Abstract
Nanoscale resistive switching devices, sometimes termed memristors, have recently generated significant interest for memory, logic and neuromorphic applications. Resistive switching effects in dielectric-based devices are normally assumed to be caused by conducting filament formation across the electrodes, but the nature of the filaments and their growth dynamics remain controversial. Here we report direct transmission electron microscopy imaging, and structural and compositional analysis of the nanoscale conducting filaments. Through systematic ex-situ and in-situ transmission electron microscopy studies on devices under different programming conditions, we found that the filament growth can be dominated by cation transport in the dielectric film. Unexpectedly, two different growth modes were observed for the first time in materials with different microstructures. Regardless of the growth direction, the narrowest region of the filament was found to be near the dielectric/inert-electrode interface in these devices, suggesting that this region deserves particular attention for continued device optimization.
Overview
CoChat Summary
## TL;DR
Using ex-situ and in-situ TEM, the paper directly visualizes conducting filaments in nanoscale resistive memories and shows that filament growth can be limited by cation transport in the dielectric. It also reports two growth modes, including an unexpected mode in which filaments start from the active electrode and grow toward the inert electrode.
## Key findings
- In over 100 devices studied, none showed more than one completed filament.
- For SiO2-based devices, the authors observed conical filaments with a typical lateral size of ~20 nm near the tip and ~70 nm at the base; the filaments were verified to be composed of elemental Ag.
- In a-Si-based devices, partially formed filaments were sometimes seen starting from the active Ag electrode, and detailed TEM/EDS/SAED showed they were also composed of elemental Ag, sometimes as a chain of nanoparticles separated by 1–4 nm gaps.
- Across device types, the narrowest region of the filament was found near the dielectric/inert-electrode interface, and erasing typically began there; in-situ TEM on vertical Ag/a-Si/W devices confirmed this active-electrode-to-inert-electrode growth and inert-interface dissolution.
## Methods
- The study combined ex-situ and in-situ transmission electron microscopy with structural and compositional analysis (TEM, STEM/HAADF, HRTEM, SAED, EDS) on resistive memory devices.
- Devices used different dielectric layers of about 15 nm thickness: SiO2, Al2O3, and a-Si; planar devices were fabricated on ultrathin 15 nm SiNx membranes, and vertical Ag/a-Si/W devices were used for in-situ TEM.
- Electrical switching was measured with current compliance; the main analysis related filament morphology and switching behavior to dielectric choice, programming current, electric field, and temperature, including 36 a-Si-based resistive switches for the field-scaling data.
## Limitations
- The authors state that the switching time and electric field used here are still different from standard ECM cell operating conditions, so the filament growth under specific conditions must be analyzed individually.
- The paper itself notes that detailed analysis of the electrochemical processes and cation transport dynamics remains for future investigation.
- Evident from the text: many conclusions are based on specific device geometries and materials under ex-situ/in-situ TEM conditions, so direct generalization to all resistive memories is not established in the paper.
Model-written summary. Check it against the paper before relying on it.
Integrity signals
Registry
Cites
Statistics
Figures





Verification
Claims the paper makes
4 Valid · 1 Not valid · 15 Not checked · 77 Own results and interpretations
Every source the paper cites for this claim was checked and supports it.
In the paper
“In general, the filament growth is determined by three dynamic processes 27 : (i) the anodic dissolution of the metal component at the active electrode; (ii) the transport of the metal ions through the dielectrics; and (iii) the reduction of metal ions and the crystallization of conducting filaments.”
What the sources say
- Supportedcites [27] Valov, I., Waser, R., Jameson, J. R & Kozicki,, M. N. Electrochemical metallization memories — fundamentals, applications, prospects. Nanotechnol. 22, 254003 (2011). source
Split into 3 atoms — 3 confirmed, 0 partially supported, 0 disputed, 0 misattributed, 0 unverifiable. Expand the claim to see per-atom verdicts.
plainstates a cause- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: passes — The paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
- Supported
The cited sources support only part of this claim — read each source’s verdict below.
In the paper
“This effect explains the observations in ECM devices that lower threshold voltages are typically required during programming processes, compared with those for the initial forming process 22,27,28 .”
What the sources say
- Not checked — no full text of the sourcecites [22] Waser, R., Dittmann, R., Staikov, G. & Szot, K. Redox-based resistive switching memories - Nanoionic mechanisms, prospects, and challenges. Adv. Mater. 21, 2632–2663 (2009). source
- Partly supportedcites [27] Valov, I., Waser, R., Jameson, J. R & Kozicki,, M. N. Electrochemical metallization memories — fundamentals, applications, prospects. Nanotechnol. 22, 254003 (2011). sourceExperimental — accuracy not yet measured
Section 3.3 (page unavailable) distinguishes the initial forming cycle from later switching cycles and suggests that forming may leave a nano-channel that aids subsequent filament growth. This supports the proposed mechanism, but the passage does not state that programming threshold voltages are typically lower than forming voltages. (LLM, conf=0.78)
- Not checked — no full text of the sourcecites [28] Schindler, C., Staikov, G. & Waser, R. Electrode kinetics of Cu–SiO2-based resistive switching cells: Overcoming the voltage-time dilemma of electrochemical metallization memories. Appl. Phys. Lett. 94, 072109 (2009). source
plainstates a cause- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: passes — The paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
A result the paper reports from its own data — it cites no other source for it, so there is none to check. The quote shows it is in the paper.
In the paper
“the filaments in Fig. 1b apparently started growth from the inert electrode side as evidenced by the locations of the partially formed filaments.”
hedgedstates a cause- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: passes — The paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
A result the paper reports from its own data — it cites no other source for it, so there is none to check. The quote shows it is in the paper.
In the paper
“many of the incomplete filaments exhibiting a noteworthy dendrite structure with the branches pointing towards the active electrode”
plainstates an association- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: passes — The paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
A result the paper reports from its own data — it cites no other source for it, so there is none to check. The quote shows it is in the paper.
In the paper
“we provide unambiguous evidence that shows that localized, nanoscale filaments composed of elemental metals (and, in some cases, consisting of discrete nanoparticles instead of a solid wire) are formed during resistive switching.”
boostedstates a cause- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: passes — The paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
51 more claims
Create a free account to see all 97 claims and every source verdict.
- It may state two separate claims as one. 36
- Probably not a substantial claim. 10
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“The change from OFF to ON state is explained by the formation of a dominating Ag filament (15,16).”
From Stochastic memristive devices for computing and neuromorphic applications (2013) · cites this paper as [16]
Citations
Cites
Strukov, D. B., Snider, G. S., Stewart, D. R., & Williams, R. S. (2008) · Nature · doi:10.1038/nature06932 · Cited by 11,828
Memristor—The Missing Circuit Element
Chua, L. (1971) · IEEE Transactions on Circuit Theory · doi:10.1109/tct.1971.1083337 · Cited by 10,268
Redox‐Based Resistive Switching Memories – Nanoionic Mechanisms, Prospects, and Challenges
Waser, R., Dittmann, R., Staikov, G., & Szot, K. (2009) · Advanced Materials · doi:10.1002/adma.200900375 · Cited by 5,080
Nanoionics-based resistive switching memories
Waser, R., & Aono, M. (2007) · Nature Materials · doi:10.1038/nmat2023 · Cited by 4,923
Nanoscale Memristor Device as Synapse in Neuromorphic Systems
Jo, S. H., Chang, T., Ebong, I., Bhadviya, B. B., Mazumder, P., & Lu, W. (2010) · Nano Letters · doi:10.1021/nl904092h · Cited by 4,174
Self-citationMemristive switching mechanism for metal/oxide/metal nanodevices
Yang, J. J., Pickett, M. D., Li, X., Ohlberg, D. A. A., Stewart, D. R., & Williams, R. S. (2008) · Nature Nanotechnology · doi:10.1038/nnano.2008.160 · Cited by 2,987
Memristive devices and systems
Chua, L. O., & Kang, S. M. (1976) · Proceedings of the IEEE · doi:10.1109/proc.1976.10092 · Cited by 2,604
Atomic structure of conducting nanofilaments in TiO2 resistive switching memory
Kwon, D.-H., Kim, K. M., Jang, J. H., Jeon, J. M., Lee, M. H., Kim, G. H., Li, X.-S., Park, G.-S., Lee, B., Han, S., et al. (2010) · Nature Nanotechnology · doi:10.1038/nnano.2009.456 · Cited by 2,092
‘Memristive’ switches enable ‘stateful’ logic operations via material implication
Borghetti, J., Snider, G. S., Kuekes, P. J., Yang, J. J., Stewart, D. R., & Williams, R. S. (2010) · Nature · doi:10.1038/nature08940 · Cited by 1,929
Complementary resistive switches for passive nanocrossbar memories
Linn, E., Rosezin, R., Kügeler, C., & Waser, R. (2010) · Nature Materials · doi:10.1038/nmat2748 · Cited by 1,274
Cited by
Items 1,101–1,200 of 1,201
Structural and Optoelectronic Properties of a-SiOx: Ag Films Used for Ag/SiOx/p-Si Memristor
Gou, Y., Hou, W., Li, D., Meng, W., Chen, Y.-C., & Li, W. (2017) · IOP Conference Series Materials Science and Engineering · doi:10.1088/1757-899x/250/1/012027
Zhang, H. (2017) · DR-NTU (Nanyang Technological University) · doi:10.32657/10356/72896
“materials and electrical switching mechanisms have demonstrated a breakthrough in the performance of RRAM [2, 19, 23, 31-50].”
Science and Technological Understanding of Nano-ionic Resistive Memories (RRAM)
Dash, C. S., & Prabaharan, S. R. S. (2018) · Nanoscience & Nanotechnology-Asia · doi:10.2174/2210681208666180621095241
Sun, Y., Ma, Z., Jiang, X., et al. (2018) · Nanotechnology · doi:10.1088/1361-6528/aad35d
Baek, G. (2018) · Japanese Journal of Applied Physics · doi:10.7567/jjap.57.124201
Hasegawa, T., & Aono, M. (2014) · Wiley eBooks · doi:10.1002/9781118958254.ch19
A novel design of a-Si based memristor with optical readout functionality utilizing silicon prism
Jiang, X., Dong, X., Wang, J., et al. (2019) · doi:10.1117/12.2506347
Neuromorphic Computing with Memristors: From Devices to Integrated Systems
Cai, F. (2019) · Deep Blue (University of Michigan)
Study on the Film of Ti-Si-C-O Oxides and Its Application in Memristor
Zhao, X., Yuan, Y., Liu, C., Li, D., & Li, W. (2020) · IOP Conference Series Materials Science and Engineering · doi:10.1088/1757-899x/711/1/012068
A non-oxidizing fabrication method for lithographic break junctions of sensitive metals
Nyáry, A., Gubicza, Á., Overbeck, J., Pósa, L., Makk, P., Calame, M., Halbritter, A., & Csontos, M. (2020) · Nanoscale Advances · doi:10.1039/d0na00498g
Redox-based memristive devices : towards highly scalable synaptic electronics
Dananjaya, P. A. (2020) · DR-NTU (Nanyang Technological University) · doi:10.32657/10356/146143
Dias, C., Castro, D., Aroso, M., Ventura, J. O., & Aguiar, P. (2021) · bioRxiv (Cold Spring Harbor Laboratory) · doi:10.1101/2021.05.20.444941
Research on emergent physical properties of integrated nanomaterials
リ, チ., & Li, Q. (2020)
Mroczyński, R. (2021) · Joint International EUROSOI Workshop and International Conference on Ultimate Integration on Silicon · doi:10.1109/eurosoi-ulis53016.2021.9560175
Processing and Switching Mechanisms of Materials for Memory Devices in Flexible Electronics
Almadhoun, M. N. (2021) · ERA: Education and Research Archive (University of Alberta) · doi:10.7939/r3-y1vd-hj60
Koch, U., Hoessbacher, C. B., Emboras, A., & Leuthold, J. (2021) · Kluwer international series in electronic materials: science and technology · doi:10.1007/978-3-030-42424-4_15
SiO2-Based Conductive-Bridging Random Access Memory
Chen, W., Tappertzhofen, S., Barnaby, H., & Kozicki, M. N. (2021) · Kluwer international series in electronic materials: science and technology · doi:10.1007/978-3-030-42424-4_7
Ionic Nanoarchitectonics: Creation of Polymer-Based Atomic Switch and Decision-Making Device
Terabe, K., Tsuruoka, T., & Tsuchiya, T. (2022) · NIMS monographs · doi:10.1007/978-4-431-56912-1_7
Optimization of the Parameters of Light-Induced Resistive Switching in Phthalocyanine Films
Drozdov, K. A., Krylov, I. V., Vasilik, V. A., et al. (2021) · Journal of Experimental and Theoretical Physics Letters · doi:10.1134/s0021364021230065
The effect of external stimuli on the performance of memristive oxides
Li, Y., Christensen, D. V., Sanna, S., Esposito, V., & Pryds, N. (2022) · Elsevier eBooks · doi:10.1016/b978-0-12-814629-3.00011-8
Purushothama, J. M., Perret, E., & Vena, A. (2022) · doi:10.1002/9781119902829.refs
Memristive crossbar circuit for neural network and its application in digit recognition
Wan, X., He, N., Liang, D., Xu, W., Wang, L., Lian, X., Liu, X., Xu, F. Y., & Tong, Y. (2022) · Japanese Journal of Applied Physics · doi:10.35848/1347-4065/ac6b01 · Cited by 1
Yang, Y., Takahashi, Y., Tsurumaki‐Fukuchi, A., 有田正志, Moors, M., Buckwell, M., Mehonić, A., & Kenyon, A. J. (2021) · Kluwer international series in electronic materials: science and technology · doi:10.1007/978-3-030-42424-4_5
Self-citationOuyang, J. (2016) · SpringerBriefs in materials · doi:10.1007/978-3-319-31572-0_5
Photoelectric modulation and resistive switching characteristic of ReSe2/WSe2 memtransistor
Yu, X., Chen, F., Xiang, T., Deng, W., Liu, J.-N., & Wang, L. (2022) · Acta Physica Sinica · doi:10.7498/aps.7120221154 · Cited by 1
Synaptic performanceof SnO2: Ag-based optoelectronicdevices
Leng, Y., Li, Y., Luo, H., et al. (2022) · doi:10.1117/12.2652337
Huang, P. C., Zhao, Y., & Kang, J. (2022) · Springer handbooks · doi:10.1007/978-3-030-79827-7_29
Qu, Z., Zhang, W., & Dong, L. (2023) · Proceedings - IEEE International Conference on Robotics and Automation/Proceedings · doi:10.1109/icra48891.2023.10161087
“When the reverse voltage is applied at both ends of the electrode, the conductive filament can be dissolved or broken, and the device changes from a low-resistance state to a high-resistance state [8-11].”
BackgroundMethodLateral Electrochemical Metallization Cells for Reconfigurable Interconnect Systems
Frahm, T., Buttberg, M., Gvozdev, G. A., Müller, R., Chen, S., Sun, B., Raffauf, L., Menzel, S., Valov, I., Wouters, D. J., et al. (2023) · IEEE Journal of the Electron Devices Society · doi:10.1109/jeds.2023.3297855
“Whereas lateral filamentary growth has recently been investigated [19], [20], [21], the separation between the electrodes is on the order of a few hundred nanometers and hence far larger than in typical vertical ECM cells.”
BackgroundGonzales, C., & Gonzales, C. (2023) · Tesis Doctorals en Xarxa (Consorci de Serveis Universitaris de Catalunya) · doi:10.6035/14104.2023.804973
Ke, Q., & Dai, Y. (2023) · Nanotechnology · doi:10.1088/1361-6528/acfb0f
“Some authors observed the growth processes of the conductive fi lament in ECM devices through systematic ex situ and in situ transmission electron microscopy [ 20 ] .”
InfluentialSilicon Oxide-based CBRAM Memory and Neuromorphic Properties
Bousoulas, P., & Tsoukalas, D. (2023) · Royal Society of Chemistry eBooks · doi:10.1039/bk9781839169946-00515
Erokhin, V. V. (2023) · Elsevier eBooks · doi:10.1016/b978-0-323-96027-4.00004-8
Memristor-Based Bayesian Spiking Neural Network for Ibd DiagnosisPreprint
ma, J. (2024) · SSRN Electronic Journal · doi:10.2139/ssrn.4778908
Hu, H., Peng, J., Yu, S., Zhao, Z., Zhang, Y., Zhang, C., Li, Z., Liu, H., Xv, H., & Wang, Y. (2024) · SSRN Electronic Journal · doi:10.2139/ssrn.4791015
Metal Oxide Neural Devices and Their Applications
Song, B. (2024) · Highlights in Science Engineering and Technology · doi:10.54097/zwgj1t76
“Since this structure can intuitively detect the movement of ions under various characterization methods, it is usually used to characterize the resistive switching mechanism of the device [16][17].”
MethodA Nanoscale Vacuum Transistor Based on Vertical Silicon Dioxide Tunneling Junctions
Yidan, H., Zhiwei, L., & Wei, X. (2024) · International Vacuum Nanoelectronics Conference · doi:10.1109/ivnc63480.2024.10652581
Atomic Scale Photomemristors Engineered by Ion Implantation
Yang, J., Khaleghi, S. S. M., Su, Z., et al. (2024) · Conference on Lasers and Electro-Optics Pacific Rim (CLEO-PR) · doi:10.1109/cleo-pr60912.2024.10676924
High On/Off Ratio Zns-Based Reram with Multi-Level SwitchingPreprint
Jang, J., Lee, S.-H., Khan, S. A., & Hong, S.-M. (2025) · SSRN Electronic Journal · doi:10.2139/ssrn.5082062
Investigation of electrophysical properties of polyimide-CuO/Cu2O composite
Boyko, A. N., Дмитриевич, К. М., Vertyanov, D. V., Gaev, D. S., Belyakov, I. A., Pebalk, D. V., Rekhviashvili, S. S., & Тимошенков, С. П. (2025) · Journal of Materials Science Materials in Electronics · doi:10.1007/s10854-025-14495-7
“…three principal categories of filaments: (1) metallic filaments, which are formed during the dissociation, migration, and reduction of metal ions [32]; (2) conductive channels based on oxygen vacancies, which are observed in binary or complex metal oxides [33]; and (3) carbon-containing…”
Self-integrating dual oxide memristor for artificial neuron functionality
Kumar, B. M., Harish, A. S., Malavika, C., et al. (2025) · APL Electronic Devices · doi:10.1063/5.0253472
Zhu, Y., Wang, X., Zhang, M., et al. (2025) · SSRN Electronic Journal · doi:10.2139/ssrn.5354757
Jia, W., Hu, L., Mu, W., & Liu, W. (2025) · IEEE Transactions on Electron Devices · doi:10.1109/ted.2025.3607913
“Restrictions apply. interface, resulting in the conductive filament forming an inverted triangular shape [42], [43], [44].”
Memristive Behavior in Carrier Accumulation-Based Optical Modulators
Korneluk, A., Brańko, K., & Stefaniuk, T. (2025) · Nano Letters · doi:10.1021/acs.nanolett.5c03443 · Cited by 1
“22 The ECM mechanism in memristors offers several advantages, including low energy consumption, fast switching speeds, and high endurance, making it a promising approach for nonvolatile memory applications.”
Voltage-Induced Power-Law Plasticity in Silver Nanocomposites Near the Percolation Threshold
Hsu, W.-C. A., Tseng, B.-W., Chen, H.-Y., & Chang, T. (2025) · IEEE Transactions on Electron Devices · doi:10.1109/ted.2025.3628808
Self-citationTu, C. W., Chiu, P.-K., Yeh, C., Hsu, H., & Shih, C. (2025) · SSRN Electronic Journal · doi:10.2139/ssrn.5812550 · Cited by 1
Tu, C. W., Chiu, P.-K., Yeh, C., Hsu, H., & Shih, C. (2025) · SSRN Electronic Journal · doi:10.2139/ssrn.5812551
Atomic-Scale Insights Into the Switching Mechanisms of RRAM Devices
Chowdhury, M. T. R., Moazzeni, A., & Tütüncüoğlu, G. (2025) · IEEE International Midwest Symposium on Circuits and Systems (MWSCAS) · doi:10.1109/mwscas53549.2025.11244428
“Experimental evidence derived from state-of-the-art characterization techniques highlights that these conductive filaments function as channels that accommodate ionic and electronic transport [10, 11].”
Improvement on Uniformity and Endurance of Ag-Based Volatile Memristor via Annealing Engineering
Yi, Y., Song, X., Tang, Z., Li, S., Sun, D., Song, S., Feng, Y., Zhou, Z., Huang, P. C., Kang, J., et al. (2025) · IEEE Transactions on Electron Devices · doi:10.1109/ted.2025.3636494
Ismail, M., Rasheed, M., Mahata, C., Kang, M., & Kim, S. (2024) · Figshare · doi:10.6084/m9.figshare.26602792
Memristor Effects and Anisotropy in a Polyimide-TiV Composite with Filamentous Conducting Channels
Boyko, A. N., Дмитриевич, К. М., Vertyanov, D. V., Gaev, D. S., & Pebalk, D. V. (2025) · Semiconductors · doi:10.1134/s1063782625700125
Ultrafast laser direct fabricating lateral-structured memristor with ultralow power
Zhang, Z., Zhao, X., Chen, Y., et al. (2026) · Optics & Laser Technology · doi:10.1016/j.optlastec.2026.115065
Metal penetration induced interfacial challenges and engineering strategies in OSV devices
Shi, D. (2026) · Frontiers in Electronics · doi:10.3389/felec.2026.1799771
“These approaches include interlayer engineering (Hu et al., 2023; Morley et al., 2013; Szulczewski et al., 2011; Yang et al., 2012), alternative selection of spacer materials (Gobbi et al., 2011; Jang and Richter, 2017; Kaushik et al., 2025a; Majumdar et al., 2006), tuning deposition parameters…”
Development of filamentary Memristive devices for synaptic plasticity implementation
Barbera, S. L. (2015) · theses.fr (ABES) · doi:10.70675/91a39e21z25c6z44d8zb0d3zd298023d1a34
Local learning with highly analog memory devices
Bennett, C. H. (2018) · theses.fr (ABES) · doi:10.70675/e49026a5z4027z44f2za795z67ee03a38150
“In [60], transmission electron microscopy revealed two different varieties of filamentary growth, and suggested that since the narrowest filament growth was near the dielectric (inert electrode), this area may need to be further optimized in future devices.”
BackgroundInvestigation of resistive memories for Storage Class Memory applications
Robayo, D. A. (2020) · theses.fr (ABES) · doi:10.70675/8cd461fezc77cz4d09zbdefzda3c8f42aec3 · Cited by 1
Artificial neural networks with radio-frequency spintronic nano-devices
Leroux, N. (2022) · theses.fr (ABES) · doi:10.70675/acc48b6dzf6c5z436dzbb4az611c0b52d106 · Cited by 1
Light from electrically driven nanogaps
Malchow, K. (2022) · theses.fr (ABES) · doi:10.70675/b8220842z2e76z43fcz99faz897c4a0f0836
Interface engineering of multilayer HfOx memristors for enhanced performance and reliability
Shvetsov, B. S., Matsukatova, A. N., Kuchumov, I. D., Ilin, A. S., Tsiniaikin, I. I., Новосельцев, А. И., Savchuk, T., Николаевич, М. М., Форш, П. А., & Kashkarov, P. K. (2026) · Microelectronics Reliability · doi:10.1016/j.microrel.2026.116146
Xu, J., & Sun, Y. (2026) · ChemElectroChem · doi:10.1002/celc.70208 · Cited by 1
Tuning the resistive switching characteristics of non-stoichiometric tantalum oxide memristors
Nithya, N., Mallikarjun, R., & Itapu, S. (2026) · Applied Physics A · doi:10.1007/s00339-026-09567-2
A Wideband Programmable Multibit RF Memristor on Passive Silicon Interposer
Xu, Z.-R., Ning, K., Dong, S., Mao, J., & Guo, Y. (2026) · IEEE Transactions on Microwave Theory and Techniques · doi:10.1109/tmtt.2026.3687963
“…studies report that the filament is much thinner at one end (a nm-scale bottleneck) while the opposite end can be significantly thicker; moreover, the weakest / narrowest region is frequently observed near the dielectric / inert-electrode interface and governs rupture and LRS behavior [40].”
Kim, G., Lee, J., Hwang, S. J., et al. (2026) · Journal of Science Advanced Materials and Devices · doi:10.1016/j.jsamd.2026.101182
Adapting Emerging Nonvolatile Memristor Technology for RF Applications
Purushothama, J. M., Ding, Y., Desmulliez, M. P. Y., Goussetis, G., Vena, A., Gadhafi, R., & Perret, E. (2026) · Wiley eBooks · doi:10.1002/9783527847419.ch26
Mohammadi, M., Sachsenweger, T., Comi, E. L., et al. (2026) · Joule · doi:10.1016/j.joule.2026.102473
Mohammadi, M., Ballantyne, T. S., Comi, E. L., et al. (2026) · Zürcher Hochschule für Angewandte Wissenschaften digital collection (Zurich University of Applied Sciences) · doi:10.21256/zhaw-36648
Silver Nano Electrode Array for Controlling Conductive Filament Formation in RRAM
Byun, J.-H., Ko, W.-S., Song, J.-C., Chang, S.-J., & Lee, G. (2026) · Transactions on Electrical and Electronic Materials · doi:10.1007/s42341-026-00709-0
“Therefore, confining the CF path can improve uniformity, but transmission electron microscope observations reveal that a diameter of CFs is tens of nanometers, making nanoscale control challenging [ 28, 29].”
Gap‐Seeded Nucleation of Single Ag Nanoparticles for Filamentary Memristors
Fischer, M., Eglin, D., Lewerenz, M., Franchini, G.-L., Passerini, E., Olalla, N. J., Srikrishnaprabhu, K., Stecher, M., Gisler, R., Fedoryshyn, Y. M., et al. (2026) · Advanced Electronic Materials · doi:10.1002/aelm.70437
Wang, Y., Lyu, Z., Liu, Y., Wang, L., Chen, Y., Jia, X., & Wang, S. (2026) · SSRN Electronic Journal · doi:10.2139/ssrn.6838696
Metal–Organic Framework-Enabled Bimodal Sensory System for Gas Leak Detection and Localization
Zhao, J. Z., Chen, Z., Zeng, W., Zheng, Y., Li, H., Ma, X. C., Li, Q., Zhong, W.-M., Gao, L., Han, S., et al. (2026) · ACS Nano · doi:10.1021/acsnano.6c03433
Cryogenic Forming/Breakdown of HfO$_{x}$ for Reduced C2C Variability in Filamentary RRAM
Kurup, S., Vadlamani, M., Mammo, F., Weinstein, A. L., Filler, M. A., Yu, S., & Vogel, E. M. (2026) · IEEE Transactions on Electron Devices · doi:10.1109/ted.2026.3696937 · Cited by 1
“Note that the following discussion assumes the formation of single or multiple conical CFs governing switching resistance and does not account for branched dendrite-like filaments, which may alter these interpretations [5], [43], [44], [45].”
Probing Ag filamentary networks in a neuromorphic device using surface-enhanced Raman scattering
Rao, T. S., & Kulkarni, G. U. (2026) · Journal of Materials Chemistry A · doi:10.1039/d6ta02559e
Threshold Dynamics of Silver Filament Formation and Rupture in Ag/SiO 2 /Au Memristors
Ranade, V., Veldhoen, W., Gibbins, F., Shradha, S., Murray, C. P., Chunin, I., McCloskey, D. M., & Shvets, I. (2026) · ACS Applied Electronic Materials · doi:10.1021/acsaelm.6c00659
Materials chemistry of resistive switching in memristors
Guan, P., Ning, K., Qin, L., Xiao, S., Li, Y., Li, H., & Zhai, T. (2026) · Scientia Sinica Chimica · doi:10.1360/ssc-2026-0131
Multifunctional and flexible conjugated polymer memristors with an asymmetric electrode structure
Tian, T., Huang, F., Zhong, Y., et al. (2026) · Materials Today Electronics · doi:10.1016/j.mtelec.2026.100231
Memristors with Low Parameter Variability Based on Ti/HfOx/Au/c-Si Structures
Николаевич, М. М., Kuchumov, I. D., Shvetsov, B. S., Matsukatova, A. N., Новосельцев, А. И., Savchuk, T., Koroleva, A. V., Zhigunov, D. M., Ильин, А. С., Форш, П. А., et al. (2026) · Nanobiotechnology Reports · doi:10.1134/s2635167625602219
Studying in vivo neuronal signal processing with memristors in the presence of external noise
Koryazhkina, M. N., Filatov, D. O., Khabibulova, V. A., et al. (2026) · Chaos Solitons & Fractals · doi:10.1016/j.chaos.2026.118889
Tu, C.-H., Chiu, P.-K., Yeh, C., Hsu, H., & Shih, C. (2026) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2026.190436
Environmentally robust organic resistive memory based on TCPB@PVP composite with synaptic plasticity
Lin, J., Ding, W., Zhou, X., Li, X., Sun, X., & Song, K. (2026) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2026.190510
Liu, Y.-Z., Li, L., Yang, K., et al. (2026) · SSRN Electronic Journal · doi:10.2139/ssrn.7324037
Liu, W., Chen, Y., Zheng, Z., Bao, X., Ma, Z., Zhang, H., Pan, S., Yang, H., & Ge, J. (2026) · physica status solidi (RRL) - Rapid Research Letters · doi:10.1002/pssr.70250
“In Ag-based ECM switching, filament formation involves Ag reduction, nucleation, and terminal-contact formation near the counter electrode [27].”
Zuo, Z., Liu, H., Yang, Y., Sun, K., Wang, S., & Chen, S. (2026) · Nanotechnology · doi:10.1088/1361-6528/ae9d2a
“Figure 4(b) shows the current distribution of the device after electrical operation, in which numerous discrete high-current spots appear within the scan area, the I rq increases to 0.296 pA, and the peak current reaches 9.60 pA [46].”
InfluentialSelf-citationCu-ion dynamics-regulated forming-free resistive switching in two-dimensional Ferroionic CuBiP2Se6
Li, Y., Zhen, W., Li, C., et al. (2026) · Microelectronic Engineering · doi:10.1016/j.mee.2026.112508
Interfacial Redox Engineering Driven Forming‐Free Intrinsic Bipolar Switching in SiO x Memristors
Jana, B., Goswami, I., Dinda, A., et al. (2026) · Advanced Electronic Materials · doi:10.1002/aelm.70568
“…is typically classified as either intrinsic, which is driven by oxygen vacancies or silicon-rich defect pathways within the oxide matrix [ 28, 29 ] or extrinsic, arising from electrochemical metallization (ECM) associated with electrochemically active metal electrodes (e.g., Cu and Ag) [ 30, 31 ].”
Mukherjee, S., Ganaie, M. M., Chatterjee, A., Auti, C. B., Adamu, J., Das, C., Kumar, P., Tyagi, L., Saliba, M., & Kumar, M. (2026) · Materials Horizons · doi:10.1039/d6mh00879h · Cited by 1
Atomic-Scale hBN Memristors Engineered by Ion Implantation
Yang, J., Zhang, J., Yang, X., Song, A., Liang, R., Gao, X., & Dan, Y. (2026) · ACS Applied Electronic Materials · doi:10.1021/acsaelm.6c01189
Jang, J., Pyo, C., Cho, Y., Park, S., & Kim, M. (2026) · Materials Horizons · doi:10.1039/d6mh01250g
In-Memory Computing Enabled by 32 × 8 1T1R Memristive Crossbar Arrays
Mikhaylov, A. N., Shchanikov, S., Koryazhkina, M. N., Bordanov, I., Lukoyanov, V., Belov, A. I., Zharkov, G. D., Серов, Д. А., Antonov, I. N., Kotina, A., et al. (2026) · Electronics · doi:10.3390/electronics15184267
Shi, J., Gao, Z., Ma, X., Cai, G., Feng, X., & Zhao, J. (2026) · Angewandte Chemie · doi:10.1002/anie.6605459
Kim, D.-E., Thean, A., Kim, M., Lee, H., Park, H., & Hong, C. (2026) · Advanced Functional Materials · doi:10.1002/adfm.78640
Bit-sliced quantization for robust memristor-based compute-in-memory
Yu, Y., Yang, J., Ye, Z., Han, S., Wang, B., Wang, S., Wang, H., Qi, X., & Wang, Z. (2026) · npj Unconventional Computing · doi:10.1038/s44335-026-00099-9
Do, V. D., Kim, H. J., Nguyen, M. C., Yun, H. W., Duong⧫, D. L., Vũ, V. T., Liao, L., Zou, X., Li, H., Phan, T. L., et al. (2026) · Small · doi:10.1002/smll.75933
Tunable dynamics via Ag-ion modulation for deterministic polarity reversal in Sb2S3 memristors
Song, C., Wang, Z., Chen, H., Liu, H., Zhang, X., Liu, X., Zhu, J., & Li, H. (2026) · Applied Physics Letters · doi:10.1063/5.0343976
Metadata
- Authors
- Yang, Y., Gao, P., Gaba, S., Chang, T., Pan, X., & Lu, W.
- Affiliations
- University of Michigan (US)
- Corresponding author
- Lu, Wei
- Venue
- Nature Communications
- Published
- 2012-03-13
- Volume
- 3
- Issue
- 1
- Pages
- 732-732
- ISSN
- 2041-1723 (ISSN-L)
- OpenAlex
- W2043707274
- Cited by
- 1,208
- References
- 32
- Citations by year
- 2026: 68 · 2025: 69 · 2024: 92 · 2023: 84 · 2022: 95 · 2021: 85 · 2020: 101 · 2019: 100 · 2018: 89 · 2017: 95 · 2016: 88 · 2015: 81 · 2014: 71 · 2013: 68 · 2012: 21
- FWCI
- 49.24
- Type
- journal article
- Language
- en
- Open access
- bronze
- doi.org
- Licence
- www.springernature.com/gp/researchers/text-and-data-mining (tdm)
- www.springernature.com/gp/researchers/text-and-data-mining (vor)
- Locations
- Nature Communications (publishedVersion)
- PubMed (publishedVersion)
- RePEc: Research Papers in Economics (submittedVersion)
- Funders
- National Science Foundation (0723032, 0907191, 0954621)
- Defense Advanced Research Projects Agency (HRL0011-09-C-001)
- Division of Materials Research (0723032, DMR-0723032)
- Division of Electrical, Communications and Cyber Systems (ECCS-0954621)
- Topics
- Physical Sciences › Engineering › Electrical and Electronic Engineering › Advanced Memory and Neural Computing
- Physical Sciences › Engineering › Electrical and Electronic Engineering › Ferroelectric and Negative Capacitance Devices
- Physical Sciences › Materials Science › Materials Chemistry › Phase-change materials and chalcogenides
- Keywords
- resistive switching, memristors, electrochemical metallization, cation transport, dielectric films, non-volatile memory, in situ transmission electron microscopy
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
The claim verdicts this report counts are experimental: their accuracy is not yet measured.
A language model drew the claims from the paper on 2026-09-30, under version 3 of the claim definition (model deepseek-v4.1-flash, prompt extract-v3).
A second model labelled each claim on 2026-09-30 (model jev-1.13-20260917, definition revision gold-guideline-v0.2).
Cited sources are checked with a language model’s help (gpt-6-sol).
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.