Observation of conducting filament growth in nanoscale resistive memories
Open accessThe DOI matches its Crossref record; 36 of the 36 references it cites were found in a registry or an index; 5 of the 42 sources its claims cite were checked for support.
Abstract
Nanoscale resistive switching devices, sometimes termed memristors, have recently generated significant interest for memory, logic and neuromorphic applications. Resistive switching effects in dielectric-based devices are normally assumed to be caused by conducting filament formation across the electrodes, but the nature of the filaments and their growth dynamics remain controversial. Here we report direct transmission electron microscopy imaging, and structural and compositional analysis of the nanoscale conducting filaments. Through systematic ex-situ and in-situ transmission electron microscopy studies on devices under different programming conditions, we found that the filament growth can be dominated by cation transport in the dielectric film. Unexpectedly, two different growth modes were observed for the first time in materials with different microstructures. Regardless of the growth direction, the narrowest region of the filament was found to be near the dielectric/inert-electrode interface in these devices, suggesting that this region deserves particular attention for continued device optimization.
Overview
CoChat Summary
## TL;DR
Using ex-situ and in-situ TEM, the paper directly visualizes conducting filaments in nanoscale resistive memories and shows that filament growth can be limited by cation transport in the dielectric. It also reports two growth modes, including an unexpected mode in which filaments start from the active electrode and grow toward the inert electrode.
## Key findings
- In over 100 devices studied, none showed more than one completed filament.
- For SiO2-based devices, the authors observed conical filaments with a typical lateral size of ~20 nm near the tip and ~70 nm at the base; the filaments were verified to be composed of elemental Ag.
- In a-Si-based devices, partially formed filaments were sometimes seen starting from the active Ag electrode, and detailed TEM/EDS/SAED showed they were also composed of elemental Ag, sometimes as a chain of nanoparticles separated by 1–4 nm gaps.
- Across device types, the narrowest region of the filament was found near the dielectric/inert-electrode interface, and erasing typically began there; in-situ TEM on vertical Ag/a-Si/W devices confirmed this active-electrode-to-inert-electrode growth and inert-interface dissolution.
## Methods
- The study combined ex-situ and in-situ transmission electron microscopy with structural and compositional analysis (TEM, STEM/HAADF, HRTEM, SAED, EDS) on resistive memory devices.
- Devices used different dielectric layers of about 15 nm thickness: SiO2, Al2O3, and a-Si; planar devices were fabricated on ultrathin 15 nm SiNx membranes, and vertical Ag/a-Si/W devices were used for in-situ TEM.
- Electrical switching was measured with current compliance; the main analysis related filament morphology and switching behavior to dielectric choice, programming current, electric field, and temperature, including 36 a-Si-based resistive switches for the field-scaling data.
## Limitations
- The authors state that the switching time and electric field used here are still different from standard ECM cell operating conditions, so the filament growth under specific conditions must be analyzed individually.
- The paper itself notes that detailed analysis of the electrochemical processes and cation transport dynamics remains for future investigation.
- Evident from the text: many conclusions are based on specific device geometries and materials under ex-situ/in-situ TEM conditions, so direct generalization to all resistive memories is not established in the paper.
Model-written summary. Check it against the paper before relying on it.
Integrity signals
Registry
Cites
Statistics
Figures





Verification
Claims the paper makes
4 Valid · 1 Not valid · 15 Not checked · 77 Own results and interpretations
Every source the paper cites for this claim was checked and supports it.
In the paper
“In general, the filament growth is determined by three dynamic processes 27 : (i) the anodic dissolution of the metal component at the active electrode; (ii) the transport of the metal ions through the dielectrics; and (iii) the reduction of metal ions and the crystallization of conducting filaments.”
What the sources say
- Supportedcites [27] Valov, I., Waser, R., Jameson, J. R & Kozicki,, M. N. Electrochemical metallization memories — fundamentals, applications, prospects. Nanotechnol. 22, 254003 (2011). source
Split into 3 atoms — 3 confirmed, 0 partially supported, 0 disputed, 0 misattributed, 0 unverifiable. Expand the claim to see per-atom verdicts.
plainstates a cause- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: passes — The paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
- Supported
The cited sources support only part of this claim — read each source’s verdict below.
In the paper
“This effect explains the observations in ECM devices that lower threshold voltages are typically required during programming processes, compared with those for the initial forming process 22,27,28 .”
What the sources say
- Not checked — no full text of the sourcecites [22] Waser, R., Dittmann, R., Staikov, G. & Szot, K. Redox-based resistive switching memories - Nanoionic mechanisms, prospects, and challenges. Adv. Mater. 21, 2632–2663 (2009). source
- Partly supportedcites [27] Valov, I., Waser, R., Jameson, J. R & Kozicki,, M. N. Electrochemical metallization memories — fundamentals, applications, prospects. Nanotechnol. 22, 254003 (2011). sourceExperimental — accuracy not yet measured
Section 3.3 (page unavailable) distinguishes the initial forming cycle from later switching cycles and suggests that forming may leave a nano-channel that aids subsequent filament growth. This supports the proposed mechanism, but the passage does not state that programming threshold voltages are typically lower than forming voltages. (LLM, conf=0.78)
- Not checked — no full text of the sourcecites [28] Schindler, C., Staikov, G. & Waser, R. Electrode kinetics of Cu–SiO2-based resistive switching cells: Overcoming the voltage-time dilemma of electrochemical metallization memories. Appl. Phys. Lett. 94, 072109 (2009). source
plainstates a cause- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: passes — The paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
A result the paper reports from its own data — it cites no other source for it, so there is none to check. The quote shows it is in the paper.
In the paper
“the filaments in Fig. 1b apparently started growth from the inert electrode side as evidenced by the locations of the partially formed filaments.”
hedgedstates a cause- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: passes — The paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
A result the paper reports from its own data — it cites no other source for it, so there is none to check. The quote shows it is in the paper.
In the paper
“many of the incomplete filaments exhibiting a noteworthy dendrite structure with the branches pointing towards the active electrode”
plainstates an association- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: passes — The paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
A result the paper reports from its own data — it cites no other source for it, so there is none to check. The quote shows it is in the paper.
In the paper
“we provide unambiguous evidence that shows that localized, nanoscale filaments composed of elemental metals (and, in some cases, consisting of discrete nanoparticles instead of a solid wire) are formed during resistive switching.”
boostedstates a cause- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: passes — The paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
51 more claims
Create a free account to see all 97 claims and every source verdict.
- It may state two separate claims as one. 36
- Probably not a substantial claim. 10
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“The change from OFF to ON state is explained by the formation of a dominating Ag filament (15,16).”
From Stochastic memristive devices for computing and neuromorphic applications (2013) · cites this paper as [16]
Citations
Cites
Strukov, D. B., Snider, G. S., Stewart, D. R., & Williams, R. S. (2008) · Nature · doi:10.1038/nature06932 · Cited by 11,828
Memristor—The Missing Circuit Element
Chua, L. (1971) · IEEE Transactions on Circuit Theory · doi:10.1109/tct.1971.1083337 · Cited by 10,268
Redox‐Based Resistive Switching Memories – Nanoionic Mechanisms, Prospects, and Challenges
Waser, R., Dittmann, R., Staikov, G., & Szot, K. (2009) · Advanced Materials · doi:10.1002/adma.200900375 · Cited by 5,080
Nanoionics-based resistive switching memories
Waser, R., & Aono, M. (2007) · Nature Materials · doi:10.1038/nmat2023 · Cited by 4,923
Nanoscale Memristor Device as Synapse in Neuromorphic Systems
Jo, S. H., Chang, T., Ebong, I., Bhadviya, B. B., Mazumder, P., & Lu, W. (2010) · Nano Letters · doi:10.1021/nl904092h · Cited by 4,174
Self-citationMemristive switching mechanism for metal/oxide/metal nanodevices
Yang, J. J., Pickett, M. D., Li, X., Ohlberg, D. A. A., Stewart, D. R., & Williams, R. S. (2008) · Nature Nanotechnology · doi:10.1038/nnano.2008.160 · Cited by 2,987
Memristive devices and systems
Chua, L. O., & Kang, S. M. (1976) · Proceedings of the IEEE · doi:10.1109/proc.1976.10092 · Cited by 2,604
Atomic structure of conducting nanofilaments in TiO2 resistive switching memory
Kwon, D.-H., Kim, K. M., Jang, J. H., Jeon, J. M., Lee, M. H., Kim, G. H., Li, X.-S., Park, G.-S., Lee, B., Han, S., et al. (2010) · Nature Nanotechnology · doi:10.1038/nnano.2009.456 · Cited by 2,092
‘Memristive’ switches enable ‘stateful’ logic operations via material implication
Borghetti, J., Snider, G. S., Kuekes, P. J., Yang, J. J., Stewart, D. R., & Williams, R. S. (2010) · Nature · doi:10.1038/nature08940 · Cited by 1,929
Complementary resistive switches for passive nanocrossbar memories
Linn, E., Rosezin, R., Kügeler, C., & Waser, R. (2010) · Nature Materials · doi:10.1038/nmat2748 · Cited by 1,274
Cited by
Items 701–800 of 1,201
Chen, H.-B., He, M.-Y., Li, T., Deng, C., Xiao, H., Qi, M., Kong, X., Li, H., Li, X., & Zheng, S. (2024) · Journal of Materials Chemistry C · doi:10.1039/d4tc02172j · Cited by 14
Koncha, G., Das, N. K., & Badhulika, S. (2024) · Materials Science in Semiconductor Processing · doi:10.1016/j.mssp.2024.108804 · Cited by 13
Exploring the potential of 2D PtTe2-based memristors for neuromorphic computing
Lian, X., Zhang, X., Li, S., Ding, B., Jiang, J., Zhang, Y., Guo, Y., Cai, Z., & Wang, L. (2025) · Applied Physics Letters · doi:10.1063/5.0244591 · Cited by 13
Ismail, M., Na, H., Rasheed, M., Mahata, C., Kim, Y., & Kim, S. (2025) · Nano Energy · doi:10.1016/j.nanoen.2025.111276 · Cited by 17
In depth nano spectroscopic analysis on homogeneously switching double barrier memristive devices
Strobel, J., Hansen, M., Dirkmann, S., Neelisetty, K. K., Ziegler, M., Haberfehlner, G., Popescu, R., Kothleitner, G., Chakravadhanula, V. S. K., Kübel, C., et al. (2017) · Journal of Applied Physics · doi:10.1063/1.4990145 · Cited by 15
Synaptic behaviors of HfO2 ReRAM by pulse frequency modulation
Lee, D. K., Kim, M., Kim, T., Bang, S., Choi, Y.-J., Kim, S., Cho, S., & Park, B. (2019) · Solid-State Electronics · doi:10.1016/j.sse.2019.02.008 · Cited by 12
Kang, D. Y., Lee, W., Park, N., Yoon, Y.-S., Kim, G., Kim, T. G., & Lee, S. (2019) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2019.03.268 · Cited by 13
Investigation of the Thermal Recovery From Reset Breakdown of a SiN x -Based RRAM
Hong, K., Min, K. K., Kim, M., Bang, S., Kim, T., Lee, D. K., Choi, Y.-J., Kim, C. S., Lee, J. Y., Kim, S., et al. (2020) · IEEE Transactions on Electron Devices · doi:10.1109/ted.2020.2976106 · Cited by 14
“As for a filamentary-type RRAM, switching speed is fast because the set and reset process occurs only in the small area of filament tip [5].”
BackgroundSwitchable Electrically Driven Optical Antenna Based on Ultrathin Amorphous Silica
Tang, J., Hu, H., He, X., et al. (2021) · Advanced Optical Materials · doi:10.1002/adom.202100191 · Cited by 13
Electrical bistability based on metal–organic frameworks
Lin, S., Chen, S., Ju, Y., Xiang, F., Wei, W., Wang, X., Xiang, S., & Zhang, Z. (2022) · Chemical Communications · doi:10.1039/d2cc03097g · Cited by 13
Resistive Switching in Ag2Te Semiconductor Modulated by Ag+‐Ion Diffusion and Phase Transition
Guo, A., Bai, H., Liang, Q., Feng, L., Su, X., Tendeloo, G. V., & Wu, J. (2022) · Advanced Electronic Materials · doi:10.1002/aelm.202200850 · Cited by 13
Li, X. Y., Park, T. H., Hyun, S. D., & Hwang, C. S. (2022) · ACS Applied Electronic Materials · doi:10.1021/acsaelm.2c01043 · Cited by 14
Temperature Control of Diffusive Memristor Hysteresis and Artificial Neuron Spiking
Pattnaik, D. P., Ushakov, Y., Zhou, Z., Borisov, P., Cropper, M. D., Wijayantha, U. W., Balanov, A. G., & Savel'ev, S. E. (2023) · Physical Review Applied · doi:10.1103/physrevapplied.19.024065 · Cited by 14
“[14, 15] Due to inhomogeneities in the composition of the dielectric film [16] and roughness of the electrodes, the NPs forming the CFs can be pinned [17, 18], this affects CF rupture and the endurance and eventually can cause degradation of the memristive devices.”
BackgroundSugiyama, I., Kim, Y., Jesse, S., Strelcov, E., Kumar, A., Tselev, A., Rahani, E. K., Shenoy, V. B., Yamamoto, T., Shibata, N., et al. (2014) · Scientific Reports · doi:10.1038/srep06725 · Cited by 14
Effects of moisture barriers on resistive switching in Pt-dispersed SiO2 nanometallic thin films
Choi, B. J., & Chen, I. (2013) · Applied Physics A · doi:10.1007/s00339-013-7776-2 · Cited by 13
Krishnan, K., Tsuruoka, T., & Aono, M. (2016) · Japanese Journal of Applied Physics · doi:10.7567/jjap.55.06gk02 · Cited by 13
Fabrication of a W/CuxO/Cu memristor with sub-micron holes for passive sensing of oxygen
Nyenke, C., & Dong, L. (2016) · Microelectronic Engineering · doi:10.1016/j.mee.2016.07.005 · Cited by 13
Tutorial: Fabrication and three-dimensional integration of nanoscale memristive devices and arrays
Lin, P., & Xia, Q. (2018) · Journal of Applied Physics · doi:10.1063/1.5038109 · Cited by 16
Inkjet assisted fabrication of planar biocompatible memristors
Illarionov, G. A., Kolchanov, D. S., Kuchur, O. A., Zhukov, M. V., Sergeeva, E., Krishtop, V. V., Vinogradov, A. V., & Morozov, M. I. (2019) · RSC Advances · doi:10.1039/c9ra08114c · Cited by 13
A dual mode electronic synapse based on layered SnSe films fabricated by pulsed laser deposition
Chen, X., Suen, C.-H., Yau, H. M., Zhou, F., Chai, Y., Tang, X., Zhou, X., Onofrio, N., & Dai, J.-Y. (2020) · Nanoscale Advances · doi:10.1039/c9na00447e · Cited by 12
Wang, L., Wen, J., Jiang, Y., Ou, Q., Yu, L., Xiong, B.-S., Yang, B.-X., Zhang, C., & Tong, Y. (2020) · Materials · doi:10.3390/ma13173671 · Cited by 14
“The unique attribute of memristor arises from its pinched hysteresis loop that exhibits a relationship between the applied voltage and resulting current, indicating various resistance states with respect to external excitations [22,23].”
BackgroundGao, S., Song, C., Chen, C., et al. (2013) · The Journal of Physical Chemistry C · doi:10.1021/jp401828m · Cited by 13
Contributing to the understanding of the dielectric breakdown channel of alumina under high voltage
Zhang, T., Du, J., Lei, Y., et al. (2019) · Ceramics International · doi:10.1016/j.ceramint.2019.05.200 · Cited by 12
Analog Ion‐Slicing LiNbO3 Memristor Based on Hopping Transport for Neuromorphic Computing
Wang, J., Zeng, H., Xie, Y., Zhao, Z., Pan, X., Luo, W., Shuai, Y., Tang, L., Zhu, D., Xie, Q., et al. (2023) · Advanced Intelligent Systems · doi:10.1002/aisy.202300155 · Cited by 15
Self-citationPhark, S.-H., & Chae, S. C. (2015) · Journal of Physics D Applied Physics · doi:10.1088/0022-3727/48/15/155102 · Cited by 11
Souchier, E., d’Acapito, F., Noé, P., Blaise, P., Bernard, M., & Jousseaume, V. (2015) · Physical Chemistry Chemical Physics · doi:10.1039/c5cp03601a · Cited by 13
Mourad, S., Ghoul, J. M. E., Khettou, A., et al. (2021) · Physica B Condensed Matter · doi:10.1016/j.physb.2021.413577 · Cited by 12
Move contrast X-ray imaging of electrochemical reaction process in electrolytic cell
Ju, X., Li, K., Yu, F., et al. (2022) · Acta Physica Sinica · doi:10.7498/aps.71.20220339 · Cited by 12
Wang, L., Zhang, Y., Zhang, P., et al. (2022) · Nanomaterials · doi:10.3390/nano12173061 · Cited by 12
Wang, J., Pan, X., Luo, W., Shuai, Y., Xie, Q., Xu, J., Song, Z., Wu, C., & Zhang, W. (2022) · Advanced Electronic Materials · doi:10.1002/aelm.202201064 · Cited by 12
Self-citationHan, S. W., & Shin, M. W. (2023) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2023.170902 · Cited by 13
Conductive filaments multiplicity as a variability factor in CBRAM
Celano, U., Goux, L., Belmonte, A., Opsomer, K., Detavernier, C., Jurczak, M., & Vandervorst, W. (2015) · IEEE International Reliability Physics Symposium proceedings · doi:10.1109/irps.2015.7112813 · Cited by 13
“The electrochemistry describing CBRAM devices does not exclude the possibility of multiple filaments-formation attempts and those have been reported by means of TEM [6], [7].”
BackgroundJana, D., Chakrabarti, S., Rahaman, S. Z., & Maikap, S. (2015) · Nanoscale Research Letters · doi:10.1186/s11671-015-1090-1 · Cited by 13
“[21].”
Optically readout write once read many memory with single active organic layer
Nguyen, V. C., & Lee, P. S. (2016) · Applied Physics Letters · doi:10.1063/1.4940204 · Cited by 12
Valov, I., & Waser, R. M. (2013) · The Journal of Physical Chemistry C · doi:10.1021/jp4014306 · Cited by 12
Zhang, T., Guérin, D., Alibart, F., et al. (2019) · Nanoscale Advances · doi:10.1039/c9na00285e · Cited by 12
Resistive switching and its modulating ferromagnetism and magnetoresistance of a ZnO-Co/SiO2-Co film
Du, F., Li, Y., Li, X., et al. (2019) · Journal of Magnetism and Magnetic Materials · doi:10.1016/j.jmmm.2019.165445 · Cited by 12
Zhao, X., Wang, Z., Lin, Y., Xu, H., & Liu, Y. (2019) · Applied Physics Letters · doi:10.1063/1.5096197 · Cited by 11
Sinter-free inkjet-printed PEDOT:PSS/WO 3 /PEDOT:PSS flexible valency change memory
Delfag, M., Katoch, R., Jehn, J., González, Y., Schindler, C., & Ruediger, A. P. (2021) · Flexible and Printed Electronics · doi:10.1088/2058-8585/ac1fd7 · Cited by 13
“ECM creates conducting filaments inside of the insulating material due to the diffusion of ions from an electrochemically active electrode, which behaves as a conducting bridge between the two electrodes, thus creating the LRS of the memory [5].”
Resistive switching in ZrO2 films: physical mechanism for filament formation and dissolution
Parreira, P., McVitie, S., & MacLaren, D. A. (2014) · Journal of Physics Conference Series · doi:10.1088/1742-6596/522/1/012045 · Cited by 12
Rahaman, S. Z., & Maikap, S. (2013) · Nanoscale Research Letters · doi:10.1186/1556-276x-8-509 · Cited by 12
“The thickness of the SiO2 layer is approximately 200 nm.”
BackgroundInfluentialYu, J.-C., Huang, W., Lü, C., Lin, G., Li, C., Chen, S., Wang, J., Xu, J., Liu, C., & Lai, H. (2017) · Japanese Journal of Applied Physics · doi:10.7567/jjap.56.050304 · Cited by 12
Liu, M., Mao, S., Qin, J., Yang, Y., Rao, Z., Lin, W. S., Yang, Y., Zhao, Y. X., & Sun, B. T. (2024) · ACS Applied Nano Materials · doi:10.1021/acsanm.3c06023 · Cited by 11
Self-citationJia, W., Hu, L., Gao, W., Mu, W., Chou, Z., & Cheng, X. (2024) · Materials Science in Semiconductor Processing · doi:10.1016/j.mssp.2024.108688 · Cited by 11
Integration of Ag-based threshold switching devices in silicon microchips
Alharbi, O., Pazos, S. M., Zhu, K., Aguirre, F. L., Yuan, Y. J., Li, X., Wu, H., & Lanza, M. (2024) · Materials Science and Engineering R Reports · doi:10.1016/j.mser.2024.100837 · Cited by 12
One Transistor−One Memristor Integrated Device Based on the Dual Conductive Filament Mechanism
Zhao, L., Pan, Z., Zhou, R., Zhao, T., Wu, X., & Huo, N. (2025) · ACS Applied Electronic Materials · doi:10.1021/acsaelm.5c00267 · Cited by 12
Zou, Y. L., Li, X. Y., Ghenzi, N., Park, T., Shin, D. H., Shin, S. J., Cho, J. M., Park, T. W., Cheong, S., Mun, S. A., et al. (2025) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.5c09911 · Cited by 14
“…resistance by setting different compliance currents or reset stop voltages, which are closely related to the partial formation or rupture of CFs. 36,37 Such a CF configuration requires more complicated pulse engineering to achieve linear LTP and LTD. Additionally, it requires asymmetrical pulses…”
Kim, J. E., Kwon, J. U., Chun, S. Y., Song, Y. G., Jeong, D. S., Kang, C., Kim, S. K., Nahm, S., & Yoon, J. H. (2022) · Advanced Electronic Materials · doi:10.1002/aelm.202200365 · Cited by 12
An improved memristive current mirror circuit for continuous adjustable current output
Cheng, M., Yang, L., Ding, Z., Li, S., & Lei, J. W. (2023) · AEU - International Journal of Electronics and Communications · doi:10.1016/j.aeue.2023.154765 · Cited by 10
Localized resistive switching in a ZnS–Ag/ZnS double-layer memory
Zhang, L., Xu, H., Wang, Z. Q., Zhao, X., G, J., & Liu, Y. (2014) · Journal of Physics D Applied Physics · doi:10.1088/0022-3727/47/45/455101 · Cited by 11
In situTEM study of reversible and irreversible electroforming in Pt/Ti:NiO/Pt heterostructures
D’Aquila, K., Liu, Y., Iddir, H. H., & Petford-Long, A. K. (2015) · physica status solidi (RRL) - Rapid Research Letters · doi:10.1002/pssr.201510063 · Cited by 11
Observation of indium ion migration-induced resistive switching in Al/Mg0.5Ca0.5TiO3/ITO
Lin, Z.-H., & Wang, Y. (2016) · Applied Physics Letters · doi:10.1063/1.4960525 · Cited by 11
Atomic Monte-Carlo simulation for CBRAM with various filament geometries
Zhao, Y., Huang, P. C., Guo, Z. H., Lun, Z., Gao, B., Liu, X. Y., & Kang, J. (2016) · International Conference on Simulation of Semiconductor Processes and Devices · doi:10.1109/sispad.2016.7605170 · Cited by 11
“INTRODUCTION CBRAM is a promising candidate among the emerging non-volatile memory technologies due to its excellent scaling and low power potential [1-8].”
BackgroundMethodInfluentialDoes platinum play a role in the resistance switching of ZnO nanowire-based devices?
Raffone, F., & Cicero, G. (2016) · Solid State Ionics · doi:10.1016/j.ssi.2016.10.020 · Cited by 11
Lee, D. K., Kim, G. H., Sohn, H., & Yang, M. (2019) · physica status solidi (RRL) - Rapid Research Letters · doi:10.1002/pssr.201900646 · Cited by 12
Park, S., Cho, K., & Kim, S. (2015) · Semiconductor Science and Technology · doi:10.1088/0268-1242/30/5/055019 · Cited by 11
Gradual electroforming and memristive switching in Pt/CuOx/Si/Pt systems
Wei, L. L., Shang, D. S., Sun, J. R., Lee, S. B., Sun, Z. G., & Shen, B. G. (2013) · Nanotechnology · doi:10.1088/0957-4484/24/32/325202 · Cited by 14
Sun, X., Wu, C., Shuai, Y., Pan, X., Luo, W., You, T., Bogusz, A., Du, N., Li, Y., & Schmidt, H. (2016) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.6b11049 · Cited by 11
Self-citationLow power and high uniformity of HfOx-based RRAM via tip-enhanced electric fields
Li, X., Zhang, B., Wang, B., Xu, X., Yang, Y., Sun, S., Cai, Q., Hu, S., An, X., Li, M., et al. (2019) · Science China Information Sciences · doi:10.1007/s11432-019-9910-x · Cited by 11
Self-citationImpedance Spectroscopy of Programmable Metallization Cells With a Thin SiO2Switching Layer
Chen, W., Barnaby, H., & Kozicki, M. N. (2016) · IEEE Electron Device Letters · doi:10.1109/led.2016.2542239 · Cited by 11
“In-situ TEM and conductive-AFM studies have provided direct evidence of such filaments in most types of resistive switching devices [4], [5].”
BackgroundEffects of pristine state on conductive percolation model of memristor
Li, Z., Liu, H., & Xu, X. (2013) · Acta Physica Sinica · doi:10.7498/aps.62.096401 · Cited by 10
Srikimkaew, O., Ricci, S., Porzani, M., Dang, T. T., Nakaoka, Y., Usami, Y., Ielmini, D., & Tanaka, H. (2024) · Advanced Electronic Materials · doi:10.1002/aelm.202300709 · Cited by 11
Mitigation of memory state variability in SiO2 memristors by Cu nanoparticles incorporation
Jana, B., Ghosh, K., & Chaudhuri, A. R. (2025) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2025.179690 · Cited by 11
Resistive switching of alkanethiolated nanoparticle monolayers patterned by electron-beam exposure
Reissner, P. A., Fedoryshyn, Y. M., Tisserant, J., et al. (2016) · Physical Chemistry Chemical Physics · doi:10.1039/c6cp03928f · Cited by 10
Electron tunneling between vibrating atoms in a copper nano-filament
Al-Mamun, M., & Orlowski, M. (2021) · Scientific Reports · doi:10.1038/s41598-021-86603-6 · Cited by 11
Krishnan, K., & Vijayaraghavan, S. (2023) · Journal of Materials Science Materials in Electronics · doi:10.1007/s10854-022-09697-2 · Cited by 12
Memristor-Based Signal Processing for Compressed Sensing
Wang, R., Zhang, W., Wang, S., Zeng, T., Ma, X., Wang, H., & Hao, Y. (2023) · Nanomaterials · doi:10.3390/nano13081354 · Cited by 13
“When the mobility of Ag + surpasses that of electrons, Ag + and electrons will be situated near BE, resulting in Ag CF growth from BE to TE [46,47].”
BackgroundSimulating the filament morphology in electrochemical metallization cells
Buttberg, M., Valov, I., & Menzel, S. (2023) · Neuromorphic Computing and Engineering · doi:10.1088/2634-4386/acdbe5 · Cited by 13
A suspended nanogap formed by field-induced atomically sharp tips
Han, J. H., Song, K., Radhakrishnan, S., et al. (2012) · Applied Physics Letters · doi:10.1063/1.4764562 · Cited by 10
Park, J., Jeon, H., Kim, H., Jang, W., Seo, H., & Jeon, H. (2014) · RSC Advances · doi:10.1039/c4ra10446c · Cited by 10
Nanoscale magnetization reversal by electric field-induced ion migration
Chen, Q., Liu, G., Gao, S., et al. (2018) · MRS Communications · doi:10.1557/mrc.2018.191 · Cited by 10
Kim, M., Beom, K., Lee, H., et al. (2019) · Applied Physics Letters · doi:10.1063/1.5109929 · Cited by 10
Electrothermal Analysis of 3D Memristive 1D-1RRAM Crossbar with Carbon Nanotube Electrodes
Zayer, F., Lahbacha, K., Dghais, W., Belgacem, H., de Magistris, M., Melnikov, A. V., & Maffucci, A. (2019) · IEEE International Conference on Design & Test of Integrated Micro & Nano-Systems (DTS) · doi:10.1109/dtss.2019.8915266 · Cited by 10
Krishnan, K., Gubicza, Á., Aono, M., Terabe, K., Valov, I., & Tsuruoka, T. (2021) · Journal of Materials Chemistry C · doi:10.1039/d1tc01654g · Cited by 10
Effects of heavy ion irradiation on Cu/Al2O3/Pt CBRAM devices
Su, C., Shan, L., Yang, D., Zhao, Y., Fu, Y., Liu, J., Zhang, G., Wang, Q., & He, D. (2021) · Microelectronic Engineering · doi:10.1016/j.mee.2021.111600 · Cited by 10
Photocatalysis‐Induced Nanopores toward Highly Reliable Organic Electrochemical Metallization Memory
Zeng, T., Su, R., Tao, Y., Lin, Y., Shan, X., Cheng, Y., Wang, Z., Zhao, X., Xu, H., & Liu, Y. (2022) · Advanced Electronic Materials · doi:10.1002/aelm.202200246 · Cited by 10
Flexibly Photo-Regulated Brain-Inspired Functions in Flexible Neuromorphic Transistors
Wang, L., Zhang, T., Shen, J., Huang, J., Li, W., Shi, W. Y., Huang, W., & Yi, M. (2023) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.2c22754 · Cited by 10
Jeon, J., Eom, K., Lee, M., Kim, S., & Lee, H. (2023) · Small · doi:10.1002/smll.202301452 · Cited by 10
Study of a Stretchable Polymer for Adjustable Flexible Organic Memristor
Ding, Q., Jiao, W., Wang, H., Zhang, X., & Gao, S. (2023) · IEEE Transactions on Electron Devices · doi:10.1109/ted.2023.3274509 · Cited by 10
Soni, R., Meuffels, P., Petraru, A., Hansen, M., Ziegler, M., Vavra, O., Kohlstedt, H., & Jeong, D. S. (2013) · Nanoscale · doi:10.1039/c3nr03993e · Cited by 10
Puyoo, E., & Albertini, D. (2020) · IEEE Electron Device Letters · doi:10.1109/led.2020.2986543 · Cited by 10
“Several approaches based on transmission electron microscopy (TEM) have already been proposed in literature in order to visualize and precisely localize the nucleation sites of conductive filaments [11], [12].”
BackgroundYang, L., Cheng, Q., Li, Y., Wu, N., Xu, Z., & Xu, W. (2025) · Advanced Science · doi:10.1002/advs.202511478 · Cited by 10
Xu, J., Wang, Y., Huo, S., Tian, Q., Wang, Y., Wang, Z., Song, Z., Xie, Y., Hu, X., Pan, C., et al. (2026) · Advanced Functional Materials · doi:10.1002/adfm.77333 · Cited by 24
Lin, X., Zhou, P., Gao, Y., Li, T., Chen, X., Li, H., Jiang, R., Chen, Z., & Zheng, H. (2023) · Inorganic Chemistry · doi:10.1021/acs.inorgchem.3c03787 · Cited by 9
Lyu, D., Shoup, J. E., Habiboglu, A., et al. (2024) · AIP Advances · doi:10.1063/9.0000818 · Cited by 9
Azari, R. K., Gao, Z., Carrière, A., & Santato, C. (2024) · RSC Applied Interfaces · doi:10.1039/d4lf00003j · Cited by 10
Kleitsiotis, G., Bousoulas, P., Mantas, S. D., Tsioustas, C., Fyrigos, I.-A., Sirakoulis, G. C., & Tsoukalas, D. (2024) · IEEE Transactions on Electron Devices · doi:10.1109/ted.2024.3421964 · Cited by 13
“This conjecture is in direct line with concrete experimental pieces of evidence concerning SiO 2 - based memristors [20], [21] and indicates the direct impact of the BE on the hysteresis pattern [22], [23].”
ResultMoon, S., Park, C., Jung, Y. K., Min, K., Ko, H., & Yoon, T. (2025) · Journal of Materials Chemistry C · doi:10.1039/d4tc05041j · Cited by 12
Xiong, J., Zhao, Y., Zhu, J., et al. (2021) · The Journal of Physical Chemistry C · doi:10.1021/acs.jpcc.1c00466 · Cited by 9
Liu, C., Wang, Y., Zhang, T., Yuan, R., & Yang, Y. (2022) · Advanced Electronic Materials · doi:10.1002/aelm.202201060 · Cited by 9
Self-citationZhang, Z., Zhan, G., Gan, W., Cheng, Y., Zhang, X., Peng, Y., Tang, J., Zhang, F., Huo, J., Xu, G., et al. (2023) · Advanced Intelligent Systems · doi:10.1002/aisy.202300275 · Cited by 9
Resistive switching memory of single BiMnO3+δ nanorods
Yan, Y., Sun, B. T., & Jian, D. (2015) · Journal of Materials Science Materials in Electronics · doi:10.1007/s10854-015-3782-9 · Cited by 9
Ion transport-related resistive switching in film sandwich structures
Zhu, X., Shang, J., Liu, G., & Li, R. (2014) · Chinese Science Bulletin · doi:10.1007/s11434-014-0284-8 · Cited by 9
Wu, Y., Liao, C.-W., & Ling, J.-J. (2014) · Applied Physics Letters · doi:10.1063/1.4884389 · Cited by 9
Gao, L., Hoskins, B. D., & Strukov, D. B. (2016) · physica status solidi (RRL) - Rapid Research Letters · doi:10.1002/pssr.201600044 · Cited by 9
Forming mechanism of Te-based conductive-bridge memories
Mendes, M. K., Martinez, E., Marty, A. M., et al. (2017) · Applied Surface Science · doi:10.1016/j.apsusc.2017.07.187 · Cited by 9
Le, N. M., & Lee, B. (2017) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.6b16404 · Cited by 9
Physics-Technological Fabrication of Memresistors for Micro- and Nanoelectronics
Belov, A. N., Perevalov, A. A., & Shevyakov, V. I. (2017) · Proceedings of Universities ELECTRONICS · doi:10.24151/1561-5405-2017-22-4-305-321 · Cited by 14
Park, N., Kang, D. Y., Lee, W., Yoon, Y.-S., Kim, G., Saitoh, E., Kim, T. G., & Lee, S. (2019) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.9b01289 · Cited by 9
Clarke, H., Deremo, L., Anderson, J. P., Ganguli, S., & Shamberger, P. J. (2019) · Nanotechnology · doi:10.1088/1361-6528/ab53a9 · Cited by 9
Metadata
- Authors
- Yang, Y., Gao, P., Gaba, S., Chang, T., Pan, X., & Lu, W.
- Affiliations
- University of Michigan (US)
- Corresponding author
- Lu, Wei
- Venue
- Nature Communications
- Published
- 2012-03-13
- Volume
- 3
- Issue
- 1
- Pages
- 732-732
- ISSN
- 2041-1723 (ISSN-L)
- OpenAlex
- W2043707274
- Cited by
- 1,208
- References
- 32
- Citations by year
- 2026: 68 · 2025: 69 · 2024: 92 · 2023: 84 · 2022: 95 · 2021: 85 · 2020: 101 · 2019: 100 · 2018: 89 · 2017: 95 · 2016: 88 · 2015: 81 · 2014: 71 · 2013: 68 · 2012: 21
- FWCI
- 49.24
- Type
- journal article
- Language
- en
- Open access
- bronze
- doi.org
- Licence
- www.springernature.com/gp/researchers/text-and-data-mining (tdm)
- www.springernature.com/gp/researchers/text-and-data-mining (vor)
- Locations
- Nature Communications (publishedVersion)
- PubMed (publishedVersion)
- RePEc: Research Papers in Economics (submittedVersion)
- Funders
- National Science Foundation (0723032, 0907191, 0954621)
- Defense Advanced Research Projects Agency (HRL0011-09-C-001)
- Division of Materials Research (0723032, DMR-0723032)
- Division of Electrical, Communications and Cyber Systems (ECCS-0954621)
- Topics
- Physical Sciences › Engineering › Electrical and Electronic Engineering › Advanced Memory and Neural Computing
- Physical Sciences › Engineering › Electrical and Electronic Engineering › Ferroelectric and Negative Capacitance Devices
- Physical Sciences › Materials Science › Materials Chemistry › Phase-change materials and chalcogenides
- Keywords
- resistive switching, memristors, electrochemical metallization, cation transport, dielectric films, non-volatile memory, in situ transmission electron microscopy
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
The claim verdicts this report counts are experimental: their accuracy is not yet measured.
A language model drew the claims from the paper on 2026-09-30, under version 3 of the claim definition (model deepseek-v4.1-flash, prompt extract-v3).
A second model labelled each claim on 2026-09-30 (model jev-1.13-20260917, definition revision gold-guideline-v0.2).
Cited sources are checked with a language model’s help (gpt-6-sol).
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.