The DOI matches its Crossref record; 11 of the 11 references it cites were found in a registry or an index.
High aspect ratio silicon etch: A review
Abstract
High aspect ratio (HAR) silicon etch is reviewed, including commonly used terms, history, main applications, different technological methods, critical challenges, and main theories of the technologies. Chronologically, HAR silicon etch has been conducted using wet etch in solution, reactive ion etch (RIE) in low density plasma, single-step etch at cryogenic conditions in inductively coupled plasma (ICP) combined with RIE, time-multiplexed deep silicon etch in ICP-RIE configuration reactor, and single-step etch in high density plasma at room or near room temperature. Key specifications are HAR, high etch rate, good trench sidewall profile with smooth surface, low aspect ratio dependent etch, and low etch loading effects. Till now, time-multiplexed etch process is a popular industrial practice but the intrinsic scalloped profile of a time-multiplexed etch process, resulting from alternating between passivation and etch, poses a challenge. Previously, HAR silicon etch was an application associated primarily with microelectromechanical systems. In recent years, through-silicon-via (TSV) etch applications for three-dimensional integrated circuit stacking technology has spurred research and development of this enabling technology. This potential large scale application requires HAR etch with high and stable throughput, controllable profile and surface properties, and low costs.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Anisotropic etching of silicon
Bean, K. E. (1978) · IEEE Transactions on Electron Devices · doi:10.1109/t-ed.1978.19250 · Cited by 803
Foreword contributions from the 50th electronic components and technology conference
Boudreau, R. (2001) · IEEE Transactions on Advanced Packaging · doi:10.1109/tadvp.2001.982823 · Cited by 517
Schaepkens, M., Standaert, T. E. F. M., Rueger, N. R., Sebel, P. G. M., Oehrlein, G. S., & Cook, J. M. (1999) · Journal of Vacuum Science & Technology A: Vacuum, Surfaces, and Films · doi:10.1116/1.582108 · Cited by 319
A MICROMACHINED VIBRATING RING GYROSCOPE
Putty, M. W., & Najafi, K. (1994) · 1994 Solid-State, Actuators, and Microsystems Workshop Technical Digest · doi:10.31438/trf.hh1994.49 · Cited by 316
A Water-Amine-Complexing Agent System for Etching Silicon
Finne, R. M., & Klein, D. L. (1967) · Journal of The Electrochemical Society · doi:10.1149/1.2426793 · Cited by 309
Standaert, T. E. F. M., Hedlund, C., Joseph, E. A., Oehrlein, G. S., & Dalton, T. J. (2003) · Journal of Vacuum Science & Technology A Vacuum Surfaces and Films · doi:10.1116/1.1626642 · Cited by 309
Fabrication of novel three-dimensional microstructures by the anisotropic etching of
Bassous, E. (1978) · IEEE Transactions on Electron Devices · doi:10.1109/t-ed.1978.19249 · Cited by 309
Fabrication of high-density electrical feed-throughs by deep-reactive-ion etching of Pyrex glass
Li, X., Abe, T., Liu, Y., & Esashi, M. (2002) · Journal of Microelectromechanical Systems · doi:10.1109/jmems.2002.805211 · Cited by 143
Morgan, B. C., Waits, C. M., Krizmanic, J. F., et al. (2004) · Journal of Microelectromechanical Systems · doi:10.1109/jmems.2003.823220 · Cited by 135
Cited by
Vacuum Electronic High Power Terahertz Sources
Booske, J. H., Dobbs, R. J., Joye, C. D., Kory, C. L., Neil, G. R., Park, G.-S., Park, J., & Temkin, R. J. (2011) · IEEE Transactions on Terahertz Science and Technology · doi:10.1109/tthz.2011.2151610 · Cited by 1,086
Anisotropic Swelling and Fracture of Silicon Nanowires during Lithiation
Liu, X. H., Zheng, H., Zhong, L., Huang, S., Karki, K., Zhang, L. Q., Liu, Y., Kushima, A., Liang, W. T., Wang, J. W., et al. (2011) · Nano Letters · doi:10.1021/nl201684d · Cited by 809
In situ TEM electrochemistry of anode materials in lithium ion batteries
Liu, X. H., & Huang, J. Y. (2011) · Energy & Environmental Science · doi:10.1039/c1ee01918j · Cited by 496
Li, X. (2012) · Current Opinion in Solid State and Materials Science · doi:10.1016/j.cossms.2011.11.002 · Cited by 426
DNA confinement in nanochannels: physics and biological applications
Reisner, W., Pedersen, J. N., & Austin, R. H. (2012) · Reports on Progress in Physics · doi:10.1088/0034-4885/75/10/106601 · Cited by 336
An overview of through-silicon-via technology and manufacturing challenges
Gambino, J. P., Adderly, S. A., & Knickerbocker, J. U. (2015) · Microelectronic Engineering · doi:10.1016/j.mee.2014.10.019 · Cited by 317
Tiwale, N., Subramanian, A., Kisslinger, K., Lu, M., Kim, J., Stein, A., & Nam, C.-Y. (2019) · Journal of Materials Chemistry C · doi:10.1039/c9tc02974e · Cited by 78
Metadata
- Authors
- Wu, B., Kumar, A., & Pamarthy, S.
- Venue
- Journal of Applied Physics
- Publisher
- AIP Publishing
- Published
- 2010-09-01
- Volume
- 108
- Issue
- 5
- ISSN
- 0021-8979 (ISSN-L)
- 1089-7550
- OpenAlex
- W1997913942
- Cited by
- 749
- References
- 11
- FWCI
- 19.94
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.