Experimental and Theoretical Analysis of Ink Dispersion Stability for Polymer Electrolyte Fuel Cell Applications
Open accessThe DOI matches its Crossref record; 43 of the 43 references it cites were found in a registry or an index.
Abstract
The aggregate size in fuel cell catalyst inks depends on the type of dispersion medium, particle concentration, and addition of stabilizing agents. In this work, ink stability and particle size of carbon black and carbon black/Nafion dispersions in four non-aqueous media, viz., methanol, ethanol, isopropanol and ethyl acetate are studied. Based on visual inspection, isopropanol is found to be the best medium for dispersion of carbon black inks. To rationalize this observation, a semi-empirical model based on diffusion-limited aggregation was developed to evaluate the rate of particle aggregation and predict the ink stability time for each dispersion medium. The proposed model supports the experimental observation by qualitatively predicting the same relationship between carbon stability and the dispersion media. The model also showed that the dielectric constant of the dispersion medium and the particle zeta potential are primarily responsible for the ink stability. Particle size for the different inks was determined by dynamic light scattering with and without dilution. Experimental results show that Nafion is a strong stabilizing agent, increasing the ink stability and decreasing the particle size of carbon aggregates. The beneficial effects of Nafion are independent of its concentration and are observed even at Nafion volume fractions of 10 wt%. The interaction energy is found to be a strong function of the surface potential for the dispersion medium with a higher dielectric constant.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Figures













Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Claims other papers make about this one
Each is checked against this paper’s own text: does it say what the citing paper says it does?
The source backs part of the claim, not all of it — or backs it for a different population, condition or comparison.
In the citing paper
“al. found that the decrease in the primary and secondary agglomerates size resulting from dilution approaches 20%, through studying the ink with and without dilution by using a recent DLS apparatus [34].”
From Effect of Catalyst Ink and Formation Process on the Multiscale Structure of Catalyst Layers in PEM Fuel Cells (2022) · cites this paper as [34]
Experimental — accuracy not yet measuredThe source backs part of the claim, not all of it — or backs it for a different population, condition or comparison.
In the citing paper
“As the catalyst agglomerates are commonly covered by ionomer in the catalyst ink, solvent affects the dispersion or dispersion stability of catalyst likely through impacting the ionomer coverage on catalyst or the conformation of the adsorbed ionomer [34].”
From Effect of Catalyst Ink and Formation Process on the Multiscale Structure of Catalyst Layers in PEM Fuel Cells (2022) · cites this paper as [34]
Experimental — accuracy not yet measuredThe source backs part of the claim, not all of it — or backs it for a different population, condition or comparison.
In the citing paper
“When the I/C ratio reaches a certain value, increasing the content of ionomer in the catalyst ink further will not contribute to the size of agglomerates or increase the colloidal stability [34].”
From Effect of Catalyst Ink and Formation Process on the Multiscale Structure of Catalyst Layers in PEM Fuel Cells (2022) · cites this paper as [34]
Experimental — accuracy not yet measuredThe source backs part of the claim, not all of it — or backs it for a different population, condition or comparison.
In the citing paper
“As shown in Fig. 15a-c, the state of the catalyst ink remarkably changes within 24 h of storage [189].”
From Recent Advances on PEM Fuel Cells: From Key Materials to Membrane Electrode Assembly (2023) · cites this paper as [189]
Experimental — accuracy not yet measuredThe cited source says what the claim attributes to it.
In the citing paper
“If the agglomerate size reaches a certain point, sedimentation would take place due to gravity, making the catalyst ink inhomogeneous [34,52].”
From Effect of Catalyst Ink and Formation Process on the Multiscale Structure of Catalyst Layers in PEM Fuel Cells (2022) · cites this paper as [34]
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Particle Deposition and Aggregation: Measurement, Modelling and Simulation
Elimelech, M. (1995) · Cited by 1,190
Electrokinetic and Colloid Transport Phenomena
Masliyah, J. H., & Bhattacharjee, S. (2006) · Wiley eBooks · doi:10.1002/0471799742 · Cited by 1,129
Self-citationFuel Cell Catalyst Layers: A Polymer Science Perspective
Holdcroft, S. (2014) · Chemistry of Materials · doi:10.1021/cm401445h · Cited by 481
Soboleva, T., Zhao, X., Malek, K., Xie, Z., Navessin, T., & Holdcroft, S. (2010) · ACS Applied Materials & Interfaces · doi:10.1021/am900600y · Cited by 424
The Impact of Platinum Loading on Oxygen Transport Resistance
Greszler, T. A., Caulk, D., & Sinha, P. (2012) · Journal of The Electrochemical Society · doi:10.1149/2.061212jes · Cited by 421
Anderson, W., Kozak, D., Coleman, V. A., Jämting, Å. K., & Trau, M. (2013) · Journal of Colloid and Interface Science · doi:10.1016/j.jcis.2013.02.030 · Cited by 373
Unexplained transport resistances for low-loaded fuel-cell catalyst layers
Weber, A. Z., & Kusoglu, A. (2014) · J. Mater. Chem. A · doi:10.1039/c4ta02952f · Cited by 333
Self-citationNew Preparation Method for Polymer‐Electrolyte Fuel Cells
Uchida, M., Aoyama, Y., Eda, N., & Ohta, A. (1995) · Journal of The Electrochemical Society · doi:10.1149/1.2044068 · Cited by 282
Wee, J.-H., Lee, K.-Y., & Kim, S. H. (2007) · Journal of Power Sources · doi:10.1016/j.jpowsour.2006.12.051 · Cited by 261 · cited 1×
“UvdW = − A 6 · ( ai a j ai + a j ) · 1 r − (ai + a j ) [2]”
Nafion in dilute solvent systems: Dispersion or solution?
Welch, C., Labouriau, A., Hjelm, R., Orler, B., Johnston, C., & Kim, Y. S. (2012) · ACS Macro Letters · doi:10.1021/mz3005204 · Cited by 211
Research works printed but not linked: 1
- Israelachvili J. , Intermolecular and surface forces: revised third edition. Academic press, 2011.
Cited by
Rabiee, H., Ge, L., Zhang, X., Hu, S., Li, M., & Yuan, Z. (2021) · Energy & Environmental Science · doi:10.1039/d0ee03756g · Cited by 509
Recent Advances on PEM Fuel Cells: From Key Materials to Membrane Electrode Assembly
Mo, S., Du, L., Huang, Z., Chen, J., Zhou, Y., Wu, P., Meng, L., Wang, N., Xing, L., Zhao, M., et al. (2023) · Electrochemical Energy Reviews · doi:10.1007/s41918-023-00190-w · Cited by 277
“15a–c, the state of the catalyst ink remarkably changes within 24 h of storage [189].”
Wang, M., Park, J. H., Kabir, S., Neyerlin, K. C., Kariuki, N. N., Lv, H., Stamenkovic, V. R., Myers, D. J., Ulsh, M., & Mauger, S. A. (2019) · ACS Applied Energy Materials · doi:10.1021/acsaem.9b01037 · Cited by 192
The Controllable Design of Catalyst Inks to Enhance PEMFC Performance: A Review
Guo, Y., Pan, F., Chen, W., Ding, Z., Yang, D., Li, B., Ming, P., & Zhang, C. (2021) · Electrochemical Energy Reviews · doi:10.1007/s41918-020-00083-2 · Cited by 175
“Overall, many factors can affect ink stability, including the dispersion medium dielectric constant, zeta potential, ionomer loading and carbon support structure [94, 131, 178, 179].”
BackgroundMethodInfluentialRheological Investigation on the Microstructure of Fuel Cell Catalyst Inks
Khandavalli, S., Park, J. H., Kariuki, N. N., Myers, D. J., Stickel, J. J., Hurst, K., Neyerlin, K. C., Ulsh, M., & Mauger, S. A. (2018) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.8b15039 · Cited by 153
Controlling cracking formation in fuel cell catalyst layers
Kumano, N., Kudo, K., Suda, A., Akimoto, Y., Ishii, M., & Nakamura, H. (2019) · Journal of Power Sources · doi:10.1016/j.jpowsour.2019.02.058 · Cited by 135
Catalyst layer ink interactions that affect coatability
Dixit, M. B., Harkey, B. A., Shen, F., & Hatzell, K. B. (2018) · Journal of The Electrochemical Society · doi:10.1149/2.0191805jes · Cited by 126
Inherent Acidity of Perfluorosulfonic Acid Ionomer Dispersions and Implications for Ink Aggregation
Berlinger, S. A., McCloskey, B. D., & Weber, A. Z. (2018) · The Journal of Physical Chemistry B · doi:10.1021/acs.jpcb.8b06493 · Cited by 122
Self-citationAnion Exchange Ionomers: Design Considerations and Recent Advances ‐ An Electrochemical Perspective
Favero, S., Stephens, I. E. L., & Titirici, M. (2023) · Advanced Materials · doi:10.1002/adma.202308238 · Cited by 120
Yuan, X., Nayoze-Coynel, C., Shaigan, N., Fisher, D. C., Zhao, N., Zamel, N., Gazdzicki, P., Ulsh, M., Friedrich, K. A., Girard, F., et al. (2021) · Journal of Power Sources · doi:10.1016/j.jpowsour.2021.229540 · Cited by 118
Electrochemical Reduction of CO 2 : Effect of Convective CO 2 Supply in Gas Diffusion Electrodes
Duarte, M., Mot, B. D., Hereijgers, J., & Breugelmans, T. (2019) · ChemElectroChem · doi:10.1002/celc.201901454 · Cited by 113
Interesting Facets of Surface, Interfacial, and Bulk Characteristics of Perfluorinated Ionomer Films
Karan, K. (2019) · Langmuir · doi:10.1021/acs.langmuir.8b03721 · Cited by 96
Linking gas diffusion electrode composition to CO 2 reduction in a flow cell
Lees, E. W., Mowbray, B. A. W., Salvatore, D. A., Simpson, G. L., Dvořák, D., Ren, S., Chau, J., Milton, K. L., & Berlinguette, C. P. (2020) · Journal of Materials Chemistry A · doi:10.1039/d0ta03570j · Cited by 102
Balu, R., Choudhury, N. R., Mata, J. P., de Campo, L., Rehm, C., Hill, A. J., & Dutta, N. K. (2019) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.8b20645 · Cited by 96
Understanding inks for porous-electrode formation
Hatzell, K. B., Dixit, M. B., Berlinger, S. A., & Weber, A. Z. (2017) · J. Mater. Chem. A · doi:10.1039/c7ta07255d · Cited by 97
Self-citationWoo, S., Lee, S., Taning, A. Z., Yang, T., Park, S., & Yim, S. (2020) · Current Opinion in Electrochemistry · doi:10.1016/j.coelec.2020.03.006 · Cited by 97
Impact of Catalyst Ink Dispersing Solvent on PEM Fuel Cell Performance and Durability
Lei, C., Yang, F., Macauley, N., Spinetta, M., Purdy, G., Jankovic, J., Cullen, D. A., More, K. L., Kim, Y. S., & Xu, H. (2021) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/abf2b0 · Cited by 93
Probing Ionomer Interactions with Electrocatalyst Particles in Solution
Berlinger, S. A., McCloskey, B. D., & Weber, A. Z. (2021) · ACS Energy Letters · doi:10.1021/acsenergylett.1c00866 · Cited by 93
Self-citationDu, S., Li, W., Wu, H., Abel Chuang, P.-Y., Pan, M., & Sui, P.-C. (2020) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2020.07.241 · Cited by 88
Liu, H., Ney, L., Zamel, N., & Li, X. (2022) · Applied Sciences · doi:10.3390/app12083776 · Cited by 85
“As the catalyst agglomerates are commonly covered by ionomer in the catalyst ink, solvent affects the dispersion or dispersion stability of catalyst likely through impacting the ionomer coverage on catalyst or the conformation of the adsorbed ionomer [34].”
BackgroundMethodInfluentialGravure coating for roll-to-roll manufacturing of proton-exchange-membrane fuel cell catalyst layers
Mauger, S. A., Neyerlin, K. C., Yang-Neyerlin, A. C., More, K. L., & Ulsh, M. (2018) · Journal of The Electrochemical Society · doi:10.1149/2.0091813jes · Cited by 81
Khandavalli, S., Park, J. H., Kariuki, N. N., Zaccarine, S. F., Pylypenko, S., Myers, D. J., Ulsh, M., & Mauger, S. A. (2019) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.9b14415 · Cited by 74
MnxCo3-xO4 spinel oxides as efficient oxygen evolution reaction catalysts in alkaline media
Lankauf, K., Cysewska, K., Karczewski, J. L., Mielewczyk-Gryń, A. D., Górnicka, K., Cempura, G., Chen, M., Jasiński, P., & Molin, S. (2020) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2020.03.188 · Cited by 75
“[41] Shukla S, Bhattacharjee S, Weber AZ, Secanell M.”
BackgroundMethodOstroverkh, A., Johánek, V., Dubau, M., Kúš, P., Khalakhan, I., Šmíd, B., Fiala, R., Václavů, M., Ostroverkh, Y., & Matolín, V. (2019) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2018.12.206 · Cited by 72
Multicomponent, multiphase interactions in fuel-cell inks
Berlinger, S. A., Garg, S., & Weber, A. Z. (2021) · Current Opinion in Electrochemistry · doi:10.1016/j.coelec.2021.100744 · Cited by 72
Self-citationHydrocarbon Ionomeric Binders for Fuel Cells and Electrolyzers
Kim, Y. S. (2023) · Advanced Science · doi:10.1002/advs.202303914 · Cited by 68
Guo, Y., Yang, D., Li, B., Yang, D., Ming, P., & Zhang, C. (2021) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.1c07070 · Cited by 65
Impact of Dispersion Solvent on Ionomer Thin Films and Membranes
Berlinger, S. A., Dudenas, P. J., Bird, A., Chen, X., Freychet, G., McCloskey, B. D., Kusoglu, A., & Weber, A. Z. (2020) · ACS Applied Polymer Materials · doi:10.1021/acsapm.0c01076 · Cited by 65
Self-citationInfluence of ionomer adsorption on agglomerate structures in high-solid catalyst inks
Kumano, N., Kudo, K., Akimoto, Y., Ishii, M., & Nakamura, H. (2020) · Carbon · doi:10.1016/j.carbon.2020.07.047 · Cited by 61
Murugaiah, D. K., & Shahgaldi, S. (2024) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2024.04.036 · Cited by 60
Khandavalli, S., Iyer, R., Park, J. H., Myers, D. J., Neyerlin, K. C., Ulsh, M., & Mauger, S. A. (2020) · Langmuir · doi:10.1021/acs.langmuir.0c02015 · Cited by 56
Ren, H., Meng, X., Lin, Y., & Shao, Z. (2022) · Journal of Power Sources · doi:10.1016/j.jpowsour.2021.230698 · Cited by 53
Liu, P., Yang, D., Li, B., Zhang, C., & Ming, P. (2023) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2023.02.022 · Cited by 49
Liu, G., McLaughlin, D., Thiele, S., & Pham, C. V. (2022) · Chemical Engineering Journal · doi:10.1016/j.cej.2023.141757 · Cited by 46
Impact of Nonadsorbed Ionomer on Viscosity of Catalyst Inks for Polymer Electrolyte Fuel Cells
Yoshimune, W., & Harada, M. (2020) · Bulletin of the Chemical Society of Japan · doi:10.1246/bcsj.20190321 · Cited by 44
Gao, S., Hu, B., Song, X. L., Dong, Z., & Kang, R. (2024) · Ceramics International · doi:10.1016/j.ceramint.2024.11.373 · Cited by 42
Liu, P., Li, B., Yang, D., Zhang, C., & Ming, P. (2022) · Journal of Power Sources · doi:10.1016/j.jpowsour.2022.232427 · Cited by 42
Ding, R. F., Yin, W., Cheng, G., Chen, Y., Wang, J., Wang, X., Han, M. S., Zhang, T., Cao, Y., Zhao, H., et al. (2022) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.1c23221 · Cited by 41
Lee, S. A., Jun, S. E., Park, S. H., Kwon, K. C., Kang, J. H., Kwon, M. S., & Jang, H. W. (2023) · EES Catalysis · doi:10.1039/d3ey00165b · Cited by 40
Zhou, Y., Guo, W., Xing, L., Li, J., Wang, N., Meng, L., Ye, S., Yang, X., Chen, H., & Du, L. (2025) · Energy & Environmental Science · doi:10.1039/d5ee03461b · Cited by 40
On the state and stability of fuel cell catalyst inks
Bapat, S., Giehl, C., Kohsakowski, S., Peinecke, V., Schäffler, M., & Segets, D. (2021) · Advanced Powder Technology · doi:10.1016/j.apt.2021.08.030 · Cited by 38
Jiang, L., Rahnama, M. B., Zhang, B., Zhu, X., Sui, P., Ye, D., & Djilali, N. (2020) · Physics of Fluids · doi:10.1063/1.5142669 · Cited by 38
Bapat, S., & Segets, D. (2020) · ACS Applied Nano Materials · doi:10.1021/acsanm.0c01467 · Cited by 37
Laghryb, I., Malki, M., Steiner, N. Y., Barrett, C. D., & Kadiri, H. E. (2025) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2025.06.052 · Cited by 35
Wu, D., Kayo, N., Jayawickrama, S. M., Phua, Y. K., Tanaka, N., & Fujigaya, T. (2022) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2022.11.116 · Cited by 35
Mehrazi, S., Sarker, M., Mojica, F., Rolfe, P., & Chuang, P. A. (2021) · Electrochimica Acta · doi:10.1016/j.electacta.2021.138690 · Cited by 35
Formulation of carbon black-ionomer dispersions for thin film formation in fuel cells
Hoffmann, E., Zhang, S., Thoma, M., Damm, C., & Peukert, W. (2019) · Particuology · doi:10.1016/j.partic.2018.08.001 · Cited by 34
Woo, S. H., Kim, S., Woo, S., Park, S., Kang, Y. S., Jung, N., & Yim, S. (2023) · Korean Journal of Chemical Engineering · doi:10.1007/s11814-023-1474-3 · Cited by 34
Regulating catalyst and ionomer interactions to promote oxygen transport in fuel cells
Wang, M., Zhang, S., Wang, H., Sun, E., Liu, D., Wu, M., Liu, D., & Li, Z. (2024) · Applied Catalysis B: Environmental · doi:10.1016/j.apcatb.2024.124894 · Cited by 33
Microstructure and macroscopic rheology of microporous layer nanoinks for PEM fuel cells
Pan, W., Chen, Z., Yao, D., Chen, X., Wang, F., & Dai, G. (2021) · Chemical Engineering Science · doi:10.1016/j.ces.2021.117001 · Cited by 33
Liu, C., Luo, M., Zeis, R., Chuang, P. A., Zhang, R., Du, S., & Sui, P. (2023) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2023.08.154 · Cited by 33
de Sousa, L. F., Harmoko, C., Benes, N. E., & Mul, G. (2021) · ACS ES&T Engineering · doi:10.1021/acsestengg.1c00228 · Cited by 31
Amorphous Ni-Nb-Y Alloys as Hydrogen Evolution Electrocatalysts
Ghobrial, S., Kirk, D. W., & Thorpe, S. J. (2019) · Electrocatalysis · doi:10.1007/s12678-019-00519-4 · Cited by 31
Role of the Ionomer in Supporting Electrolyte-Fed Anion Exchange Membrane Water Electrolyzers
Volk, E. K., Clauser, A. L., Kreider, M. E., Soetrisno, D. D., Khandavalli, S., Sugar, J. D., Kwon, S., & Alia, S. M. (2024) · ACS electrochemistry. · doi:10.1021/acselectrochem.4c00061 · Cited by 30
Park, K., Ohnishi, T., Goto, M., So, M., Takenaka, S., Tsuge, Y., & Inoue, G. (2019) · International Journal of Hydrogen Energy · doi:10.1016/j.ijhydene.2019.11.097 · Cited by 29
Nanoparticle Tracing during Laser Powder Bed Fusion of Oxide Dispersion Strengthened Steels
Yang, Y., Doñate‐Buendía, C., Oyedeji, T. D., Gökce, B., & Xu, B. (2021) · Materials · doi:10.3390/ma14133463 · Cited by 28
Mehrazi, S., Homayouni, T., Kakati, N., Sarker, M., Rolfe, P., & Chuang, P. A. (2024) · Applied Energy · doi:10.1016/j.apenergy.2024.122680 · Cited by 28
Mechanisms and Strategies to Achieve Stability in Inkjet Printed 2D Materials Electronics
Tian, L., Liu, J., Chen, X., Branicio, P. S., & Lei, Q. (2024) · Advanced Electronic Materials · doi:10.1002/aelm.202400143 · Cited by 27
Review—Meeting Fuel Cell Catalyst Requirements for Heavy-Duty Vehicle Applications
Ramaswamy, N., Kongkanand, A., Wortman, J., & Gu, W. (2025) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/adae3b · Cited by 27
The state of art of nanocarbon black as analyte in a variety of matrices: A review
Sanjuan-Navarro, L., Moliner-Martínez, Y., & Campíns-Falcó, P. (2022) · TrAC Trends in Analytical Chemistry · doi:10.1016/j.trac.2022.116769 · Cited by 27
Lin, R., Lu, J., Liu, S., Hua, S., Cai, X. L., & Friedrich, K. A. (2024) · Applied Surface Science · doi:10.1016/j.apsusc.2024.159608 · Cited by 26
A Review of Dispersion Film Drying Research
Zhang, B., Fan, B., Huang, Z., Higa, K., Battaglia, V., & Prasher, R. (2022) · Journal of Electrochemical Energy Conversion and Storage · doi:10.1115/1.4055392 · Cited by 23
Wei, F., Kosakian, A., & Secanell, M. (2023) · Chemical Engineering Journal · doi:10.1016/j.cej.2023.144423 · Cited by 23
Self-citationSolvent Effects on the Catalyst Ink and Layer Microstructure for Anion Exchange Membrane Fuel Cells
Han, C., Shi, W., Huang, M., Wang, Q., Yang, J., Chen, J., Ding, R., & Yin, X. (2024) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.3c14404 · Cited by 23
Liu, P., Yang, D., Li, B., Qu, T., Ming, P., Zhang, C., & Pan, X. (2024) · Journal of Power Sources · doi:10.1016/j.jpowsour.2024.234309 · Cited by 23
Temperature-induced shear-thinning in catalyst inks
Yoshimune, W., & Harada, M. (2021) · Electrochemistry Communications · doi:10.1016/j.elecom.2021.107099 · Cited by 22
Durable Fuel Cell Electrode Design via Efficient Distribution of the Acidic Ionomer
Ramaswamy, N., & Wortman, J. (2024) · ACS Energy Letters · doi:10.1021/acsenergylett.4c02704 · Cited by 23
Choi, M., Kim, J. K., Kim, J., Yang, S., Park, J.-E., Kim, O.-H., & Cho, Y.-H. (2018) · RSC Advances · doi:10.1039/c8ra07754a · Cited by 21
Wang, X., Zhao, S., Wang, S., Hou, X., Yang, J., Liang, C., Zhao, Y., Wang, L., Shen, C., Gao, N., et al. (2024) · Journal of Membrane Science · doi:10.1016/j.memsci.2024.123605 · Cited by 21
Lee, S., Woo, S. H., Pak, B., Kim, S., Kang, Y. S., Woo, S., Park, S., Yang, T.-H., & Yim, S. (2023) · Journal of Power Sources · doi:10.1016/j.jpowsour.2023.233644 · Cited by 21
Influence of Ionomer Content in the Catalytic Layer of MEAs Based on Aquivion® Ionomer
Gatto, I., Saccà, A., Sebastián, D., Baglio, V., Aricò, A. S., Oldani, C., Merlo, L., & Carbone, A. (2021) · Polymers · doi:10.3390/polym13213832 · Cited by 19
Taning, A. Z., Lee, S., Woo, S., Park, S., Bae, B., & Yim, S. (2021) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/ac2c13 · Cited by 18
Guo, Y., Yang, D., Tang, H., Li, B., Yang, D., Ming, P., & Zhang, C. (2022) · Physics of Fluids · doi:10.1063/5.0102157 · Cited by 16
Xie, Y., Guo, Y., Yang, D., Yang, D., Ming, P., Zhang, C., & Li, B. (2023) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.3c01943 · Cited by 16
Zhou, Y., Kang, J., Chen, B., Zheng, W., Zhang, C., Ming, P., Pan, F., Wang, J., & Li, B. (2025) · Advances in Colloid and Interface Science · doi:10.1016/j.cis.2025.103468 · Cited by 17
Understanding the Behavior of Electrosprayed Carbon Black‐Nafion Composite Layers
Conde, J. J., Chaparro, A. M., & Ferreira-Aparicio, P. (2018) · Fuel Cells · doi:10.1002/fuce.201700218 · Cited by 16
Mehrazi, S., Sarker, M., & Chuang, P. A. (2023) · Journal of Power Sources · doi:10.1016/j.jpowsour.2023.233361 · Cited by 16
Screen Printing Catalyst Inks With Enhanced Process Stability for PEM Fuel Cell Production
Ney, L., Seidl, N., Singh, R., Schneider, P., Stross, D., Göppentin, A., Tepner, S., Klingele, M., & Keding, R. J. (2024) · Fuel Cells · doi:10.1002/fuce.202400158 · Cited by 16
Mora, J. M., Li, G., Ocon, J. D., & Chuang, P. A. (2025) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.5c06148 · Cited by 15
Surface enrichment of ionomer in fuel cell catalyst layer prepared using slot-die coating method
Ren, H., Meng, X., Lin, Y., Li, X., & Shao, Z. (2023) · Journal of Power Sources · doi:10.1016/j.jpowsour.2023.233399 · Cited by 15
Kräenbring, M., Wickert, L., Hansen, M., Sanden, S., Pellumbi, K., Wolf, J., Siegmund, D., Özcan, F., Apfel, U., & Segets, D. (2023) · ChemCatChem · doi:10.1002/cctc.202301273 · Cited by 15
Srivastav, H., Weber, A. Z., & Radke, C. J. (2024) · Langmuir · doi:10.1021/acs.langmuir.3c03904 · Cited by 14
Self-citationColloidal Quantum Dot:Organic Ternary Ink for Efficient Solution-Processed Hybrid Solar Cells
Jeong, H.-S., Kim, D.-E., Jee, S., Si, M., Kim, C., Lee, J., Jung, Y., & Baek, S. (2023) · International Journal of Energy Research · doi:10.1155/2023/4911750 · Cited by 14
“We examined the stability of hybrid ink using UV-vis spectroscopy [41, 42] and con fi rmed the clear peaks of PM6 and Y6 in hybrid ink even after 120 hours of storage under ambient conditions (Figure S6, Supporting Information).”
The stability of disperse red/reactive-red dye inks
Chu, R., Zhang, Y., Xing, T., & Chen, G. (2020) · RSC Advances · doi:10.1039/d0ra07333d · Cited by 13
Choi, H. S., Roy, S. M., & Kim, T. H. (2024) · International Journal of Biological Macromolecules · doi:10.1016/j.ijbiomac.2024.135797 · Cited by 12
Grebener, L., Odungat, A. S., Zhu, Y., Pasdag, O., Radev, I., Nürenberg, E., Kubina, A., Peinecke, V., Kohsakowski, S., Segets, D., et al. (2025) · Journal of Power Sources · doi:10.1016/j.jpowsour.2025.236457 · Cited by 12
Gao, N., Zhang, C., Song, M., Fan, J., Li, J., Li, S., Lou, N., Wu, G., Liu, Y., Xue, J., et al. (2025) · Carbohydrate Polymers · doi:10.1016/j.carbpol.2025.124302 · Cited by 12
Kariuki, N. N., Haug, A. T., Park, J. W., Lindell, M. J., & Myers, D. J. (2022) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/ac94a4 · Cited by 11
Chan, T., Zorić, M. R., Shandilya, A., Loeb, C. K., Barrett, J. A., Cordones, A. A., & Kubiak, C. P. (2024) · ACS Applied Energy Materials · doi:10.1021/acsaem.3c02953 · Cited by 11
Srivastav, H., Weber, A. Z., & Radke, C. J. (2024) · Langmuir · doi:10.1021/acs.langmuir.3c03903 · Cited by 11
Self-citationFavero, S., Li, A. Y., Wang, M., Uddin, F., Kuzuoglu, B., Georgeson, A., Stephens, I. E. L., & Titirici, M. (2024) · ACS Catalysis · doi:10.1021/acscatal.4c01418 · Cited by 11
Combined Infrared Thermography, X-ray Radiography, and Computed Tomography for Ink Drying Studies
Fournier, R., Shum, A. D., Liu, J., Sabarirajan, D. C., Xiao, X., & Zenyuk, I. V. (2018) · ACS Applied Energy Materials · doi:10.1021/acsaem.8b01147 · Cited by 11
Burghart, J., Ovarlez, G., & Medina‐González, Y. (2025) · Journal of Power Sources · doi:10.1016/j.jpowsour.2025.238497 · Cited by 10
Jain, A., Marcks, C., Mahler, G., Odungat, A. S., Grebener, L., Johny, J., Chatwani, M., Shaji, A., Melchert, T., Tesch, M. F., et al. (2025) · ACS Applied Materials & Interfaces · doi:10.1021/acsami.5c15573 · Cited by 9
Choi, W.-J., Kang, I., Yu, D. M., Yoon, S. J., So, S., & Oh, K. (2024) · Korean Journal of Chemical Engineering · doi:10.1007/s11814-024-00221-2 · Cited by 10
Amphiphilic Polymers for Color Dispersion: Toward Stable and Low-Viscosity Inkjet Ink
Ohtake, T., Ito, H., & Toyoda, N. (2022) · Langmuir · doi:10.1021/acs.langmuir.2c01010 · Cited by 9
Characterization of Catalyst Inks By Rheology and Microscopic Particle Properties
Suzuki, T., Okada, S., & Tsushima, S. (2018) · ECS Transactions · doi:10.1149/08613.0193ecst · Cited by 9
Role of ionomer in membrane electrode assembly for proton exchange membrane fuel cells
Liang, X., Wu, L., & Xu, T. (2018) · Scientia Sinica Chimica · doi:10.1360/n032018-00048 · Cited by 8
Kang, J., Zheng, W., Zhou, Y., Chen, B., Chen, S., Li, B., Zhang, C., Gong, Z., & Ming, P. (2025) · Journal of Power Sources · doi:10.1016/j.jpowsour.2025.236991 · Cited by 7
Aboalhassan, A. A., Babar, A. A., Iqbal, N., Yan, J., El-Newehy, M. H., Yu, J., & Ding, B. (2024) · Polymers · doi:10.3390/polym16030327 · Cited by 7
“…the non-treated CB@CNF exhibited an interconnected fibrous structure similar to pure CNF; however, numerous agglomerates in the CNF matrix were obvious in CB@CNF (Figure 2b), which was attributed to the uncontrolled distribution of CB NPs in the polymer before the electrospinning process [29].”
Background
Metadata
- Authors
- Shukla, S., Bhattacharjee, S., Weber, A. Z., & Secanell, M.
- Affiliations
- University of Alberta (CA)
- Lawrence Berkeley National Laboratory (US)
- Venue
- Journal of The Electrochemical Society
- Publisher
- The Electrochemical Society
- Published
- 2017
- Volume
- 164
- Issue
- 6
- Pages
- F600-F609
- ISSN
- 0013-4651 (ISSN-L)
- 1945-7111
- OpenAlex
- W2604338135
- Cited by
- 137
- References
- 43
- Citations by year
- 2026: 10 · 2025: 21 · 2024: 23 · 2023: 18 · 2022: 12 · 2021: 19 · 2020: 14 · 2019: 10 · 2018: 9 · 2017: 1
- FWCI
- 3.87
- Type
- journal article
- Language
- en
- Open access
- hybrid
- doi.org
- Licence
- cc-by
- Locations
- Journal of The Electrochemical Society (publishedVersion, cc-by)
- OSTI OAI (U.S. Department of Energy Office of Scientific and Technical Information) (submittedVersion)
- eScholarship (California Digital Library) (submittedVersion)
- Funders
- Natural Science and Engineering Research Council of Canada (371088-10)
- Helmholtz-Alberta Innitiative (0)
- APC/NSERC Catalyst Research for Polymer Electrolyte Fuel Cell Network (14323)
- Canadian Foundation for Innovation (0)
- Department of Energy | EERE | Fuel Cell Technologies Program (FCT) (DE-AC02-05CH11231)
- Canadian School of Energy and Environment (0)
- Topics
- Physical Sciences › Engineering › Electrical and Electronic Engineering › Fuel Cells and Related Materials
- Physical Sciences › Energy › Renewable Energy, Sustainability and the Environment › Electrocatalysts for Energy Conversion
- Physical Sciences › Chemistry › Physical and Theoretical Chemistry › Electrostatics and Colloid Interactions
- Keywords
- proton exchange membrane fuel cells, catalyst ink, ink stability, carbon black, Nafion, particle aggregation, dispersion medium, isopropanol, dielectric constant, zeta potential, particle size, interaction energy, non-aqueous media
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.