, C. L., & Barsoum, M. W. (2009) · Materials and Structures · doi:10.1617/s11527-009-9563-2 · Cited by 51
Composite alkaline activator on cemented soil: Multiple tests and mechanism analyses
Xu, F., Hua, W. D., Qian, W., & Cai, Y. (2018) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2018.08.118 · Cited by 50
Zhang, Y., Wan, X., Hou, D., Zhao, T., & Cui, Y. (2018) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2018.09.009 · Cited by 48
Schilling, P. J., Roy, A. D., Eaton, H. C., Malone, P. G., & Brabston, N. W. (1994) · Journal of materials research/Pratt's guide to venture capital sources · doi:10.1557/jmr.1994.0188 · Cited by 47
Wang, S. Y., McCaslin, E., & White, C. E. (2020) · Cement and Concrete Research · doi:10.1016/j.cemconres.2020.105979 · Cited by 46
The effect of the blaine fineness on the mechanical properties of the alkali-activated slag cement
Saedi, M., Behfarnia, K., & Soltanian, H. (2019) · Journal of Building Engineering · doi:10.1016/j.jobe.2019.100897 · Cited by 45
Soriano, L., Font, A., TASHIMA, M. M., Monzó, J., Borrachero, M. V., Bonifacio, T. T. C., & Payá, J. (2021) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2021.123251 · Cited by 45
Jiao, Z., Wang, Y., Zheng, W., & Huang, W. (2018) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2018.11.178 · Cited by 43
Hydration of alkali-slag cements at 150°C
Shi, C., Wu, X., & Tang, M. (1991) · Cement and Concrete Research · doi:10.1016/0008-8846(91)90035-g · Cited by 40
Effect of TiO2 on the hydration of tricalcium silicate
Katyal, N. K., Ahluwalia, S. C., & Parkash, R. (1999) · Cement and Concrete Research · doi:10.1016/s0008-8846(99)00171-4 · Cited by 37
Liquid concentration changes during slag cement hydration by alkali activation
Kim, J. C., & Hong, S. Y. (2001) · Cement and Concrete Research · doi:10.1016/s0008-8846(00)00455-5 · Cited by 33
Puertas, F., Palacios, M., Manzano, H., et al. (2014) · MATEC Web of Conferences · doi:10.1051/matecconf/20141101002 · Cited by 24
Jin, Y., Feng, W., Zheng, D., Dong, Z., Cui, H., Li, M. K., Sang, G., & Tang, W. (2020) · Construction and Building Materials · doi:10.1016/j.conbuildmat.2020.118900 · Cited by 23
Optimising Ambient Setting Bayer Derived Fly Ash Geopolymers
Jamieson, E., Kealley, C. S., van Riessen, A., & Hart, R. (2016) · Materials · doi:10.3390/ma9050392 · Cited by 18
Gamma irradiation resistance of early age Ba(OH)2-Na2SO4-slag cementitious grouts
Mobasher, N., Bernal, S. A., Kinoshita, H., & Provis, J. L. (2016) · Journal of Nuclear Materials · doi:10.1016/j.jnucmat.2016.10.032 · Cited by 14
Cited by
Reddy, A. S., Pagano, A. G., Iyer, K. K. R., & Dave, T. N. (2026) · International Journal of Geosynthetics and Ground Engineering · doi:10.1007/s40891-026-00744-0
Metadata
- Authors
- Fu, Q., Bu, M., Zhang, Z., Xu, W., Yuan, Q., & Niu, D.
- Venue
- Engineering
- Publisher
- Elsevier BV
- Published
- 2023-01
- Volume
- 20
- Pages
- 162-179
- ISSN
- 2095-8099 (ISSN-L)
- OpenAlex
- W4200559231
- Cited by
- 272
- References
- 120
- FWCI
- 13.77
- Type
- journal article
- Language
- en
- Open access
- gold
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.