Lithium-Ion Battery Operation, Degradation, and Aging Mechanism in Electric Vehicles: An Overview
Open accessThe DOI matches its Crossref record; 83 of the 83 references it cites were found in a registry or an index.
Abstract
Understanding the aging mechanism for lithium-ion batteries (LiBs) is crucial for optimizing the battery operation in real-life applications. This article gives a systematic description of the LiBs aging in real-life electric vehicle (EV) applications. First, the characteristics of the common EVs and the lithium-ion chemistries used in these applications are described. The battery operation in EVs is then classified into three modes: charging, standby, and driving, which are subsequently described. Finally, the aging behavior of LiBs in the actual charging, standby, and driving modes are reviewed, and the influence of different working conditions are considered. The degradation mechanisms of cathode, electrolyte, and anode during those processes are also discussed. Thus, a systematic analysis of the aging mechanisms of LiBs in real-life EV applications is achieved, providing practical guidance, methods to prolong the battery life for users, battery designers, vehicle manufacturers, and material recovery companies.
Overview
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Integrity signals
Registry
Cites
Statistics
Verification
Claims the paper makes
The claims and statistics of this paper haven’t been checked yet.
Free: it reads the open-access text and checks the first 5 claims that cite a source we can check. Create a free account to check every claim.
Self-check
Percentages, sums and reported differences re-computed from the paper’s own numbers.
The self-check needs the paper’s full text.
Citations
Cites
Noh, H.-J., Youn, S., Yoon, C. S., & Sun, Y.-K. (2013) · Journal of Power Sources · doi:10.1016/j.jpowsour.2013.01.063 · Cited by 2,302
Guidelines and trends for next-generation rechargeable lithium and lithium-ion batteries
Wu, F., Maier, J., & Yu, Y. (2020) · Chemical Society Reviews · doi:10.1039/c7cs00863e · Cited by 2,229 · cited 2×
“A brief comparative analysis of these chemistries is presented in Table 3 [30].”
BackgroundA review of lithium-ion battery safety concerns: The issues, strategies, and testing standards
Chen, Y., Kang, Y., Zhao, Y., Wang, L., Liu, J., Li, Y., Liang, Z., He, X., Li, X., Tavajohi, N., et al. (2021) · Journal of Energy Chemistry · doi:10.1016/j.jechem.2020.10.017 · Cited by 2,178
Self-citationAn, S. J., Li, J., Daniel, C., Mohanty, D., Nagpure, S., & Wood, D. L. (2016) · Carbon · doi:10.1016/j.carbon.2016.04.008 · Cited by 2,121 · cited 1×
“Because of their intrinsic properties, such as higher energy densities and low cost, Ni-based LiBs chemistries (i.e., NMC and NCA) are the preferred choices for powering”
BackgroundDegradation diagnostics for lithium ion cells
Birkl, C. R., Roberts, M. R., McTurk, E., Bruce, P. G., & Howey, D. A. (2017) · Journal of Power Sources · doi:10.1016/j.jpowsour.2016.12.011 · Cited by 1,945 · cited 1×
“The cathode structure is prone to changes during both standby, charging and driving aging [12].”
BackgroundA review on lithium-ion battery ageing mechanisms and estimations for automotive applications
Barré, A., Deguilhem, B., Grolleau, S., Gérard, M., Suard, F., & Riu, D. (2013) · Journal of Power Sources · doi:10.1016/j.jpowsour.2013.05.040 · Cited by 1,758
A review on the key issues of the lithium ion battery degradation among the whole life cycle
Han, X., Lu, L., Zheng, Y., Feng, X., Li, Z., Li, J., & Ouyang, M. (2019) · eTransportation · doi:10.1016/j.etran.2019.100005 · Cited by 1,745 · cited 1×
“Changes in the cathode, such as phase transition, cracking in particles, transition metal dissolution (TMD), CEI film formation, binder decomposition, and loss contrast with collector have an evident influence on the aging of LiBs [5,8].”
BackgroundLithium-ion battery fast charging: A review
Tomaszewska, A., Chu, Z., Feng, X., O'Kane, S., Liu, X., Chen, J., Ji, C., Endler, E., Li, R., Liu, L., et al. (2019) · eTransportation · doi:10.1016/j.etran.2019.100011 · Cited by 1,592
Self-citationClosed-loop optimization of fast-charging protocols for batteries with machine learning
Attia, P. M., Grover, A., Jin, N., Severson, K. A., Markov, T. M., Liao, Y.-H., Chen, M. H., Cheong, B., Perkins, N., Yang, Z., et al. (2020) · Nature · doi:10.1038/s41586-020-1994-5 · Cited by 1,180
Main aging mechanisms in Li ion batteries
Broussely, M., Biensan, P., Bonhomme, F., Blanchard, P., Herreyre, S., Nechev, K., & Staniewicz, R. J. (2005) · Journal of Power Sources · doi:10.1016/j.jpowsour.2005.03.172 · Cited by 1,159
Safety mechanisms in lithium-ion batteries
Balakrishnan, P. G., Ramesh, R., & Prem Kumar, T. (2006) · Journal of Power Sources · doi:10.1016/j.jpowsour.2005.12.002 · Cited by 1,132 · cited 1×
“Because of their intrinsic properties, such as higher energy densities and low cost, Ni-based LiBs chemistries (i.e., NMC and NCA) are the preferred choices for powering”
BackgroundGeneration and Evolution of the Solid Electrolyte Interphase of Lithium-Ion Batteries
Heiskanen, S. K., Kim, J., & Lucht, B. L. (2019) · Joule · doi:10.1016/j.joule.2019.08.018 · Cited by 1,036 · cited 1×
“The LiPF 6 is not stable, and it can be easily decomposed into LiF and PF 5 [82].”
BackgroundLithium Diffusion in Graphitic Carbon
Persson, K., Sethuraman, V. A., Hardwick, L. J., Hinuma, Y., Meng, Y. S., van der Ven, A., Srinivasan, V., Kostecki, R., & Ceder, G. (2010) · The Journal of Physical Chemistry Letters · doi:10.1021/jz100188d · Cited by 852 · cited 1×
“Because of their intrinsic properties, such as higher energy densities and low cost, Ni-based LiBs chemistries (i.e., NMC and NCA) are the preferred choices for powering”
BackgroundElectric Vehicles Batteries: Requirements and Challenges
Deng, J., Bae, C., Denlinger, A., & Miller, T. (2020) · Joule · doi:10.1016/j.joule.2020.01.013 · Cited by 761 · cited 1×
“Lithium-ion batteries (LiBs) with high energy density are receiving increasing attention because of their environmental friendliness and are widely used in electric vehicles (EVs) worldwide [1].”
BackgroundXiong, R., Pan, Y., Shen, W., Li, H., & Sun, F. (2020) · Renewable and Sustainable Energy Reviews · doi:10.1016/j.rser.2020.110048 · Cited by 725
Calendar Aging of Lithium-Ion Batteries: I. Impact of the Graphite Anode on Capacity Fade
Keil, P., Schuster, S. F., Wilhelm, J., Travi, J., Hauser, A., Karl, R. C., & Jossen, A. (2016) · Journal of The Electrochemical Society · doi:10.1149/2.0411609jes · Cited by 669
A review of the state of health for lithium-ion batteries: Research status and suggestions
Tian, H., Qin, P., Li, K., & Zhao, Z. (2020) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2020.120813 · Cited by 651
Dual‐Layered Film Protected Lithium Metal Anode to Enable Dendrite‐Free Lithium Deposition
Yan, C., Cheng, X., Tian, Y., Chen, X., Zhang, X., Li, W., Huang, J., & Zhang, Q. (2018) · Advanced Materials · doi:10.1002/adma.201707629 · Cited by 513 · cited 1×
“Because of their intrinsic properties, such as higher energy densities and low cost, Ni-based LiBs chemistries (i.e., NMC and NCA) are the preferred choices for powering”
BackgroundKeil, P., & Jossen, A. (2016) · Journal of Energy Storage · doi:10.1016/j.est.2016.02.005 · Cited by 477 · cited 2×
“…battery from high currents, several alternative charging protocols are proposed in the literature, which are: Multistage Constant Current (MCC) charging, Pulse Charging (PC), Constant Power Constant Voltage (CP-CV), Variable Current Profile (VCP) and Constant Current Pulsed Charging (CC-PC) [38–41].”
BackgroundElectrolyte Oxidation Pathways in Lithium-Ion Batteries
Rinkel, B. L. D., Hall, D. S., Temprano, I., & Grey, C. P. (2020) · Journal of the American Chemical Society · doi:10.1021/jacs.0c06363 · Cited by 455
Review on state-of-health of lithium-ion batteries: Characterizations, estimations and applications
Yang, S., Zhang, C., Jiang, J., Zhang, W., Zhang, L., & Wang, Y. (2021) · Journal of Cleaner Production · doi:10.1016/j.jclepro.2021.128015 · Cited by 435
Lithium Ion Battery Anode Aging Mechanisms
Agubra, V., & Fergus, J. (2013) · Materials · doi:10.3390/ma6041310 · Cited by 418 · cited 1×
“Because of their intrinsic properties, such as higher energy densities and low cost, Ni-based LiBs chemistries (i.e., NMC and NCA) are the preferred choices for powering”
BackgroundHigh‐Nickel NMA: A Cobalt‐Free Alternative to NMC and NCA Cathodes for Lithium‐Ion Batteries
Li, W., Lee, S. S. W., & Manthiram, A. (2020) · Advanced Materials · doi:10.1002/adma.202002718 · Cited by 399 · cited 1×
“Therefore, the NMC and NCA are widely used in current EV models [31].”
MethodPerformance of batteries for electric vehicles on short and longer term
Gerssen-Gondelach, S. J., & Faaij, A. P. C. (2012) · Journal of Power Sources · doi:10.1016/j.jpowsour.2012.03.085 · Cited by 359 · cited 1×
“The electric motor is used to power the vehicle for a short distance or to support the main engine (e.g., at a stoplight) [21].”
BackgroundAdvanced Liquid Electrolytes for Rechargeable Li Metal Batteries
Jie, Y., Ren, X., Cao, R., Cai, W., & Jiao, S. (2020) · Advanced Functional Materials · doi:10.1002/adfm.201910777 · Cited by 330 · cited 1×
“The CEI film, which is similar to SEI film, consists of lithium alkyl carbonates, lithium alkoxides (ROLi), Li 2 CO 3 , etc. [78].”
Nonflammable organic electrolytes for high-safety lithium-ion batteries
Deng, K., Zeng, Q., Wang, D., Liu, Z., Wang, G., Qiu, Z., Zhang, Y., Xiao, M., & Meng, Y. (2020) · Energy Storage Materials · doi:10.1016/j.ensm.2020.07.018 · Cited by 322
Quantifying electric vehicle battery degradation from driving vs. vehicle-to-grid services
Wang, D., Coignard, J., Zeng, T., Zhang, C., & Saxena, S. (2016) · Journal of Power Sources · doi:10.1016/j.jpowsour.2016.09.116 · Cited by 320 · cited 1×
“Aging during standby operation is a very slow process, and it may take more than ten years at room temperature before a battery reaches its end-of-life (EOL); however, this operation takes up to 80% of the battery operation time in EV applications [72].”
BackgroundZhu, J., Dewi Darma, M. S., Knapp, M., Sørensen, D. R., Heere, M., Fang, Q., Wang, X., Dai, H., Mereacre, L., Senyshyn, A., et al. (2020) · Journal of Power Sources · doi:10.1016/j.jpowsour.2019.227575 · Cited by 313 · cited 1×
“Furthermore, in [54], the author analyzed the contribution of the constant voltage process to the battery charging, and charged 18650-type batteries (2.5 Ah, NMC/Graphite, and NCA/Graphite) by the CC (2.5 A to 4.2 V) (Figure 8g) and CC-CV protocols (2.5 A to 4.2 V and 0.1 A cut-off current) at room…”
BackgroundInfluentialZhao, C., Zhao, Q., Liu, X., Zheng, J., Stalin, S., Zhang, Q., & Archer, L. A. (2020) · Advanced Materials · doi:10.1002/adma.201905629 · Cited by 261 · cited 1×
“The degradation of the binder will lead to the structure of the positive electrode being unstable, as a loss of contact in the electrodes results in an internal resistance rise in battery [80].”
BackgroundReview of energy storage systems for vehicles based on technology, environmental impacts, and costs
Balali, Y., & Stegen, S. (2021) · Renewable and Sustainable Energy Reviews · doi:10.1016/j.rser.2020.110185 · Cited by 260 · cited 3×
“Depending on the EV manufacture, batteries powering BEV usually have a capacity between 20 kWh and 80 kWh, which ensure a range of up to 663 km [19,20].”
BackgroundInfluentialLiu, J., Duan, Q., Ma, M., Zhao, C., Sun, J., & Wang, Q. (2020) · Journal of Power Sources · doi:10.1016/j.jpowsour.2019.227263 · Cited by 257 · cited 1×
“In [52] the author accelerated the battery aging by 300 mV overcharging.”
Backgroundde Hoog, J., Timmermans, J.-M., Ioan-Stroe, D., Swierczynski, M., Jaguemont, J., Goutam, S., Omar, N., Van Mierlo, J., & Van Den Bossche, P. (2017) · Applied Energy · doi:10.1016/j.apenergy.2017.05.018 · Cited by 254
Understanding ageing in Li-ion batteries: a chemical issue
Palacín, M. R. (2018) · Chemical Society Reviews · doi:10.1039/c7cs00889a · Cited by 240
Lithium-Ion Battery State-of-Health Estimation Using the Incremental Capacity Analysis Technique
Stroe, D.-I., & Schaltz, E. (2020) · IEEE Transactions on Industry Applications · doi:10.1109/tia.2019.2955396 · Cited by 214 · cited 1×
“However, as reported in [66], when the cells (i.e., LMO+NMC/graphite) were stored at a middle SOC (i.e., 50%), the degradation is faster than for the cells which were stored at extreme SOCs (i.e., 10% and 90%).”
BackgroundSelf-citationAlbertsen, L., Richter, J. L., Peck, P., Dalhammar, C., & Plepys, A. (2021) · Resources, Conservation and Recycling · doi:10.1016/j.resconrec.2021.105658 · Cited by 210 · cited 1×
“These cause great trouble to users and manufacturers [2].”
BackgroundWoody, M., Arbabzadeh, M., Lewis, G. M., Keoleian, G. A., & Stefanopoulou, A. (2020) · Journal of Energy Storage · doi:10.1016/j.est.2020.101231 · Cited by 209 · cited 2×
“Changes in the cathode, such as phase transition, cracking in particles, transition metal dissolution (TMD), CEI film formation, binder decomposition, and loss contrast with collector have an evident influence on the aging of LiBs [5,8].”
BackgroundPrediction of Electric Vehicle Range: A Comprehensive Review of Current Issues and Challenges
Varga, B. O., Sagoian, A., & Mariasiu, F. (2019) · Energies · doi:10.3390/en12050946 · Cited by 203 · cited 1×
“Generally, the vehicle design considers multiple factors in order to meet the needs of different consumers, including the overall dimensions, passenger capacity, tire type and shape, specific front area, and body type [46].”
BackgroundEffect of extreme temperatures on battery charging and performance of electric vehicles
Lindgren, J., & Lund, P. D. (2016) · Journal of Power Sources · doi:10.1016/j.jpowsour.2016.07.038 · Cited by 203 · cited 2×
“In contrast, at higher temperatures (>+40 °C), the charging capacity increases and the internal resistance decreases further, compared with charging at room temperature [57].”
BackgroundAlipour, M., Ziebert, C., Conte, F. V., & Kizilel, R. (2020) · Batteries · doi:10.3390/batteries6030035 · Cited by 200
Investigation of a commercial lithium-ion battery under overcharge/over-discharge failure conditions
Ouyang, D., Chen, M., Liu, J., Wei, R., Weng, J., & Wang, J. (2018) · RSC Advances · doi:10.1039/c8ra05564e · Cited by 196 · cited 1×
“Even worse, an explosion caused by overdischarge when the external temperature is high has been reported [63].”
BackgroundJafari, M., Gauchia, A., Zhao, S., Zhang, K., & Gauchia, L. (2018) · IEEE Transactions on Transportation Electrification · doi:10.1109/tte.2017.2764320 · Cited by 177 · cited 2×
“Usually, the main aging of the battery is caused by driving [47].”
BackgroundRemaining useful life prediction of lithium batteries in calendar ageing for automotive applications
Eddahech, A., Briat, O., Woirgard, E., & Vinassa, J. M. (2012) · Microelectronics Reliability · doi:10.1016/j.microrel.2012.06.085 · Cited by 165 · cited 1×
“As presented in [50], the standby time can reach 90% of the total vehicle operation.”
BackgroundLiu, K., Ashwin, T. R., Hu, X., Lucu, M., & Widanage, W. D. (2020) · Renewable and Sustainable Energy Reviews · doi:10.1016/j.rser.2020.110017 · Cited by 161
Degradation and Aging Routes of Ni-Rich Cathode Based Li-Ion Batteries
Teichert, P., Eshetu, G. G., Jahnke, H., & Figgemeier, E. (2020) · Batteries · doi:10.3390/batteries6010008 · Cited by 157
Zilberman, I., Sturm, J., & Jossen, A. (2019) · Journal of Power Sources · doi:10.1016/j.jpowsour.2019.03.109 · Cited by 156 · cited 2×
“…Higher SOC accelerates capacity fade, which Self-discharge is also an important process during calendar aging, which results in voltage decay and lower available energy. moderate temperature In [71], the authors analyzed the self-discharge dependence on the temperature and SOC in a commercial cell.”
BackgroundPellow, M. A., Ambrose, H., Mulvaney, D., Betita, R., & Shaw, S. (2020) · Sustainable Materials and Technologies · doi:10.1016/j.susmat.2019.e00120 · Cited by 152 · cited 1×
“Some scientists specifically discussed the impacts of environmental and operational factors on battery degradation [3], while others studied the battery aging mechanism through the post-mortem analysis of the internal components of the battery cell [4].”
BackgroundA Novel Electrolyte Salt Additive for Lithium‐Ion Batteries with Voltages Greater than 4.7 V
Li, Y., Wan, S., Veith, G. M., Unocic, R. R., Paranthaman, M. P., Dai, S., & Sun, X. (2017) · Advanced Energy Materials · doi:10.1002/aenm.201601397 · Cited by 151 · cited 1×
“The cycle stability, capacity, safety, and operating condition of LiBs are dependent on the electrolyte [81].”
BackgroundSelf-citationElectrical behavior of overdischarge-induced internal short circuit in lithium-ion cells
Lai, X., Zheng, Y., Zhou, L., & Gao, W. (2018) · Electrochimica Acta · doi:10.1016/j.electacta.2018.05.048 · Cited by 149 · cited 1×
“As presented by Lai et al. in [62], the critical over-discharging range for the DOD is from 115% to 120%.”
BackgroundA Review on Plug-in Electric Vehicles: Introduction, Current Status, and Load Modeling Techniques
Ahmadian, A., Mohammadi-Ivatloo, B., & Elkamel, A. (2020) · Journal of Modern Power Systems and Clean Energy · doi:10.35833/mpce.2018.000802 · Cited by 149 · cited 1×
“4 of 23 The most popular EVs in the market, classified according to their type, are summarized in Table 2 [19,23,24].”
BackgroundFedorov, R. G., Maletti, S., Heubner, C., Michaelis, A., & Ein‐Eli, Y. (2021) · Advanced Energy Materials · doi:10.1002/aenm.202101173 · Cited by 141
A Review of Pulsed Current Technique for Lithium-ion Batteries
Huang, X., Li, Y., Acharya, A. B., Sui, X., Meng, J., Teodorescu, R., & Stroe, D. (2020) · Energies · doi:10.3390/en13102458 · Cited by 130 · cited 2×
“…battery from high currents, several alternative charging protocols are proposed in the literature, which are: Multistage Constant Current (MCC) charging, Pulse Charging (PC), Constant Power Constant Voltage (CP-CV), Variable Current Profile (VCP) and Constant Current Pulsed Charging (CC-PC) [38–41].”
BackgroundSelf-citationThe suppression of lithium dendrite growth in lithium sulfur batteries: A review
Xu, X., Wang, S., Wang, H., Xu, B., Hu, C., Jin, Y., Liu, J., & Yan, H. (2017) · Journal of Energy Storage · doi:10.1016/j.est.2017.07.031 · Cited by 125 · cited 1×
“Because of their intrinsic properties, such as higher energy densities and low cost, Ni-based LiBs chemistries (i.e., NMC and NCA) are the preferred choices for powering”
BackgroundOptimum fast charging of lithium-ion pouch cells based on local volume expansion criteria
Spingler, F. B., Wittmann, W., Sturm, J., Rieger, B., & Jossen, A. (2018) · Journal of Power Sources · doi:10.1016/j.jpowsour.2018.04.095 · Cited by 122
Swierczynski, M., Stroe, D.-I., Stan, A.-I., Teodorescu, R., & Kaer, S. K. (2015) · IEEE Transactions on Industry Applications · doi:10.1109/tia.2015.2405500 · Cited by 121
Self-citationComparison of the capacity fade of Sony US 18650 cells charged with different protocols
Sikha, G., Ramadass, P., Haran, B. S., White, R. E., & Popov, B. N. (2003) · Journal of Power Sources · doi:10.1016/s0378-7753(03)00027-2 · Cited by 110
Mathieu, R., Briat, O., Gyan, P., & Vinassa, J.-M. (2020) · Applied Energy · doi:10.1016/j.apenergy.2020.116344 · Cited by 110 · cited 2×
“In contrast, in [53], Rathieu et al. charged two different types of batteries with a slight reduction of 100 mV in the cut-off voltage, as shown in Figure 8d.”
BackgroundResultElectric vehicles: solution or new problem?
Ajanović, A., & Haas, R. (2018) · Environment Development and Sustainability · doi:10.1007/s10668-018-0190-3 · Cited by 97 · cited 1×
“The size of the battery capacity for PHEV applications is usually between 4.5 kWh and 10 kWh [22].”
BackgroundInfluentialWang, C., Yu, L., Fan, W., Liu, J., Ouyang, L., Yang, L., & Zhu, M. H. (2018) · ACS Applied Energy Materials · doi:10.1021/acsaem.8b00342 · Cited by 94
The Degradation Behavior of LiFePO4/C Batteries during Long-Term Calendar Aging
Sui, X., Swierczynski, M. J., Teodorescu, R., & Stroe, D. (2021) · Energies · doi:10.3390/en14061732 · Cited by 93 · cited 1×
“There are many types of LiBs with wide application prospects, such as spinel LMO/LNMO cathode [26], olivine LFP cathode [27,28], and layered NMC/NCA [29].”
BackgroundSelf-citationKeil, P., & Jossen, A. (2017) · Journal of The Electrochemical Society · doi:10.1149/2.0801713jes · Cited by 91
Schultz, C., Vedder, S., Streipert, B., Winter, M., & Nowak, S. (2017) · RSC Advances · doi:10.1039/c7ra03839a · Cited by 81
Hosen, M. S., Karimi, D., Kalogiannis, T., Pirooz, A., Jaguemont, J., Berecibar, M., & Mierlo, J. V. (2020) · Journal of Energy Storage · doi:10.1016/j.est.2020.101265 · Cited by 71
Effect of the different charging techniques on battery life-time: Review
Serhan, H. A., & Ahmed, E. M. (2018) · doi:10.1109/itce.2018.8316661 · Cited by 65
Understanding self-discharge mechanism of layered nickel cobalt manganese oxide at high potential
Liao, X., Huang, Q., Mai, S., Wang, X., Xu, M., Xing, L., Liao, Y., & Li, W. (2015) · Journal of Power Sources · doi:10.1016/j.jpowsour.2015.04.032 · Cited by 65 · cited 1×
“Because of their intrinsic properties, such as higher energy densities and low cost, Ni-based LiBs chemistries (i.e., NMC and NCA) are the preferred choices for powering”
BackgroundState of Charge Estimation for Lithium-Ion Battery with a Temperature-Compensated Model
Yang, S., Deng, C. L., Zhang, Y., & He, Y. (2017) · Energies · doi:10.3390/en10101560 · Cited by 64 · cited 2×
“Low temperatures (e.g., 0–25 ◦ C) and a low SOC can effectively slow down the battery aging in standby [73].”
BackgroundZhang, B., Xu, Y., Wang, J., Lin, J., Wang, C., & Chen, Y. (2019) · Electrochimica Acta · doi:10.1016/j.electacta.2019.134686 · Cited by 55
Ouyang, D., Weng, J., Chen, M., Liu, J., & Wang, J. (2019) · International Journal of Energy Research · doi:10.1002/er.4898 · Cited by 54 · cited 1×
“In [61], the author found that overdischarging deteriorates the electrode materials.”
BackgroundHemmelmann, H., Dinter, J. K., & Elm, M. T. (2021) · Advanced Materials Interfaces · doi:10.1002/admi.202002074 · Cited by 54
Simolka, M., Heger, J., Käß, H., Biswas, I., & Friedrich, K. A. (2020) · Journal of Applied Electrochemistry · doi:10.1007/s10800-020-01465-6 · Cited by 53
Hekmatfar, M., Hasa, I., Eghbal, R., Carvalho, D. V., Moretti, A., & Passerini, S. (2019) · Advanced Materials Interfaces · doi:10.1002/admi.201901500 · Cited by 52
Bank, T., Feldmann, J., Klamor, S., Bihn, S., & Sauer, D. U. (2020) · Journal of Power Sources · doi:10.1016/j.jpowsour.2020.228566 · Cited by 51 · cited 1×
“In [65], the authors varied the storage SOC from 5% to 95%, and obtained a similar conclusion that a higher SOC (i.e., over 70”
ResultAccelerated aging of Lithium-ion batteries based on electric vehicle mission profile
Stroe, D., Swierczynski, M. J., Kær, S. K., Martinez-Laserna, E., & Sarasketa-Zabala, E. (2017) · IEEE Energy Conversion Congress and Exposition (ECCE) · doi:10.1109/ecce.2017.8096937 · Cited by 48
Self-citationZhu, J., Cao, G., Li, Y., Wang, S., Deng, S., Guo, J., Chen, Y., Lei, T., Zhang, J., & Chang, S. (2019) · Electrochimica Acta · doi:10.1016/j.electacta.2019.134889 · Cited by 44
Self-citationLi, S.-D., Zhao, Y., Wang, C., & Gao, K. (2016) · Cited by 41
Study of aging mechanisms in lithium-ion batteries for working vehicle applications
Mocera, F., Somà, A., & Clerici, D. (2020) · International Conference on Ecological Vehicles and Renewable Energies (EVER) · doi:10.1109/ever48776.2020.9243079 · Cited by 33
Ben-Marzouk, M., Pélissier, S., Clerc, G., Sarı, A., & Venet, P. (2021) · IEEE Transactions on Vehicular Technology · doi:10.1109/tvt.2021.3077671 · Cited by 32
Post-Mortem Analysis of Lithium-Ion Capacitors after Accelerated Aging Tests
Ghossein, N. E., Sarı, A., Venet, P., Géniès, S., & Azaïs, P. (2020) · Journal of Energy Storage · doi:10.1016/j.est.2020.102039 · Cited by 31 · cited 1×
“Some scientists specifically discussed the impacts of environmental and operational factors on battery degradation [3], while others studied the battery aging mechanism through the post-mortem analysis of the internal components of the battery cell [4].”
BackgroundWang, S., Li, Y., Liu, S., Deng, S., Chen, Y., Zhu, J., Zhang, J., Guo, J., & Chang, S. (2020) · Journal of The Electrochemical Society · doi:10.1149/1945-7111/ab7879 · Cited by 29
Self-citationGerelt-Od, B., Kim, J., Shin, E., Kang, H., Kim, N., Jo, C., Son, H., & Yoon, S. (2021) · Journal of Industrial and Engineering Chemistry · doi:10.1016/j.jiec.2021.01.039 · Cited by 28 · cited 1×
“In [88], Gerelt-Od In [88], Gerelt-Od et al. investigated the overcharging of battery cells from 4.2 to 4.4 V in moderate temperatures of 35–45 °C, which are the normal operating conditions in real life.”
BackgroundInfluentialBen-Marzouk, M., Chaumond, A., Redondo-Iglesias, E., Montaru, M., & Pélissier, S. (2016) · World Electric Vehicle Journal · doi:10.3390/wevj8020388 · Cited by 28
Paul, T., Mesbahi, T., Durand, S., Flieller, D., & Uhring, W. (2019) · IEEE Vehicle Power and Propulsion Conference (VPPC) · doi:10.1109/vppc46532.2019.8952494 · Cited by 22
Horsthemke, F., Leißing, M., Winkler, V., Friesen, A., Ibing, L., Winter, M., & Nowak, S. (2020) · Electrochimica Acta · doi:10.1016/j.electacta.2020.135894 · Cited by 19 · cited 1×
“From From the electrochemical reaction at the charged anode, these products will then form a surface film on the anode, known as SEI film [83]. the electro-chemical reaction at the charged anode, these products will then form a surface film on the anode, known as SEI film [83].”
BackgroundThe Aging Law of Low Temperature Charging of Lithium-Ion Battery
You, H., Dai, H., & Li, L. (2019) · SAE technical papers on CD-ROM/SAE technical paper series · doi:10.4271/2019-01-1204 · Cited by 13 · cited 1×
“In [56], the authors assessed the battery (i.e., NCA/graphite, 2.9 Ah) charging in different low temperatures (i.e., − 5 ◦ C, − 10 ◦ C, − 15 ◦ C and − 20 ◦ C).”
Influential
Cited by
Muzammal Islam, M., Yu, T., Giannoccaro, G., Mi, Y., la Scala, M., Rajabi Nasab, M., & Wang, J. (2024) · IEEE Access · doi:10.1109/access.2024.3476959 · Cited by 224
“Similarly, [170] addressed Li-ion battery degradation and aging mechanisms in EVs.”
BackgroundRahman, T., & Alharbi, T. (2024) · Batteries · doi:10.3390/batteries10070220 · Cited by 200
“Authors have claimed that the degradation mechanism of lithium-ion batteries affected anode, cathode and other battery structures, which are influenced by some external factors such as temperature.”
BackgroundChallenges and opportunities toward long-life lithium-ion batteries
Xu, X., Han, X., Lu, L., Wang, F., Yang, M., Liu, X., Wu, Y., Tang, S., Hou, Y., Hou, J., et al. (2024) · Journal of Power Sources · doi:10.1016/j.jpowsour.2024.234445 · Cited by 195
Senol, M., Bayram, I. S., Naderi, Y., & Galloway, S. (2023) · IEEE Access · doi:10.1109/access.2023.3268615 · Cited by 110
Xiong, R., He, Y., Sun, Y., Jia, Y., & Shen, W. (2025) · Journal of Energy Chemistry · doi:10.1016/j.jechem.2025.01.019 · Cited by 52
Metadata
- Authors
- Guo, J., Li, Y., Pedersen, K., & Stroe, D.-I.
- Venue
- Energies
- Publisher
- MDPI AG
- Published
- 2021-08-24
- Volume
- 14
- Issue
- 17
- Pages
- 5220
- ISSN
- 1996-1073 (ISSN-L)
- OpenAlex
- W3194373144
- Cited by
- 166
- References
- 83
- FWCI
- 6.09
- Type
- journal article
- Language
- en
- Open access
- gold
About these checks
Registry, retraction, Cites and statistics results are computed, not judged, with one exception: a printed reference that no index lists is read once by a model before it counts as a citation error. Claims are extracted by a model and kept only when their quote appears verbatim in the text; each cited source is then checked, with a model’s help, for whether it says what the claim relies on. Those verdicts can be wrong — read the claim’s quote and the cited source before relying on one.
Statistics and arithmetic are recomputed, not judged.
Confidence bands are shown only for fields calibrated on our annotated test set. None is calibrated yet, so no band is shown.
What counts as a claim ›How we measure confidence ›How we check this ›
Are you an author, or do you see a problem with this page? Request a review
Data sources
Bibliographic data: Semantic Scholar, OpenAlex, Crossref.
Contains information from the Semantic Scholar Academic Graph Datasets, made available under the ODC Attribution License (ODC-BY 1.0).
Semantic Scholar’s data is described in: Kinney, R., et al. (2023). The Semantic Scholar Open Data Platform. arXiv:2301.10140.