Abstract
Purpose: Obtaining the required part top surface roughness and side roughness is critical in some applications. Each of these part properties can often be improved to the detriment of the other during selective laser melting (SLM). The purpose of this paper is to investigate the selective laser melting of Inconel 625 using an Nd:YAG pulsed laser to produce thin wall parts with an emphasis on attaining parts with minimum top surface and side surface roughness. Design/methodology/approach: A full factorial approach was used to vary process parameters and identify a usable Inconel 625 processing region. The effects laser process parameters had on the formation of part surface roughness for multi‐layer parts were examined. Processing parameters that specifically affected top surface and side roughness were identified. Findings: Higher peak powers tended to reduce top surface roughness and reduce side roughness as recoil pressures flatten out the melt pool and reduce balling formation by increasing wettability of the melt. Increased repetition rate and reduced scan speed reduced top surface roughness but increased side roughness. A compromise between attaining a relatively low surface roughness and side roughness can be attained by comparing part surface roughness values and understanding the factors that affect them. A sample with 9 μ m top surface roughness and 10 μ m side roughness was produced. Originality/value: The research is the first of its kind directly processing Inconel 625 using SLM and investigating processing parameters that affect top surface and side roughness simultaneously. It is a useful aid in unveiling a relationship between process parameters and top/side roughness of thin walled parts.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Selective laser melting of iron-based powder
Kruth, J. P., Froyen, L., Van Vaerenbergh, J., Mercelis, P., Rombouts, M., & Lauwers, B. (2004) · Journal of Materials Processing Technology · doi:10.1016/j.jmatprotec.2003.11.051 · Cited by 1,550
Binding mechanisms in selective laser sintering and selective laser melting
Kruth, J., Mercelis, P., Van Vaerenbergh, J., Froyen, L., & Rombouts, M. (2005) · Rapid Prototyping Journal · doi:10.1108/13552540510573365 · Cited by 1,383
Investigations on residual stresses and deformations in selective laser melting
Zaeh, M. F., & Branner, G. (2010) · Production Engineering · doi:10.1007/s11740-009-0192-y · Cited by 666
Direct selective laser sintering of metals
Agarwala, M., Bourell, D., Beaman, J., Marcus, H., & Barlow, J. (1995) · Rapid Prototyping Journal · doi:10.1108/13552549510078113 · Cited by 571
Physical Aspects of Process Control in Selective Laser Sintering of Metals
Das, S. (2003) · Advanced Engineering Materials · doi:10.1002/adem.200310099 · Cited by 434
Sintering of commercially pure titanium powder with a Nd:YAG laser source
Fischer, P., Romano, V., Weber, H. P., Karapatis, N. P., Boillat, É., & Glardon, R. (2003) · Acta Materialia · doi:10.1016/s1359-6454(02)00567-0 · Cited by 408
Fundamentals of Selective Laser Melting of alloyed steel powders
Rombouts, M., Kruth, J. P., Froyen, L., & Mercelis, P. (2006) · CIRP Annals · doi:10.1016/s0007-8506(07)60395-3 · Cited by 400
High density selective laser melting of Waspaloy®
Mumtaz, K. A., Erasenthiran, P., & Hopkinson, N. (2008) · Journal of Materials Processing Technology · doi:10.1016/j.jmatprotec.2007.04.117 · Cited by 245
Self-citationSelective Laser Melting of thin wall parts using pulse shaping
Mumtaz, K. A., & Hopkinson, N. (2010) · Journal of Materials Processing Technology · doi:10.1016/j.jmatprotec.2009.09.011 · Cited by 234
Self-citationSelective laser sintering (melting) of stainless and tool steel powders: Experiments and modelling
Childs, T. H. C., Hauser, C., & Badrossamay, M. (2005) · Proceedings of the Institution of Mechanical Engineers, Part B: Journal of Engineering Manufacture · doi:10.1243/095440505x8109 · Cited by 199
Cited by
Additive manufacturing of metallic components – Process, structure and properties
DebRoy, T., Wei, H. L., Zuback, J. S., Mukherjee, T., Elmer, J. W., Milewski, J. O., Beese, A. M., Wilson-Heid, A., De, A., & Zhang, W. (2018) · Progress in Materials Science · doi:10.1016/j.pmatsci.2017.10.001 · Cited by 8,805
“Due to the surface tension gradient driven flow inside the molten pool, these small balls are dragged to the outer edges of the molten pool [125,195].”
BackgroundMethodInfluentialLaser additive manufacturing of metallic components: materials, processes and mechanisms
Gu, D. D., Meiners, W., Wissenbach, K., & Poprawe, R. (2012) · International Materials Reviews · doi:10.1179/1743280411y.0000000014 · Cited by 3,197
Review of selective laser melting: Materials and applications
Yap, C. Y., Chua, C. K., Dong, Z. L., Liu, Z. H., Zhang, D. Q., Loh, L. E., & Sing, S. L. (2015) · Applied Physics Reviews · doi:10.1063/1.4935926 · Cited by 2,353
Ding, D., Pan, Z., Cuiuri, D., & Li, H. (2015) · The International Journal of Advanced Manufacturing Technology · doi:10.1007/s00170-015-7077-3 · Cited by 1,648
Sanaei, N., & Fatemi, A. (2021) · Progress in Materials Science · doi:10.1016/j.pmatsci.2020.100724 · Cited by 1,029
Surface roughness analysis, modelling and prediction in selective laser melting
Strano, G., Hao, L., Everson, R. M., & Evans, K. E. (2013) · Journal of Materials Processing Technology · doi:10.1016/j.jmatprotec.2012.11.011 · Cited by 876
Chowdhury, S., Yadaiah, N., Prakash, C., Ramakrishna, S., Dixit, S., Gupta, L. R., & Buddhi, D. (2022) · Journal of Materials Research and Technology · doi:10.1016/j.jmrt.2022.07.121 · Cited by 784
Surface texture metrology for metal additive manufacturing: a review
Townsend, A., Senin, N., Blunt, L., Leach, R. K., & Taylor, J. S. (2016) · Precision Engineering · doi:10.1016/j.precisioneng.2016.06.001 · Cited by 743
Investigations on residual stresses and deformations in selective laser melting
Zaeh, M. F., & Branner, G. (2010) · Production Engineering · doi:10.1007/s11740-009-0192-y · Cited by 666
Li, P., Warner, D. H., Fatemi, A., & Phan, N. (2016) · International Journal of Fatigue · doi:10.1016/j.ijfatigue.2015.12.003 · Cited by 546
Narasimharaju, S. R., Zeng, W., See, T. L., Zhu, Z., Scott, P., Jiang, X., & Lou, S. (2022) · Journal of Manufacturing Processes · doi:10.1016/j.jmapro.2021.12.033 · Cited by 508
Defects and anomalies in powder bed fusion metal additive manufacturing
Mostafaei, A., Zhao, C., He, Y., Reza Ghiaasiaan, S., Shi, B., Shao, S., Shamsaei, N., Wu, Z., Kouraytem, N., Sun, T., et al. (2022) · Current Opinion in Solid State and Materials Science · doi:10.1016/j.cossms.2021.100974 · Cited by 491
Hybrid additive and subtractive machine tools – Research and industrial developments
Flynn, J. M., Shokrani, A., Newman, S. T., & Dhokia, V. (2016) · International Journal of Machine Tools and Manufacture · doi:10.1016/j.ijmachtools.2015.11.007 · Cited by 459
Lasers in additive manufacturing: A review
Lee, H., Lim, C. H. J., Low, M. J., Tham, N., Murukeshan, V. M., & Kim, Y.-J. (2017) · International Journal of Precision Engineering and Manufacturing-Green Technology · doi:10.1007/s40684-017-0037-7 · Cited by 449
Song, B., Zhao, X., Li, S., Han, C., Wei, Q., Wen, S., Liu, J., & Shi, Y. (2015) · Frontiers of Mechanical Engineering · doi:10.1007/s11465-015-0341-2 · Cited by 427
Tan, J. H., Wong, W. L. E., & Dalgarno, K. W. (2017) · Additive Manufacturing · doi:10.1016/j.addma.2017.10.011 · Cited by 407
Multi-scale defects in powder-based additively manufactured metals and alloys
Fu, J., Li, H., Song, X., & Fu, M. W. (2022) · Journal of Materials Science & Technology · doi:10.1016/j.jmst.2022.02.015 · Cited by 391
Fox, J. C., Moylan, S. P., & Lane, B. M. (2016) · Procedia CIRP · doi:10.1016/j.procir.2016.02.347 · Cited by 377
Tian, Y., Tomus, D., Rometsch, P., & Wu, X. (2017) · Additive Manufacturing · doi:10.1016/j.addma.2016.10.010 · Cited by 363
Bagherifard, S., Beretta, N., Monti, S., Riccio, M., Bandini, M., & Guagliano, M. (2018) · Materials & Design · doi:10.1016/j.matdes.2018.02.055 · Cited by 327
A big data-driven framework for sustainable and smart additive manufacturing
Majeed, A., Zhang, Y., Ren, S., Lv, J., Peng, T., Waqar, S., & Yin, E. (2021) · Robotics and Computer-Integrated Manufacturing · doi:10.1016/j.rcim.2020.102026 · Cited by 313
Ahn, D.-G. (2016) · International Journal of Precision Engineering and Manufacturing-Green Technology · doi:10.1007/s40684-016-0048-9 · Cited by 268
Abd-Elaziem, W., Elkatatny, S., Abd-Elaziem, A.-E., Khedr, M., Abd El-baky, M. A., Hassan, M. A., Abu-Okail, M., Mohammed, M., Järvenpää, A., Allam, T., et al. (2022) · Journal of Materials Research and Technology · doi:10.1016/j.jmrt.2022.07.085 · Cited by 257
Wang, D., Liu, Y., Yang, Y., & Xiao, D. (2016) · Rapid Prototyping Journal · doi:10.1108/rpj-06-2015-0078 · Cited by 254
Biomedical applications of additive manufacturing: Present and future
Singh, S., & Ramakrishna, S. (2017) · Current Opinion in Biomedical Engineering · doi:10.1016/j.cobme.2017.05.006 · Cited by 248
Rickenbacher, L., Etter, T., Hövel, S., & Wegener, K. (2013) · Rapid Prototyping Journal · doi:10.1108/13552541311323281 · Cited by 239
Pegues, J. W., Shao, S., Shamsaei, N., Sanaei, N., Fatemi, A., Warner, D. H., Li, P., & Phan, N. (2020) · International Journal of Fatigue · doi:10.1016/j.ijfatigue.2019.105358 · Cited by 236
“In contrast, another study analyzing the top and side surface roughness of laser beam melted parts showed that there is a compromise between them, i.e. improving the R a on the top is always accompanied by deterioration R a of the side and vice versa [65].”
ResultSelective Laser Melting of thin wall parts using pulse shaping
Mumtaz, K. A., & Hopkinson, N. (2010) · Journal of Materials Processing Technology · doi:10.1016/j.jmatprotec.2009.09.011 · Cited by 234
Self-citationThe development of design rules for selective laser melting
Thomas, D. (2009) · Cardiff Metropolitan Research Repository (Cardiff Metropolitan University) · doi:10.25401/cardiffmet.20974597 · Cited by 211
A Review on Laser Powder Bed Fusion of Inconel 625 Nickel-Based Alloy
Tian, Z., Zhang, C., Wang, D., Liu, W., Fang, X., Wellmann, D., Zhao, Y., & Tian, Y. (2019) · Applied Sciences · doi:10.3390/app10010081 · Cited by 196
“By controlling these factors reasonably, low Ra on the top surface and side can be obtained simultaneously [56,57].”
BackgroundMethodGonzalez, J. A., Mireles, J., Stafford, S. W., Perez, M. A., Terrazas, C. A., & Wicker, R. B. (2019) · Journal of Materials Processing Technology · doi:10.1016/j.jmatprotec.2018.08.031 · Cited by 186
Review of Powder Bed Fusion Additive Manufacturing for Metals
Ladani, L., & Sadeghilaridjani, M. (2021) · Metals · doi:10.3390/met11091391 · Cited by 181
Wen, P., Voshage, M., Jauer, L., Chen, Y., Qin, Y., Poprawe, R., & Schleifenbaum, J. H. (2018) · Materials & Design · doi:10.1016/j.matdes.2018.05.057 · Cited by 179
Lee, J.-Y., Nagalingam, A. P., & Yeo, S. H. (2021) · Virtual and Physical Prototyping · doi:10.1080/17452759.2020.1830346 · Cited by 177
“High thermal energy at the melted edge attracts the surrounding powders, leading to partial melting and solidification along the edges (Mumtaz and Hopkinson 2009).”
BackgroundSing, S. L., Wiria, F. E., & Yeong, W. Y. (2018) · International Journal of Refractory Metals and Hard Materials · doi:10.1016/j.ijrmhm.2018.08.006 · Cited by 163
Soliman, A., AlAmoodi, N., Karanikolos, G. N., Doumanidis, C. C., & Polychronopoulou, K. (2020) · Nanomaterials · doi:10.3390/nano10112198 · Cited by 53
Effect of Additive Manufacturing Process Parameters on Turbine Cooling
Snyder, J. C., & Thole, K. A. (2019) · Volume 5B: Heat Transfer · doi:10.1115/gt2019-90862 · Cited by 21
“Mumtaz and Hopkinson [10] built single-pass thin-wall parts with Inconel 625 using a pulsed laser.”
MethodResultInfluential
Metadata
- Authors
- Mumtaz, K., & Hopkinson, N.
- Venue
- Rapid Prototyping Journal
- Publisher
- Emerald
- Published
- 2009-03-27
- Volume
- 15
- Issue
- 2
- Pages
- 96-103
- ISSN
- 1355-2546 (ISSN-L)
- OpenAlex
- W1992486005
- Cited by
- 429
- References
- 14
- FWCI
- 7.32
- Type
- journal article
- Language
- en
- Open access
- closed
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.