Abstract
Nanoscale resistive switching devices, sometimes termed memristors, have recently generated significant interest for memory, logic and neuromorphic applications. Resistive switching effects in dielectric-based devices are normally assumed to be caused by conducting filament formation across the electrodes, but the nature of the filaments and their growth dynamics remain controversial. Here we report direct transmission electron microscopy imaging, and structural and compositional analysis of the nanoscale conducting filaments. Through systematic ex-situ and in-situ transmission electron microscopy studies on devices under different programming conditions, we found that the filament growth can be dominated by cation transport in the dielectric film. Unexpectedly, two different growth modes were observed for the first time in materials with different microstructures. Regardless of the growth direction, the narrowest region of the filament was found to be near the dielectric/inert-electrode interface in these devices, suggesting that this region deserves particular attention for continued device optimization.
Overview
CoChat Summary
## TL;DR
Using ex-situ and in-situ TEM, the paper directly visualizes conducting filaments in nanoscale resistive memories and shows that filament growth can be limited by cation transport in the dielectric. It also reports two growth modes, including an unexpected mode in which filaments start from the active electrode and grow toward the inert electrode.
## Key findings
- In over 100 devices studied, none showed more than one completed filament.
- For SiO2-based devices, the authors observed conical filaments with a typical lateral size of ~20 nm near the tip and ~70 nm at the base; the filaments were verified to be composed of elemental Ag.
- In a-Si-based devices, partially formed filaments were sometimes seen starting from the active Ag electrode, and detailed TEM/EDS/SAED showed they were also composed of elemental Ag, sometimes as a chain of nanoparticles separated by 1–4 nm gaps.
- Across device types, the narrowest region of the filament was found near the dielectric/inert-electrode interface, and erasing typically began there; in-situ TEM on vertical Ag/a-Si/W devices confirmed this active-electrode-to-inert-electrode growth and inert-interface dissolution.
## Methods
- The study combined ex-situ and in-situ transmission electron microscopy with structural and compositional analysis (TEM, STEM/HAADF, HRTEM, SAED, EDS) on resistive memory devices.
- Devices used different dielectric layers of about 15 nm thickness: SiO2, Al2O3, and a-Si; planar devices were fabricated on ultrathin 15 nm SiNx membranes, and vertical Ag/a-Si/W devices were used for in-situ TEM.
- Electrical switching was measured with current compliance; the main analysis related filament morphology and switching behavior to dielectric choice, programming current, electric field, and temperature, including 36 a-Si-based resistive switches for the field-scaling data.
## Limitations
- The authors state that the switching time and electric field used here are still different from standard ECM cell operating conditions, so the filament growth under specific conditions must be analyzed individually.
- The paper itself notes that detailed analysis of the electrochemical processes and cation transport dynamics remains for future investigation.
- Evident from the text: many conclusions are based on specific device geometries and materials under ex-situ/in-situ TEM conditions, so direct generalization to all resistive memories is not established in the paper.
Model-written summary. Check it against the paper before relying on it.
Integrity signals
Registry
Cites
Statistics
Figures





Verification
Claims the paper makes
4 Valid · 1 Not valid · 15 Not checked · 77 Own results and interpretations
Every source the paper cites for this claim was checked and supports it.
In the paper
“In general, the filament growth is determined by three dynamic processes 27 : (i) the anodic dissolution of the metal component at the active electrode; (ii) the transport of the metal ions through the dielectrics; and (iii) the reduction of metal ions and the crystallization of conducting filaments.”
What the sources say
- Supportedcites [27] Valov, I., Waser, R., Jameson, J. R & Kozicki,, M. N. Electrochemical metallization memories — fundamentals, applications, prospects. Nanotechnol. 22, 254003 (2011). source
Split into 3 atoms — 3 confirmed, 0 partially supported, 0 disputed, 0 misattributed, 0 unverifiable. Expand the claim to see per-atom verdicts.
plainstates a cause- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: passes — The paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
- Supported
The cited sources support only part of this claim — read each source’s verdict below.
In the paper
“This effect explains the observations in ECM devices that lower threshold voltages are typically required during programming processes, compared with those for the initial forming process 22,27,28 .”
What the sources say
- Not checked — no full text of the sourcecites [22] Waser, R., Dittmann, R., Staikov, G. & Szot, K. Redox-based resistive switching memories - Nanoionic mechanisms, prospects, and challenges. Adv. Mater. 21, 2632–2663 (2009). source
- Partly supportedcites [27] Valov, I., Waser, R., Jameson, J. R & Kozicki,, M. N. Electrochemical metallization memories — fundamentals, applications, prospects. Nanotechnol. 22, 254003 (2011). sourceExperimental — accuracy not yet measured
Section 3.3 (page unavailable) distinguishes the initial forming cycle from later switching cycles and suggests that forming may leave a nano-channel that aids subsequent filament growth. This supports the proposed mechanism, but the passage does not state that programming threshold voltages are typically lower than forming voltages. (LLM, conf=0.78)
- Not checked — no full text of the sourcecites [28] Schindler, C., Staikov, G. & Waser, R. Electrode kinetics of Cu–SiO2-based resistive switching cells: Overcoming the voltage-time dilemma of electrochemical metallization memories. Appl. Phys. Lett. 94, 072109 (2009). source
plainstates a cause- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: passes — The paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
A result the paper reports from its own data — it cites no other source for it, so there is none to check. The quote shows it is in the paper.
In the paper
“the filaments in Fig. 1b apparently started growth from the inert electrode side as evidenced by the locations of the partially formed filaments.”
hedgedstates a cause- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: passes — The paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
A result the paper reports from its own data — it cites no other source for it, so there is none to check. The quote shows it is in the paper.
In the paper
“many of the incomplete filaments exhibiting a noteworthy dendrite structure with the branches pointing towards the active electrode”
plainstates an association- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: passes — The paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
A result the paper reports from its own data — it cites no other source for it, so there is none to check. The quote shows it is in the paper.
In the paper
“we provide unambiguous evidence that shows that localized, nanoscale filaments composed of elemental metals (and, in some cases, consisting of discrete nanoparticles instead of a solid wire) are formed during resistive switching.”
boostedstates a cause- Asserted: passes — The authors put it forward as true.
- Checkable: passes — It can be checked against evidence.
- Load-bearing: passes — The paper’s conclusions depend on it.
- Based: passes — The paper gives a reason why it holds.
51 more claims
Create a free account to see all 97 claims and every source verdict.
- It may state two separate claims as one. 36
- Probably not a substantial claim. 10
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
In the citing paper
“The change from OFF to ON state is explained by the formation of a dominating Ag filament (15,16).”
From Stochastic memristive devices for computing and neuromorphic applications (2013) · cites this paper as [16]
Citations
Cites
Strukov, D. B., Snider, G. S., Stewart, D. R., & Williams, R. S. (2008) · Nature · doi:10.1038/nature06932 · Cited by 11,828
Memristor—The Missing Circuit Element
Chua, L. (1971) · IEEE Transactions on Circuit Theory · doi:10.1109/tct.1971.1083337 · Cited by 10,268
Redox‐Based Resistive Switching Memories – Nanoionic Mechanisms, Prospects, and Challenges
Waser, R., Dittmann, R., Staikov, G., & Szot, K. (2009) · Advanced Materials · doi:10.1002/adma.200900375 · Cited by 5,080
Nanoionics-based resistive switching memories
Waser, R., & Aono, M. (2007) · Nature Materials · doi:10.1038/nmat2023 · Cited by 4,923
Nanoscale Memristor Device as Synapse in Neuromorphic Systems
Jo, S. H., Chang, T., Ebong, I., Bhadviya, B. B., Mazumder, P., & Lu, W. (2010) · Nano Letters · doi:10.1021/nl904092h · Cited by 4,174
Self-citationMemristive switching mechanism for metal/oxide/metal nanodevices
Yang, J. J., Pickett, M. D., Li, X., Ohlberg, D. A. A., Stewart, D. R., & Williams, R. S. (2008) · Nature Nanotechnology · doi:10.1038/nnano.2008.160 · Cited by 2,987
Memristive devices and systems
Chua, L. O., & Kang, S. M. (1976) · Proceedings of the IEEE · doi:10.1109/proc.1976.10092 · Cited by 2,604
Atomic structure of conducting nanofilaments in TiO2 resistive switching memory
Kwon, D.-H., Kim, K. M., Jang, J. H., Jeon, J. M., Lee, M. H., Kim, G. H., Li, X.-S., Park, G.-S., Lee, B., Han, S., et al. (2010) · Nature Nanotechnology · doi:10.1038/nnano.2009.456 · Cited by 2,092
‘Memristive’ switches enable ‘stateful’ logic operations via material implication
Borghetti, J., Snider, G. S., Kuekes, P. J., Yang, J. J., Stewart, D. R., & Williams, R. S. (2010) · Nature · doi:10.1038/nature08940 · Cited by 1,929
Complementary resistive switches for passive nanocrossbar memories
Linn, E., Rosezin, R., Kügeler, C., & Waser, R. (2010) · Nature Materials · doi:10.1038/nmat2748 · Cited by 1,274
Cited by
Items 401–500 of 1,201
Lim, Z. X., & Cheong, K. Y. (2018) · Advanced Materials Technologies · doi:10.1002/admt.201800007 · Cited by 40
Chen, J., Wu, Y., Zhu, K., Sun, F., Guo, C., Wu, X., Cheng, G., & Zheng, R. (2019) · Electrochimica Acta · doi:10.1016/j.electacta.2019.05.110 · Cited by 36
Park, J., Park, E., Kim, S., & Yu, H. (2019) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.9b11319 · Cited by 38
Nguyen, D. A., Jo, Y., Tran, T. U., Jeong, M. S., Kim, H., & Im, H. (2021) · Small Methods · doi:10.1002/smtd.202101303 · Cited by 37
Wang, Y., Li, W., Guo, Y., Huang, X., Luo, Z., Wu, S., Wang, H., Chen, J., Li, X., Zhan, X., et al. (2022) · Journal of Material Science and Technology · doi:10.1016/j.jmst.2022.04.021 · Cited by 36
Artificial sensory system based on memristive devices
Kwon, J. Y., Kim, J. E., Kim, J. S., Chun, S. Y., Soh, K., & Yoon, J. H. (2023) · Exploration · doi:10.1002/exp.20220162 · Cited by 49
Programmable Resistive-Switch Nanowire Transistor Logic Circuits
Shim, W., Yao, J., & Lieber, C. M. (2014) · Nano Letters · doi:10.1021/nl502654f · Cited by 34
First principles investigation of copper and silver intercalated molybdenum disulfide
Guzman, D., Onofrio, N., & Strachan, A. H. (2017) · Journal of Applied Physics · doi:10.1063/1.4975035 · Cited by 36
Reproducible switching effect of an all-inorganic halide perovskite CsPbBr 3 for memory applications
Hongzhang, L., Wu, Y., & Hu, Y. (2017) · Ceramics International · doi:10.1016/j.ceramint.2017.02.128 · Cited by 36
An oxygen vacancy mediated Ag reduction and nucleation mechanism in SiO2 RRAM devices
Patel, K., Cottom, J. P., Bosman, M., et al. (2019) · Microelectronics Reliability · doi:10.1016/j.microrel.2019.05.005 · Cited by 36
“In this study, Ag/a-SiO2 RRAM devices are considered due to the wealth of experimental data allowing for a reliable comparison between theory and experiment [9], [10].”
BackgroundA UV damage-sensing nociceptive device for bionic applications
Zhou, L., Zhang, S., Yang, J., Mao, J., Ren, Y., Shan, H., Xu, Z., Zhou, Y., & Han, S. (2019) · Nanoscale · doi:10.1039/c9nr08872e · Cited by 36
Water-Mediated Ionic Migration in Memristive Nanowires with a Tunable Resistive Switching Mechanism
Milano, G., Raffone, F., Lübben, M., Boarino, L., Cicero, G., Valov, I., & Ricciardi, C. (2020) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.0c13020 · Cited by 38
Hui, F., Liu, P., Hodge, S. A., Carey, T., Wen, C., Torrisi, F., Galhena, D. T. L., Tomarchio, F., Lin, Y., Moreno, E., et al. (2021) · Small · doi:10.1002/smll.202101100 · Cited by 36
Realistic Hodgkin–Huxley Axons Using Stochastic Behavior of Memristors
Feali, M. S., & Ahmadi, A. (2016) · Neural Processing Letters · doi:10.1007/s11063-016-9502-5 · Cited by 36
Li, Y., Yin, L., Wu, Z., Li, X., Song, X., Gao, X., & Fu, L. (2019) · IEEE Electron Device Letters · doi:10.1109/led.2019.2934145 · Cited by 37
“It has been demonstrated that the growth mode and the morphology of the CF are closely related to diffusion coefficient of cations in the electrolyte layer during the forming process [13]–[16].”
BackgroundWlaźlak, E., Zawal, P., & Szacilowski, K. T. (2020) · ACS Applied Electronic Materials · doi:10.1021/acsaelm.9b00750 · Cited by 34
Sangwan, V. K., Rangnekar, S. V., Kang, J., Shen, J., Lee, H., Lam, D. K., Shen, J., Liu, X., de Moraes, A. C. M., Kuo, L., et al. (2021) · Advanced Functional Materials · doi:10.1002/adfm.202107385 · Cited by 37
Review of applications of 2D materials in memristive neuromorphic circuits
Wang, L., Shen, X., Gao, Z., Fu, J., Yao, S., Cheng, L., & Lian, X. (2022) · Journal of Materials Science · doi:10.1007/s10853-022-06954-x · Cited by 36
“[21] directly observed the nano CFs using transmission electron microscopy (TEM), as shown in Fig.”
BackgroundMethodInfluentialSong, M., Lee, S., Nibhanupudi, S. S. T., Singh, J. V., Disiena, M. N., Luth, C. J., Wu, Y., Coupin, M. J., Warner, J. H., & Banerjee, S. K. (2023) · Nano Letters · doi:10.1021/acs.nanolett.3c00327 · Cited by 36
Tang, G., Zeng, F., Chen, C., Liu, H., Gao, S., Li, S. Z., Song, C., Wang, G. Y., & Pan, F. (2013) · Journal of Applied Physics · doi:10.1063/1.4812318 · Cited by 37
Electroforming-free resistive switching memory effect in transparent p-type tin monoxide
Hota, M. K., Caraveo-Frescas, J. A., McLachlan, M. A., et al. (2014) · Applied Physics Letters · doi:10.1063/1.4870405 · Cited by 35
Resistive Switching Characteristics of Li-Doped ZnO Thin Films Based on Magnetron Sputtering
Zhao, X., Li, Y., Ai, C., & Wen, D. (2019) · Materials · doi:10.3390/ma12081282 · Cited by 34
“The conduction mechanism of the resistive switching devices can be best understood by the space-charge-limited conduction (SCLC) model and conductive filament model [37,38].”
BackgroundLiquid-based memory and artificial synapse
Kim, D., & Lee, J. (2019) · Nanoscale · doi:10.1039/c9nr02767j · Cited by 37
Fu, J., Liao, Z., & Wang, J. (2022) · IEEE Transactions on Electron Devices · doi:10.1109/ted.2022.3146801 · Cited by 38
Liu, D., Cheng, H., Wang, G., et al. (2013) · Journal of Applied Physics · doi:10.1063/1.4826362 · Cited by 34
Jeen, H., & Biswas, A. (2013) · Physical Review B · doi:10.1103/physrevb.88.024415 · Cited by 34
Wang, L., Wang, Z., Lin, J., Yang, J., Xie, L., Yi, M., Li, W., Ling, H., Ou, C., & Huang, W. (2016) · Scientific Reports · doi:10.1038/srep35273 · Cited by 35
Ahn, Y., Shin, H. W., Lee, T. H., Kim, W., & Son, J. Y. (2018) · Nanoscale · doi:10.1039/c8nr02986e · Cited by 34
Conductive-AFM tomography for 3D filament observation in resistive switching devices
Celano, U., Goux, L., Belmonte, A., Schulze, A., Opsomer, K., Detavernier, C., Richard, O., Bender, H., Jurczak, M., & Vandervorst, W. (2013) · Technical digest - International Electron Devices Meeting/Technical digest · doi:10.1109/iedm.2013.6724679 · Cited by 35
Cause and Prevention of Moisture-Induced Degradation of Resistance Random Access Memory Nanodevices
Yang, X. Y., Choi, B. J., Chen, A. B. K., & Chen, I. (2013) · ACS Nano · doi:10.1021/nn3054544 · Cited by 33
“Most of these devices switch by forming (soft breakdown) conducting nanofilaments, undergoing redox reactions, or both.(10) 16 Naturally, redox reactions are often moisture-sensitive,(17) 19 but”
BackgroundResultInfluentialIn situ TEM Observation of Resistance Switching in Titanate Based Device
Yang, Y., Lü, W., Yao, Y., Sun, J., Gu, C., Gu, L., Wang, Y., Duan, X., & Yu, R. (2014) · Scientific Reports · doi:10.1038/srep03890 · Cited by 33
Self-citationFilament growth dynamics in solid electrolyte-based resistive memories revealed by in situ TEM
Tian, X., Wang, L., Wei, J., Yang, S., Wang, W., Xu, Z. Q., & Bai, X. (2014) · Nano Research · doi:10.1007/s12274-014-0469-0 · Cited by 36
“The above mentioned CF model has been testified by various experiments and theoretical works [16-19].”
Zhang, H. Z., Ang, D. S., Gu, C., Yew, K. S., Wang, X. P., & Lo, G. Q. (2014) · Applied Physics Letters · doi:10.1063/1.4903341 · Cited by 33
Filamentary Conduction in Aloe Vera Film for Memory Application
Lim, Z. X., Sasidharan, S., Wong, Y. H., Zhao, F., & Cheong, K. Y. (2017) · Procedia Engineering · doi:10.1016/j.proeng.2017.04.133 · Cited by 37
“However, successful observation of the conductive filament using SEM and TEM requires either modifications from vertical to planar device structure [30,31], or complex preparation steps, such as ion milling and sample thinning [32], that are not applicable to bio-organic materials.”
BackgroundWlaźlak, E., Marzec, M. M., Zawal, P., & Szacilowski, K. T. (2019) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.9b01841 · Cited by 32
Deng, Y., Keum, C., Hillebrandt, S. G. H., et al. (2020) · Advanced Optical Materials · doi:10.1002/adom.202001642 · Cited by 33
Bousoulas, P., Panagopoulou, M., Boukos, N. K., & Tsoukalas, D. (2021) · Journal of Physics D Applied Physics · doi:10.1088/1361-6463/abea3b · Cited by 37
“This selection is also in line with concrete experimental and theoretical evidences for SiO 2 -based CBRAM [46, 47].”
Mixed Ionic‐Electronic Charge Transport in Layered Black‐Phosphorus for Low‐Power Memory
Ahmed, T., Kuriakose, S., Tawfik, S. A., Mayes, E. L. H., Mazumder, A., Balendhran, S., Spencer, M. J. S., Akinwande, D., Bhaskaran, M. C., Sriram, S., et al. (2021) · Advanced Functional Materials · doi:10.1002/adfm.202107068 · Cited by 34
Tsuruoka, T., Hasegawa, T., Terabe, K., & Aono, M. (2017) · Journal of Electroceramics · doi:10.1007/s10832-016-0063-9 · Cited by 35
ReRAM‐Based Neuromorphic Computing
Indiveri, G., Linn, E., & Ambrogio, S. (2016) · Wiley eBooks · doi:10.1002/9783527680870.ch25 · Cited by 43
Mei, T., Chen, F., Huang, T., Feng, Z., Wan, T., Han, Z., Li, Z., Hu, L., Lin, C., Lu, Y., et al. (2025) · ACS Nano · doi:10.1021/acsnano.5c02397 · Cited by 38
Metal oxide-based resistive switching memristors for neuromorphic computing
Tian, Q., Shan, X., Bian, J., Cheng, Y., Zheng, J., Wang, Z., Zhao, X., Xu, H., & Liu, Y. (2025) · Journal of Materials Chemistry C · doi:10.1039/d5tc01467k · Cited by 37
Yang, W., Wang, J., Luo, S., Yu, S., Huang, H., Sun, R., & Wong, C. (2016) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.6b11492 · Cited by 32
Kim, H. J., Yoon, K. J., Park, T. H., Kim, H., Kwon, Y. J., Shao, X. L., Kwon, D. E., Kim, Y. M., & Hwang, C. S. (2017) · Advanced Electronic Materials · doi:10.1002/aelm.201600404 · Cited by 35
Transverse barrier formation by electrical triggering of a metal-to-insulator transition
Salev, P., Fratino, L., Sasaki, D., Berkoun, R., del Valle, J., Kalcheim, Y., Takamura, Y., Rozenberg, M. J., & Schuller, I. K. (2021) · Nature Communications · doi:10.1038/s41467-021-25802-1 · Cited by 34
Nanoscale Cross‐Point Resistive Switching Memory Comprising p‐Type SnO Bilayers
Hota, M. K., Hedhili, M. N., Wang, Q., Melnikov, V. A., Mohammed, O. F., & Alshareef, H. N. (2015) · Advanced Electronic Materials · doi:10.1002/aelm.201400035 · Cited by 33
Rahaman, S. Z., Maikap, S., Das, A., Prakash, A., Wu, Y. H., Lai, C., Tien, T., Chen, W.-S., Lee, H.-Y., Chen, F. T., et al. (2012) · Nanoscale Research Letters · doi:10.1186/1556-276x-7-614 · Cited by 34
“mation in these GexSe1 − x solid electrolytes is different from oxide-based materials reported elsewhere [34-36].”
BackgroundMemlumor: A Luminescent Memory Device for Energy-Efficient Photonic Neuromorphic Computing
Marunchenko, A., Kumar, J., Kiligaridis, A., Tatarinov, D., Pushkarev, A. P., Vaynzof, Y., & Scheblykin, I. G. (2024) · ACS Energy Letters · doi:10.1021/acsenergylett.4c00691 · Cited by 41
Li, C., Xu, T., Pan, R. Y., Bao, S., Yin, K., Shen, J., Zhu, Y., Hou, S., & Sun, L. (2024) · ACS Nano · doi:10.1021/acsnano.4c11598 · Cited by 38
Kinetic simulation of filament growth dynamics in memristive electrochemical metallization devices
Dirkmann, S., Ziegler, M., Hansen, M., Kohlstedt, H., Trieschmann, J., & Mussenbrock, T. (2015) · Journal of Applied Physics · doi:10.1063/1.4936107 · Cited by 40
Yang, F., Zhao, Q., Xu, C., Zou, Y., Dong, H., Zheng, Y., & Hu, W. (2016) · Advanced Materials · doi:10.1002/adma.201600902 · Cited by 31
Silicon compatible Sn-based resistive switching memory
Sonde, S. S., Chakrabarti, B., Liu, Y., Sasikumar, K., Lin, J., Stan, L., Divan, R., Ocola, L. E., Rosenmann, D., Choudhury, P., et al. (2018) · Nanoscale · doi:10.1039/c8nr01540f · Cited by 32
Liu, J., Jin, J., Yang, Z. H., Cai, J., Yue, J., Impundu, J., Liu, H., Wei, H., Peng, Z., Li, Y. J., et al. (2020) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.0c07186 · Cited by 32
Review of resistive switching mechanisms for memristive neuromorphic devices*
Yang, R. (2020) · Chinese Physics B · doi:10.1088/1674-1056/aba9c7 · Cited by 34
Factors Determining the Resistive Switching Behavior of Transparent InGaZnO‐Based Memristors
Qin, F. H., Zhang, Y., Park, H., Kim, C. S., Lee, D., Jiang, Z., Park, J.-M., No, K., Park, H., Song, H. W., et al. (2022) · physica status solidi (RRL) - Rapid Research Letters · doi:10.1002/pssr.202200075 · Cited by 35
Khan, M. U., Kim, J., Chougale, M. Y., Furqan, C. M., Saqib, Q. M., Shaukat, R. A., Kobayashi, N. P., Mohammad, B. S., Bae, J., & Kwok, H. S. (2022) · Microsystems & Nanoengineering · doi:10.1038/s41378-022-00390-2 · Cited by 31
“The human brain is composed of interconnected neurons, where the presynaptic neuron passes information to the postsynaptic neuron and results in the transmission of neurotransmitters that control synaptic plasticity 18,39,40 .”
BackgroundResistive random access memory and its applications in storage and nonvolatile logic
Zhu, D., Li, Y., Shen, W., Zhou, Z., Liu, L., & Zhang, X. (2017) · Journal of Semiconductors · doi:10.1088/1674-4926/38/7/071002 · Cited by 34
Ultrafast Multilevel Switching in Au/YIG/n‐Si RRAM
Chen, Z., Huang, W., Zhao, W., Hou, C., Ma, C., Liu, C., Sun, H., Yin, Y., & Li, X. (2018) · Advanced Electronic Materials · doi:10.1002/aelm.201800418 · Cited by 33
Multilevel Reset Dependent Set of a Biodegradable Memristor with Physically Transient
Shaikh, M. T. A. S., Nguyen, T. H. V., Jeon, H. J., et al. (2023) · Advanced Science · doi:10.1002/advs.202306206 · Cited by 30
Qin, F. H., Zhang, Y., Guo, Z., Park, T. J., Park, H., Kim, C. S., Park, J.-M., Fu, X., No, K., Song, H. W., et al. (2024) · Materials Advances · doi:10.1039/d3ma01142a · Cited by 34
Multielement Filament Memristor Enabling Multifunctional Neuromorphic Device
Jang, M., Song, H., Kim, H. J., Yoon, J. H., & Kim, K. M. (2025) · Advanced Functional Materials · doi:10.1002/adfm.202423273 · Cited by 35
Conducting-Interlayer SiOx Memory Devices on Rigid and Flexible Substrates
Wang, G., Raji, A. O., Lee, J., & Tour, J. M. (2014) · ACS Nano · doi:10.1021/nn4052327 · Cited by 35
Accelerating Dynamic Time Warping With Memristor-Based Customized Fabrics
Xu, X., Lin, F., Wang, A., Yao, X., Lu, Q. H., Xu, W., Shi, Y., & Hu, Y. H. (2017) · IEEE Transactions on Computer-Aided Design of Integrated Circuits and Systems · doi:10.1109/tcad.2017.2729344 · Cited by 28
“Recently studies show that memristors also have nondeterministic digital dynamics [49].”
BackgroundKumari, K., Kumar, A., Kotnees, D. K., Balakrishnan, J., Thakur, A. D., & Ray, S. J. (2019) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2019.152213 · Cited by 30
Ahn, Y., & Son, J. Y. (2020) · Ceramics International · doi:10.1016/j.ceramint.2020.12.064 · Cited by 30
Low-energy Resistive Random Access Memory Devices with No Need for a Compliance Current
Xu, Z., Yu, L., Wu, Y., Dong, C., Deng, N., Xu, X., Miao, J., & Jiang, Y. (2015) · Scientific Reports · doi:10.1038/srep10409 · Cited by 31
Qian, K., Nguyen, V. C., Chen, T. P., & Lee, P. S. (2016) · Advanced Electronic Materials · doi:10.1002/aelm.201500370 · Cited by 32
Perspective: Uniform switching of artificial synapses for large-scale neuromorphic arrays
Tan, S. H., Lin, P., Yeon, H., Choi, S., Park, Y., & Kim, J. (2018) · APL Materials · doi:10.1063/1.5049137 · Cited by 33
Sohn, W., Kim, H., Lee, J. H., Shim, Y., Moon, C. W., & Kim, H. (2025) · Materials Advances · doi:10.1039/d5ma00337g · Cited by 36
Memristor-Based Spiking Neuromorphic Systems Toward Brain-Inspired Perception and Computing
Wang, X., Zhu, Y., Zhou, Z., Chen, X., & Jia, X. (2025) · Nanomaterials · doi:10.3390/nano15141130 · Cited by 40
Memory Devices for Flexible and Neuromorphic Device Applications
Kim, D., Kim, I., & Lee, J. (2021) · Advanced Intelligent Systems · doi:10.1002/aisy.202000206 · Cited by 31
Noise Tailoring in Memristive Filaments
Sánta, B., Balogh, Z., Pósa, L., Krisztián, D., Török, T. N., Molnár, D., Sinkó, C., Hauert, R., Csontos, M., & Halbritter, A. (2021) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.0c21156 · Cited by 32
Xue, Q., Peng, Y., Cao, L., et al. (2022) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.2c03978 · Cited by 29
Koryazhkina, M. N., Филатов, Д. О., Shishmakova, V. A., Шенина, М. Е., Belov, A. I., Antonov, I. N., Kotomina, V. E., Mikhaylov, A. N., Gorshkov, O. N., Викторович, А. Н., et al. (2022) · Chaos Solitons & Fractals · doi:10.1016/j.chaos.2022.112459 · Cited by 29
Analysis on the Filament Structure Evolution in Reset Transition of Cu/HfO2/Pt RRAM Device
Zhang, M., Long, S., Li, Y., Liu, Q., Lv, H., Miranda, E. A., Suñé, J., & Liu, M. (2016) · Nanoscale Research Letters · doi:10.1186/s11671-016-1484-8 · Cited by 27
Li, J., Duan, Q., Zhang, T., Yin, M., Sun, X., Cai, Y., Li, L., Yang, Y., & Huang, R. (2017) · RSC Advances · doi:10.1039/c7ra07522g · Cited by 28
Self-citationWouters, D. J., Menzel, S., Rupp, J. A. J., Hennen, T., & Waser, R. M. (2018) · Faraday Discussions · doi:10.1039/c8fd00116b · Cited by 30
Zhao, X., Xu, H., Wang, Z., Xu, Z., Zhang, C., Wang, G., Liu, W., Ma, J., & Liu, Y. (2017) · Journal of Materials Chemistry C · doi:10.1039/c7tc00712d · Cited by 28
In-situ XAFS and SERS study of self-healing of passive film on Ti in Hank's physiological solution
Wang, L., Yu, H., Wang, S., et al. (2019) · Applied Surface Science · doi:10.1016/j.apsusc.2019.143657 · Cited by 28
Murthy, A. A., Stanev, T. K., dos Reis, R., Hao, S., Wolverton, C., Stern, N. P., & Dravid, V. P. (2020) · ACS Nano · doi:10.1021/acsnano.9b06581 · Cited by 29
Multilevel resistance switching of individual Cu2S nanowires with inert electrodes
Liu, P.-H., Lin, C.-C., Manekkathodi, A., et al. (2015) · Nano Energy · doi:10.1016/j.nanoen.2015.05.001 · Cited by 28
Memristor-Based Image Enhancement: High Efficiency and Robustness
Zhu, R., Tang, Z., Ye, S., Huang, Q., Guo, L., & Chang, S. (2020) · IEEE Transactions on Electron Devices · doi:10.1109/ted.2020.3045684 · Cited by 29
“Several pivotal articles had illustrated that the CFs played an essential role in the switching mechanisms in the memristors [22]–[24], and various memristor models were constructed.”
BackgroundUnconventional Resistive Switching Behavior in Fibroin‐Based Memristor
Chang, K., Dong, A., Yu, X., Liu, B., Zhao, X., REN-ZHI, W., Gan, Z., Jiang, K., Niu, Y., Dong, X., et al. (2021) · Advanced Electronic Materials · doi:10.1002/aelm.202100843 · Cited by 28
Xue, Q., Hang, T., Liang, J., Chen, C., Wu, Y., Ling, H., & Li, M. (2022) · Journal of Material Science and Technology · doi:10.1016/j.jmst.2021.09.007 · Cited by 27
Mandal, R., Mandal, A., Mitra, A., & Som, T. (2022) · Applied Surface Science · doi:10.1016/j.apsusc.2022.154860 · Cited by 30
Patil, S. L., Redekar, R. S., Pawar, O. Y., et al. (2023) · Journal of Materials Science Materials in Electronics · doi:10.1007/s10854-022-09436-7 · Cited by 28
“Under the electric field, the device can switch from a high resistance state (HRS, logic ‘0’ state) to a low resistance state (LRS, logic ‘1’ state) and vice versa [6].”
BackgroundLu, B., Du, J., Lü, J., Li, S., Yang, R., Liu, P., Huang, J., Chen, L., Zhuge, F., & Ye, Z. (2023) · ACS Materials Letters · doi:10.1021/acsmaterialslett.2c01218 · Cited by 28
Ren, S., Song, X.-T., Sun, G.-W., et al. (2013) · Journal of Materials Chemistry C · doi:10.1039/c3tc31779j · Cited by 28
Wang, L., Yang, J., Zhu, Y., Yi, M., Xie, L., Ju, R., Wang, Z., Liu, L., Li, T., Zhang, C., et al. (2017) · Advanced Electronic Materials · doi:10.1002/aelm.201700063 · Cited by 28
Modeling resistive switching materials and devices across scales
Ambrogio, S., Magyari‐Köpe, B., Onofrio, N., Islam, M. M., Duncan, D. L., Nishi, Y., & Strachan, A. H. (2017) · Journal of Electroceramics · doi:10.1007/s10832-017-0093-y · Cited by 31
Wu, Q., Lu, C., Wang, H., et al. (2018) · IEEE Electron Device Letters · doi:10.1109/led.2018.2880735 · Cited by 28
“2880735 form of cross-bar array design [1]–[4].”
Emulating dynamic synaptic plasticity over broad timescales with memristive device
Zhang, Y., Zhong, S., Song, L., Ji, X., & Zhao, R. J. (2018) · Applied Physics Letters · doi:10.1063/1.5052556 · Cited by 30
Nanofluidic Volatile Threshold Switching Ionic Memristor: A Perspective
Zhang, M., Xu, G., Zhang, H., & Xiao, K. (2025) · ACS Nano · doi:10.1021/acsnano.4c17760 · Cited by 32
Emerging 2D Material‐Based Synaptic Devices: Principles, Mechanisms, Improvements, and Applications
Yang, Z., Zhang, Z., Huo, S., Meng, F., Wang, Y., Ma, Y., Liu, B., Meng, F., Xie, Y., & Wu, E. (2025) · SmartMat · doi:10.1002/smm2.70005 · Cited by 34
“In memristor ‐ based synaptic devices, the evolution of conductive filaments involves redox reactions and ion migration [39 – 47].”
Evolution of conduction channel and its effect on resistance switching for Au-WO3-x–Au devices
Hong, D., Chen, Y. S., Li, Y., Yang, H., Wei, L. L., Shen, B., & Sun, J. R. (2014) · Scientific Reports · doi:10.1038/srep04058 · Cited by 27
A Study of Gamma-Ray Exposure of Cu–SiO$_2$ Programmable Metallization Cells
Chen, W., Barnaby, H., Kozicki, M. N., Edwards, A. H., Gonzalez-Velo, Y., Fang, R., Holbert, K. E., Yu, S., & Yu, W. (2015) · IEEE Transactions on Nuclear Science · doi:10.1109/tns.2015.2478883 · Cited by 33
“Resistance change occurs through the electrochemical creation and annihilation of nanoscale filaments in the solid electrolyte layer [13].”
BackgroundIn Situ Transmission Electron Microscopy
Ross, F. M., & Minor, A. M. (2019) · Springer handbooks · doi:10.1007/978-3-030-00069-1_3 · Cited by 30
Song, K., Yang, H., Chen, B., et al. (2022) · Applied Surface Science · doi:10.1016/j.apsusc.2022.155161 · Cited by 27
Kim, D., Bang, H., Baac, H. W., Lee, J., Truong, P. L., Jeong, B. H., Appadurai, T., Park, K. K., Heo, D., Nam, V. B., et al. (2023) · Advanced Functional Materials · doi:10.1002/adfm.202213064 · Cited by 28
Unipolar resistive switching with forming-free and self-rectifying effects in Cu/HfO2/n-Si devices
Wang, M. J., Gao, S., Zeng, F., Song, C., & Pan, F. (2016) · AIP Advances · doi:10.1063/1.4941839 · Cited by 27
Metadata
- Authors
- Yang, Y., Gao, P., Gaba, S., Chang, T., Pan, X., & Lu, W.
- Affiliations
- University of Michigan (US)
- Corresponding author
- Lu, Wei
- Venue
- Nature Communications
- Published
- 2012-03-13
- Volume
- 3
- Issue
- 1
- Pages
- 732-732
- ISSN
- 2041-1723 (ISSN-L)
- OpenAlex
- W2043707274
- Cited by
- 1,208
- References
- 32
- Citations by year
- 2026: 68 · 2025: 69 · 2024: 92 · 2023: 84 · 2022: 95 · 2021: 85 · 2020: 101 · 2019: 100 · 2018: 89 · 2017: 95 · 2016: 88 · 2015: 81 · 2014: 71 · 2013: 68 · 2012: 21
- FWCI
- 49.24
- Type
- journal article
- Language
- en
- Open access
- bronze
- doi.org
- Licence
- www.springernature.com/gp/researchers/text-and-data-mining (tdm)
- www.springernature.com/gp/researchers/text-and-data-mining (vor)
- Locations
- Nature Communications (publishedVersion)
- PubMed (publishedVersion)
- RePEc: Research Papers in Economics (submittedVersion)
- Funders
- National Science Foundation (0723032, 0907191, 0954621)
- Defense Advanced Research Projects Agency (HRL0011-09-C-001)
- Division of Materials Research (0723032, DMR-0723032)
- Division of Electrical, Communications and Cyber Systems (ECCS-0954621)
- Topics
- Physical Sciences › Engineering › Electrical and Electronic Engineering › Advanced Memory and Neural Computing
- Physical Sciences › Engineering › Electrical and Electronic Engineering › Ferroelectric and Negative Capacitance Devices
- Physical Sciences › Materials Science › Materials Chemistry › Phase-change materials and chalcogenides
- Keywords
- resistive switching, memristors, electrochemical metallization, cation transport, dielectric films, non-volatile memory, in situ transmission electron microscopy
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
The claim verdicts this report counts are experimental: their accuracy is not yet measured.
A language model drew the claims from the paper on 2026-09-30, under version 3 of the claim definition (model deepseek-v4.1-flash, prompt extract-v3).
A second model labelled each claim on 2026-09-30 (model jev-1.13-20260917, definition revision gold-guideline-v0.2).
Cited sources are checked with a language model’s help (gpt-6-sol).
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.