Additive manufacturing of Ti6Al4V alloy: A review
Open accessAbstract
In this paper, the recent progress on Ti6Al4V fabricated by three mostly developed additive manufacturing (AM) techniques-directed energy deposition (DED), selective laser melting (SLM) and electron beam melting (EBM)-is thoroughly investigated and compared. Fundamental knowledge is provided for the creation of links between processing parameters, resultant microstructures and associated mechanical properties. Room temperature tensile and fatigue properties are also reviewed and compared to traditionally manufactured Ti6Al4V parts. The presence of defects in as-built AM Ti6Al4V components and the influences of these defects on mechanical performances are also critically discussed.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Metal Additive Manufacturing: A Review
Frazier, W. E. (2014) · Journal of Materials Engineering and Performance · doi:10.1007/s11665-014-0958-z · Cited by 5,984
Additive manufacturing of metals
Herzog, D., Seyda, V., Wycisk, E., & Emmelmann, C. (2016) · Acta Materialia · doi:10.1016/j.actamat.2016.07.019 · Cited by 4,759
Gibson, I., Rosen, D., & Stucker, B. (2015) · doi:10.1007/978-1-4939-2113-3 · Cited by 3,299
A study of the microstructural evolution during selective laser melting of Ti–6Al–4V
Thijs, L., Verhaeghe, F., Craeghs, T., Humbeeck, J. V., & Kruth, J.-P. (2010) · Acta Materialia · doi:10.1016/j.actamat.2010.02.004 · Cited by 2,929
An overview on the use of titanium in the aerospace industry
Boyer, R. R. (1996) · Materials Science and Engineering: A · doi:10.1016/0921-5093(96)10233-1 · Cited by 2,442
Additive manufacturing: technology, applications and research needs
Guo, N., & Leu, M. C. (2013) · Frontiers of Mechanical Engineering · doi:10.1007/s11465-013-0248-8 · Cited by 2,073
Residual stresses in selective laser sintering and selective laser melting
Mercelis, P., & Kruth, J. (2006) · Rapid Prototyping Journal · doi:10.1108/13552540610707013 · Cited by 2,015
Vrancken, B., Thijs, L., Kruth, J.-P., & Van Humbeeck, J. (2012) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2012.07.022 · Cited by 1,896
Donachie, M. J. (1988) · Cited by 1,662
Carroll, B. E., Palmer, T. A., & Beese, A. M. (2015) · Acta Materialia · doi:10.1016/j.actamat.2014.12.054 · Cited by 1,507
Leuders, S., Thöne, M., Riemer, A., Niendorf, T., Tröster, T., Richard, H. A., & Maier, H. J. (2013) · International Journal of Fatigue · doi:10.1016/j.ijfatigue.2012.11.011 · Cited by 1,475
Vilaro, T., Colin, C., & Bartout, J. D. (2011) · Metallurgical and Materials Transactions A · doi:10.1007/s11661-011-0731-y · Cited by 1,283
Phase transformations during cooling in α+β titanium alloys
Ahmed, T., & Rack, H. J. (1998) · Materials Science and Engineering A · doi:10.1016/s0921-5093(97)00802-2 · Cited by 1,224
Thompson, S. M., Bian, L., Shamsaei, N., & Yadollahi, A. (2015) · Additive Manufacturing · doi:10.1016/j.addma.2015.07.001 · Cited by 1,179
Effect of the build orientation on the mechanical properties and fracture modes of SLM Ti–6Al–4V
Simonelli, M., Tse, Y. Y., & Tuck, C. (2014) · Materials Science and Engineering: A · doi:10.1016/j.msea.2014.07.086 · Cited by 1,010
Mechanical behavior of additive manufactured, powder-bed laser-fused materials
Mower, T. M., & Long, M. J. (2016) · Materials Science and Engineering: A · doi:10.1016/j.msea.2015.10.068 · Cited by 1,001
Murr, L. E., Quinones, S. A., Gaytan, S. M., Lopez, M. I., Rodela, A., Martinez, E. Y., Hernandez, D. H., Martinez, E., Medina, F., & Wicker, R. B. (2009) · Journal of the Mechanical Behavior of Biomedical Materials · doi:10.1016/j.jmbbm.2008.05.004 · Cited by 997
Rafi, H. K., Karthik, N. V., Gong, H., Starr, T. L., & Stucker, B. E. (2013) · Journal of Materials Engineering and Performance · doi:10.1007/s11665-013-0658-0 · Cited by 987
Gong, H., Rafi, K., Gu, H., Janaki Ram, G. D., Starr, T., & Stucker, B. (2015) · Materials & Design · doi:10.1016/j.matdes.2015.07.147 · Cited by 940
Formation and control of martensite in Ti-6Al-4V alloy produced by selective laser melting
Yang, J., Yu, H., Yin, J., Gao, M. X., Wang, Z., & Zeng, X. (2016) · Materials & Design · doi:10.1016/j.matdes.2016.06.117 · Cited by 913
Fatigue performance evaluation of selective laser melted Ti–6Al–4V
Edwards, P., & Ramulu, M. (2014) · Materials Science and Engineering: A · doi:10.1016/j.msea.2014.01.041 · Cited by 874
Al-Bermani, S. S., Blackmore, M., Zhang, W., & Todd, I. (2010) · Metallurgical and Materials Transactions A · doi:10.1007/s11661-010-0397-x · Cited by 860
Qiu, C., Adkins, N. J. E., & Attallah, M. M. (2013) · Materials Science and Engineering: A · doi:10.1016/j.msea.2013.04.099 · Cited by 821
Effect of interstitial solutes on the strength and ductility of titanium
Conrad, H. (1981) · Progress in Materials Science · doi:10.1016/0079-6425(81)90001-3 · Cited by 821
Huang, R., Riddle, M., Graziano, D., Warren, J., Das, S., Nimbalkar, S., Cresko, J., & Masanet, E. (2016) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2015.04.109 · Cited by 805
Gokuldoss, P. K., Kolla, S., & Eckert, J. (2017) · Materials · doi:10.3390/ma10060672 · Cited by 804
Antonysamy, A. A., Meyer, J., & Prangnell, P. B. (2013) · Materials Characterization · doi:10.1016/j.matchar.2013.07.012 · Cited by 747
Parry, L., Ashcroft, I. A., & Wildman, R. D. (2016) · Additive Manufacturing · doi:10.1016/j.addma.2016.05.014 · Cited by 739
Improvement of fatigue resistance and ductility of TiAl6V4 processed by selective laser melting
Kasperovich, G., & Hausmann, J. (2015) · Journal of Materials Processing Technology · doi:10.1016/j.jmatprotec.2015.01.025 · Cited by 735
Zhao, X., Li, S., Zhang, M., Liu, Y., Sercombe, T. B., Wang, S., Hao, Y., Yang, R., & Murr, L. E. (2016) · Materials & Design · doi:10.1016/j.matdes.2015.12.135 · Cited by 673
Beretta, S., & Romano, S. (2017) · International Journal of Fatigue · doi:10.1016/j.ijfatigue.2016.06.020 · Cited by 635
Overview of Materials Qualification Needs for Metal Additive Manufacturing
Seifi, M., Salem, A., Beuth, J., Harrysson, O., & Lewandowski, J. J. (2016) · JOM · doi:10.1007/s11837-015-1810-0 · Cited by 630
Tammas-Williams, S., Zhao, H., Léonard, F., Derguti, F., Todd, I., & Prangnell, P. B. (2015) · Materials Characterization · doi:10.1016/j.matchar.2015.02.008 · Cited by 590
A study on the residual stress during selective laser melting (SLM) of metallic powder
Liu, Y., Yang, Y., & Wang, D. (2016) · The International Journal of Advanced Manufacturing Technology · doi:10.1007/s00170-016-8466-y · Cited by 573
Wang, T., Zhu, Y. Y., Zhang, S. Q., Tang, H., & Wang, H. M. (2015) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2015.01.256 · Cited by 557
Li, P., Warner, D. H., Fatemi, A., & Phan, N. (2016) · International Journal of Fatigue · doi:10.1016/j.ijfatigue.2015.12.003 · Cited by 546
Wilson, J. M., Piya, C., Shin, Y. C., Zhao, F., & Ramani, K. (2014) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2014.05.084 · Cited by 543
Self-citationMurr, L. E., Gaytan, S. M., Ceylan, A., Martinez, E., Martinez, J. L., Hernandez, D. H., Machado, B. I., Ramirez, D. A., Medina, F., Collins, S., et al. (2010) · Acta Materialia · doi:10.1016/j.actamat.2009.11.032 · Cited by 526
Yadroitsev, I., Krakhmalev, P., & Yadroitsava, I. (2014) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2013.08.183 · Cited by 515
Ductility of a Ti‐6Al‐4V alloy produced by selective laser melting of prealloyed powders
Facchini, L., Magalini, E., Robotti, P., Molinari, A., Höges, S., & Wissenbach, K. (2010) · Rapid Prototyping Journal · doi:10.1108/13552541011083371 · Cited by 512
Characterization of titanium alloy Ti-6Al-4V for chemical, marine and industrial applications
Gurrappa, I. (2003) · Materials Characterization · doi:10.1016/j.matchar.2003.10.006 · Cited by 512
Effects of Defects in Laser Additive Manufactured Ti-6Al-4V on Fatigue Properties
Wycisk, E., Solbach, A., Siddique, S., Herzog, D., Walther, F., & Emmelmann, C. (2014) · Physics Procedia · doi:10.1016/j.phpro.2014.08.120 · Cited by 509
The Influence of Porosity on Fatigue Crack Initiation in Additively Manufactured Titanium Components
Tammas-Williams, S., Withers, P. J., Todd, I., & Prangnell, P. B. (2017) · Scientific Reports · doi:10.1038/s41598-017-06504-5 · Cited by 494
Hollander, D. A., von Walter, M., Wirtz, T., Sellei, R., Schmidt-Rohlfing, B., Paar, O., & Erli, H.-J. (2006) · Biomaterials · doi:10.1016/j.biomaterials.2005.07.041 · Cited by 482
Fatigue life of additively manufactured Ti–6Al–4V in the very high cycle fatigue regime
Günther, J., Krewerth, D., Lippmann, T., Leuders, S., Tröster, T., Weidner, A., Biermann, H., & Niendorf, T. (2017) · International Journal of Fatigue · doi:10.1016/j.ijfatigue.2016.05.018 · Cited by 475
Wauthle, R., Vrancken, B., Beynaerts, B., Jorissen, K., Schrooten, J., Kruth, J.-P., & Van Humbeeck, J. (2015) · Additive Manufacturing · doi:10.1016/j.addma.2014.12.008 · Cited by 463
Closed loop direct metal deposition: art to part
Mazumder, J., Dutta, D., Kikuchi, N., & Ghosh, A. (2000) · Optics and Lasers in Engineering · doi:10.1016/s0143-8166(00)00072-5 · Cited by 452
Electron Beam Additive Manufacturing of Titanium Components: Properties and Performance
Edwards, P., O'Conner, A., & Ramulu, M. (2013) · Journal of Manufacturing Science and Engineering · doi:10.1115/1.4025773 · Cited by 450
Microstructures of laser-deposited Ti–6Al–4V
Wu, X., Liang, J., Mei, J., Mitchell, C., Goodwin, P. S., & Voice, W. (2004) · Materials & Design · doi:10.1016/j.matdes.2003.09.009 · Cited by 436
Kobryn, P. A., Moore, E. H., & Semiatin, S. L. (2000) · Scripta Materialia · doi:10.1016/s1359-6462(00)00408-5 · Cited by 428
de Formanoir, C., Michotte, S., Rigo, O., Germain, L., & Godet, S. (2015) · Materials Science and Engineering A · doi:10.1016/j.msea.2015.11.052 · Cited by 404
Additive fabrication technologies applied to medicine and health care: a review
Giannatsis, J., & Dedoussis, V. (2009) · The International Journal of Advanced Manufacturing Technology · doi:10.1007/s00170-007-1308-1 · Cited by 389
Additive manufacturing of titanium alloy for aircraft components
Uhlmann, E., Kersting, R., Klein, T. B., Cruz, M. F., & Borille, A. V. (2015) · Procedia CIRP · doi:10.1016/j.procir.2015.08.061 · Cited by 386
Effect of surface roughness on fatigue performance of additive manufactured Ti–6Al–4V
Greitemeier, D., Donne, C. D., Syassen, F., Eufinger, J., & Melz, T. (2015) · Materials Science and Technology · doi:10.1179/1743284715y.0000000053 · Cited by 379
Hrabe, N., Gnäupel-Herold, T., & Quinn, T. (2017) · International Journal of Fatigue · doi:10.1016/j.ijfatigue.2016.04.022 · Cited by 355
Defect generation and propagation mechanism during additive manufacturing by selective beam melting
Bauereiß, A., Scharowsky, T., & Körner, C. (2014) · Journal of Materials Processing Technology · doi:10.1016/j.jmatprotec.2014.05.002 · Cited by 351
Hrabe, N. W., & Quinn, T. P. (2013) · Materials Science and Engineering A · doi:10.1016/j.msea.2013.02.065 · Cited by 349
Microstructure and mechanical behavior of porous Ti–6Al–4V parts obtained by selective laser melting
Sallica-Leva, E., Jardini, A. L., & Fogagnolo, J. B. (2013) · Journal of the Mechanical Behavior of Biomedical Materials · doi:10.1016/j.jmbbm.2013.05.011 · Cited by 340
Galarraga, H., Lados, D. A., Dehoff, R., Kirka, M. M., & Nandwana, P. (2016) · Additive manufacturing · doi:10.1016/j.addma.2016.02.003 · Cited by 334
Chan, K. S., Koike, M., Mason, R. L., & Okabe, T. (2013) · Metallurgical and Materials Transactions A · doi:10.1007/s11661-012-1470-4 · Cited by 320
Titanium alloys for marine application
Gorynin, I. V. (1999) · Materials Science and Engineering A · doi:10.1016/s0921-5093(98)01180-0 · Cited by 316
Laser and Electron Beam Additive Manufacturing Methods of Fabricating Titanium Bone Implants
Wysocki, B., Maj, P., Sitek, R., Buhagiar, J., Kurzydłowski, K., & Święszkowski, W. (2017) · Applied Sciences · doi:10.3390/app7070657 · Cited by 300
Seifi, M., Salem, A. A., Satko, D. P., Shaffer, J., & Lewandowski, J. J. (2016) · International Journal of Fatigue · doi:10.1016/j.ijfatigue.2016.06.001 · Cited by 291
Fabrication of Ti-6Al-4V Scaffolds by Direct Metal Deposition
Dinda, G. P., Song, L., & Mazumder, J. (2008) · Metallurgical and Materials Transactions A · doi:10.1007/s11661-008-9634-y · Cited by 288
Tensile Properties and Microstructures of Laser-Formed Ti-6Al-4V
Alcisto, J., Enriquez, A., Garcia, H., Hinkson, S., Steelman, T., Silverman, E. M., Valdovino, P., Gigerenzer, H., Foyos, J., Ogren, J. R., et al. (2010) · Journal of Materials Engineering and Performance · doi:10.1007/s11665-010-9670-9 · Cited by 284
Koike, M., Greer, P., Owen, K., Guo, L., Murr, L. E., Gaytan, S. M., Martinez, E., & Okabe, T. H. (2011) · Materials · doi:10.3390/ma4101776 · Cited by 270
Biomedical titanium alloys and their additive manufacturing
Hao, Y., Li, S., & Yang, R. (2016) · Rare Metals · doi:10.1007/s12598-016-0793-5 · Cited by 267
Predicting tensile properties of Ti-6Al-4V produced via directed energy deposition
Hayes, B. J., Martin, B. W., Welk, B. A., Kuhr, S. J., Ales, T. K., Brice, D. A., Ghamarian, I., Baker, A. H., Haden, C. V., Harlow, D. G., et al. (2017) · Acta Materialia · doi:10.1016/j.actamat.2017.05.025 · Cited by 257
Zhang, J., Wang, X., Paddea, S., & Zhang, X. (2015) · Materials & Design · doi:10.1016/j.matdes.2015.10.141 · Cited by 248
Ti-6Al-4V Additively Manufactured by Selective Laser Melting with Superior Mechanical Properties
Xu, W., Sun, S., Elambasseril, J., Liu, Q., Brandt, M., & Qian, M. (2015) · JOM · doi:10.1007/s11837-015-1297-8 · Cited by 244
Advanced metal powder based manufacturing of complex components by electron beam melting
Gaytan, S. M., Murr, L. E., Medina, F. R., Martinez, E., Lopez, M. I., & Wicker, R. B. (2009) · Materials Technology · doi:10.1179/106678509x12475882446133 · Cited by 235
Chastand, V., Quaegebeur, P., Maia, W., & Charkaluk, E. (2018) · Materials Characterization · doi:10.1016/j.matchar.2018.03.028 · Cited by 234
Porosity formation and gas bubble retention in laser metal deposition
Ng, G. K. L., Jarfors, A. E. W., Bi, G., & Zheng, H. Y. (2009) · Applied Physics A · doi:10.1007/s00339-009-5266-3 · Cited by 230
Influence of tempering temperature and time on the α′-Ti-6Al-4V martensite
Gil, F. X., Rius, D. R., & Planell, J. A. (1996) · Journal of Alloys and Compounds · doi:10.1016/0925-8388(95)02057-8 · Cited by 230
Bermingham, M. J., Nicastro, L., Kent, D., Chen, Y., & Dargusch, M. S. (2018) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2018.04.158 · Cited by 227
Controlling of residual stress in additive manufacturing of Ti6Al4V by finite element modeling
Vastola, G., Zhang, G., Pei, Q. X., & Zhang, Y.-W. (2016) · Additive Manufacturing · doi:10.1016/j.addma.2016.05.010 · Cited by 226
Gasser, A., Backes, G., Kelbassa, I., Weisheit, A., & Wissenbach, K. (2010) · Laser Technik Journal · doi:10.1002/latj.201090029 · Cited by 223
Laser Additive Manufacturing and Bionics: Redefining Lightweight Design
Emmelmann, C., Sander, P., Kranz, J., & Wycisk, E. (2011) · Physics Procedia · doi:10.1016/j.phpro.2011.03.046 · Cited by 222
High Cycle Fatigue (HCF) Performance of Ti-6Al-4V Alloy Processed by Selective Laser Melting
Wycisk, E., Emmelmann, C., Siddique, S., & Walther, F. (2013) · Advanced Materials Research · doi:10.4028/www.scientific.net/amr.816-817.134 · Cited by 215
Characteristics of laser aided direct metal/material deposition process for tool steel
Choi, J. R., & Chang, Y. (2004) · International Journal of Machine Tools and Manufacture · doi:10.1016/j.ijmachtools.2004.08.014 · Cited by 209
Agius, D., Kourousis, K. I., & Wallbrink, C. (2018) · Metals · doi:10.3390/met8010075 · Cited by 205
Hönnige, J. R., Colegrove, P. A., Ahmad, B., Fitzpatrick, M. E., Ganguly, S., Lee, T. L., & Williams, S. W. (2018) · Materials & Design · doi:10.1016/j.matdes.2018.03.065 · Cited by 200
Microstructure and Mechanical Properties of High Strength Two-Phase Titanium Alloys
Sieniawski, J., Ziaja, W., Kubiak, K., & Motyk, M. (2013) · InTech eBooks · doi:10.5772/56197 · Cited by 198
Material Properties of Ti6Al4V Parts Produced by Laser Metal Deposition
Yu, J., Rombouts, M., Maes, G., & Motmans, F. (2012) · Physics Procedia · doi:10.1016/j.phpro.2012.10.056 · Cited by 193
Mahamood, R. M., & Akinlabi, E. T. (2017) · 3D Printing · doi:10.4018/978-1-5225-1677-4.ch008 · Cited by 183
Additive manufacturing for aerospace flight applications
Shapiro, A. A., Borgonia, J. P., Chen, Q. N., Dillon, R. P., McEnerney, B., Polit-Casillas, R., & Soloway, L. (2016) · Journal of Spacecraft and Rockets · doi:10.2514/1.a33544 · Cited by 178
The formation of α + β microstructure in as-fabricated selective laser melting of Ti–6Al–4V
Simonelli, M., Tse, Y. Y., & Tuck, C. J. (2014) · Journal of materials research/Pratt's guide to venture capital sources · doi:10.1557/jmr.2014.166 · Cited by 154
Characterization of Effect of Support Structures in Laser Additive Manufacturing of Stainless Steel
Järvinen, J.-P., Matilainen, V., Li, X., Piili, H., Salminen, A., Mäkelä, I., & Nyrhilä, O. (2014) · Physics Procedia · doi:10.1016/j.phpro.2014.08.099 · Cited by 142
Li, P., Guo, W., Huang, W., Su, Y., Lin, X., & Yuan, K. (2015) · Materials Science and Engineering A · doi:10.1016/j.msea.2015.08.043 · Cited by 140
Baumers, M., Tuck, C. J., Wildman, R. D., Ashcroft, I., & Hague, R. (2016) · Journal of Industrial Ecology · doi:10.1111/jiec.12397 · Cited by 137
Laser Metal Deposition as Repair Technology for a Gas Turbine Burner Made of Inconel 718
Petrat, T., Graf, B., Gumenyuk, A., & Rethmeier, M. (2016) · Physics Procedia · doi:10.1016/j.phpro.2016.08.078 · Cited by 131
Li, X.-L., Xie, J., & Zhou, Y. (2005) · Journal of Materials Science · doi:10.1007/s10853-005-0447-8 · Cited by 126
Seifi, M., Dahar, M. S., Aman, R., Harrysson, O. L. A., Beuth, J., & Lewandowski, J. J. (2015) · JOM · doi:10.1007/s11837-015-1298-7 · Cited by 123
Biswas, N., Ding, J., Balla, V. K., Field, D. P., & Bandyopadhyay, A. K. (2012) · Materials Science and Engineering A · doi:10.1016/j.msea.2012.04.036 · Cited by 112
Crystallographic texture and microstructure of pulsed diode laser-deposited Waspaloy
Moat, R. J., Pinkerton, A. J., Li, L., Withers, P. J., & Preuß, M. (2008) · Acta Materialia · doi:10.1016/j.actamat.2008.11.004 · Cited by 89
Effect of Melt Scan Rate on Microstructure and Macrostructure for Electron Beam Melting of Ti-6Al-4V
Puebla, K., Murr, L. E., Gaytan, S. M., Martinez, E., Medina, F. R., & Wicker, R. B. (2012) · Materials Sciences and Applications · doi:10.4236/msa.2012.35038 · Cited by 85
Process Analysis of Laser Beam Cladding
Kaplan, A. F. H., & Groboth, G. (2000) · Journal of Manufacturing Science and Engineering · doi:10.1115/1.1344899 · Cited by 82
High Cycle Fatigue of Laser Beam Deposited Ti-6Al-4V and Inconel 718
Amsterdam, E., & Kool, G. A. (2009) · Springer eBooks · doi:10.1007/978-90-481-2746-7_71 · Cited by 75
Rapid Product Development in the USA, Europe and Japan
Waterman, N. A., & Dickens, P. (1994) · World Class Design to Manufacture · doi:10.1108/09642369210056629 · Cited by 74
Effect of microstructure and defects on fatigue behaviour of directed energy deposited Ti–6Al–4V
Prabhu, A. W., Vincent, T., Chaudhary, A., Zhang, W., & Babu, S. S. (2015) · Science and Technology of Welding & Joining · doi:10.1179/1362171815y.0000000050 · Cited by 69
Allen, J. H. (2006) · Cited by 68
Solid Freeform Fabrication Proceedings
Bourell, D. L., & Wood, K. L. (2003) · Defense Technical Information Center (DTIC) · doi:10.21236/ada422996 · Cited by 61
Dislocation Strengthening without Ductility Trade-off in Metastable Austenitic Steels
Liu, J., Jin, Y., Fang, X., Chen, C., Feng, Q., Liu, X., Chen, Y. Z., Suo, T., Zhao, F., Huang, T., et al. (2016) · Scientific Reports · doi:10.1038/srep35345 · Cited by 57
Experimental Temperature Analysis of Powder-Based Electron Beam Additive Manufacturing
Price, S., Lydon, J., Cooper, K., & Chou, K. (2013) · doi:10.26153/tsw/15422 · Cited by 54
An investigation into the recycling of Ti-6Al-4V powder used within SLM to improve sustainability
O’Leary, R., Setchi, R., & Prickett, P. W. (2015) · ORCA Online Research @Cardiff (Cardiff University) · Cited by 42
Precision Finishing of Bevel Gears by Electrochemical Honing
Shaikh, J. H., Jain, N. K., & Venkatesh, V. C. (2013) · Materials and Manufacturing Processes · doi:10.1080/10426914.2013.811737 · Cited by 35
Cited by
Material-structure-performance integrated laser-metal additive manufacturing
Gu, D., Shi, X., Poprawe, R., Bourell, D. L., Setchi, R., & Zhu, J. (2021) · Science · doi:10.1126/science.abg1487 · Cited by 1,703
Svetlizky, D., Das, M., Zheng, B., Vyatskikh, A. L., Bose, S., Bandyopadhyay, A., Schoenung, J. M., Lavernia, E. J., & Eliaz, N. (2021) · Materials Today · doi:10.1016/j.mattod.2021.03.020 · Cited by 1,371
Sanaei, N., & Fatemi, A. (2021) · Progress in Materials Science · doi:10.1016/j.pmatsci.2020.100724 · Cited by 1,029
Directed Energy Deposition (DED) Process: State of the Art
Ahn, D.-G. (2021) · International Journal of Precision Engineering and Manufacturing-Green Technology · doi:10.1007/s40684-020-00302-7 · Cited by 803
Nguyen, H. D., Pramanik, A., Basak, A. K., Dong, Y., Prakash, C., Debnath, S., Shankar, S., Jawahir, I. S., Dixit, S., & Buddhi, D. (2022) · Journal of Materials Research and Technology · doi:10.1016/j.jmrt.2022.04.055 · Cited by 634
Metadata
- Authors
- Liu, S., & Shin, Y. C.
- Venue
- Materials & Design
- Publisher
- Elsevier BV
- Published
- 2019-02
- Volume
- 164
- Pages
- 107552
- ISSN
- 0264-1275 (ISSN-L)
- OpenAlex
- W2904619063
- Cited by
- 2,472
- References
- 106
- FWCI
- 106.17
- Type
- journal article
- Language
- en
- Open access
- hybrid
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.