The Influence of Small Amounts of KCl(s) on the Initial Stages of the Corrosion of Alloy Sanicro 28 at 600 °C
The DOI matches its Crossref record; 18 of the 18 references it cites were found in a registry or an index.
Overview
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
Citations
Cites
Thermochemical data of pure substances
(1993) · Choice Reviews Online · doi:10.5860/choice.31-0632 · Cited by 4,494
Thermochemical Data of Pure Substances
Barin, I. (1995) · doi:10.1002/9783527619825 · Cited by 4,241
The implications of chlorine-associated corrosion on the operation of biomass-fired boilers
Nielsen, H. P., Frandsen, F. J., Dam-Johansen, K., & Baxter, L. L. (2000) · Progress in Energy and Combustion Science · doi:10.1016/s0360-1285(00)00003-4 · Cited by 785
Grabke, H. J., Reese, E., & Spiegel, M. (1995) · Corrosion Science · doi:10.1016/0010-938x(95)00011-8 · Cited by 537
Asteman, H., Svensson, J.-E., Norell, M., & Johansson, L.-G. (2000) · Oxidation of Metals · doi:10.1023/a:1004642310974 · Cited by 325
Self-citationAsteman, H., Svensson, J.-E., Johansson, L.-G., & Norell, M. (1999) · Oxidation of Metals · doi:10.1023/a:1018875024306 · Cited by 304
Self-citationDeposition and high temperature corrosion in a 10 MW straw fired boiler
Michelsen, H. P., Frandsen, F., Dam-Johansen, K., & Larsen, O. H. (1998) · Fuel Processing Technology · doi:10.1016/s0378-3820(97)00062-3 · Cited by 258
KCl Induced Corrosion of a 304-type Austenitic Stainless Steel at 600°C; The Role of Potassium
Pettersson, J., Asteman, H., Svensson, J. E., & Johansson, L. G. (2005) · Oxidation of Metals · doi:10.1007/s11085-005-5704-3 · Cited by 182
Self-citationAsteman, H., Svensson, J.-E., & Johansson, L.-G. (2002) · Corrosion Science · doi:10.1016/s0010-938x(02)00056-2 · Cited by 147
Self-citationZahs, A., Spiegel, M., & Grabke, H. (1999) · Materials and Corrosion · doi:10.1002/(sici)1521-4176(199910)50:10<561::aid-maco561>3.0.co;2-l · Cited by 131
Research works printed but not linked: 1
- M. J. McNallan et al., International Corrosion Conference Series NACE-6, 316 (1983).
Cited by
Antunes, R. A., & de Oliveira, M. C. L. (2013) · Corrosion Science · doi:10.1016/j.corsci.2013.07.013 · Cited by 184
Alkali Induced High Temperature Corrosion of Stainless Steel: The Influence of NaCl, KCl and CaCl2
Karlsson, S., Pettersson, J., Johansson, L. G., & Svensson, J. E. (2012) · Oxidation of Metals · doi:10.1007/s11085-012-9293-7 · Cited by 118
Self-citationPettersson, J., Folkeson, N., Johansson, L.-G., & Svensson, J.-E. (2011) · Oxidation of Metals · doi:10.1007/s11085-011-9240-z · Cited by 117
Self-citationFolkeson, N., Jonsson, T., Halvarsson, M., Johansson, L. ‐., & Svensson, J. ‐. (2011) · Materials and Corrosion · doi:10.1002/maco.201005942 · Cited by 93
Self-citationJonsson, T., Folkeson, N., Svensson, J., Johansson, L.-G., & Halvarsson, M. (2011) · Corrosion Science · doi:10.1016/j.corsci.2011.03.007 · Cited by 88
Self-citationStudies on the corrosion behavior of Fe-20Cr alloy in NaCl solution spray at 600 °C
Cao, M., Liu, L., Yu, Z., Fan, L., Li, Y., & Wang, F. (2018) · Corrosion Science · doi:10.1016/j.corsci.2018.01.033 · Cited by 66
Eklund, J., Jönsson, B., Persdotter, A., Liske, J., Svensson, J.-E., & Jonsson, T. (2018) · Corrosion Science · doi:10.1016/j.corsci.2018.09.004 · Cited by 55
Self-citationIsraelsson, N., Unocic, K. A., Hellström, K., Jonsson, T., Norell, M., Svensson, J.-E., & Johansson, L.-G. (2015) · Oxidation of Metals · doi:10.1007/s11085-015-9546-3 · Cited by 54
Self-citationThermogravimetric studies of high temperature reactions between potassium salts and chromium
Lehmusto, J., Lindberg, D., Yrjas, P., Skrifvars, B.-J., & Hupa, M. M. (2012) · Corrosion Science · doi:10.1016/j.corsci.2012.02.013 · Cited by 54
Israelsson, N., Engkvist, J., Hellström, K., Halvarsson, M., Svensson, J.-E., & Johansson, L.-G. (2015) · Oxidation of Metals · doi:10.1007/s11085-014-9507-2 · Cited by 53
Self-citationMa, H. T., Zhou, C., & Wang, L. (2009) · Corrosion Science · doi:10.1016/j.corsci.2009.05.014 · Cited by 49
KCl-Induced Corrosion of the FeCrAl Alloy Kanthal ® AF at 600 °C and the Effect of H2O
Israelsson, N., Hellström, K., Svensson, J.-E., & Johansson, L.-G. (2015) · Oxidation of Metals · doi:10.1007/s11085-014-9506-3 · Cited by 46
Self-citationMlonka-Mędrala, A., Gołombek, K., Buk, P., Cieślik, E., & Nowak, W. (2019) · Energy · doi:10.1016/j.energy.2019.116062 · Cited by 46
Persdotter, A., Eklund, J., Liske, J., & Jonsson, T. (2020) · Corrosion Science · doi:10.1016/j.corsci.2020.108961 · Cited by 44
Cyclic Corrosion and Chlorination of an FeCrAl Alloy in the Presence of KCl
Israelsson, N., Unocic, K. A., Hellström, K., Svensson, J. E., & Johansson, L. (2015) · Oxidation of Metals · doi:10.1007/s11085-015-9554-3 · Cited by 29
Self-citationSui, J., Lehmusto, J., Bergelin, M., & Hupa, L. (2019) · Corrosion Science · doi:10.1016/j.corsci.2019.04.010 · Cited by 26
Eklund, J., Hanif, I., Bigdeli, S., & Jonsson, T. (2022) · Corrosion Science · doi:10.1016/j.corsci.2022.110114 · Cited by 25
Persdotter, A., Sattari, M., Larsson, E., Ogaz, M. A. O., Liske, J., & Jonsson, T. (2019) · Corrosion Science · doi:10.1016/j.corsci.2019.108234 · Cited by 26
The long-term corrosion behavior of fecral(Si) alloys after breakaway oxidation at 600 °C
Eklund, J., Persdotter, A., Ssenteza, V., & Jonsson, T. (2023) · Corrosion Science · doi:10.1016/j.corsci.2023.111155 · Cited by 22
Fantozzi, D., Matikainen, V., Uusitalo, M. A., Koivuluoto, H., & Vuoristo, P. M. J. (2019) · Corrosion Science · doi:10.1016/j.corsci.2019.108166 · Cited by 22
Phother-Simon, J., Hanif, I., Jonsson, T., & Liske, J. (2024) · Fuel · doi:10.1016/j.fuel.2023.130012 · Cited by 21
Bigdeli, S., Kjellqvist, L., Naraghi, R., Höglund, L., Larsson, H., & Jonsson, T. (2021) · Journal of Phase Equilibria and Diffusion · doi:10.1007/s11669-021-00893-x · Cited by 19
Proff, C., Jonsson, T., Pettersson, C., Svensson, J.-E., Johansson, L.-G., & Halvarsson, M. (2009) · Materials at High Temperatures · doi:10.1179/096034009x464339 · Cited by 19
Self-citationThe Effects of KCl, NaCl and K2CO3 on the High-Temperature Oxidation Onset of Sanicro 28 Steel
Sui, J., Lehmusto, J., Bergelin, M., & Hupa, M. (2016) · Oxidation of Metals · doi:10.1007/s11085-016-9613-4 · Cited by 19
Lehmusto, J., Lindberg, D., Yrjas, P., Skrifvars, B.-J., & Hupa, M. M. (2011) · Oxidation of Metals · doi:10.1007/s11085-011-9277-z · Cited by 19
Fan, L., Liu, L., Lv, Y. L., Wang, H., Fu, A., Yuan, J., Li, Y., Wang, F., & Yin, C. (2020) · Scientific Reports · doi:10.1038/s41598-020-73034-y · Cited by 20
Eklund, J., Paz, M. D., Jönsson, B., Liske, J., Svensson, J., & Jonsson, T. (2019) · Materials and Corrosion · doi:10.1002/maco.201810618 · Cited by 18
Self-citationPersdotter, A., Boll, T., & Jonsson, T. (2021) · Corrosion Science · doi:10.1016/j.corsci.2021.109779 · Cited by 16
The Effect of Temperature on the Formation of Oxide Scales Regarding Commercial Superheater Steels
Lehmusto, J., Lindberg, D., Yrjas, P., & Hupa, L. (2017) · Oxidation of Metals · doi:10.1007/s11085-017-9785-6 · Cited by 14
Mortazavi, N., Intiso, L., Israelsson, N., Johansson, L., & Halvarsson, M. (2015) · Journal of The Electrochemical Society · doi:10.1149/2.0581514jes · Cited by 12
Self-citationPre-oxidation as a Means to Increase Corrosion Resistance of Commercial Superheater Steels
Lehmusto, J., Yrjas, P., & Hupa, L. (2019) · Oxidation of Metals · doi:10.1007/s11085-019-09898-x · Cited by 11
Comparison between oxidation of Fe–Cr–Al sputter coatings in air and air–HCl environments at 550°C
Orlicka, D., Simms, N. J., Hussain, T., & Nicholls, J. R. (2015) · Materials at High Temperatures · doi:10.1179/0960340914z.00000000095 · Cited by 8
“, alkali chloride and chromate formation instead of alkali iron tri-sulphate formation).(6,7) Gases containing chlorine in the form of HCl, Cl2, NaCl or KCl can accelerate the fireside corrosion rate causing increased oxidation processes, metal wastage and/or defects in the metal structure.”
BackgroundLehmusto, J., Yrjas, P., Skrifvars, B. J., & Hupa, M. M. (2011) · Materials science forum · doi:10.4028/www.scientific.net/msf.696.218 · Cited by 7
Mortazavi, N., Intiso, L., Israelsson, N., Johansson, L., & Halvarsson, M. (2015) · CORROSION · doi:10.5006/1874 · Cited by 7
Self-citationZhou, Y., Xie, G., & Zhang, J. (2025) · Journal of Alloys and Compounds · doi:10.1016/j.jallcom.2025.182417 · Cited by 4
Reducing High Temperature Corrosion when Burning Waste by Adding Digested Sewage Sludge
Karlsson, S., Åmand, L.-E., & Pettersson, J. (2011) · Chalmers Publication Library (Chalmers University of Technology) · Cited by 6
Ssenteza, V., Olausson, M. D. P., Eklund, J., Nockert, J., Liske, J., & Jonsson, T. (2025) · Energy & Fuels · doi:10.1021/acs.energyfuels.4c04806 · Cited by 1
Persdotter, A., Larsson, H., Eklund, J., Bigdeli, S., & Jonsson, T. (2024) · Corrosion Science · doi:10.1016/j.corsci.2024.112473 · Cited by 1
Pompe, R., Svensson, J., Pettersson, C., & Johansson, L. (2011) · NACE CORROSION Conference · doi:10.5006/c2011-11194 · Cited by 1
Self-citationHigh Temperature Corrosion of Stainless Steels - The Effects of Chloride Salts and SO2(g)
Karlsson, S. (2011) · Chalmers Publication Library (Chalmers University of Technology) · Cited by 1
Couture, L. (2011) · theses.fr (ABES) · doi:10.70675/d5076b6dzdb61z49f1z962dzb1a17cc9d342 · Cited by 1
Metadata
- Authors
- Pettersson, C., Johansson, L.-G., & Svensson, J.-E.
- Affiliations
- Chalmers University of Technology (SE)
- Corresponding author
- Pettersson, C.
- Venue
- Oxidation of Metals
- Published
- 2008-08-16
- Volume
- 70
- Issue
- 5-6
- Pages
- 241-256
- ISSN
- 0030-770X (ISSN-L)
- 1573-4889
- OpenAlex
- W2001400594
- Cited by
- 40
- References
- 17
- Citations by year
- 2025: 1 · 2024: 2 · 2023: 2 · 2022: 1 · 2021: 2 · 2020: 2 · 2019: 6 · 2018: 2 · 2017: 1 · 2016: 1 · 2015: 5 · 2014: 2 · 2013: 1 · 2012: 2
- FWCI
- 6.86
- Type
- journal article
- Language
- en
- Open access
- closed
- Licence
- www.springer.com/tdm (tdm)
- Locations
- Oxidation of Metals (publishedVersion)
- Chalmers Publication Library (Chalmers University of Technology) (submittedVersion)
- Chalmers Research (Chalmers University of Technology) (submittedVersion)
- Topics
- Physical Sciences › Materials Science › Surfaces, Coatings and Films › High-Temperature Coating Behaviors
- Physical Sciences › Materials Science › Metals and Alloys › Hydrogen embrittlement and corrosion behaviors in metals
- Physical Sciences › Materials Science › Materials Chemistry › Corrosion Behavior and Inhibition
- Keywords
- Sanicro 28, austenitic stainless steel, potassium chloride, high-temperature oxidation, potassium chromate, chloride attack, chromium depletion, corrosion initiation, oxide scale
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.