Abstract

The periodic table elements involved in electrochemical water splitting.

Overview

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Integrity signals

Registry

Crossref · 10.1039/d2ra07642j

Cites

257 of 257 references verified0 citation errors · 0 not checkable

Statistics

Figures

Fig. 1 A schematic illustration of a potential HER reaction pathway on cathode.48
Fig. 1 A schematic illustration of a potential HER reaction pathway on cathode.48CC BY-NC · PubMed Central
Fig. 2 Hydrogen evolution reaction (HER) volcano plot on metal electrodes under low pH environment. For each metal surface, the logarithm of the exchange current density j0 is plotted against M–H bond energy. Reproduced with permission2 Copyright 2010, American Chemical Society.
Fig. 2 Hydrogen evolution reaction (HER) volcano plot on metal electrodes under low pH environment. For each metal surface, the logarithm of the exchange current density j0 is plotted against M–H bond energy. Reproduced with permission2 Copyright 2010, American Chemical Society.CC BY-NC · PubMed Central
Fig. 3 The mechanisms governing the oxygen evolution reaction in acidic (blue line) and alkaline electrolytes, respectively. The corresponding black and green lines represent the two likely intermediates, M–OOH and M–O. Reproduced with permission64 Copyright 2020, Elsevier.
Fig. 3 The mechanisms governing the oxygen evolution reaction in acidic (blue line) and alkaline electrolytes, respectively. The corresponding black and green lines represent the two likely intermediates, M–OOH and M–O. Reproduced with permission64 Copyright 2020, Elsevier.CC BY-NC · PubMed Central
Fig. 4 Volcano plot demonstrates the relationship between the rate of O2 oxidation on transition metal oxide surfaces and change in enthalpy in acidic () and basic () solutions. Measurement of overpotential in relation to 0.1 mA cm2 current density. Reproduced with permission2 Copyright 2010, American Chemical Society.
Fig. 4 Volcano plot demonstrates the relationship between the rate of O2 oxidation on transition metal oxide surfaces and change in enthalpy in acidic () and basic () solutions. Measurement of overpotential in relation to 0.1 mA cm2 current density. Reproduced with permission2 Copyright 2010, American Chemical Society.CC BY-NC · PubMed Central
Fig. 5 Endangered species of elements and their potential application as electrocatalysts for water splitting, according to the aster diagram. Reproduced with permission67 Copyright 2022, Elsevier.
Fig. 5 Endangered species of elements and their potential application as electrocatalysts for water splitting, according to the aster diagram. Reproduced with permission67 Copyright 2022, Elsevier.CC BY-NC · PubMed Central
Fig. 6 The evaluation parameters of electrochemical water splitting.
Fig. 6 The evaluation parameters of electrochemical water splitting.CC BY-NC · PubMed Central
Fig. 7 IrTiO2 electrode's Tafel curves were obtained using both chronoamperometry in 0.1 M perchloric acid and CV at 5 mV s−1. Reproduced with permission from ref. 58 Copyright 2014, Royal Society of Chemistry.
Fig. 7 IrTiO2 electrode's Tafel curves were obtained using both chronoamperometry in 0.1 M perchloric acid and CV at 5 mV s−1. Reproduced with permission from ref. 58 Copyright 2014, Royal Society of Chemistry.CC BY-NC · PubMed Central
Fig. 8 (a) Linear sweep voltammograms recorded at 5 mV s−1 in 0.5 M H2SO4 exhibits the Tafel plot of Pt/C 20 wt% catalyst (b) & (c) are Tafel plots of the same obtained using Chronoamperometry & EIS methods, respectively,under similar experimental circumstances. Reproduced with permission from ref. 68 Copyright 2018, Royal Society of Chemistry.
Fig. 8 (a) Linear sweep voltammograms recorded at 5 mV s−1 in 0.5 M H2SO4 exhibits the Tafel plot of Pt/C 20 wt% catalyst (b) & (c) are Tafel plots of the same obtained using Chronoamperometry & EIS methods, respectively,under similar experimental circumstances. Reproduced with permission from ref. 68 Copyright 2018, Royal Society of Chemistry.CC BY-NC · PubMed Central
Fig. 9 The surface regions of LiCoO2 and LiCoPO4 are shown in HRTEM images and (right) FFTs in the following order: (a) pristine LiCoO2; (b) cycled LiCoO2 in 0.1 M KPi (pH 7) (c) cycled LiCoO2 in 0.1 M KOH (pH 13); (d) pristine LiCoPO4; (e) cycled LiCoPO4 in 0.1 M KPi (pH 7); (f) cycled LiCoPO4 in 0.1 M KOH (pH 13). The interface between amorphous and crystalline areas is denoted by white dashed lines. The electrodes underwent 100 uninterrupted cycles at a scan rate of 10 mV s−1 at 900 rpm between 1.2 and 1.8 V vs. RHE in 0.1 M KPi at pH 7 and between 1.0 and 1.7 V vs. RHE in 0.1 M KOH at pH 13. Reproduced with permission from ref. 113 Copyright 2018, American Chemical Society.
Fig. 9 The surface regions of LiCoO2 and LiCoPO4 are shown in HRTEM images and (right) FFTs in the following order: (a) pristine LiCoO2; (b) cycled LiCoO2 in 0.1 M KPi (pH 7) (c) cycled LiCoO2 in 0.1 M KOH (pH 13); (d) pristine LiCoPO4; (e) cycled LiCoPO4 in 0.1 M KPi (pH 7); (f) cycled LiCoPO4 in 0.1 M KOH (pH 13). The interface between amorphous and crystalline areas is denoted by white dashed lines. The electrodes underwent 100 uninterrupted cycles at a scan rate of 10 mV s−1 at 900 rpm between 1.2 and 1.8 V vs. RHE in 0.1 M KPi at pH 7 and between 1.0 and 1.7 V vs. RHE in 0.1 M KOH at pH 13. Reproduced with permission from ref. 113 Copyright 2018, American Chemical Society.CC BY-NC · PubMed Central
Fig. 10 (a) LiCoO2 and (b) LiCoPO4 electrodes were subjected to 10 mV s−1, 900 rpm CV scans in 0.1 M KPi electrolyte with a pH of 7.0. Dashed arrows indicate the progression of consecutive cycling, and the number labels indicate the number of cycles 0.1 M KOH at pH 13 was used for the CV scans of electrodes (c) LiCoO2 and (d) LiCoPO4 at a scan rate of 10 mV s−1 at 900 rpm. The results of 100 uninterrupted cycles are displayed CV scans in (e) 0.1 M KPi at pH 7 and (f) 0.1 M KOH at pH 13 for LiCoO2 (100th cycle), LiCoPO4 (100th cycle), and electrodeposited Co-Pi. Reproduced with permission from ref. 113. Copyright 2018, American Chemical Society.
Fig. 10 (a) LiCoO2 and (b) LiCoPO4 electrodes were subjected to 10 mV s−1, 900 rpm CV scans in 0.1 M KPi electrolyte with a pH of 7.0. Dashed arrows indicate the progression of consecutive cycling, and the number labels indicate the number of cycles 0.1 M KOH at pH 13 was used for the CV scans of electrodes (c) LiCoO2 and (d) LiCoPO4 at a scan rate of 10 mV s−1 at 900 rpm. The results of 100 uninterrupted cycles are displayed CV scans in (e) 0.1 M KPi at pH 7 and (f) 0.1 M KOH at pH 13 for LiCoO2 (100th cycle), LiCoPO4 (100th cycle), and electrodeposited Co-Pi. Reproduced with permission from ref. 113. Copyright 2018, American Chemical Society.CC BY-NC · PubMed Central
Fig. 11 Dependency on content of Sr (a) strain energies (gray) of the La2−xSrxNiO4±δ (LSNO) thin films with 0.0 ≤ xSr ≤ 1.0 derived using the surface energies and strain energy density equation, and (b) oxygen molecule adsorption energies on the (100)tetra. (blue) and (001)tetra. (red) surfaces of the LSNO thin films were acquired from density functional theory (DFT). Adsorption sites of surface oxygen on (c) the (100) tetra. slabs and (d) the (001)tetra. slabs. Anisotropy in LSNO thin films is represented by both surface and adsorption energies. AES data of the La2−xSrxNiO4±δ (LSNO) thin films with 0.0 ≤ xSr ≤ 1.0 annealed at 550 °C in an 1 atm partial pressure of oxygen. (e) LaMNN cation variation (RSF: 0.059), (f) SrLMM cation variation (RSF: 0.027), and (g) NiLMM cation variation (RSF: 0.277) as a function of Sr contents. The shift in the spectra of La and Sr cations scales with the concentration of La and Sr, indicating that the surface chemistry is characteristic of the surface cationic ratio desired. The increase in NiO6 octahedra population (normalised by surface area) with increasing Sr content is represented by a change in the Ni cation spectra which indicate a change in the thin film orientation. Reproduced with permission from ref. 127 Copyright 2014, Royal Society of Chemistry.
Fig. 11 Dependency on content of Sr (a) strain energies (gray) of the La2−xSrxNiO4±δ (LSNO) thin films with 0.0 ≤ xSr ≤ 1.0 derived using the surface energies and strain energy density equation, and (b) oxygen molecule adsorption energies on the (100)tetra. (blue) and (001)tetra. (red) surfaces of the LSNO thin films were acquired from density functional theory (DFT). Adsorption sites of surface oxygen on (c) the (100) tetra. slabs and (d) the (001)tetra. slabs. Anisotropy in LSNO thin films is represented by both surface and adsorption energies. AES data of the La2−xSrxNiO4±δ (LSNO) thin films with 0.0 ≤ xSr ≤ 1.0 annealed at 550 °C in an 1 atm partial pressure of oxygen. (e) LaMNN cation variation (RSF: 0.059), (f) SrLMM cation variation (RSF: 0.027), and (g) NiLMM cation variation (RSF: 0.277) as a function of Sr contents. The shift in the spectra of La and Sr cations scales with the concentration of La and Sr, indicating that the surface chemistry is characteristic of the surface cationic ratio desired. The increase in NiO6 octahedra population (normalised by surface area) with increasing Sr content is represented by a change in the Ni cation spectra which indicate a change in the thin film orientation. Reproduced with permission from ref. 127 Copyright 2014, Royal Society of Chemistry.CC BY-NC · PubMed Central
Fig. 12 In 1.0 M KOH, the electrocatalytic behaviour of BaMoO3 perovskite toward the HER was investigated. (a) BaMoO4 and BaMoO3 LSV curves, where currents are normalised to the geometric area of GCE (in mA cmgeo−2) and for reference, the GCE's LSV curve is shown in (a). The inset shows an enlarged version of the low current density region (b) LSV curves of BaMoO4 and BaMoO3, where currents are normalised to the BET surface area to calculate specific activity (in mA cmoxide−2). (c)BaMoO4 and BaMoO3's electrical conductivity was measured in ambient conditions. Schematic representations of the scheelite-to-perovskite phase transition and the shift from insulating to metallic conduction are shown in the inset. Reproduced with permission from ref. 128 Copyright 2020, Elsevier.
Fig. 12 In 1.0 M KOH, the electrocatalytic behaviour of BaMoO3 perovskite toward the HER was investigated. (a) BaMoO4 and BaMoO3 LSV curves, where currents are normalised to the geometric area of GCE (in mA cmgeo−2) and for reference, the GCE's LSV curve is shown in (a). The inset shows an enlarged version of the low current density region (b) LSV curves of BaMoO4 and BaMoO3, where currents are normalised to the BET surface area to calculate specific activity (in mA cmoxide−2). (c)BaMoO4 and BaMoO3's electrical conductivity was measured in ambient conditions. Schematic representations of the scheelite-to-perovskite phase transition and the shift from insulating to metallic conduction are shown in the inset. Reproduced with permission from ref. 128 Copyright 2020, Elsevier.CC BY-NC · PubMed Central
Fig. 13 Ru nanosheets with and without Al doping, calculated using DFT: optimised 2D Ru structure in (a); charge-density distribution on the surface with hydrogen adsorption sites indicated in (b); DOSs in (c and d) (inset: enlarged images for states near the Fermi level); and (e) HER free-energy diagrams. Electrochemical characteristics (f) LSV curves; (g) the necessary overpotential for 10 and 50 mA cm−2; (h) Tafel slopes; (i) the EIS at a 150 mV overpotential; (j) the CO stripping measurement; and (k) the LSV curves for the durability assessment. Inset: overpotential for 10 A cm−2 measured every 500 cycles. Reproduced with permission from ref. 136 Copyright 2019, American Chemical Society.
Fig. 13 Ru nanosheets with and without Al doping, calculated using DFT: optimised 2D Ru structure in (a); charge-density distribution on the surface with hydrogen adsorption sites indicated in (b); DOSs in (c and d) (inset: enlarged images for states near the Fermi level); and (e) HER free-energy diagrams. Electrochemical characteristics (f) LSV curves; (g) the necessary overpotential for 10 and 50 mA cm−2; (h) Tafel slopes; (i) the EIS at a 150 mV overpotential; (j) the CO stripping measurement; and (k) the LSV curves for the durability assessment. Inset: overpotential for 10 A cm−2 measured every 500 cycles. Reproduced with permission from ref. 136 Copyright 2019, American Chemical Society.CC BY-NC · PubMed Central
Fig. 14 (a) and (b) Represents the CoIn2Se4, In2Se3, CoSe2 and Ir/C electrocatalysts respectively (c) the determined capacitive currents plotted as a function of scan rate for CoIn2Se4, and CoSe2, (d) LSV curves of CoIn2Se4 before and after 1000 CV cycles (inset is the time-dependent current density curves on CoIn2Se4 and Ir/C), (e) ORR polarization curves and (f) the Eonset and E1/2 of CoIn2Se4, In2Se3, CoSe2 and Pt/C. Reproduced with permission from ref. 146 Copyright 2020, American Chemical Society.
Fig. 14 (a) and (b) Represents the CoIn2Se4, In2Se3, CoSe2 and Ir/C electrocatalysts respectively (c) the determined capacitive currents plotted as a function of scan rate for CoIn2Se4, and CoSe2, (d) LSV curves of CoIn2Se4 before and after 1000 CV cycles (inset is the time-dependent current density curves on CoIn2Se4 and Ir/C), (e) ORR polarization curves and (f) the Eonset and E1/2 of CoIn2Se4, In2Se3, CoSe2 and Pt/C. Reproduced with permission from ref. 146 Copyright 2020, American Chemical Society.CC BY-NC · PubMed Central
Fig. 15 (a) Polarization curves of Cu substrate, commercial Pt/C, and Ni–Co–Sn catalysts with a scan rate of 2 mV s−1 in 1 M NaOH for HER (b) Ni–Co–Sn catalyst, Cu substrate, and commercial Ir/C polarisation curves in 1.0 M NaOH for OER at a scan rate of 2 mV s−1. (c) The double-layer capacitances for OER catalysts with pH values of 5, 6, and 7. Reproduced with permission from ref. 154 Copyright 2019, Elsevier.
Fig. 15 (a) Polarization curves of Cu substrate, commercial Pt/C, and Ni–Co–Sn catalysts with a scan rate of 2 mV s−1 in 1 M NaOH for HER (b) Ni–Co–Sn catalyst, Cu substrate, and commercial Ir/C polarisation curves in 1.0 M NaOH for OER at a scan rate of 2 mV s−1. (c) The double-layer capacitances for OER catalysts with pH values of 5, 6, and 7. Reproduced with permission from ref. 154 Copyright 2019, Elsevier.CC BY-NC · PubMed Central
Fig. 16 Performance of various metal boride/borate electrocatalysts was compared at pH 9.2. The graph also displays the most efficient catalysts from different nonprecious metal catalyst families and precious metal-based catalysts. (Acronyms used—C: Vulcan carbon; CC: carbon cloth; CP: carbon paper; NF: Ni foam; Ni: Ni foil/plate; Ti: Ti mesh/foil.)48
Fig. 16 Performance of various metal boride/borate electrocatalysts was compared at pH 9.2. The graph also displays the most efficient catalysts from different nonprecious metal catalyst families and precious metal-based catalysts. (Acronyms used—C: Vulcan carbon; CC: carbon cloth; CP: carbon paper; NF: Ni foam; Ni: Ni foil/plate; Ti: Ti mesh/foil.)48CC BY-NC · PubMed Central
Fig. 17 At pH 9.2, the effectiveness of various metal boride/borate electrocatalysts was evaluated. Additionally, the most effective catalysts from various non-precious metal catalyst families and precious metal-based catalysts are shown in the graph. Reproduced with permission from ref. 185 Copyright 2021, Elsevier.
Fig. 17 At pH 9.2, the effectiveness of various metal boride/borate electrocatalysts was evaluated. Additionally, the most effective catalysts from various non-precious metal catalyst families and precious metal-based catalysts are shown in the graph. Reproduced with permission from ref. 185 Copyright 2021, Elsevier.CC BY-NC · PubMed Central
Fig. 18 (a) Mo2CTx electrocatalytic OER schematic illustration. (b) Image of the Mo2CTx MFs obtained using scanning electron microscopy. (c) A comparison of different Mo2CTx samples' Linear Sweep Voltammogram curves Reproduced with permission208 Copyright 2021, Elsevier.
Fig. 18 (a) Mo2CTx electrocatalytic OER schematic illustration. (b) Image of the Mo2CTx MFs obtained using scanning electron microscopy. (c) A comparison of different Mo2CTx samples' Linear Sweep Voltammogram curves Reproduced with permission208 Copyright 2021, Elsevier.CC BY-NC · PubMed Central
Fig. 19 (a) Schematic diagram depicts the preparation of 2D h-W2N3. (b) Images of 2D h-W2N3 nanosheets from STEM, AFM, and EDS. 2D h-W2N3, bulk-W2N3, and 20% Pt/C polarisation curves are shown in (c). Reproduced with permission212 Copyright 2021, Elsevier.
Fig. 19 (a) Schematic diagram depicts the preparation of 2D h-W2N3. (b) Images of 2D h-W2N3 nanosheets from STEM, AFM, and EDS. 2D h-W2N3, bulk-W2N3, and 20% Pt/C polarisation curves are shown in (c). Reproduced with permission212 Copyright 2021, Elsevier.CC BY-NC · PubMed Central
Fig. 20 Fe doped CoP electrocatalyst TEM (a), electrocatalyst Tafel plots (b), and LSV curves before and after a 24 hours test for Fe CoP HNSs (c). Reproduced with permission225 Copyright 2021, Elsevier.
Fig. 20 Fe doped CoP electrocatalyst TEM (a), electrocatalyst Tafel plots (b), and LSV curves before and after a 24 hours test for Fe CoP HNSs (c). Reproduced with permission225 Copyright 2021, Elsevier.CC BY-NC · PubMed Central
Fig. 21 (a) Polarization curves of P-NiSe2/CC, NiSe2/CC, Pt/C, and CC electrodes in 1.0 M KOH, (b) corresponding Tafel plots of P-NiSe2/CC, NiSe2/CC, and Pt/C electrodes, (c) Nyquist plots of P-NiSe2/CC and NiSe2/CC electrodes and inset has equivalent circuit, (d) the Cdl values of P-NiSe2/CC and NiSe2/CC electrodes at scanning rate of 5, 25, 50, 75 and 100 mV s. (e) Based on the electrochemical active surface area, the specific activity of P-NiSe2/CC and NiSe2/CC electrodes are depicted (f) durability testing showing the P-NiSe2/CC electrode's first and 3000th polarization curves; inset shows a time-dependent current density curve recorded on the P-NiSe2/CC electrode for 55 hours at a constant overpotential of 10 mV (vs. RHE). (g) Fabrication process schematic illustration. Reproduced with permission.245 Copyright 2021, Elsevier.
Fig. 21 (a) Polarization curves of P-NiSe2/CC, NiSe2/CC, Pt/C, and CC electrodes in 1.0 M KOH, (b) corresponding Tafel plots of P-NiSe2/CC, NiSe2/CC, and Pt/C electrodes, (c) Nyquist plots of P-NiSe2/CC and NiSe2/CC electrodes and inset has equivalent circuit, (d) the Cdl values of P-NiSe2/CC and NiSe2/CC electrodes at scanning rate of 5, 25, 50, 75 and 100 mV s. (e) Based on the electrochemical active surface area, the specific activity of P-NiSe2/CC and NiSe2/CC electrodes are depicted (f) durability testing showing the P-NiSe2/CC electrode's first and 3000th polarization curves; inset shows a time-dependent current density curve recorded on the P-NiSe2/CC electrode for 55 hours at a constant overpotential of 10 mV (vs. RHE). (g) Fabrication process schematic illustration. Reproduced with permission.245 Copyright 2021, Elsevier.CC BY-NC · PubMed Central
Fig. 22 Atomic-resolution HAADF-STEM images of the (A) Pd3Pb and (B) AL-Pt/Pd3Pb. (C) Pt and Pd3Pb charge density differences in AL-Pt/Pd3Pb. (D) The calculated average binding energy of H* at various hydrogen coverages on Pt(100), strained Pt(100), and Pt/Pd3Pb(100) Reproduced with permission258 Copyright 2019, American Chemical Society.
Fig. 22 Atomic-resolution HAADF-STEM images of the (A) Pd3Pb and (B) AL-Pt/Pd3Pb. (C) Pt and Pd3Pb charge density differences in AL-Pt/Pd3Pb. (D) The calculated average binding energy of H* at various hydrogen coverages on Pt(100), strained Pt(100), and Pt/Pd3Pb(100) Reproduced with permission258 Copyright 2019, American Chemical Society.CC BY-NC · PubMed Central
Asha Raveendran
Asha RaveendranCC BY-NC · PubMed Central
Mijun Chandran
Mijun ChandranCC BY-NC · PubMed Central
Ragupathy Dhanusuraman
Ragupathy DhanusuramanCC BY-NC · PubMed Central

Verification

Claims the paper makes

The claims and statistics of this paper haven’t been checked yet.

Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.

A few free checks a day · papers already verified open instantly · results are public

Claims other papers make about this one

Each is checked against this paper’s own text: does it say what the citing paper says it does?

Self-check

Percentages, sums and reported differences re-computed from the paper’s own numbers.

The self-check needs the paper’s full text.

Citations

Cites

Research works printed but not linked: 6

  1. Bard, 2001, Electrochem., 2, 580
  2. M.Ni , M. K.Leung and D. Y.Leung , Proceeding of the WHEC , 2006 , vol. 16
  3. Kumar, 2019, Mater. Sci. Energy Technol., 2, 442
  4. Lu, 2014, Nat. Commun., 5, 1
  5. Wu, 2015, Nat. Commun., 6, 1
  6. Zhang, 2018, ACS Appl. Energy Mater., 1, 5482

Cited by

See all 926

Metadata

Authors
Raveendran, A., Chandran, M., & Dhanusuraman, R.
Affiliations
  • National Institute of Technology, Puducherry (IN)
  • Central University of Tamil Nadu (IN)
Corresponding author
Dhanusuraman, Ragupathy
Venue
RSC Advances
Published
2023
Volume
13
Issue
6
Pages
3843-3876
ISSN
2046-2069 (ISSN-L)
OpenAlex
W4318068234
Cited by
892
References
258
Citations by year
2026: 320 · 2025: 305 · 2024: 211 · 2023: 56
FWCI
13.67
Type
journal article
Language
en
Open access
Locations
  • RSC Advances (publishedVersion, cc-by-nc)
  • PubMed Central (publishedVersion, cc-by-nc)
  • PubMed (publishedVersion)
Topics
  • Physical Sciences › Energy › Renewable Energy, Sustainability and the Environment › Electrocatalysts for Energy Conversion
  • Physical Sciences › Energy › Renewable Energy, Sustainability and the Environment › CO2 Reduction Techniques and Catalysts
  • Physical Sciences › Engineering › Electrical and Electronic Engineering › Fuel Cells and Related Materials
Keywords
electrochemical water splitting, electrocatalysts, hydrogen evolution reaction, oxygen evolution reaction, water electrolysis, noble metal alternatives, electrochemical parameters

About these checks

Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.

Statistics and arithmetic are recomputed, not judged.

Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.

What counts as a claim ›How we measure confidence ›How we check this ›

Are you an author, or do you see a problem with this page? Request a review

Data sources

Bibliographic data: Semantic Scholar, OpenAlex, Crossref.

Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).

Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.